Based on the attributes of nonflammability,environmental benignity,and cost-effectiveness of aqueous electrolytes,as well as the favorable compatibility of zinc metal with them,aqueous zinc ions batteries(AZIBs)become...Based on the attributes of nonflammability,environmental benignity,and cost-effectiveness of aqueous electrolytes,as well as the favorable compatibility of zinc metal with them,aqueous zinc ions batteries(AZIBs)become the leading energy storage candidate to meet the requirements of safety and low cost.Yet,aqueous electrolytes,acting as a double-edged sword,also play a negative role by directly or indirectly causing various parasitic reactions at the zinc anode side.These reactions include hydrogen evolution reaction,passivation,and dendrites,resulting in poor Coulombic efficiency and short lifespan of AZIBs.A comprehensive review of aqueous electrolytes chemistry,zinc chemistry,mechanism and chemistry of parasitic reactions,and their relationship is lacking.Moreover,the understanding of strategies for suppressing parasitic reactions from an electrochemical perspective is not profound enough.In this review,firstly,the chemistry of electrolytes,zinc anodes,and parasitic reactions and their relationship in AZIBs are deeply disclosed.Subsequently,the strategies for suppressing parasitic reactions from the perspective of enhancing the inherent thermodynamic stability of electrolytes and anodes,and lowering the dynamics of parasitic reactions at Zn/electrolyte interfaces are reviewed.Lastly,the perspectives on the future development direction of aqueous electrolytes,zinc anodes,and Zn/electrolyte interfaces are presented.展开更多
Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonethel...Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonetheless,the intricate energy storage mechanisms in aqueous electrolytes place stringent require-ments on the host materials.Prussian blue analogs(PBAs),with their open three-dimensional framework and facile synthesis,stand out as leading candidates for aqueous energy storage.However,PBAs possess a swift capacity fade and limited cycle longevity,for their structural integrity is compromised by the pronounced dis-solution of transition metal(TM)ions in the aqueous milieu.This manuscript provides an exhaustive review of the recent advancements concerning PBAs in ASIBs and APIBs.The dissolution mechanisms of TM ions in PBAs,informed by their structural attributes and redox processes,are thoroughly examined.Moreover,this study delves into innovative design tactics to alleviate the dissolution issue of TM ions.In conclusion,the paper consolidates various strategies for suppressing the dissolution of TM ions in PBAs and posits avenues for prospective exploration of high-safety aqueous sodium-/potassium-ion batteries.展开更多
Aqueous zinc-ion batteries(AZIBs) are promising candidates for the large-scale energy storage systems due to their high intrinsic safety,cost-effectiveness and environmental friendliness.However,issues such as dendrit...Aqueous zinc-ion batteries(AZIBs) are promising candidates for the large-scale energy storage systems due to their high intrinsic safety,cost-effectiveness and environmental friendliness.However,issues such as dendrite growth,hydrogen evolution reaction,and interfacial passivation occurring at the anode/electrolyte interface(AEI) have hindered their practical application.Constructing a stable AEI plays a key role in regulating zinc deposition and improving the cycle life of AZIBs.The fundamentals of AEI and the challenges faced by the Zn anode due to unstable interfaces are discussed.A comprehensive summary of electrolyte regulation strategies by electrolyte engineering to achieve a stable Zn anode is provided.The effectiveness evaluation techniques for stable AEI are also analyzed,including the interfacial chemistry and surface morphology evolution of the Zn anode.Finally,suggestions and perspectives for future research are offered about enabling a durable and stable AEI via electrolyte engineering,which may pave the way for developing high-performance AZIBs.展开更多
Aqueous sodium-ion batteries are known for poor rechargeability because of the competitive water decomposition reactions and the high electrode solubility.Improvements have been reported by saltconcentrated and organi...Aqueous sodium-ion batteries are known for poor rechargeability because of the competitive water decomposition reactions and the high electrode solubility.Improvements have been reported by saltconcentrated and organic-hybridized electrolyte designs,however,at the expense of cost and safety.Here,we report the prolonged cycling of ASIBs in routine dilute electrolytes by employing artificial electrode coatings consisting of NaX zeolite and NaOH-neutralized perfluorinated sulfonic polymer.The as-formed composite interphase exhibits a molecularsieving effect jointly played by zeolite channels and size-shrunken ionic domains in the polymer matrix,which enables high rejection of hydrated Na^(+)ions while allowing fast dehydrated Na^(+)permeance.Applying this coating to electrode surfaces expands the electrochemical window of a practically feasible 2 mol kg^(-1) sodium trifluoromethanesulfonate aqueous electrolyte to 2.70 V and affords Na_(2)MnFe(CN)_(6)//NaTi_(2)(PO_(4))_(3) full cells with an unprecedented cycling stability of 94.9%capacity retention after 200 cycles at 1 C.Combined with emerging electrolyte modifications,this molecular-sieving interphase brings amplified benefits in long-term operation of ASIBs.展开更多
Aqueous redox-active organic materials-base electrolytes are sustainable alternatives to vanadium-based electrolyte for redoxflow batteries(RFBs)due to the advantages of high ionic conductivity,environmentally benign,s...Aqueous redox-active organic materials-base electrolytes are sustainable alternatives to vanadium-based electrolyte for redoxflow batteries(RFBs)due to the advantages of high ionic conductivity,environmentally benign,safety and low cost.However,the underexplored redox properties of organic materials and the narrow thermodynamic electrolysis window of water(1.23 V)hinder their wide applications.Therefore,seeking suitable organic redox couples and aqueous electrolytes with a high output voltage is highly suggested for advancing the aqueous organic RFBs.In this work,the functionalized phenazine and nitroxyl radical with electron-donating and electron-withdrawing group exhibit redox potential of-0.88 V and 0.78 V vs.Ag,respectively,in“water-in-ionic liquid”supporting electrolytes.Raman spectra reveal that the activity of water is largely suppressed in“water-in-ionic liquid”due to the enhanced hydrogen bond interactions between ionic liquid and water,enabling an electrochemical stability window above 3 V.“Water-in-ionic liquid”supporting electrolytes help to shift redox potential of nitroxyl radical and enable the redox activity of functionalized phenazine.The assembled aqueous RFB allows a theoretical cell voltage of 1.66 V and shows a practical discharge voltage of 1.5 V in the“water-in-ionic liquid”electrolytes.Meanwhile,capacity retention of 99.91%per cycle is achieved over 500 charge/discharge cycles.A power density of 112 mW cm^(-2) is obtained at a current density of 30 mA cm^(-2).This work highlights the importance of rationally combining supporting electrolytes and organic molecules to achieve high-voltage aqueous RFBs.展开更多
Current lithium-ion batteries(LIBs)rely on organic liquid electrolytes that pose significant risks due to their flammability and toxicity.The potential for environmental pollution and explosions resulting from battery...Current lithium-ion batteries(LIBs)rely on organic liquid electrolytes that pose significant risks due to their flammability and toxicity.The potential for environmental pollution and explosions resulting from battery damage or fracture is a critical concern.Water-based(aqueous)electrolytes have been receiving attention as an alternative to organic electrolytes.However,a narrow electrochemicalstability window,water decomposition,and the consequent low battery operating voltage and energy density hinder the practical use of aqueous electrolytes.Therefore,developing novel aqueous electrolytes for sustainable,safe,high-performance LIBs remains challenging.This Review first commences by summarizing the roles and requirements of electrolytes–separators and then delineates the progression of aqueous electrolytes for LIBs,encompassing aqueous liquid and gel electrolyte development trends along with detailed principles of the electrolytes.These aqueous electrolytes are progressed based on strategies using superconcentrated salts,concentrated diluents,polymer additives,polymer networks,and artificial passivation layers,which are used for suppressing water decomposition and widening the electrochemical stability window of water of the electrolytes.In addition,this Review discusses potential strategies for the implementation of aqueous Li-metal batteries with improved electrolyte–electrode interfaces.A comprehensive understanding of each strategy in the aqueous system will assist in the design of an aqueous electrolyte and the development of sustainable and safe high-performance batteries.展开更多
Aqueous zinc-ion batteries(AZIBs) hold great promise as a viable alternative to lithium-ion batteries owing to their high energy density and environmental friendliness.However,AZIBs are consistently plagued by the for...Aqueous zinc-ion batteries(AZIBs) hold great promise as a viable alternative to lithium-ion batteries owing to their high energy density and environmental friendliness.However,AZIBs are consistently plagued by the formation of zinc dendrites and concurrent side reactions,which significantly diminish their overall service life,In this study,the glass fiber separator(GF) is modified using zeolite imidazole salt framework-8(ZIF-8),enabling the development of efficient AZIBs.ZIF-8,which is abundant in nitrogen content,efficiently regulates the desolvation of [Zn(H_(2)O)_(6)]^(2+) to inhibit hydrogen production.Moreover,it possesses abundant nanochannels that facilitate the uniform deposition of Zn~(2+) via a localized action,thereby hindering the formation of dendrites.The insulating properties of ZIF-8 help prevent Zn^(2+) and water from trapping electron reduction at the layer surface,which reduces corrosion of the zinc anode.Consequently,ZIF-8-GF achieves the even transport of Zn^(2+) and regulates the homogeneous deposition along the Zn(002) crystal surface,thus significantly enhancing the electrochemical performance of the AZIBs,In particular,the Zn|Zn symmetric cell with the ZIF-8-GF separator delivers a stable cycle life at0.5 mA cm^(-2) of 2300 h.The Zn|ZIF-8-GF|MnO_(2) cell exhibits reduced voltage polarization while maintaining a capacity retention rate(93.4%) after 1200 cycles at 1.2 A g^(-1) The unique design of the modified diaphragm provides a new approach to realizing high-performance AZIBs.展开更多
With the increasing demand for scalable and cost-effective electrochemical energy storage,aqueous zinc ion batteries(AZIBs)have a broad application prospect as an inexpensive,efficient,and naturally secure energy stor...With the increasing demand for scalable and cost-effective electrochemical energy storage,aqueous zinc ion batteries(AZIBs)have a broad application prospect as an inexpensive,efficient,and naturally secure energy storage device.However,the limitations suffered by AZIBs,including volume expansion and active materials dissolution of the cathode,electrochemical corrosion,irreversible side reactions,zinc dendrites of the anode,have seriously decelerated the civilianization process of AZIBs.Currently,polymers have tremendous superiority for application in AZIBs attributed to their exceptional chemical stability,tunable structure,high energy density and outstanding mechanical properties.Considering the expanding applications of AZIBs and the superiority of polymers,this comprehensive paper meticulously reviews the benefits of utilizing polymeric applied to cathodes and anodes,respectively.To begin with,with adjustable structure as an entry point,the correlation between polymer structure and the function of energy storage as well as optimization is deeply investigated in respect to the mechanism.Then,depending on the diversity of properties and structures,the development of polymers in AZIBs is summarized,including conductive polymers,redox polymers as well as carbon composite polymers for cathode and polyvinylidene fluoride-,carbonyl-,amino-,nitrile-based polymers for anode,and a comprehensive evaluation of the shortcomings of these strategies is provided.Finally,an outlook highlights some of the challenges posed by the application of polymers and offers insights into the potential future direction of polymers in AZIBs.It is designed to provide a thorough reference for researchers and developers working on polymer for AZIBs.展开更多
Aqueous zinc-ion batteries(AZIBs)are one of the most compelling alternatives of lithium-ion batteries due to their inherent safety and economics viability.In response to the growing demand for green and sustainable en...Aqueous zinc-ion batteries(AZIBs)are one of the most compelling alternatives of lithium-ion batteries due to their inherent safety and economics viability.In response to the growing demand for green and sustainable energy storage solutions,organic electrodes with the scalability from inexpensive starting materials and potential for biodegradation after use have become a prominent choice for AZIBs.Despite gratifying progresses of organic molecules with electrochemical performance in AZIBs,the research is still in infancy and hampered by certain issues due to the underlying complex electrochemistry.Strategies for designing organic electrode materials for AZIBs with high specific capacity and long cycling life are discussed in detail in this review.Specifically,we put emphasis on the unique electrochemistry of different redox-active structures to provide in-depth understanding of their working mechanisms.In addition,we highlight the importance of molecular size/dimension regarding their profound impact on electrochemical performances.Finally,challenges and perspectives are discussed from the developing point of view for future AZIBs.We hope to provide a valuable evaluation on organic electrode materials for AZIBs in our context and give inspiration for the rational design of high-performance AZIBs.展开更多
AIM:To investigate the efficacy of aflibercept combined with sub-tenon injection of triamcinolone acetonide(TA)in treating diabetic macular edema(DME)and to examine changes in growth factors and inflammatory mediator ...AIM:To investigate the efficacy of aflibercept combined with sub-tenon injection of triamcinolone acetonide(TA)in treating diabetic macular edema(DME)and to examine changes in growth factors and inflammatory mediator levels in aqueous humor after injection.METHODS:Totally 67 DME patients(67 eyes)and 30 cataract patients(32 eyes)were enrolled as the DME group and the control group,respectively.The DME group was divided into the aflibercept group(34 cases)and the aflibercept combined with TA group(combined group,33 cases).The aqueous humor of both groups was collected during the study period.The aqueous levels of vascular endothelial growth factor(VEGF),monocyte chemoattractant protein-1(MCP-1),interleukin-6(IL-6),interleukin-8(IL-8),and interleukin-1β(IL-1β)were detected using a microsphere suspension array technology(Luminex 200TM).Aqueous cytokines,best-corrected visual acuity(BCVA),central macular thickness(CMT),and complications before and after treatment were compared between the aflibercept group and combined group.RESULTS:The concentrations of VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor were significantly higher in the DME group than those of the control group(all P<0.01).After 1mo of surgery,the concentrations of VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor were significantly lower in the combined group than those of the aflibercept group(all P<0.01).The BCVA and CMT values of the two groups were statistically different after 1 and 2mo of treatment(P<0.01).However,the difference was not statistically significant after 3mo of treatment(P>0.05).CONCLUSION:The cytokines VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor of DME patients are significantly increased.Aflibercept and aflibercept combined with TA have good efficacy in DME patients,can effectively reduce CMT,improve the patient’s vision,and have high safety.Aflibercept combined with TA can quickly downregulate the aqueous humor cytokines and help to relieve macular edema rapidly.However,the long-term efficacy is comparable to that of aflibercept alone.展开更多
Developing sustainable and clean energy sources(e.g.,solar,wind,and tide energy)is essential to achieve the goal of carbon neutrality.Due to the discontinuous and inco nsistent nature of common clean energy sources,hi...Developing sustainable and clean energy sources(e.g.,solar,wind,and tide energy)is essential to achieve the goal of carbon neutrality.Due to the discontinuous and inco nsistent nature of common clean energy sources,high-performance energy storage technologies are a critical part of achieving this target.Aqueous zinc metal batteries(AZMBs)with inherent safety,low cost,and competitive performance are regarded as one of the promising candidates for grid-scale energy storage.However,zinc metal anodes(ZMAs)with irreversible problems of dendrite growth,hydrogen evolution reaction,self-corrosio n,and other side reactions have seriously hindered the development and commercialization of AZMBs.An increasing number of researchers are focusing on the stability of ZMAs,so assessing the effectiveness of existing research strategies is critical to the development of AZMBs.This review aims to provide a comprehensive overview of the fundamentals and challenges of AZMBs.Resea rch strategies for interfacial modification of ZMAs are systematically presented.The features of artificial interfacial coating and in-situ interfacial coating of ZMAs are compared and discussed in detail,as well as the effect of modified interfacial ZMA on the full-battery performance.Finally,perspectives are provided on the problems and challenges of ZMAs.This review is expected to offer a constructive reference for the further development and commercialization of AZMBs.展开更多
With the rapid development of portable electronics and electric road vehicles,high-energy-density batteries have been becoming front-burner issues.Traditionally,homogeneous electrolyte cannot simultaneously meet diame...With the rapid development of portable electronics and electric road vehicles,high-energy-density batteries have been becoming front-burner issues.Traditionally,homogeneous electrolyte cannot simultaneously meet diametrically opposed demands of high-potential cathode and low-potential anode,which are essential for high-voltage batteries.Meanwhile,homogeneous electrolyte is difficult to achieve bi-or multi-functions to meet different requirements of electrodes.In comparison,the asymmetric electrolyte with bi-or multi-layer disparate components can satisfy distinct requirements by playing different roles of each electrolyte layer and meanwhile compensates weakness of individual electrolyte.Consequently,the asymmetric electrolyte can not only suppress by-product sedimentation and continuous electrolyte decomposition at the anode while preserving active substances at the cathode for high-voltage batteries with long cyclic lifespan.In this review,we comprehensively divide asymmetric electrolytes into three categories:decoupled liquid-state electrolytes,bi-phase solid/liquid electrolytes and decoupled asymmetric solid-state electrolytes.The design principles,reaction mechanism and mutual compatibility are also studied,respectively.Finally,we provide a comprehensive vision for the simplification of structure to reduce costs and increase device energy density,and the optimization of solvation structure at anolyte/catholyte interface to realize fast ion transport kinetics.展开更多
Recently,rechargeable aqueous zinc-based batteries using manganese oxide as the cathode(e.g.,MnO_(2))have gained attention due to their inherent safety,environmental friendliness,and low cost.Despite their potential,a...Recently,rechargeable aqueous zinc-based batteries using manganese oxide as the cathode(e.g.,MnO_(2))have gained attention due to their inherent safety,environmental friendliness,and low cost.Despite their potential,achieving high energy density in Zn||MnO_(2)batteries remains challenging,highlighting the need to understand the electrochemical reaction mechanisms underlying these batteries more deeply and optimize battery components,including electrodes and electrolytes.This review comprehensively summarizes the latest advancements for understanding the electrochemistry reaction mechanisms and designing electrodes and electrolytes for Zn||MnO_(2)batteries in mildly and strongly acidic environments.Furthermore,we highlight the key challenges hindering the extensive application of Zn||MnO_(2)batteries,including high-voltage requirements and areal capacity,and propose innovative solutions to overcome these challenges.We suggest that MnO_(2)/Mn^(2+)conversion in neutral electrolytes is a crucial aspect that needs to be addressed to achieve high-performance Zn||MnO_(2)batteries.These approaches could lead to breakthroughs in the future development of Zn||MnO_(2)batteries,off ering a more sustainable,costeff ective,and high-performance alternative to traditional batteries.展开更多
Aqueous organic redox flow batteries(AORFBs),which exploit the reversible electrochemical reactions of water-soluble organic electrolytes to store electricity,have emerged as an efficient electrochemical energy storag...Aqueous organic redox flow batteries(AORFBs),which exploit the reversible electrochemical reactions of water-soluble organic electrolytes to store electricity,have emerged as an efficient electrochemical energy storage technology for the grid-scale integration of renewable electricity.pH-neutral AORFBs that feature high safety,low corrosivity,and environmental benignity are particularly promising,and their battery performance is significantly impacted by redox-active molecules and ion-exchange membranes(IEMs).Here,representative anolytes and catholytes engineered for use in pH-neutral AORFBs are outlined and summarized,as well as their side reactions that cause irreversible battery capacity fading.In addition,the recent achievements of IEMs for pH-neutral AORFBs are discussed,with a focus on the construction and tuning of ion transport channels.Finally,the critical challenges and potential research opportunities for developing practically relevant pH-neutral AORFBs are presented.展开更多
Aqueous humor provides the necessary nutrition for the lens and transports the metabolites in the eye.It was a liquid that can directly reflect the microenvironment in the eye'and it can be easily obtained during ...Aqueous humor provides the necessary nutrition for the lens and transports the metabolites in the eye.It was a liquid that can directly reflect the microenvironment in the eye'and it can be easily obtained during the operation.This review intended to analyze the components of aqueous humor in patients with different types of cataracts'so as to reflect the pathogenesis and development of the disease'evaluate the incidence of postoperative complications and provide reference value for the surgical design of sequential cataract surgery.The aqueous humor components of different types of cataracts showed different degrees of inflammation'oxidative stress and extracellular matrix remodeling.The biomarker of early neuropathy in diabetic cataract was neural cell adhesion molecule-1(NCAM1).Transforming growth factor-β(TGF-β)was the evaluation factor of disease development in patients with pseudoexfoliation syndrome.The relationships between postoperative complications of different types of cataracts and aqueous humor components were as follows:Macular edema after diabetic cataract surgery was associated with tumor necrosis factor-alpha;capsular contraction after high myopic cataract surgery was related to monocyte chemoattractant protein-1(MCP-1)and TGF-β2;Klotho and glutathione S-transferase P 1(GSTP1)were associated with high intraocular pressure after primary open-angle glaucoma complicated by cataract surgery;capsular contraction after retinitis pigmentosa complicated by cataract surgery was associated with matrix metalloproteinases;pro-inflammatory cytokines and fibroblast growth factor 4 in the aqueous humor of congenital cataracts were associated with posterior capsular opacification after surgery.Granulocyte colony stimulating factor 3 and MCP-1 were the main cytokines mediating the pain of the second eye in the binocular sequential cataract surgery short interval(1 wk)'while MCP-1 mediated pain in the long interval(6 wk).The second eye after binocular sequential cataract surgery had a higher level of proinflammatory factors.The components of aqueous humor in patients with different types of cataracts were related to the pathogenesis and postoperative complications of the disease.Monitoring the components of the aqueous humor could help better understand the intraocular microenvironment of different types of cataracts and provide a reference for predicting the development of the disease and implementing relevant targeted therapy.展开更多
Viologens known as a kind of promising negolyte materials for aqueous organic redox flow batteries,face a critical stability challenge due to the S_N2 nucleophilic attack by hydroxide ions(OH-)during the battery cycli...Viologens known as a kind of promising negolyte materials for aqueous organic redox flow batteries,face a critical stability challenge due to the S_N2 nucleophilic attack by hydroxide ions(OH-)during the battery cycling.In this work,a N-cyclic quaternary ammonium-grafted viologen molecule,viz.1,1'-bis(4,4'-dime thylpiperidiniumyl)-4,4'-bipyridinium tetrachloride((DBPPy)Cl_(4)),is developed by the molecular engineering strategy.The obtained(DBPPy)Cl_(4) molecule shows a decent solubility of 1.84 M and a redox potential of-0.52 V vs.Ag/AgCl,Experimental and theoretical results reveal that the grafted N-cyclic quaternary ammonium groups act as the steric hindrance to prevent nucleophilic attack by OH~-,increasing the alkali resistance of the electroactive molecule.The symmetrical battery with 0.50 M(DBPPy)Cl4shows negligible decay during the 13-day cycling test.As demonstration,the flow battery utilizing 1.0 M(DBPPy)Cl_(4) as the negolyte and 1-(1-oxyl-2,2',6,6'-tetramethylpiperidin-4-yl)-1'-(3-(trimethylammonio)propyl)-4,4'-bipyridinium trichloride as the posolyte exhibits a high capacity retention rate of 99.99%per cycle at 60 mA cm^(-2).展开更多
Aqueous zinc-ion batteries are promising due to inherent safety,low cost,low toxicity,and high volumetric capacity.However,issues of dendrites and side reactions between zinc metal anode and the electrolyte need to be...Aqueous zinc-ion batteries are promising due to inherent safety,low cost,low toxicity,and high volumetric capacity.However,issues of dendrites and side reactions between zinc metal anode and the electrolyte need to be solved for extended storage and cycle life.Here,we proposed that an electrolyte additive with an intermediate chelation strength of zinc ion—strong enough to exclude water molecules from the zinc metal-electrolyte interface and not too strong to cause a significant energy barrier for zinc ion dissociation—can benefit the electrochemical stability by suppressing hydrogen evolution reaction,overpotential growth,and den-drite formation.Penta-sodium diethylene-triaminepentaacetic acid salt was selected for such a purpose.It has a suitable chelating ability in aqueous solutions to adjust solvation sheath and can be readily polarized under electrical loading conditions to further improve the passivation.Zn||Zn symmetric cells can be stably operated over 3500 h at 1 mA cm^(-2).Zn||NH4V4O10 full cells with the additive show great cycling stability with 84.6%capacity retention after 500 cycles at 1 A g^(-1).Since the additive not only reduces H2 evolution and corrosion but also modifies Zn2+diffusion and deposition,highlyreversible Zn electrodes can be achieved as verified by the experimental results.Our work offers a practical approach to the logical design of reliable electrolytes for high-performance aqueous batteries.展开更多
The voltage drop appearing at Mg anode-electrolyte interface is a critical issue for the battery power and energy density of aqueous primary Mg-air batteries.The respective voltage loss is typically assigned to the de...The voltage drop appearing at Mg anode-electrolyte interface is a critical issue for the battery power and energy density of aqueous primary Mg-air batteries.The respective voltage loss is typically assigned to the deposits layer forming on the anode surface during discharge.In this work,we experimentally and computationally investigate the critical factors affecting the voltage drop at Mg anode towards a deeper understanding of the contribution of deposit and its growth.A two-dimensional(2D)mathematical model is proposed to compute the voltage drop of Mg-0.15Ca wt.%alloy(Mg-0.15Ca)by means of a semi-empirical formulas and experiments-based modification model,considering the effect of discharge current density,the negative difference effect(NDE)and surface deposits layer itself.This model is utilized to simulate the discharge potential of the anode at predefined experimental current densities.The computed voltage drop(half-cell voltage)is in good agreement with the experimental value.The applicability of the mathematical model is successfully validated on the second material(namely high-purity Mg).展开更多
Developing high-performance aqueous Zn-ion batteries from sustainable biomass becomes increasingly vital for large-scale energy storage in the foreseeable future.Therefore,γ-MnO_(2) uniformly loaded on N-doped carbon...Developing high-performance aqueous Zn-ion batteries from sustainable biomass becomes increasingly vital for large-scale energy storage in the foreseeable future.Therefore,γ-MnO_(2) uniformly loaded on N-doped carbon derived from grapefruit peel is successfully fabricated in this work,and particularly the composite cathode with carbon carrier quality percentage of 20 wt%delivers the specific capacity of 391.2 mAh g^(−1)at 0.1 A g^(−1),outstanding cyclic stability of 92.17%after 3000 cycles at 5 A g^(−1),and remarkable energy density of 553.12 Wh kg^(−1) together with superior coulombic efficiency of~100%.Additionally,the cathodic biosafety is further explored specifically through in vitro cell toxicity experiments,which verifies its tremendous potential in the application of clinical medicine.Besides,Zinc ion energy storage mechanism of the cathode is mainly discussed from the aspects of Jahn–Teller effect and Mn domains distribution combined with theoretical analysis and experimental data.Thus,a novel perspective of the conversion from biomass waste to biocompatible Mn-based cathode is successfully developed.展开更多
As a nonmetallic charge carrier,ammonium ion(NH_(4)^(+))has garnered significant attention in the construction of aqueous batteries due to its advantages of low molar mass,small hydration size and rapid diffusion in a...As a nonmetallic charge carrier,ammonium ion(NH_(4)^(+))has garnered significant attention in the construction of aqueous batteries due to its advantages of low molar mass,small hydration size and rapid diffusion in aqueous solutions.Polymers are a kind of potential electro-active materials for aqueous NH_(4)^(+)storage.However,traditional polymer electrodes are typically created by covering the bulky collectors with excessive additives,which could lead to low volume capacity and unsatisfactory stability.Herein,a nanoparticle-like polyimide(PI)was synthesized and then combined with MXene nanosheets to synergistically construct an additive-free and self-standing PI@MXene composite electrode.Significantly,the redox-active PI nanoparticles are enclosed between conductive MXene flakes to create a 3D lamination-like network that promotes electron transmission,while theπ-πinteractions existing between PI and MXene contribute to the enhanced structural integrity and stability within the composite electrode.As such,it delivers superior aqueous NH_(4)^(+)storage behaviors in terms of a notable specific capacity of 110.7 mA·h·cm^(–3) and a long lifespan with only 0.0064%drop each cycle.Furthermore,in-situ Raman and UV–Vis examinations provide evidence of reversible and stable redox mechanism of the PI@MXene composite electrode during NH_(4)^(+)uptake/removal,highlighting its significance in the area of electrochemical energy storage.展开更多
基金supported by the Academic Excellence Foundation of BUAA for PhD Studentsthe National Natural Science Foundation of China (Grant Number: 52001016)
文摘Based on the attributes of nonflammability,environmental benignity,and cost-effectiveness of aqueous electrolytes,as well as the favorable compatibility of zinc metal with them,aqueous zinc ions batteries(AZIBs)become the leading energy storage candidate to meet the requirements of safety and low cost.Yet,aqueous electrolytes,acting as a double-edged sword,also play a negative role by directly or indirectly causing various parasitic reactions at the zinc anode side.These reactions include hydrogen evolution reaction,passivation,and dendrites,resulting in poor Coulombic efficiency and short lifespan of AZIBs.A comprehensive review of aqueous electrolytes chemistry,zinc chemistry,mechanism and chemistry of parasitic reactions,and their relationship is lacking.Moreover,the understanding of strategies for suppressing parasitic reactions from an electrochemical perspective is not profound enough.In this review,firstly,the chemistry of electrolytes,zinc anodes,and parasitic reactions and their relationship in AZIBs are deeply disclosed.Subsequently,the strategies for suppressing parasitic reactions from the perspective of enhancing the inherent thermodynamic stability of electrolytes and anodes,and lowering the dynamics of parasitic reactions at Zn/electrolyte interfaces are reviewed.Lastly,the perspectives on the future development direction of aqueous electrolytes,zinc anodes,and Zn/electrolyte interfaces are presented.
基金This work was supported by the National Natural Science Foundation of China(52373306,52172233,and 51832004)the Natural Science Foundation of Hubei Province(2023AFA053)the Hainan Provincial Joint Project of Sanya Yazhou Bay Science and Technology City(2021CXLH0007).
文摘Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonetheless,the intricate energy storage mechanisms in aqueous electrolytes place stringent require-ments on the host materials.Prussian blue analogs(PBAs),with their open three-dimensional framework and facile synthesis,stand out as leading candidates for aqueous energy storage.However,PBAs possess a swift capacity fade and limited cycle longevity,for their structural integrity is compromised by the pronounced dis-solution of transition metal(TM)ions in the aqueous milieu.This manuscript provides an exhaustive review of the recent advancements concerning PBAs in ASIBs and APIBs.The dissolution mechanisms of TM ions in PBAs,informed by their structural attributes and redox processes,are thoroughly examined.Moreover,this study delves into innovative design tactics to alleviate the dissolution issue of TM ions.In conclusion,the paper consolidates various strategies for suppressing the dissolution of TM ions in PBAs and posits avenues for prospective exploration of high-safety aqueous sodium-/potassium-ion batteries.
基金financially supported by the National Natural Science Foundation of China (No. 52377222)the Natural Science Foundation of Hunan Province, China (Nos. 2023JJ20064, 2023JJ40759)。
文摘Aqueous zinc-ion batteries(AZIBs) are promising candidates for the large-scale energy storage systems due to their high intrinsic safety,cost-effectiveness and environmental friendliness.However,issues such as dendrite growth,hydrogen evolution reaction,and interfacial passivation occurring at the anode/electrolyte interface(AEI) have hindered their practical application.Constructing a stable AEI plays a key role in regulating zinc deposition and improving the cycle life of AZIBs.The fundamentals of AEI and the challenges faced by the Zn anode due to unstable interfaces are discussed.A comprehensive summary of electrolyte regulation strategies by electrolyte engineering to achieve a stable Zn anode is provided.The effectiveness evaluation techniques for stable AEI are also analyzed,including the interfacial chemistry and surface morphology evolution of the Zn anode.Finally,suggestions and perspectives for future research are offered about enabling a durable and stable AEI via electrolyte engineering,which may pave the way for developing high-performance AZIBs.
基金supported by the National Key R&D Program of China(Grant No.2022YFB2402604)the National Natural Science Foundation of China(21975271,22209194)+3 种基金Shandong Natural Science Foundation(ZR2020ZD07,ZR2023YQ010 and ZR2021QB106)the Taishan Scholars of Shandong Province(No.ts201511063,tsqn202211277)the Shandong Energy Institute(SEI I202127)Qingdao New Energy Shandong Laboratory(QIBEBT/SEI/QNESLS202304).
文摘Aqueous sodium-ion batteries are known for poor rechargeability because of the competitive water decomposition reactions and the high electrode solubility.Improvements have been reported by saltconcentrated and organic-hybridized electrolyte designs,however,at the expense of cost and safety.Here,we report the prolonged cycling of ASIBs in routine dilute electrolytes by employing artificial electrode coatings consisting of NaX zeolite and NaOH-neutralized perfluorinated sulfonic polymer.The as-formed composite interphase exhibits a molecularsieving effect jointly played by zeolite channels and size-shrunken ionic domains in the polymer matrix,which enables high rejection of hydrated Na^(+)ions while allowing fast dehydrated Na^(+)permeance.Applying this coating to electrode surfaces expands the electrochemical window of a practically feasible 2 mol kg^(-1) sodium trifluoromethanesulfonate aqueous electrolyte to 2.70 V and affords Na_(2)MnFe(CN)_(6)//NaTi_(2)(PO_(4))_(3) full cells with an unprecedented cycling stability of 94.9%capacity retention after 200 cycles at 1 C.Combined with emerging electrolyte modifications,this molecular-sieving interphase brings amplified benefits in long-term operation of ASIBs.
基金support from China Postdoctoral Science Foundation(Grant No.2021M690960)China CSC abroad studying fellowship.R.C.thanks the KIST Europe basic research funding“new electrolytes for redox flow batteries”and the partial financial support from the CMBlu Energy AG.Y.Z.thanks to the support received from the National Natural Science Foundation of China(Grant No.22002009)the Natural Science Foundation of Hunan Province(Grant No.2021JJ40565).
文摘Aqueous redox-active organic materials-base electrolytes are sustainable alternatives to vanadium-based electrolyte for redoxflow batteries(RFBs)due to the advantages of high ionic conductivity,environmentally benign,safety and low cost.However,the underexplored redox properties of organic materials and the narrow thermodynamic electrolysis window of water(1.23 V)hinder their wide applications.Therefore,seeking suitable organic redox couples and aqueous electrolytes with a high output voltage is highly suggested for advancing the aqueous organic RFBs.In this work,the functionalized phenazine and nitroxyl radical with electron-donating and electron-withdrawing group exhibit redox potential of-0.88 V and 0.78 V vs.Ag,respectively,in“water-in-ionic liquid”supporting electrolytes.Raman spectra reveal that the activity of water is largely suppressed in“water-in-ionic liquid”due to the enhanced hydrogen bond interactions between ionic liquid and water,enabling an electrochemical stability window above 3 V.“Water-in-ionic liquid”supporting electrolytes help to shift redox potential of nitroxyl radical and enable the redox activity of functionalized phenazine.The assembled aqueous RFB allows a theoretical cell voltage of 1.66 V and shows a practical discharge voltage of 1.5 V in the“water-in-ionic liquid”electrolytes.Meanwhile,capacity retention of 99.91%per cycle is achieved over 500 charge/discharge cycles.A power density of 112 mW cm^(-2) is obtained at a current density of 30 mA cm^(-2).This work highlights the importance of rationally combining supporting electrolytes and organic molecules to achieve high-voltage aqueous RFBs.
基金the National Research Foundation(NRF)of Korea(No.2022R1A2B5B02002097),funded by the Korea government(MSIT).
文摘Current lithium-ion batteries(LIBs)rely on organic liquid electrolytes that pose significant risks due to their flammability and toxicity.The potential for environmental pollution and explosions resulting from battery damage or fracture is a critical concern.Water-based(aqueous)electrolytes have been receiving attention as an alternative to organic electrolytes.However,a narrow electrochemicalstability window,water decomposition,and the consequent low battery operating voltage and energy density hinder the practical use of aqueous electrolytes.Therefore,developing novel aqueous electrolytes for sustainable,safe,high-performance LIBs remains challenging.This Review first commences by summarizing the roles and requirements of electrolytes–separators and then delineates the progression of aqueous electrolytes for LIBs,encompassing aqueous liquid and gel electrolyte development trends along with detailed principles of the electrolytes.These aqueous electrolytes are progressed based on strategies using superconcentrated salts,concentrated diluents,polymer additives,polymer networks,and artificial passivation layers,which are used for suppressing water decomposition and widening the electrochemical stability window of water of the electrolytes.In addition,this Review discusses potential strategies for the implementation of aqueous Li-metal batteries with improved electrolyte–electrode interfaces.A comprehensive understanding of each strategy in the aqueous system will assist in the design of an aqueous electrolyte and the development of sustainable and safe high-performance batteries.
基金financially supported by National Natural Science Foundation of China(No.51872090,51772097)Hebei Natural Science Fund for Distinguished Young Scholar(No.E2019209433)+2 种基金Youth Talent Program of Hebei Provincial Education Department(No.BJ2018020)Natural Science Foundation of Hebei Province(No.E2020209151)the financial support from Donghua University(101-08-0241022,23D210105,and 101-07-005759)。
文摘Aqueous zinc-ion batteries(AZIBs) hold great promise as a viable alternative to lithium-ion batteries owing to their high energy density and environmental friendliness.However,AZIBs are consistently plagued by the formation of zinc dendrites and concurrent side reactions,which significantly diminish their overall service life,In this study,the glass fiber separator(GF) is modified using zeolite imidazole salt framework-8(ZIF-8),enabling the development of efficient AZIBs.ZIF-8,which is abundant in nitrogen content,efficiently regulates the desolvation of [Zn(H_(2)O)_(6)]^(2+) to inhibit hydrogen production.Moreover,it possesses abundant nanochannels that facilitate the uniform deposition of Zn~(2+) via a localized action,thereby hindering the formation of dendrites.The insulating properties of ZIF-8 help prevent Zn^(2+) and water from trapping electron reduction at the layer surface,which reduces corrosion of the zinc anode.Consequently,ZIF-8-GF achieves the even transport of Zn^(2+) and regulates the homogeneous deposition along the Zn(002) crystal surface,thus significantly enhancing the electrochemical performance of the AZIBs,In particular,the Zn|Zn symmetric cell with the ZIF-8-GF separator delivers a stable cycle life at0.5 mA cm^(-2) of 2300 h.The Zn|ZIF-8-GF|MnO_(2) cell exhibits reduced voltage polarization while maintaining a capacity retention rate(93.4%) after 1200 cycles at 1.2 A g^(-1) The unique design of the modified diaphragm provides a new approach to realizing high-performance AZIBs.
基金financially supported by the National Natural Science Foundation of China(51872090,51772097,22304055)the Hebei Natural Science Fund for Distinguished Young Scholar(E2019209433)+4 种基金the Youth Talent Program of Hebei Provincial Education Department(BJ2018020)the Natural Science Foundation of Hebei Province(E2020209151,E2022209158,B2022209026,D2023209012)the Central Guiding Local Science and Technology Development Fund Project(236Z4409G)the Science and Technology Project of Hebei Education Department(SLRC2019028)the Science and Technology Planning Project of Tangshan City(22130227H)。
文摘With the increasing demand for scalable and cost-effective electrochemical energy storage,aqueous zinc ion batteries(AZIBs)have a broad application prospect as an inexpensive,efficient,and naturally secure energy storage device.However,the limitations suffered by AZIBs,including volume expansion and active materials dissolution of the cathode,electrochemical corrosion,irreversible side reactions,zinc dendrites of the anode,have seriously decelerated the civilianization process of AZIBs.Currently,polymers have tremendous superiority for application in AZIBs attributed to their exceptional chemical stability,tunable structure,high energy density and outstanding mechanical properties.Considering the expanding applications of AZIBs and the superiority of polymers,this comprehensive paper meticulously reviews the benefits of utilizing polymeric applied to cathodes and anodes,respectively.To begin with,with adjustable structure as an entry point,the correlation between polymer structure and the function of energy storage as well as optimization is deeply investigated in respect to the mechanism.Then,depending on the diversity of properties and structures,the development of polymers in AZIBs is summarized,including conductive polymers,redox polymers as well as carbon composite polymers for cathode and polyvinylidene fluoride-,carbonyl-,amino-,nitrile-based polymers for anode,and a comprehensive evaluation of the shortcomings of these strategies is provided.Finally,an outlook highlights some of the challenges posed by the application of polymers and offers insights into the potential future direction of polymers in AZIBs.It is designed to provide a thorough reference for researchers and developers working on polymer for AZIBs.
基金supported in part by the National Natural Science Foundation of China(Nos.22075027,52003030)Starting Grant from Beijing Institute of Technology and financial support from the State Key Laboratory of Explosion Science and Technology(YBKT21-06,YKBT23-05).
文摘Aqueous zinc-ion batteries(AZIBs)are one of the most compelling alternatives of lithium-ion batteries due to their inherent safety and economics viability.In response to the growing demand for green and sustainable energy storage solutions,organic electrodes with the scalability from inexpensive starting materials and potential for biodegradation after use have become a prominent choice for AZIBs.Despite gratifying progresses of organic molecules with electrochemical performance in AZIBs,the research is still in infancy and hampered by certain issues due to the underlying complex electrochemistry.Strategies for designing organic electrode materials for AZIBs with high specific capacity and long cycling life are discussed in detail in this review.Specifically,we put emphasis on the unique electrochemistry of different redox-active structures to provide in-depth understanding of their working mechanisms.In addition,we highlight the importance of molecular size/dimension regarding their profound impact on electrochemical performances.Finally,challenges and perspectives are discussed from the developing point of view for future AZIBs.We hope to provide a valuable evaluation on organic electrode materials for AZIBs in our context and give inspiration for the rational design of high-performance AZIBs.
基金Supported by the Shenzhen Science and Technology Innovation Committee,China(No.JCYJ20220530164600002)Scientific Research Program of Xiangjiang Philanthropy FoundationScience Research Grant of Aier Eye Hospital Group(No.AF2201D06).
文摘AIM:To investigate the efficacy of aflibercept combined with sub-tenon injection of triamcinolone acetonide(TA)in treating diabetic macular edema(DME)and to examine changes in growth factors and inflammatory mediator levels in aqueous humor after injection.METHODS:Totally 67 DME patients(67 eyes)and 30 cataract patients(32 eyes)were enrolled as the DME group and the control group,respectively.The DME group was divided into the aflibercept group(34 cases)and the aflibercept combined with TA group(combined group,33 cases).The aqueous humor of both groups was collected during the study period.The aqueous levels of vascular endothelial growth factor(VEGF),monocyte chemoattractant protein-1(MCP-1),interleukin-6(IL-6),interleukin-8(IL-8),and interleukin-1β(IL-1β)were detected using a microsphere suspension array technology(Luminex 200TM).Aqueous cytokines,best-corrected visual acuity(BCVA),central macular thickness(CMT),and complications before and after treatment were compared between the aflibercept group and combined group.RESULTS:The concentrations of VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor were significantly higher in the DME group than those of the control group(all P<0.01).After 1mo of surgery,the concentrations of VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor were significantly lower in the combined group than those of the aflibercept group(all P<0.01).The BCVA and CMT values of the two groups were statistically different after 1 and 2mo of treatment(P<0.01).However,the difference was not statistically significant after 3mo of treatment(P>0.05).CONCLUSION:The cytokines VEGF,MCP-1,IL-6,and IL-8 in the aqueous humor of DME patients are significantly increased.Aflibercept and aflibercept combined with TA have good efficacy in DME patients,can effectively reduce CMT,improve the patient’s vision,and have high safety.Aflibercept combined with TA can quickly downregulate the aqueous humor cytokines and help to relieve macular edema rapidly.However,the long-term efficacy is comparable to that of aflibercept alone.
基金the financial support from the Australian Research Council,Centre for Materials Science,Queensland University of Technologythe Supported by the Fundamental Research Funds for the Central Universities。
文摘Developing sustainable and clean energy sources(e.g.,solar,wind,and tide energy)is essential to achieve the goal of carbon neutrality.Due to the discontinuous and inco nsistent nature of common clean energy sources,high-performance energy storage technologies are a critical part of achieving this target.Aqueous zinc metal batteries(AZMBs)with inherent safety,low cost,and competitive performance are regarded as one of the promising candidates for grid-scale energy storage.However,zinc metal anodes(ZMAs)with irreversible problems of dendrite growth,hydrogen evolution reaction,self-corrosio n,and other side reactions have seriously hindered the development and commercialization of AZMBs.An increasing number of researchers are focusing on the stability of ZMAs,so assessing the effectiveness of existing research strategies is critical to the development of AZMBs.This review aims to provide a comprehensive overview of the fundamentals and challenges of AZMBs.Resea rch strategies for interfacial modification of ZMAs are systematically presented.The features of artificial interfacial coating and in-situ interfacial coating of ZMAs are compared and discussed in detail,as well as the effect of modified interfacial ZMA on the full-battery performance.Finally,perspectives are provided on the problems and challenges of ZMAs.This review is expected to offer a constructive reference for the further development and commercialization of AZMBs.
基金National Natural Science Foundation of China(52202299)the Analytical&Testing Center of Northwestern Polytechnical University(2022T006).
文摘With the rapid development of portable electronics and electric road vehicles,high-energy-density batteries have been becoming front-burner issues.Traditionally,homogeneous electrolyte cannot simultaneously meet diametrically opposed demands of high-potential cathode and low-potential anode,which are essential for high-voltage batteries.Meanwhile,homogeneous electrolyte is difficult to achieve bi-or multi-functions to meet different requirements of electrodes.In comparison,the asymmetric electrolyte with bi-or multi-layer disparate components can satisfy distinct requirements by playing different roles of each electrolyte layer and meanwhile compensates weakness of individual electrolyte.Consequently,the asymmetric electrolyte can not only suppress by-product sedimentation and continuous electrolyte decomposition at the anode while preserving active substances at the cathode for high-voltage batteries with long cyclic lifespan.In this review,we comprehensively divide asymmetric electrolytes into three categories:decoupled liquid-state electrolytes,bi-phase solid/liquid electrolytes and decoupled asymmetric solid-state electrolytes.The design principles,reaction mechanism and mutual compatibility are also studied,respectively.Finally,we provide a comprehensive vision for the simplification of structure to reduce costs and increase device energy density,and the optimization of solvation structure at anolyte/catholyte interface to realize fast ion transport kinetics.
文摘Recently,rechargeable aqueous zinc-based batteries using manganese oxide as the cathode(e.g.,MnO_(2))have gained attention due to their inherent safety,environmental friendliness,and low cost.Despite their potential,achieving high energy density in Zn||MnO_(2)batteries remains challenging,highlighting the need to understand the electrochemical reaction mechanisms underlying these batteries more deeply and optimize battery components,including electrodes and electrolytes.This review comprehensively summarizes the latest advancements for understanding the electrochemistry reaction mechanisms and designing electrodes and electrolytes for Zn||MnO_(2)batteries in mildly and strongly acidic environments.Furthermore,we highlight the key challenges hindering the extensive application of Zn||MnO_(2)batteries,including high-voltage requirements and areal capacity,and propose innovative solutions to overcome these challenges.We suggest that MnO_(2)/Mn^(2+)conversion in neutral electrolytes is a crucial aspect that needs to be addressed to achieve high-performance Zn||MnO_(2)batteries.These approaches could lead to breakthroughs in the future development of Zn||MnO_(2)batteries,off ering a more sustainable,costeff ective,and high-performance alternative to traditional batteries.
基金funded by the National Key Research and Development Program of China(Nos.2022YFB3805303,2022YFB3805304)the National Natural Science Foundation of China(Grant/Award Numbers:22308345,U20A20127)+1 种基金the Anhui Provincial Natural Science Foundation(No.2308085QB68)the Fundamental Research Funds for the Central Universities(No.WK2060000059).
文摘Aqueous organic redox flow batteries(AORFBs),which exploit the reversible electrochemical reactions of water-soluble organic electrolytes to store electricity,have emerged as an efficient electrochemical energy storage technology for the grid-scale integration of renewable electricity.pH-neutral AORFBs that feature high safety,low corrosivity,and environmental benignity are particularly promising,and their battery performance is significantly impacted by redox-active molecules and ion-exchange membranes(IEMs).Here,representative anolytes and catholytes engineered for use in pH-neutral AORFBs are outlined and summarized,as well as their side reactions that cause irreversible battery capacity fading.In addition,the recent achievements of IEMs for pH-neutral AORFBs are discussed,with a focus on the construction and tuning of ion transport channels.Finally,the critical challenges and potential research opportunities for developing practically relevant pH-neutral AORFBs are presented.
文摘Aqueous humor provides the necessary nutrition for the lens and transports the metabolites in the eye.It was a liquid that can directly reflect the microenvironment in the eye'and it can be easily obtained during the operation.This review intended to analyze the components of aqueous humor in patients with different types of cataracts'so as to reflect the pathogenesis and development of the disease'evaluate the incidence of postoperative complications and provide reference value for the surgical design of sequential cataract surgery.The aqueous humor components of different types of cataracts showed different degrees of inflammation'oxidative stress and extracellular matrix remodeling.The biomarker of early neuropathy in diabetic cataract was neural cell adhesion molecule-1(NCAM1).Transforming growth factor-β(TGF-β)was the evaluation factor of disease development in patients with pseudoexfoliation syndrome.The relationships between postoperative complications of different types of cataracts and aqueous humor components were as follows:Macular edema after diabetic cataract surgery was associated with tumor necrosis factor-alpha;capsular contraction after high myopic cataract surgery was related to monocyte chemoattractant protein-1(MCP-1)and TGF-β2;Klotho and glutathione S-transferase P 1(GSTP1)were associated with high intraocular pressure after primary open-angle glaucoma complicated by cataract surgery;capsular contraction after retinitis pigmentosa complicated by cataract surgery was associated with matrix metalloproteinases;pro-inflammatory cytokines and fibroblast growth factor 4 in the aqueous humor of congenital cataracts were associated with posterior capsular opacification after surgery.Granulocyte colony stimulating factor 3 and MCP-1 were the main cytokines mediating the pain of the second eye in the binocular sequential cataract surgery short interval(1 wk)'while MCP-1 mediated pain in the long interval(6 wk).The second eye after binocular sequential cataract surgery had a higher level of proinflammatory factors.The components of aqueous humor in patients with different types of cataracts were related to the pathogenesis and postoperative complications of the disease.Monitoring the components of the aqueous humor could help better understand the intraocular microenvironment of different types of cataracts and provide a reference for predicting the development of the disease and implementing relevant targeted therapy.
基金jointly supported by the Guangdong Major Project of Basic and Applied Basic Research (2023B0303000002)National Natural Science Foundation of China (22178126,22325802,U22A20417,22208110)+3 种基金Guangdong Basic and Applied Basic Research Foundation (2023B1515120005)Science and Technology Program of Guangzhou (2023B03J1281,2023A04J1357)China Postdoctoral Science Foundation (2023T160223)the State Key Laboratory of Pulp and Paper Engineering (2023ZD03)。
文摘Viologens known as a kind of promising negolyte materials for aqueous organic redox flow batteries,face a critical stability challenge due to the S_N2 nucleophilic attack by hydroxide ions(OH-)during the battery cycling.In this work,a N-cyclic quaternary ammonium-grafted viologen molecule,viz.1,1'-bis(4,4'-dime thylpiperidiniumyl)-4,4'-bipyridinium tetrachloride((DBPPy)Cl_(4)),is developed by the molecular engineering strategy.The obtained(DBPPy)Cl_(4) molecule shows a decent solubility of 1.84 M and a redox potential of-0.52 V vs.Ag/AgCl,Experimental and theoretical results reveal that the grafted N-cyclic quaternary ammonium groups act as the steric hindrance to prevent nucleophilic attack by OH~-,increasing the alkali resistance of the electroactive molecule.The symmetrical battery with 0.50 M(DBPPy)Cl4shows negligible decay during the 13-day cycling test.As demonstration,the flow battery utilizing 1.0 M(DBPPy)Cl_(4) as the negolyte and 1-(1-oxyl-2,2',6,6'-tetramethylpiperidin-4-yl)-1'-(3-(trimethylammonio)propyl)-4,4'-bipyridinium trichloride as the posolyte exhibits a high capacity retention rate of 99.99%per cycle at 60 mA cm^(-2).
基金This work is financially supported by National Natural Science Foundation of China(NSFC-No.52173257 and 52372064).
文摘Aqueous zinc-ion batteries are promising due to inherent safety,low cost,low toxicity,and high volumetric capacity.However,issues of dendrites and side reactions between zinc metal anode and the electrolyte need to be solved for extended storage and cycle life.Here,we proposed that an electrolyte additive with an intermediate chelation strength of zinc ion—strong enough to exclude water molecules from the zinc metal-electrolyte interface and not too strong to cause a significant energy barrier for zinc ion dissociation—can benefit the electrochemical stability by suppressing hydrogen evolution reaction,overpotential growth,and den-drite formation.Penta-sodium diethylene-triaminepentaacetic acid salt was selected for such a purpose.It has a suitable chelating ability in aqueous solutions to adjust solvation sheath and can be readily polarized under electrical loading conditions to further improve the passivation.Zn||Zn symmetric cells can be stably operated over 3500 h at 1 mA cm^(-2).Zn||NH4V4O10 full cells with the additive show great cycling stability with 84.6%capacity retention after 500 cycles at 1 A g^(-1).Since the additive not only reduces H2 evolution and corrosion but also modifies Zn2+diffusion and deposition,highlyreversible Zn electrodes can be achieved as verified by the experimental results.Our work offers a practical approach to the logical design of reliable electrolytes for high-performance aqueous batteries.
基金the China Scholarship Council for the award of fellowship and funding No.201908510177 and No.202106050030funded by dtec.bw-Digitalization and Technology Research Center of the Bundeswehr which project DMF+1 种基金The AMABML project founded by the Zentrum für Hochleistungsmaterialien(ZHM)DEZAIN project for financial support via grant from GIF,the German-Israeli Foundation for Scientific Research and Development。
文摘The voltage drop appearing at Mg anode-electrolyte interface is a critical issue for the battery power and energy density of aqueous primary Mg-air batteries.The respective voltage loss is typically assigned to the deposits layer forming on the anode surface during discharge.In this work,we experimentally and computationally investigate the critical factors affecting the voltage drop at Mg anode towards a deeper understanding of the contribution of deposit and its growth.A two-dimensional(2D)mathematical model is proposed to compute the voltage drop of Mg-0.15Ca wt.%alloy(Mg-0.15Ca)by means of a semi-empirical formulas and experiments-based modification model,considering the effect of discharge current density,the negative difference effect(NDE)and surface deposits layer itself.This model is utilized to simulate the discharge potential of the anode at predefined experimental current densities.The computed voltage drop(half-cell voltage)is in good agreement with the experimental value.The applicability of the mathematical model is successfully validated on the second material(namely high-purity Mg).
基金supported by the National Natural Science Foundation of China[Grant no.51821004].
文摘Developing high-performance aqueous Zn-ion batteries from sustainable biomass becomes increasingly vital for large-scale energy storage in the foreseeable future.Therefore,γ-MnO_(2) uniformly loaded on N-doped carbon derived from grapefruit peel is successfully fabricated in this work,and particularly the composite cathode with carbon carrier quality percentage of 20 wt%delivers the specific capacity of 391.2 mAh g^(−1)at 0.1 A g^(−1),outstanding cyclic stability of 92.17%after 3000 cycles at 5 A g^(−1),and remarkable energy density of 553.12 Wh kg^(−1) together with superior coulombic efficiency of~100%.Additionally,the cathodic biosafety is further explored specifically through in vitro cell toxicity experiments,which verifies its tremendous potential in the application of clinical medicine.Besides,Zinc ion energy storage mechanism of the cathode is mainly discussed from the aspects of Jahn–Teller effect and Mn domains distribution combined with theoretical analysis and experimental data.Thus,a novel perspective of the conversion from biomass waste to biocompatible Mn-based cathode is successfully developed.
基金supported by the National Natural Science Foundation of China(52002157)the Undergraduate Research&Practice Innovation Program of Jiangsu Province(202310289033Z).
文摘As a nonmetallic charge carrier,ammonium ion(NH_(4)^(+))has garnered significant attention in the construction of aqueous batteries due to its advantages of low molar mass,small hydration size and rapid diffusion in aqueous solutions.Polymers are a kind of potential electro-active materials for aqueous NH_(4)^(+)storage.However,traditional polymer electrodes are typically created by covering the bulky collectors with excessive additives,which could lead to low volume capacity and unsatisfactory stability.Herein,a nanoparticle-like polyimide(PI)was synthesized and then combined with MXene nanosheets to synergistically construct an additive-free and self-standing PI@MXene composite electrode.Significantly,the redox-active PI nanoparticles are enclosed between conductive MXene flakes to create a 3D lamination-like network that promotes electron transmission,while theπ-πinteractions existing between PI and MXene contribute to the enhanced structural integrity and stability within the composite electrode.As such,it delivers superior aqueous NH_(4)^(+)storage behaviors in terms of a notable specific capacity of 110.7 mA·h·cm^(–3) and a long lifespan with only 0.0064%drop each cycle.Furthermore,in-situ Raman and UV–Vis examinations provide evidence of reversible and stable redox mechanism of the PI@MXene composite electrode during NH_(4)^(+)uptake/removal,highlighting its significance in the area of electrochemical energy storage.