Semi-solid gravity sand casting using gas induced semi-solid process 被引量:3
1
作者 T.CHUCHEEP R.BURAPA +2 位作者 S.JANUDOM S.WISUTMETHANGOON J.WANNASIN 《中国有色金属学会会刊:英文版》 CSCD 2010年第S3期981-987,共7页
The semi-solid metal forming using high pressures has been applied for several years.In contrast,low pressure casting,such as gravity sand casting,has not been widely studied even though it may help reduce porosity de... The semi-solid metal forming using high pressures has been applied for several years.In contrast,low pressure casting,such as gravity sand casting,has not been widely studied even though it may help reduce porosity defects and offer a better casting yield.A semi-solid gravity sand casting process using the Gas Induced Semi-Solid process was investigated.The results show that the process can produce complete parts with no observable defects.The ultimate tensile strength and elongation data of semi-solid cast samples are higher than those of the liquid cast samples.In addition,the semi-solid sand casting process gives a better casting yield.It can be concluded that the semi-solid sand casting of an aluminum alloy using the GISS process is a feasible process. 展开更多
关键词 GRAVITY SAND CASTING SEMI-SOLID SAND CAST al7si0.3mgfe GAS induced SEMI-SOLID
下载PDF
Al7Si0.3Mg-Y合金半固态初生α-Al形貌的研究
2
作者 刘政 胡咏梅 《江西理工大学学报》 CAS 2007年第3期1-5,共5页
利用低过热度浇注工艺制备了Al7Si0.3Mg-Y铝合金半固态浆料,研究了稀土Y对合金半固态初生α-Al形貌的影响.采用正交设计方法,优化了Al7Si0.3Mg-Y铝合金半固态初生α-Al形貌的影响因素,通过直观分析与方差分析表明,经稀土Y变质处理及低... 利用低过热度浇注工艺制备了Al7Si0.3Mg-Y铝合金半固态浆料,研究了稀土Y对合金半固态初生α-Al形貌的影响.采用正交设计方法,优化了Al7Si0.3Mg-Y铝合金半固态初生α-Al形貌的影响因素,通过直观分析与方差分析表明,经稀土Y变质处理及低过热度浇注获得Al7Si0.3Mg-Y半固态初生球晶的最佳工艺条件为:浇注温度595℃,保温时间3min,Y加入量0.5%.此时其晶粒在铸态下的形状因子为0.74等效圆直径为42.01μm,其中浇注温度是晶粒形貌和尺寸的最主要影响因素,可信度达到95%;其次是Y的加入量和保温时间. 展开更多
关键词 稀土Y 半固态 Al7Si0.3Mg合金 初生μ-Al 正交设计
下载PDF
Refining mechanism of yttrium on primary α-Al in semi-solid Al alloy 被引量:5
3
作者 Zheng LIU Yongmei HU Xiaomei LIU 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2010年第4期277-284,共8页
Semi-solid Al7Si0.3Mg alloy slurry, which is grain-refined by yttrium, is manufactured by low temperature pouring. The effects of grain-refined by yttrium on the morphology and the grain size of the primary α-Al in s... Semi-solid Al7Si0.3Mg alloy slurry, which is grain-refined by yttrium, is manufactured by low temperature pouring. The effects of grain-refined by yttrium on the morphology and the grain size of the primary α-Al in semi-solid Al7Si0.3Mg alloy are researched. The results indicate that semi-solid Al7Si0.3Mg alloy with particle-like and rosette-like primary α-Al can be prepared by low temperature pouring from liquid Al7Si0.3Mg alloy grain-refined by yttrium. The grain size and particle morphology of primary α-Al in Al7Si0.3Mg alloy are markedly improved by 0.5 wt pet Y. The refining mechanism of Y on the morphology and the grain size of the primary α-Al in semi-solid Al7Si0.3Mg alloy are delved. 展开更多
关键词 SEMI-SOLID YTTRIUM Al7Si0.3Mg alloy Refining mechanism
原文传递
添加Yb和Zr对Al7Si0.3Mg合金组织及力学性能的影响
4
作者 吉全鑫 杜景红 +5 位作者 张艺杰 李玉章 冯炜光 孙彦华 严继康 甘国友 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2022年第10期3580-3587,共8页
研究了添加Yb和Zr元素对Al7Si0.3Mg合金组织及力学性能的影响,以及细化变质机理。结果表明,Yb、Zr元素的添加明显细化了α-Al基体,使其从粗大的树枝状晶转变为细小的花瓣状晶,晶粒尺寸明显减小,并且使共晶硅由粗大的针状变质为短棒状,... 研究了添加Yb和Zr元素对Al7Si0.3Mg合金组织及力学性能的影响,以及细化变质机理。结果表明,Yb、Zr元素的添加明显细化了α-Al基体,使其从粗大的树枝状晶转变为细小的花瓣状晶,晶粒尺寸明显减小,并且使共晶硅由粗大的针状变质为短棒状,这是由于Yb、Zr吸附在孪晶凹槽处(TPRE)改变共晶硅生长方式,最终改变共晶硅形貌;经热处理(T6)后,大量析出的Al_(3)(Yb,Zr)粒子起到了沉淀强化进而细化晶粒的作用。当Yb质量分数为0.3%、Zr质量分数为0.25%时,合金(T6)的抗拉强度和延伸率为296.3 MPa和9.2%,较未细化变质的合金分别提高了17%和1.1倍。 展开更多
关键词 Al7Si0.3Mg YB ZR 微观组织 力学性能 细化变质机理