期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
Al_(7.8)Co_(20.6)Cr_(12.2)Fe_(11.5)Ni_(40.7)Ti_(7.2)高熵超合金的摩擦磨损行为研究
1
作者 李光俊 段宏 +3 位作者 徐磊 阚琛 刘忠亮 高晓东 《中国机械工程》 EI CAS CSCD 北大核心 2023年第13期1568-1575,共8页
使用真空非自耗电弧熔炼技术制备了Al_(7.8)Co_(20.6)Cr_(12.2)Fe_(11.5)Ni_(40.7)Ti_(7.2)高熵超合金,表征了该合金的显微结构和力学性能,考察了该合金在硝酸介质和高温环境中的摩擦磨损性能。结果表明:该高熵超合金的显微组织以树枝... 使用真空非自耗电弧熔炼技术制备了Al_(7.8)Co_(20.6)Cr_(12.2)Fe_(11.5)Ni_(40.7)Ti_(7.2)高熵超合金,表征了该合金的显微结构和力学性能,考察了该合金在硝酸介质和高温环境中的摩擦磨损性能。结果表明:该高熵超合金的显微组织以树枝晶为主,其维氏硬度、屈服强度、抗压强度和断裂韧性分别为422±8 HV0.2、991±32 MPa、2121±197 MPa和49.5±0.1 MPa·m 0.5。在硝酸介质中,该高熵超合金的抗腐蚀性能优于0Cr17Ni7Al不锈钢,在硝酸介质中的摩擦因数和磨损率均低于干摩擦状态,主要是因为磨损表面氧化物的生成降低了摩擦因数并提高了抗磨损性能。在高温环境中,温度对其摩擦因数有显著的影响;随着温度的升高,摩擦因数和磨损率均呈下降趋势。不同温度下磨损表面的氧含量具有显著的差异,温度越高,其氧含量越高。 展开更多
关键词 高熵超合金 腐蚀磨损 温磨损 力学性能 硝酸腐蚀
下载PDF
Comparative study on dry sliding wear and oxidation performance of HVOF and laser re-melted Al_(0.2)CrFeNi(Co,Cu)alloys 被引量:5
2
作者 Azmi ERDOGAN Kadir Mert DOLEKER 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2021年第8期2428-2441,共14页
Al_(0.2) CrFeNiCo and Al_(0.2) CrFeNiCu high entropy alloys were deposited with high velocity oxygen fuel(HVOF)on 316 L substrate.Later,a laser re-melting(LR)process was applied to enhancing the coating microstructure... Al_(0.2) CrFeNiCo and Al_(0.2) CrFeNiCu high entropy alloys were deposited with high velocity oxygen fuel(HVOF)on 316 L substrate.Later,a laser re-melting(LR)process was applied to enhancing the coating microstructure.LR process effects on dry sliding wear and oxidation behaviors were investigated.The mixture of powders with free elements led to the formation of inner oxides in HVOF coatings.The oxide and porosity were eliminated using LR.After LR,FCC was the dominant phase in both alloys,while BCC,sigma and Cr2 O3 phases were observed in Al_(0.2) CrFeNiCo alloy.The hardnesses of the Al_(0.2) CrFeNiCo and Al_(0.2) CrFeNiCu coatings after HVOF were HV 591 and HV 361,respectively.After LR,the hardnesses decreased to HV 259 and HV 270,respectively.Although HVOF coatings were most affected by increased load,they showed the highest wear resistance compared to other samples.The lowest wear resistance could be seen in the substrate.After the oxidation tests,HVOF coating layer was completely oxidized and also,the coating layer was delaminated from the substrate after 50 h oxidation due to its porous structure.LR coatings exhibited better oxidation performance.Al_(0.2) CrFeNiCo was dominantly composed of Cr2 O3,exhibiting a slower-growing tendency at the end of the oxidation tests,while Al_(0.2) CrFeNiCu was composed of spinel phases. 展开更多
关键词 high entropy alloy laser re-melting HVOF WEAR OXIDATION
下载PDF
上一页 1 下一页 到第