Finite element analysis of stress-strain localization and distribution in Al-4.5Cu-2Mg alloy 被引量:1
1
作者 Rahul BHANDARI Prosanta BISWAS +1 位作者 Manas Kumar MONDAL Durbadal MANDAL 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2018年第6期1200-1215,共16页
Finite element analysis has been carried out to understand the effect of various processing routes and condition on the microscale deformation behavior of Al–4.5 Cu–2 Mg alloy. The alloy has been developed through f... Finite element analysis has been carried out to understand the effect of various processing routes and condition on the microscale deformation behavior of Al–4.5 Cu–2 Mg alloy. The alloy has been developed through four different routes and condition, i.e. conventional gravity casting with and without refiner, rheocasting and SIMA process. The optical microstructures of the alloy have been used to develop representative volume elements(RVEs). Two different boundary conditions have been employed to simulate the deformation behavior of the alloy under uniaxial loading. Finally, the simulated stress-strain behavior of the alloy is compared with the experimental result. It is found that the microstructural morphology has a significant impact on stress and strain distribution and load carrying capacity. The eutectic phase always carries a higher load than the α(Al) phase. The globular α(Al) grains with thinner and uniformly distributed eutectic network provide a better stress and strain distribution. Owing to this, SIMA processed alloy has better stress and strain distribution than other processes. Finally, the simulated yield strength of the alloy is verified by experiment and they have great agreement. 展开更多
关键词 al-4.5cu-2Mg alloy MICROSTRUCTURE a(Al) phase eutectic phase finite element analysis micromechanical response
下载PDF
Effect of abruptly changing withdrawal rate on solidification microstructure in directionally solidified Al-4.5wt%Cu alloy
2
作者 Yang Luyan Li Shuangming +2 位作者 Zhong Hong Ren Ruohua Fu Hengzhi 《China Foundry》 SCIE CAS 2014年第1期8-13,共6页
Al-4.5wt.%Cu alloy has been directionally solidified at constant and abruptly changing withdrawal rates, respectively. The effects of the withdrawal rate on solidification microstructure, primary dendrite arm spacing(... Al-4.5wt.%Cu alloy has been directionally solidified at constant and abruptly changing withdrawal rates, respectively. The effects of the withdrawal rate on solidification microstructure, primary dendrite arm spacing(PDAS) and liquid solute distribution in front of the solid-liquid interface were investigated. The experimental results for the PDAS at a constant withdrawal rate agree well with the values calculated by the Hunt, Trivedi and Hunt-Lu models. At an abrupt change in the withdrawal rate, the maximum to minimum ratio of the PDAS at a given solidification parameter, i.e. λ1max/λ1min, is more than 2, and the PDAS values are remarkably history-dependent. Further, the liquid-solute distribution curve based on theoretical calculation shows that the larger the initial withdrawal rate is, the smaller the minimum of liquid solute concentration in front of the solid-liquid interface is after the abrupt change in withdrawal rate. 展开更多
关键词 directional solidification abrupt change of withdrawal rate primary dendrite arm spacing liquid-solute distribution al-4.5wt.%cu alloy
下载PDF
合金元素对铸造Al-4.5Cu合金准固态力学行为的影响(英文) 被引量:7
3
作者 董晟全 周敬恩 严文 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2005年第11期1721-1725,共5页
研究了铸造Al-4.5Cu合金的准固态力学行为及几种合金元素对其凝固行为的影响。结果表明:Si,Ce,La,Ti及Zr元素可有效减小Al-4.5Cu合金的结晶范围,从而使其热裂倾向性降低;La元素的加入可提高Al-4.5Cu合金的热裂抗力;并研制了一种新型Al-4... 研究了铸造Al-4.5Cu合金的准固态力学行为及几种合金元素对其凝固行为的影响。结果表明:Si,Ce,La,Ti及Zr元素可有效减小Al-4.5Cu合金的结晶范围,从而使其热裂倾向性降低;La元素的加入可提高Al-4.5Cu合金的热裂抗力;并研制了一种新型Al-4.5Cu合金,该合金具有良好的室温与高温综合性能。 展开更多
关键词 热裂 铸造al-4.5cu合金 准固态 新型al-4.5
下载PDF
定向凝固Al-4.5%Cu合金枝晶组织与抽拉速率的关系 被引量:9
4
作者 吴强 司乃潮 +1 位作者 郭毅 李达云 《中国有色金属学报》 EI CAS CSCD 北大核心 2007年第7期1101-1106,共6页
用自制下拉式定向凝固设备,在一定的温度梯度下,在20-220μm/s的抽拉速率范围制备定向凝固Al-4.5%Cu合金,并对其微观组织、特别是一次枝晶间距随抽拉速率的变化规律进行研究。结果表明:定向凝固微观组织随抽拉速率的增大呈细化趋势,其... 用自制下拉式定向凝固设备,在一定的温度梯度下,在20-220μm/s的抽拉速率范围制备定向凝固Al-4.5%Cu合金,并对其微观组织、特别是一次枝晶间距随抽拉速率的变化规律进行研究。结果表明:定向凝固微观组织随抽拉速率的增大呈细化趋势,其一次枝晶间距减小;当抽拉速率小于100μm/s时,枝晶间距随抽拉速率而减小的幅度较大;当抽拉速率大于100μm/s时,枝晶间距减小幅度较为平缓。在综合分析抽拉速率、界面生长速率、温度梯度等影响因素的基础上,推导出界面局域平衡条件下预测定向凝固次枝晶间距的理论模型,该模型能够较为准确地反映定向凝固一次枝晶间距随抽拉速率在100-220μm/s范围的变化规律,为定向凝固工艺获得特定组织而预先选配合适的工艺参数提供理论参考。 展开更多
关键词 al-4.5%cu合金 定向凝固 一次枝晶间距 抽拉速率 传热
下载PDF
Si,La对Al-4.5Cu合金准固态凝固行为的影响 被引量:2
5
作者 董晟全 刘江南 +4 位作者 周敬恩 严文 梁艳峰 李建平 杨通 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2004年第3期285-288,共4页
通过对合金的收缩应变和热裂抗力及准固态拉伸行为进行测试,研究了合金元素(Si,La)对Al-4.5Cu合金凝固行为的影响。结果表明,Si,La能使Al-4.5Cu的热裂倾向性降低;加入2%Si使合金的再辉现象非常严重,导致合金不可能有很高的强度而很快断... 通过对合金的收缩应变和热裂抗力及准固态拉伸行为进行测试,研究了合金元素(Si,La)对Al-4.5Cu合金凝固行为的影响。结果表明,Si,La能使Al-4.5Cu的热裂倾向性降低;加入2%Si使合金的再辉现象非常严重,导致合金不可能有很高的强度而很快断裂;与其它Al-4.5Cu-Si合金相比,Al4.5Cu3Si合金具有很强的补缩能力,断裂应力值最高;La的加入能缩小二次枝晶间距,明显提高合金的抗热裂性能。 展开更多
关键词 al-4.5cu合金 准固态凝固行为 抗热裂力 收缩应变 SI LA 断裂应力
下载PDF
Ti对Al-4.5%Cu合金热疲劳性能的影响 被引量:9
6
作者 司乃潮 吴强 李国强 《铸造》 EI CAS CSCD 北大核心 2006年第7期731-734,共4页
在接近材料实际工况的试验条件下,以铝铜合金(4.5%Cu)为研究对象,用自约束型热疲劳试验机进行了热疲劳试验以及热疲劳裂纹萌生及扩展规律研究。试验结果表明,随Ti元素加入量的增加(0.1%~0.5%),合金热疲劳性能和部分力学性能(抗拉强度... 在接近材料实际工况的试验条件下,以铝铜合金(4.5%Cu)为研究对象,用自约束型热疲劳试验机进行了热疲劳试验以及热疲劳裂纹萌生及扩展规律研究。试验结果表明,随Ti元素加入量的增加(0.1%~0.5%),合金热疲劳性能和部分力学性能(抗拉强度、屈服强度)都呈现先升高后降低的变化趋势,合金热疲劳性能基本上是0.35%Ti最好,0.2%Ti次之,0.5%Ti最差。合金热疲劳裂纹的扩展方式为混合扩展。 展开更多
关键词 铝铜合金 热疲劳 晶粒细化 裂纹扩展
下载PDF
Al-4.5Cu和Mullite增强Al-4.5Cu复合材料时效析出行为的DSC研究 被引量:3
7
作者 李伟 龙剑平 +2 位作者 沈保罗 高升吉 涂铭旌 《分析测试学报》 CAS CSCD 北大核心 2002年第1期8-11,共4页
用差示扫描量热法(DSC)对Al-4 5Cu合金和莫来石(Mullite)短纤维增强Al-4 5Cu复合材料的时效析出行为进行了研究 ;结果表明Al-4 5Cu合金和Mullite增强Al-4 5Cu复合材料固溶淬火试样的DSC扫描曲线存在较大不同 ,溶质原子富集区(GP)形成和... 用差示扫描量热法(DSC)对Al-4 5Cu合金和莫来石(Mullite)短纤维增强Al-4 5Cu复合材料的时效析出行为进行了研究 ;结果表明Al-4 5Cu合金和Mullite增强Al-4 5Cu复合材料固溶淬火试样的DSC扫描曲线存在较大不同 ,溶质原子富集区(GP)形成和溶解的信息在基体合金的DSC曲线上清晰可见 ,但在复合材料的DSC曲线上则很难确认 ,表明纤维推延或抑制了GP区的形成 ;中间沉淀析出相θ″和θ′的析出过程由于纤维的引入而得到明显加快 ,峰值温度降低 ,活化能减小 ,时效析出过程加快 ;但是 ,扫描参数选择不当时 ,容易对析出相的析出过程产生错误判断 ,应引起重视。 展开更多
关键词 差示扫描量热法 莫来石纤维 铝铜基复合材料 时效析出行为 DSC 铝铜合金 al-4.5cu合金
下载PDF
Al-4.5Cu合金半固态坯料制备研究 被引量:2
8
作者 谢世坤 易荣喜 +1 位作者 邓晓春 艾永平 《热加工工艺》 CSCD 北大核心 2010年第5期21-23,26,共4页
研究了稀土Ce对铝铜合金微观组织的影响以及Al4.5Cu合金半固态坯料的制备工艺。实验表明:在Al-4.5Cu合金中加入稀土Ce,细化了合金的微观组织,固液两相区间变窄,改善了合金的凝固性能。浇注温度和浇注方式对合金坯料制备也有明显的影响。... 研究了稀土Ce对铝铜合金微观组织的影响以及Al4.5Cu合金半固态坯料的制备工艺。实验表明:在Al-4.5Cu合金中加入稀土Ce,细化了合金的微观组织,固液两相区间变窄,改善了合金的凝固性能。浇注温度和浇注方式对合金坯料制备也有明显的影响。在700℃采用斜坡振动铜模水冷浇注可制备性能优良的稀土Al-4.5Cu半固态坯料,其组织为细小均匀的等轴球状晶,且制备工艺简单。 展开更多
关键词 al-4.5cu合金 稀土Ce 斜坡振动 微观组织
下载PDF
原位增强TiB_2/Al-4.5Cu复合材料的组织与力学性能 被引量:4
9
作者 梁艳峰 董晟全 杨通 《铸造技术》 EI CAS 北大核心 2004年第2期125-127,共3页
通过不同配比的混合盐体系 (K2 TiF6 KBF4 Na3 AlF6 Al 4.5Cu )制备原位增强TiB2 /Al 4.5Cu复合材料 ,分析该复合材料的凝固组织 ,测试其力学性能 ,并与基体合金进行对比。结果表明 :K2 TiF6 KBF4 Na3 AlF6在Al 4.5Cu合金熔体中能够反... 通过不同配比的混合盐体系 (K2 TiF6 KBF4 Na3 AlF6 Al 4.5Cu )制备原位增强TiB2 /Al 4.5Cu复合材料 ,分析该复合材料的凝固组织 ,测试其力学性能 ,并与基体合金进行对比。结果表明 :K2 TiF6 KBF4 Na3 AlF6在Al 4.5Cu合金熔体中能够反应生成弥散分布的TiB2 颗粒 ,从而起到细化和强化基体的作用。当K2 TiF6和KBF4混合物加入量w为基体的 2 0 %时 ,复合材料的力学性能最优 ,抗拉强度σb 达到 414 .3MPa ,伸长率δ为 4.2 % ,硬度HB为 13 2 ,分别比基体提高 5 4% ,3 5 % ,40 %。 展开更多
关键词 TiB2/al-4.5cu复合材料 原位 力学性能
下载PDF
Effects of grain refining and modification on mechanical properties and microstructures of Al-7.5Si-4Cu cast alloy 被引量:2
10
作者 刘光磊 司乃潮 +1 位作者 孙少纯 吴勤方 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第4期946-953,共8页
Al-7.5Si-4Cu cast alloy melt modified by Al-5Ti-B, RE and Al-10Sr master alloys were poured in the chromite sand moulds, to investigate comparatively the effects of individual or combined additions of grain refiners a... Al-7.5Si-4Cu cast alloy melt modified by Al-5Ti-B, RE and Al-10Sr master alloys were poured in the chromite sand moulds, to investigate comparatively the effects of individual or combined additions of grain refiners and modifiers on the mechanical properties, microstructures, grain refining and modification, and intermetallic compounds of the alloy. The results show that the mechanical properties and the microstructures of Al-7.5Si-4Cu cast alloys are improved immensely by combining addition of 0.8%Al-5Ti-B, 0.1%RE and 0.1%Al-10Sr grain refiners and modifiers compared with the individual addition and cast conditions. For individual addition condition, addition of 0.8%Al-5Ti-B master alloy can obtain superior tensile strength, Brinell hardness and finer equiaxedα(Al) dendrites. The alloy with 0.1%RE master alloy shows the highest improvement in ductility because the rare earth can purify the molten metal and change the shape of intermetallic compounds. While the alloy with 0.1%Al-10Sr modifier shows only good improvement in yield strength, and the improvement of other performance is unsatisfactory. The Al-10Sr modifier has a significant metamorphism for the eutectic silicon, but will make the gas content in the aluminum alloy melt increase to form serious columnar grain structures. The effects of grain refining and modification on mean area and aspect ratio have the same conclusions obtained in the mechanical properties and the microstructures analyses. 展开更多
关键词 al-7.5Si-4cu cast alloy grain refinement modification treatment mechanical properties MICROSTRUCTURES
下载PDF
La对定向凝固Al-4.5%Cu合金热疲劳性能的影响 被引量:3
11
作者 司乃潮 华雄飞 +2 位作者 司松海 袁婷婷 李达云 《铸造》 CAS CSCD 北大核心 2009年第3期262-265,共4页
采用自约束热疲劳试验机,对加入La的定向凝固Al-4.5%Cu合金进行热疲劳性能试验。结果表明,加入适量La对定向凝固Al-4.5%Cu合金的热疲劳性能有不同程度提高,其中,加入0.3%La的热疲劳试样疲劳性能较佳,达到热疲劳裂纹萌生所需的热疲劳循... 采用自约束热疲劳试验机,对加入La的定向凝固Al-4.5%Cu合金进行热疲劳性能试验。结果表明,加入适量La对定向凝固Al-4.5%Cu合金的热疲劳性能有不同程度提高,其中,加入0.3%La的热疲劳试样疲劳性能较佳,达到热疲劳裂纹萌生所需的热疲劳循环次数最多;通过热疲劳循环次数与主裂纹长度的动态关系图,发现热疲劳裂纹的扩展有别于一般由机械交变载荷造成的常温疲劳,呈现先快后慢,阶段性扩展。 展开更多
关键词 定向凝固 al-4.5%cu合金 热疲劳 热疲劳裂纹的萌生与扩展
下载PDF
试样尺寸对Al-4.5%Cu合金定向凝固组织和界面稳定性的影响 被引量:2
12
作者 蒋明伟 杜卫东 +2 位作者 宋长江 高玉来 翟启杰 《铸造》 EI CAS CSCD 北大核心 2007年第12期1307-1309,共3页
在传统Bridgeman方法下,利用Al-4.5%Cu合金内外同心嵌套试样,研究了自然对流对凝固过程及组织的影响。试验结果显示,温度梯度和抽拉速率均相同的定向凝固试样,尺寸较大试样的组织呈规则胞状或树枝状时,对应尺寸较小试样组织胞晶尖端发... 在传统Bridgeman方法下,利用Al-4.5%Cu合金内外同心嵌套试样,研究了自然对流对凝固过程及组织的影响。试验结果显示,温度梯度和抽拉速率均相同的定向凝固试样,尺寸较大试样的组织呈规则胞状或树枝状时,对应尺寸较小试样组织胞晶尖端发生分叉或杂乱树枝状,表明尺寸较小的试样液-固界面稳定性较差。较小试样尺寸限制了液相中自然对流致使溶质原子液-固界面处大量富集是凝固组织不规则与液-固界面不稳定的主要原因。 展开更多
关键词 自然对流 al-4.5%cu合金 定向凝固 凝固组织
下载PDF
强磁场与交变电流的复合作用对Al-4.5%Cu合金凝固组织的影响 被引量:2
13
作者 王俊 邓康 +4 位作者 任忠鸣 任维丽 李喜 钟云波 徐匡迪 《上海金属》 CAS 2006年第6期7-12,共6页
研究强磁场(0—10T)与工频(f=50Hz)交变电流(0-10A)的复合作用对Al-4.5mass%Cu合金凝固组织的影响。发现在施加垂直于磁场方向的交变电流时,会使电极间液态金属在电磁压力P作用下产生波动,导致合金凝固时枝晶组织的生长被打... 研究强磁场(0—10T)与工频(f=50Hz)交变电流(0-10A)的复合作用对Al-4.5mass%Cu合金凝固组织的影响。发现在施加垂直于磁场方向的交变电流时,会使电极间液态金属在电磁压力P作用下产生波动,导致合金凝固时枝晶组织的生长被打碎,出现等轴晶和颗粒状晶。在10T磁感应强度下,交变电流越大,波动越强,越易生成等轴晶和颗粒状晶;在10A交变电流下,磁感应强度增加到4T以后,等轴晶未随磁场的增加而完全转变成颗粒状晶;当P^→相同时,磁感应强度小的,容易出现等轴晶和颗粒状晶。 展开更多
关键词 强磁场 交流电 复合作用 al-4.5%cu合金 凝固组织
下载PDF
稀土元素和浇注温度对Al-4.5Cu合金初生相形貌的影响 被引量:1
14
作者 周全 陈乐平 尹健 《热加工工艺》 CSCD 北大核心 2011年第3期36-38,共3页
研究了不同稀土(RE)加入量和浇注温度对Al-4.5Cu合金初生相形貌的影响。结果表明:添加微量的RE并降低合金的浇注温度,可获得非枝晶组织的半固态Al-4.5Cu合金坯料;添加了0.5%RE的合金,随浇注温度的降低,其初生相由树枝晶转变成细小的球... 研究了不同稀土(RE)加入量和浇注温度对Al-4.5Cu合金初生相形貌的影响。结果表明:添加微量的RE并降低合金的浇注温度,可获得非枝晶组织的半固态Al-4.5Cu合金坯料;添加了0.5%RE的合金,随浇注温度的降低,其初生相由树枝晶转变成细小的球状晶粒;当浇注温度为660℃,随RE加入量的增加,合金的初生相由等轴枝晶转变成细小的蔷薇状晶体,最后转化为球状晶粒;未添加RE的合金,随浇注温度的下降,其初生相由发达的树枝晶转变成等轴枝晶。 展开更多
关键词 al-4.5cu合金 稀土元素 浇注温度
下载PDF
热电磁流体动力学对Al-4.5Cu合金定向凝固组织的影响 被引量:1
15
作者 刘晴 肖荔 +1 位作者 时海芳 张伟强 《铸造技术》 CAS 北大核心 2002年第6期330-331,共2页
在定向凝固条件下 ,施加横向磁场。当磁感应强度 <1T时 ,有磁场存在时的显微组织较无磁场时枝晶间距增大 ,且随磁感应强度的增大 ,枝晶间距增大 ,二次枝晶间臂变粗 ,这是热电磁流体动力学影响的结果。
关键词 al-4.5cu合金 定向凝固 液体流动 枝晶间距 热电磁流体动力学 铝合金
下载PDF
Microstructure and Wear Characteristics of Al-4.5Cu-5Pb Alloy
16
作者 Om Prakas Pandey(School of Basic and Applied Sciences, Thapar Institute of Engineering & Technology, Patiala-147001, India) 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 1998年第2期125-131,共7页
Al-4. 5Cu-5Pb alloy was prepared by sand and chill casting. The same alloy was also spray deposited at a gas pressure of 1.6 MPa. The microstructural features exhibit a coarse to fine dendritic morphology for sand ... Al-4. 5Cu-5Pb alloy was prepared by sand and chill casting. The same alloy was also spray deposited at a gas pressure of 1.6 MPa. The microstructural features exhibit a coarse to fine dendritic morphology for sand and chill cast alloys. Equiaxed grains were observed for spray formed alloys. Wear testing employing a pin-on-disc type set-up, reveals considerably lower wear of spray deposited alloy compared to that of chill and sand cast alloys. The morphological features of wear track on specimen and debris indicated a mixed oxidative-cum-adhesive wear mechanisms for these alloys tested in the present investigation. (Edited author abstract) 36 Refs. 展开更多
关键词 AL cu Microstructure and Wear Characteristics of al-4.5cu-5Pb alloy PB
全文增补中
Al-4.5 Cu柱状晶的顺流生长 被引量:1
17
作者 丁恒敏 《中国铸造装备与技术》 CAS 2007年第4期4-6,共3页
利用自行研制的电磁泵驱动液流定向凝固装置,在给定冷却条件下,系统地研究了液相流动对Al-4.5Cu合金柱状晶生长方向的影响。发现:低生长速度区,柱状晶以胞状生长方式顺流偏转;高生长速度区,柱状晶以枝晶方式生长,随液流速度由小增大,经... 利用自行研制的电磁泵驱动液流定向凝固装置,在给定冷却条件下,系统地研究了液相流动对Al-4.5Cu合金柱状晶生长方向的影响。发现:低生长速度区,柱状晶以胞状生长方式顺流偏转;高生长速度区,柱状晶以枝晶方式生长,随液流速度由小增大,经历了等轴晶生长、迎流生长、近垂直生长及顺流生长四种变化。 展开更多
关键词 al-4.5cu合金 柱状晶 顺流生长
下载PDF
Mullite/Al-4.5Cu复合材料的时效析出行为
18
作者 龙剑平 李伟 +3 位作者 景山 沈保罗 高升吉 涂铭旌 《四川大学学报(工程科学版)》 EI CAS CSCD 2001年第5期94-97,共4页
选用挤压铸造法制备mullite/Al - 4.5Cu复合材料 ,采用硬度测试 (HB)、差示扫描量热DSC、透射电镜(TEM)等手段研究了mullite/Al- 4.5Cu复合材料的时效特性。结果表明 :莫来石纤维的引入明显提高了基体合金的时效硬度 ,加速了基体合金的... 选用挤压铸造法制备mullite/Al - 4.5Cu复合材料 ,采用硬度测试 (HB)、差示扫描量热DSC、透射电镜(TEM)等手段研究了mullite/Al- 4.5Cu复合材料的时效特性。结果表明 :莫来石纤维的引入明显提高了基体合金的时效硬度 ,加速了基体合金的时效硬化速度 ,对GP区的形成有抑制作用 ,但没有改变基体合金的时效析出序列。复合材料具有和基体合金相似的时效硬化曲线。 展开更多
关键词 铝基复合材料 莫来石短纤维 al-cu合金 时效 Mullite/al-4.5cu合金 时效析出序列 时效硬度
下载PDF
原位增强铸造Al-4.5Cu复合材料的固溶与时效工艺
19
作者 董晟全 梁艳峰 杨通 《铸造技术》 CAS 北大核心 2004年第11期851-854,共4页
通过正交试验的方法,研究了固溶温度对时间、时效温度和时间对原位增强铸造Al 4.5Cu复合材料力学性能的影响,并分析其作用机理。结果表明,各因子对复合材料力学性能的影响由大到小依次为:固溶温度>时效温度>时效时间>固溶时间... 通过正交试验的方法,研究了固溶温度对时间、时效温度和时间对原位增强铸造Al 4.5Cu复合材料力学性能的影响,并分析其作用机理。结果表明,各因子对复合材料力学性能的影响由大到小依次为:固溶温度>时效温度>时效时间>固溶时间。固溶温度对复合材料的抗拉强度有显著影响;固溶温度、时效温度和时效时间对复合材料的伸长率和硬度都有显著影响。较优的固溶与时效工艺为:复合材料在533℃固溶12~16h,165℃时效7h。 展开更多
关键词 al-4.5cu 原位复合材料 固溶与时效
下载PDF
复合稀土对Al-4.5%Cu合金定向凝固组织及力学性能的影响
20
作者 崔联合 李达云 《铸造技术》 CAS 北大核心 2013年第12期1631-1633,共3页
对添加不同含量La、Ce复合稀土的Al-4.5%Cu合金定向凝固微观组织进行了分析研究,并测定了试样的力学性能。结果表明:添加复合稀土的试样,其热裂纹、缩松缺陷明显减少。当添加0.22%的复合稀土时,试样定向凝固组织不明显,枝晶本身也不能... 对添加不同含量La、Ce复合稀土的Al-4.5%Cu合金定向凝固微观组织进行了分析研究,并测定了试样的力学性能。结果表明:添加复合稀土的试样,其热裂纹、缩松缺陷明显减少。当添加0.22%的复合稀土时,试样定向凝固组织不明显,枝晶本身也不能得到细化,但能得到互相交错的树枝晶。与不加稀土试样相比,添加复合稀土的试样抗拉强度和伸长率都有一定程度的提高,添加量超过0.30%时,效果比较明显。当复合稀土加入量达到0.40%时,能得到比较理想的定向凝固组织,试样的抗拉强度达到194.65 MPa,伸长率为12.71%,弹性模量为0.170 MPa。 展开更多
关键词 复合稀土 定向凝固 A1 4 5%cu合金 凝固组织 枝晶间距