期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
Solubility of ammonium paratungstate in the system NH_3·H_2O·H_2O 被引量:3
1
作者 WAN Linsheng, XU Zhifeng, and SHI ZhonglingFaculty of Materials and Chemical Engineering, Southern Institute of Metallurgy, Ganzhou 341000, China 《Rare Metals》 SCIE EI CAS CSCD 2003年第1期10-13,18,共5页
The equilibrium solubilities of 5(NH4)O·12WO3·5H2O (APT·5H2O) were determined at the terminal ammonia concentration of 2 mol/L at 87-95℃. Experimental data were regressed. The linear functional relatio... The equilibrium solubilities of 5(NH4)O·12WO3·5H2O (APT·5H2O) were determined at the terminal ammonia concentration of 2 mol/L at 87-95℃. Experimental data were regressed. The linear functional relation between the solubility of APT- 5H2O and the temperature (t /℃) is given as y = - 588.08 + 7.28t. The solubility of the species as a function of the terminal ammonia concentration (x / mol · L-1) is also achieved: y = 36.76 + 18.86x. The solubility of APT · 5H2O produced by ion-exchange method in China is much lower, which is due to much lower silica, much higher NH4Cl, and a small amount of APT · 7H2O with low solubility in the APT crystals. APT · 7H2O forms because of a large amount of NH4Cl and the low activity of water in the crystallization. 展开更多
关键词 HYDROMETALLURGY ammonium paratungstate (APT) regressive analysis SOLUBILITY
下载PDF
Cleaner production of ammonium paratungstate by membrane electrolysis-precipitation of sodium tungstate solution
2
作者 Afolabi Uthmon Olayiwola Hao Du +3 位作者 Shao-Na Wang Biao Liu Ye-Qing Lv Bo Pan 《Tungsten》 EI CSCD 2023年第1期145-159,共15页
The production of ammonium paratungstate(APT) is riddled with the generation of wastewater,which causes environmental problems.To solve the problem of wastewater generation at source,a membrane electrolysis-NH3·H... The production of ammonium paratungstate(APT) is riddled with the generation of wastewater,which causes environmental problems.To solve the problem of wastewater generation at source,a membrane electrolysis-NH3·H2O precipitation method,which prevents wastewater generation and recycles the reagents used in the process,was proposed and investigated in this study.The electrolysis process was investigated based on parameters such as initial cathodic and anodic NaOH concentrations,and current density.The results showed that an increase in current density and initial cathodic NaOH concentration and a decrease in the initial anodic NaOH concentration would enhance the separation of tungsten and sodium.The optimum condition was found at a current density of 666 A·m^(-2),initial anodic and cathodic NaOH concentrations of 69 g·L^(-1) and 40 g·L^(-1),with a current efficiency of 75.40%,and energy consumption for producing 1 ton of NaOH was 2184 kW·h.The precipitation process was investigated based on the acidic high W/Na molar ratio solution obtained by the electrolysis process with NH3·H2O as the precipitant.Parameters such as excessive coefficient,temperature,and W/Na molar ratio were studied.The result showed that the variation of excessive coefficient and solution temperature had an opposite effect on the purity of the APT,while an increase in the W/Na molar ratio would increase the product purity.The precipitation product obtained had a purity of 99.6% and was characterized using X-ray diffraction,inductively coupled plasma,and scanning electron microscopy.The methods proposed in this study could provide fundamental information for the design of a cleaner APT production process. 展开更多
关键词 Membrane electrolysis ammonium paratungstate Separation of sodium and tungsten ions Ion states of tungsten Cleaner production