作者 杜新宇 《轻合金加工技术》 CAS 北大核心 2015年第5期25-29,共5页
为提高火焰熔铝炉的热效率,分析了目前常用熔铝炉型的工作原理及结构,找出各自的优缺点,指出火焰熔铝炉充分利用高温炉气是提高热效率的主要方法。针对现有火焰炉加热时局部温度过高、传热受限的弊端,设计了可上下调节、左右摆动的高速... 为提高火焰熔铝炉的热效率,分析了目前常用熔铝炉型的工作原理及结构,找出各自的优缺点,指出火焰熔铝炉充分利用高温炉气是提高热效率的主要方法。针对现有火焰炉加热时局部温度过高、传热受限的弊端,设计了可上下调节、左右摆动的高速烧嘴。运用对流传热的牛顿定律,设计了适用于重熔铝锭及废料的加热与预热同时进行的双层膛火焰炉,增加了高温气流与炉料的接触面积,强化了对流传热的作用。新型熔铝炉充分利用了余热预热炉料和助燃空气,使熔铝炉的热效率提高到55%以上。 展开更多
关键词 高温炉气 热效率 对流传热 高速烧嘴 预热膛
下载PDF
High Temperature Corrosion of Water Wall Materials T23 and T24 in Simulated Furnace Atmospheres 被引量:8
2
作者 赵钦新 张知翔 +2 位作者 成丁南 王云刚 邓翔 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2012年第4期814-822,共9页
Candidate materials for water wall of supercritical and ultra-supercritical utility boilers,T23 and T24,were chosen as the experimental samples and exposed to oxidizing atmosphere,reducing atmosphere and oxidizing/red... Candidate materials for water wall of supercritical and ultra-supercritical utility boilers,T23 and T24,were chosen as the experimental samples and exposed to oxidizing atmosphere,reducing atmosphere and oxidizing/reducing alternating atmosphere separately.The corrosion temperature was 450-550?C.The effects of oxygen con-tent and temperature on the corrosion in reducing atmosphere and alternating atmosphere were investigated.The scanning electron microscope(SEM) and energy dispersive spectrometer(EDS) were used to examine the corroded samples.The results show that the corrosion kinetics of T23 and T24 can be described by the double logarithmic equation and parabolic equation respectively.To describe the corrosion of materials accurately it is not sufficient to analyze the macro-mass gain and the macro-thickness of the corroded layer only,but the EDS should be applied to examine the migration depth of corrosive elements O and S.It is revealed that the corrosion becomes more severe when H2S is present in the corrosive gas.S is more active than O,and Cr can reduce the migration of oxygen but not S.The combination corrosion of S and O and pure [S] has a stronger corrodibility than pure H2S.T24 suffers the most severe corrosion at oxygen content of 0.8%.Corrosion is aggravated when the corrosion temperature is above 450 ℃ in the alternating atmosphere.T23 has better corrosion resistance than T24 and W contributes a lot to the corrosion resistance of T23. 展开更多
关键词 stainless steel mass gain element migration high temperature corrosion