Synthesis of super absorbent resin was studied by using graft copolymerization of cornstarch and acrlyic acid.The effects of various factors including that the initiator and its concentration,monomer concentration,rea...Synthesis of super absorbent resin was studied by using graft copolymerization of cornstarch and acrlyic acid.The effects of various factors including that the initiator and its concentration,monomer concentration,reaction temperature,pH valuse,reaction time and cornstarch gelatimzed on resin absorbing water ratio was investigated,respectively.The optimal technological condition waas obtained via the comparative analysis.Under the optimal technological condition,the resin absorbing water ratio may reached 880g*g-1.展开更多
文摘Synthesis of super absorbent resin was studied by using graft copolymerization of cornstarch and acrlyic acid.The effects of various factors including that the initiator and its concentration,monomer concentration,reaction temperature,pH valuse,reaction time and cornstarch gelatimzed on resin absorbing water ratio was investigated,respectively.The optimal technological condition waas obtained via the comparative analysis.Under the optimal technological condition,the resin absorbing water ratio may reached 880g*g-1.