通过H2程序升温脱附实验,在H2还原的Ni/La2O3/-αAl2O3催化剂上可以明显观察到高温脱附氢(高温氢).动力学实验结果表明,随催化剂上高温氢含量的增加,CH4/CO2重整反应的初始活性升高,同时高温氢也可在重整反应过程中原位生成,并使重整反... 通过H2程序升温脱附实验,在H2还原的Ni/La2O3/-αAl2O3催化剂上可以明显观察到高温脱附氢(高温氢).动力学实验结果表明,随催化剂上高温氢含量的增加,CH4/CO2重整反应的初始活性升高,同时高温氢也可在重整反应过程中原位生成,并使重整反应的活性最终达到稳定.脉冲实验结果表明,随催化剂上高温氢含量的增加,CH4解离后生成的活性中间体CHx物种的x值也增大,进而降低了CHx与CO2反应的活化能,提高了CHx与CO2反应的速率.La2O3助剂的添加提高了Ni/La2O3/-αAl2O3催化剂上逆水气变换反应的速率,并且对CO2的活化也有促进作用.La2O3助剂的加入对于CH4/CO2重整反应的重要作用是使高温氢的数量增多且稳定性提高,有利于保持CHx物种中较高的x值,促进重整反应. 展开更多
关键词 高温 镍基催化剂 氧化镧 甲烷重整反应 初始速率
下载PDF
Effect of cobalt loading on reducibility, dispersion and crystallite size of Co/Al_2O_3 Fischer-Tropsch catalyst 被引量:1
2
作者 熊海峰 张煜华 +1 位作者 李金林 古映莹 《Journal of Central South University of Technology》 2004年第4期414-418,共5页
Co/Al2O3 Fischer-Tropsch synthesis catalysts with different cobalt loadings were prepared using incipient wetness impregnation method. The effects of cobalt loading on the properties of catalysts were studied by means... Co/Al2O3 Fischer-Tropsch synthesis catalysts with different cobalt loadings were prepared using incipient wetness impregnation method. The effects of cobalt loading on the properties of catalysts were studied by means of X-ray diffraction (XRD), temperature programmed reduction (TPR), hydrogen temperature programmed desorption (H2-TPD) and O2 titration. Co-support compound formation can be detected in catalyst system by XRD. For the Co/Al2O3 catalysts with low cobalt loading, CoAl2O4 phase appears visibly. Two different reduction regions can be presented for Co/Al2O3 catalysts, which belong to Co3O4 crystallites (reduction at 320 ℃) and cobalt oxide-alumina interaction species (reduction at above 400 ℃). Increasing Co loading results in the increase of Co3O4 crystallite size. The reduced Co/Al2O3 catalysts have two adsorption sites, and cobalt loading greatly influences the adsorption behavior. With the increase of cobalt loading, the amount of low temperature adsorption is increased, the amount of high temperature adsorption is decreased, and the percentage reduction and cobalt crystallite size are increased. 展开更多