Transformation Behavior and Microstructure in a 40Cr_2Ni_2MoV Cast Steel
1
作者 ChengLiu ZhenboZhao +1 位作者 Sanjiwan.D.Bhole DerekO.Northwood 《材料热处理学报》 EI CAS CSCD 北大核心 2004年第5期186-190,共5页
The transformation behavior of a 40Cr2Ni2MoV cast steel manufactured by electroslag remelting (ESR) has been investigated. Compared to a forged steel, the incubation periods for both the pearlite and bainite transform... The transformation behavior of a 40Cr2Ni2MoV cast steel manufactured by electroslag remelting (ESR) has been investigated. Compared to a forged steel, the incubation periods for both the pearlite and bainite transformations are shorter, but the transformation times are longer. The austenite is easier to transform into martensite. Optical microscopy and TEM indicated that there were variations in microstructure during the super-cooled austenite transformation. This is attributed to an inhomogeneous austenite, resulting from the segregation of elements during the ESR solidification. 展开更多
关键词 显微结构 40cr2Ni2MoV铸钢 TTT线图 偏析
下载PDF
ADI破碎机棒锤的研制 被引量:2
2
作者 张军 李志华 +3 位作者 文宏 陶汉德 朱松林 向纲玉 《现代铸铁》 CAS 2012年第2期26-28,共3页
针对破碎机棒锤的工况条件和失效形式,合理设计了棒锤的试制方案。通过化学成分、熔炼和热处理工艺的控制,最终获得洛氏硬度≥40 HRC、抗拉强度>1 300 MPa、伸长率>3%的ADI铸件。同等工况下,ADI棒锤的使用寿命是40Cr铸钢材料棒锤... 针对破碎机棒锤的工况条件和失效形式,合理设计了棒锤的试制方案。通过化学成分、熔炼和热处理工艺的控制,最终获得洛氏硬度≥40 HRC、抗拉强度>1 300 MPa、伸长率>3%的ADI铸件。同等工况下,ADI棒锤的使用寿命是40Cr铸钢材料棒锤的2倍以上。 展开更多
关键词 ADI 40cr铸钢 棒锤
下载PDF
1305滑动叉的失效金相检验
3
作者 宗斌 王国红 魏建忠 《机械工人(热加工)》 2005年第3期49-49,57,共2页
关键词 1305滑动叉 40cr铸钢 金相组织 裂纹