联醇催化剂还原技术的发展
1
作者 颜鑫 《中氮肥》 2012年第3期1-3,7,共4页
论述了联醇催化剂升温还原的基本原理,对还原理论出水量和实际出水量进行了计算,重点介绍了2种还原方法——低氢还原法和高氢还原法的操作注意事项及特点。低氢还原法注重催化剂的还原质量,高氢还原法注重催化剂的还原效率,2者各有特点... 论述了联醇催化剂升温还原的基本原理,对还原理论出水量和实际出水量进行了计算,重点介绍了2种还原方法——低氢还原法和高氢还原法的操作注意事项及特点。低氢还原法注重催化剂的还原质量,高氢还原法注重催化剂的还原效率,2者各有特点,联醇生产企业可选择性加以采用。 展开更多
关键词 联醇催化剂 还原技术 理论出水量 实际出水量 还原法 高氢还原法
下载PDF
Preparation and properties of Ni-coated WC powder and highly impact resistant and corrosion resistant WC-Ni cemented carbides 被引量:5
2
作者 Fan-lu MIN Song-bai YU +4 位作者 Sheng WANG Zhan-hu YAO Jacques Guillaume NOUDEM Si-jin LIU Jian-feng ZHANG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第6期1935-1947,共13页
WC powders were uniformly coated by Ni nanoparticles through a combined chemical co-precipitation and subsequent high temperature hydrogen reduction strategy(abbreviated as CM-WCN),and then were consolidated by vacuum... WC powders were uniformly coated by Ni nanoparticles through a combined chemical co-precipitation and subsequent high temperature hydrogen reduction strategy(abbreviated as CM-WCN),and then were consolidated by vacuum sintering at 1450°C for 1 h to obtain WC−Ni cemented carbides.The microstructure and properties of the as-consolidated CM-WCN were investigated.The average grain size of WC in the consolidated CM-WCN was calculated to be in the range of 3.0−3.8μm and only few pores were observed.A relative density of 99.6%,hardness of HRA 86.5 and bending strength of 1860 MPa were obtained for the CM-WCN−10wt.%Ni,and the highest impact toughness of 6.17 J/cm^(2 )was obtained for the CM-WCN−12wt.%Ni,surpassing those of the hand mixed WC−Ni(HM-WCN)cemented carbides examined in this study and the other similar materials in the literature.CM-WCN cemented carbides possess excellent mechanical properties,due to their highly uniform structure and low porosity that could be ascribed to the intergranular-dominated fracture mode accompanied by a large number of plastic deformation tears of the bonding phase.In addition,the corrosion resistance of CM-WCN was superior to that of HM-WCN at the Ni content of 6−12 wt.%. 展开更多
关键词 WC−Ni cemented carbides chemical co-precipitation method high temperature hydrogen reduction strategy Ni content microstructure impact toughness corrosion resistance
下载PDF