用离心 SHS 法制造钢管陶瓷内衬的工艺研究
1
作者 沈巧玲 眭润舟 《华东船舶工业学院学报》 1997年第3期43-49,共7页
用离心自蔓延高温合成(SHS)法制造钢管陶瓷内衬,并初探了内衬构造以及离心力、添加剂Al2O3、SiO2对陶瓷内衬显微组织的影响,测定了陶瓷层的硬度,对比了陶瓷层与淬火硬化态45#钢试样的抗磨损性能。
关键词 防腐 陶瓷内衬 钢管 离心SHS法 制造 陶瓷层硬度
下载PDF
Preparation and properties of flame-sprayed Mo-FeB-Fe cermet coatings 被引量:8
2
作者 马壮 王伟 +3 位作者 邹积峰 董世知 张连勇 李智超 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第6期1314-1321,共8页
The powders of Mo2FeB2 cermet were prepared with Mo powders, Fe-B alloy powders and Fe powders as raw materials. Mo2FeB2 cermet coatings were prepared on Q235 steel by reactive thermal spraying (RTS) method and heat... The powders of Mo2FeB2 cermet were prepared with Mo powders, Fe-B alloy powders and Fe powders as raw materials. Mo2FeB2 cermet coatings were prepared on Q235 steel by reactive thermal spraying (RTS) method and heated at 1 000 ℃ in vacuum oven of 1 kPa for 5 h. The properties of coatings were investigated. The results indicate that Fe2B appears after milling for 15 h in the powder at room temperature, a part of ternary borides (Mo2FeB2) are generated in powder sintered at 900 ℃. The coatings are composed of the major phases Mo2FeB2 and a-Fe, a little of Fe203, FeO and some pores. The bonding strength between the substrate and the ceramic coating is 32.73 MPa, the thermal-shock times is about 43 and the wear resistance is enhanced by approximately 5.28 times compared with that of the substrate, respectively. The comprehensive properties of Mo2FeB2 cermet coatings can be imoroved further after vacuum heat-treatment at 1 000 ℃ for 5 h. 展开更多
关键词 Mo2FeB2 cermet coating reactive thermal spraying HARDNESS thermal shock resistance wear resistance
下载PDF