我国船舶铸锻业的现状、存在的问题和建议
1
作者 李基棠 《船舶物资与市场》 2001年第5期33-35,共3页
一、现状 改革开放以来,随着船舶柴油机的发展,我国船舶铸锻业也取得了可喜的成就,不少单位经过技术改造,设备更新,技术攻关和技术引进,船舶铸锻有了较大发展和提高,目前已具备了相当大的生产规模和生产能力,为船舶、柴油机、辅机、修... 一、现状 改革开放以来,随着船舶柴油机的发展,我国船舶铸锻业也取得了可喜的成就,不少单位经过技术改造,设备更新,技术攻关和技术引进,船舶铸锻有了较大发展和提高,目前已具备了相当大的生产规模和生产能力,为船舶、柴油机、辅机、修造船、仪器仪表等提供了大量的铸锻件. 展开更多
关键词 中国 船舶铸锻业 科学管理 政策
下载PDF
铸锻业的结构调整与规模经济—探索专业铸锻厂点走出困境之路
2
作者 黄志翔 赵建平 《中国特区机电》 1991年第5期13-16,共4页
关键词 铸锻业 铸锻 结构调整 规模经济
下载PDF
Mechanical characterization of cp-Ti produced by investment casting
3
作者 Khaled M.IBRAHIM Mansour MHAEDE Lothar WAGNER 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第8期1735-1740,共6页
The influence of hot swaging(SW) and annealing treatment on microstructure and mechanical properties of commercially pure titanium produced by investment casting was evaluated.The as-cast samples showed a typical mi... The influence of hot swaging(SW) and annealing treatment on microstructure and mechanical properties of commercially pure titanium produced by investment casting was evaluated.The as-cast samples showed a typical microstructure consisting of a variety of α-morphologies,while the hot swaged samples exhibited a kinked lamellar microstructure.Annealing at 500 °C did not significantly change this microstructure while annealing at 700 and 870 °C led to recrystallization and formation of equiaxed microstructures.The cast bars exhibited a typical hard α-layer in near-surface regions with a maximum depth and maximum hardness of 720 μm and HV0.5 660,respectively.Due to SW,the tensile strength of the as-cast material drastically increased from 605 MPa to 895 MPa.Annealing at 500 °C decreased the tensile strength slightly from 895 to 865 MPa while annealing at 700 °C led to a further pronounced drop in tensile strength from 865 to 710 MPa.No additional decrease in tensile strength was noticed with increasing the annealing temperature from 700 to 870 °C.The true fracture strain of the as-cast and hot swaged samples was in the range of 0.05 to 0.12,while the annealed samples showed values in the range of 0.25 to 0.53.In addition,the as-cast and hot swaged samples revealed a brittle cleavage fracture surfaces.However,the annealed samples showed a transgranular ductile fracture with formation of dimples. 展开更多
关键词 pure titanium investment casting SWAGING thermo-mechanical processing mechanical properties