Impact of Corrosive Liquid on Trivalent Chromium over Aluminium Alloys 被引量:1
1
作者 Kalaivanan Thirupathi Pál Bárczy Béla Márton Somosvári 《Journal of Surface Engineered Materials and Advanced Technology》 2017年第3期51-60,共10页
Considering aviation and space sectors, aluminium alloys are commonly used due to its excellent mechanical and physical properties. Though satellite hard-ware is confined to controlled environment, it requires anticor... Considering aviation and space sectors, aluminium alloys are commonly used due to its excellent mechanical and physical properties. Though satellite hard-ware is confined to controlled environment, it requires anticorrosive treatment over metal substrate followed by a systematic coating scheme. The trivalent chromium coating was deposited over three aluminium alloys namely AA6063, AA7075 and AA6082. The variation in corrosion resistance property of trivalent chromium over each aluminium alloy has been studied in detail. The Neutral Salt Spray (NSS) test result shows that trivalent chromium coating over AA7075 alloy is affected by pitting corrosion compared to other two alloys. In addition to that, NSS test also proves that thickness of the layer does not have any influence corrosion resistance property of trivalent chromium coating. Furthermore, ions in trivalent chromium coating was identified using Secondary Neutral Mass Spectroscopy (SNMS) and degradation of coating in a corrosive liquid studied using Inductively Coupled Plasma Optical Emission Spectroscopy (ICP-OES) instrument to understand mechanism of corrosion. The results indicated that both coating and substrate is involved in corrosion process. The number of elements dissolved in to salt solution reveals the weak ionic bonding of coating towards substrates. In comparison, AA7075 alloy has weaker bonding than AA6082 and AA6063 series. The alloying elements such as zinc and copper are removed from substrate by corrosive solution. 展开更多
关键词 TRIVALENT Chromium ChROMATE Conversion Coating ASTM B117 neutral salt spray test
下载PDF
热镀锌钢板无铬钝化膜耐腐蚀性研究 被引量:2
2
作者 亢业峰 《山东冶金》 CAS 2020年第4期37-39,共3页
针对某冷轧厂投产初期生产的无铬钝化热镀锌产品耐盐雾腐蚀性差的问题,从分析影响无铬钝化镀锌产品耐腐蚀性能的因素入手,优化带钢表面粗糙度、无铬钝化膜膜重、涂覆辊硬度等工艺,使热镀锌钢板无铬钝化膜的耐蚀性得到明显改善,72 h中性... 针对某冷轧厂投产初期生产的无铬钝化热镀锌产品耐盐雾腐蚀性差的问题,从分析影响无铬钝化镀锌产品耐腐蚀性能的因素入手,优化带钢表面粗糙度、无铬钝化膜膜重、涂覆辊硬度等工艺,使热镀锌钢板无铬钝化膜的耐蚀性得到明显改善,72 h中性盐雾试验腐蚀面积≤5%的合格率达到94%以上。 展开更多
关键词 热镀锌 无铬钝化膜 耐腐蚀性 中性盐雾试验