Work Hardening Behavior of 1020 Steel During Cold-Beating Simulation 被引量:2
1
作者 Fengkui CUI Yuanfei LING +3 位作者 Jinxue XUE Jia LIU Yuhui LIU Yan LI 《Chinese Journal of Mechanical Engineering》 SCIE EI CAS CSCD 2017年第2期321-331,共11页
The present research of cold-beating formation mainly focused on roller design and manufacture, kinematics, constitutive relation, metal flow law, thermo-mechanical coupling, surface micro-topography and microstructur... The present research of cold-beating formation mainly focused on roller design and manufacture, kinematics, constitutive relation, metal flow law, thermo-mechanical coupling, surface micro-topography and microstructure evolution. However, the research on surface quality and performance of workpieces in the process of cold-beating is rare. Cold-beating simulation experiment of 1020 steel is conducted at room temperature and strain rates ranging from 2000 to 4000 s^-1 base on the law of plastic forming. According to the experimental data, the model of strain hardening of 1020 steel is established, Scanning Electron Microscopy(SEM) is conducted, the mechanism of the work hardening of 1020 steel is clarified by analyzing microstructure variation of 1020 steel. It is found that the strain rate hardening effect of 1020 steel is stronger than the softening effect induced by increasing temperatures, the process of simulation cold-beating cause the grain shape of 1020 steel significant change and microstructure elongate significantly to form a fibrous tis- sue parallel to the direction of deformation, the higher strain rate, the more obvious grain refinement and the more hardening effect. Additionally, the change law of the work hardening rate is investigated, the relationship between dislocation density and strain, the relationship between work hardening rate and dislocation density is obtained. Results show that the change trend of the work hardening rate of 1020 steel is divided into two stages, the work hardening rate decreases dramatically in the first stage and slowly decreases in the second stage, finally tending toward zero. Dislocation density increases with increasing strain and strain rate, work hardening rate decreases with increasing dislocation density. The research results provide the basis for solving the problem of improving the surface quality and performance of workpieces under cold-beating formation of 1020 steel. 展开更多
关键词 1020 steel Cold·beating Work hardening Grain Dislocation density
下载PDF
20钢动态力学性能及本构模型的建立 被引量:8
2
作者 薛进学 凌远非 +3 位作者 崔凤奎 韩坤鹏 解克各 王宇 《河南理工大学学报(自然科学版)》 CAS 北大核心 2016年第6期841-847,共7页
为研究20钢大应变高速冷滚打成形的流动规律,进行20钢常温准静态压缩实验和应变率为2 000 - 4 000 s^-1、温度为100 - 400℃时的动态压缩实验,分析动态力学性能和应变率及温度对流动应力的影响,建立2 0 钢JC 模型.并依据实验数据进行JC... 为研究20钢大应变高速冷滚打成形的流动规律,进行20钢常温准静态压缩实验和应变率为2 000 - 4 000 s^-1、温度为100 - 400℃时的动态压缩实验,分析动态力学性能和应变率及温度对流动应力的影响,建立2 0 钢JC 模型.并依据实验数据进行JC 模型的修正.运用标准的统计参数方法,进行修正JC 模型、标准JC 模型及实验结果的对比分析.结果表明,修正的JC 模型更能准确地描述2 0 钢流动应力与应变,应变率和温度的关系. 展开更多
关键词 20钢 动态力学性能 流动应力 本构模型
下载PDF
带法兰厚壁锥体的爆炸成形研究
3
作者 胡八一 刘大敏 +1 位作者 韩长生 李华 《兵器材料科学与工程》 CAS CSCD 北大核心 1997年第5期27-31,共5页
用水作能量传输介质,采用有模自然排气成形法,对直径为506mm,厚度为14mm、12mm、10mm、8mm的LY12铝板和厚度为5.6mm、4.5mm、3.0mm的20号钢板进行了爆炸拉深成形,成形锥体锥底直径400... 用水作能量传输介质,采用有模自然排气成形法,对直径为506mm,厚度为14mm、12mm、10mm、8mm的LY12铝板和厚度为5.6mm、4.5mm、3.0mm的20号钢板进行了爆炸拉深成形,成形锥体锥底直径400mm,法兰外径480mm,最大挠度126mm。实验得到了这两种金属板料的成形工艺参数,结果表明完全退火能极大改善LY12铝的成形性能。 展开更多
关键词 爆炸成形 LY12铝 20号钢