均匀化处理对航空用Al-8.5Zn-2.3Cu-2.2Mg合金相组织的影响 被引量:2
1
作者 祝贞凤 隋信举 +2 位作者 杨丽娟 汪洪波 史春丽 《材料热处理学报》 EI CAS CSCD 北大核心 2018年第1期20-26,共7页
通过扫描电镜和透射电镜观察,研究了单级和双级均匀化工艺对铸态Al-8.5Zn-2.3Cu-2.2Mg(mass%)合金相组织的影响。结果表明:经465℃×(12~36 h)单级均匀化处理,残留相仍然较多;经430℃×12 h+470℃×24 h、465℃×... 通过扫描电镜和透射电镜观察,研究了单级和双级均匀化工艺对铸态Al-8.5Zn-2.3Cu-2.2Mg(mass%)合金相组织的影响。结果表明:经465℃×(12~36 h)单级均匀化处理,残留相仍然较多;经430℃×12 h+470℃×24 h、465℃×24 h+475℃×12 h双级均匀化处理,残留相的数量显著减少,465℃×24 h+475℃×12 h处理残留相更少;465℃×24 h单级均匀化处理残留相主要为Al_2CuMg,少量Al7Cu2Fe,经430℃×12 h+470℃×24 h、465℃×24 h+475℃×12 h处理除还有少量Al(ZnMgCu)相没溶外,没有发现Al2CuMg;此外,430℃×12 h+470℃×24 h双级均匀化处理相比于465℃×24 h单级处理,有利于析出弥散、均匀的Al3Zr粒子。 展开更多
关键词 al-8 5zn-2 3Cu-2 2mg合金 微观组织 均匀化退火 金属间化合物
下载PDF
Microstructure of Mg-8Zn-4Al-1Ca aged alloy 被引量:1
2
作者 董允 林小娉 +2 位作者 叶杰 郑润国 何娜 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第2期310-315,共6页
The microstructure of Mg-8Zn-4Al-1Ca aged alloy was investigated by TEM and HRTEM. The results show that the hardening produced in the Mg-8Zn-4Al-1Ca alloy is considerably higher than that in the Mg-8Zn-4A1 alloy. A d... The microstructure of Mg-8Zn-4Al-1Ca aged alloy was investigated by TEM and HRTEM. The results show that the hardening produced in the Mg-8Zn-4Al-1Ca alloy is considerably higher than that in the Mg-8Zn-4A1 alloy. A dense dispersion of disc-like Ca2Mg6Zn3 precipitates are formed in Mg-8Zn-4Al-1Ca alloy aged at 160 ℃ for 16 h. In addition, the lattice distortions, honeycomb-looking Moir&#233; fringes, edge dislocations and dislocation loop also exist in the microstructure. The precipitates of alloy aged at 160 ℃ for 48 h are coarse disc-like and fine dispersed grainy. When the alloy is subjected to aging at 160 ℃ for 227 h, the microstructure consists of numerous MgZn2 precipitates and Ca2Mg6Zn3 precipitates. All the analyses show that Ca is a particularly effective trace addition in improving the age-hardening and postponing the formation of MgZn2 precipitates in Mg-8Zn-4Al alloy aged at 160 ℃. 展开更多
关键词 mg-8zn-4al-1 Ca alloy age hardening Ca2mg6Zn3 Moire fringe