期刊文献+
共找到1篇文章
< 1 >
每页显示 20 50 100
Regeneration of waste SCR catalyst by air lift loop reactor 被引量:10
1
作者 LEE Jung-bin EOM Yong-seok +1 位作者 KIM Jun-han CHUN Sung-nam 《Journal of Central South University》 SCIE EI CAS 2013年第5期1314-1318,共5页
A solution of 0.1 mol/L to 1.0 mol/L H2SO4 can dissolve alkali metals and alkaline earth metals which weaken an active site of SCR catalyst. The waste catalyst washed with 0.5 mol/L H2SO4 regained the best catalytic a... A solution of 0.1 mol/L to 1.0 mol/L H2SO4 can dissolve alkali metals and alkaline earth metals which weaken an active site of SCR catalyst. The waste catalyst washed with 0.5 mol/L H2SO4 regained the best catalytic activity. When a concentration of the sulfuric acid is less than 0.5 mol/L, sufficient cleaning effects cannot be obtained. In contrast, when the concentration is greater than 1.0 tool/L, the active components, vanadium and tungsten are undesirably eluted. The total BET surface of the catalyst regenerated by air lift loop reactor showed almost the same as that of fresh catalyst due to the removal of insoluble compounds which may be penetrated into pores of catalyst. The addition of a solution of 0.075 mol/L ammonium vanadate (NHnVO3) and 0.075 mol/L ammonium paratungstate (5(NH4)20· 12WO3-5H20) to 0.1 mol/L H2SO4 significantly increases the activity of the waste catalyst. 展开更多
关键词 nitrogen oxide REGENERATION selective catalyst reduction air lift loop reactor catalyst
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部