BaCe_(0.9)Nd_(0.1)O_(3-δ)柠檬酸盐法合成、表征及其在中温区的电导率 被引量:8
1
作者 刘瑞泉 宿新泰 +3 位作者 王吉德 岳凡 谢亚红 胡云霞 《无机化学学报》 SCIE CAS CSCD 北大核心 2004年第1期57-60,共4页
A precursor of BaCe 0.9 Nd 0.1 O 3-δ solid electrolyte was synthesized by the sol-gel method and sintered at14 00℃.The obtained gels and powder were characterized by differential and ther mogravimetric thermal analy... A precursor of BaCe 0.9 Nd 0.1 O 3-δ solid electrolyte was synthesized by the sol-gel method and sintered at14 00℃.The obtained gels and powder were characterized by differential and ther mogravimetric thermal analysis(TG-DTA),X-ray diffraction(XRD),transmissi on electron microscopy(TEM).Using the sintered samples as solid electrolyte a nd silver-palladium alloy as electrodes,electrical conductivities under differ ent gas ambiences at intermediate temperature(400~600℃)were measured. In moist hydrogen atmosphere,the conduction is a little higher than that of dry hydrogen atmosphere.In hydrogen atmosphere,proton conduction may predominate ,leading to an increase in conductivity and a decrease in activation energy. 展开更多
关键词 bace0.9Nd0.1o3-δ 柠檬酸盐法 合成 表征 中温区 电导率 溶胶-凝胶法 高温质子导体 钕铈钡复合氧化物
下载PDF
多层膜结构BaCe_(0.9)Nd_(0.1)O_(3-δ)的制备及其在常压合成氨中的应用 被引量:2
2
作者 张蔚 宿新泰 刘瑞泉 《中国稀土学报》 CAS CSCD 北大核心 2006年第z1期102-106,共5页
用干压法制备了Ni-BaCe0.9Nd0.1O3-δ多孔金属陶瓷阳极,并在阳极基膜上制备出致密的BaCe0.9Nd0.1O3-δ固体电解质薄膜。薄膜的厚度约为40μm,致密均匀。测定了多层膜结构BaCe0.9Nd0.1O3-δ在干燥氮气/湿润氢气气氛中的电导率,结果表明... 用干压法制备了Ni-BaCe0.9Nd0.1O3-δ多孔金属陶瓷阳极,并在阳极基膜上制备出致密的BaCe0.9Nd0.1O3-δ固体电解质薄膜。薄膜的厚度约为40μm,致密均匀。测定了多层膜结构BaCe0.9Nd0.1O3-δ在干燥氮气/湿润氢气气氛中的电导率,结果表明其电导率要比厚膜BaCe0.9Nd0.1O3-δ和SrCe0.95Y0.05O3-δ(SCY)要高。将多层膜材料用于固态质子传导电池中,在常压下以氮气和氢气为原料合成了氨气。结果表明,与SCY固体电解质比较,氨的产率提高了一个数量级以上。 展开更多
关键词 高温质子导体 bace0.9Nd0.1o3-δ 氨合成 多层膜 稀土
下载PDF
BaCe_(0.9)Y_(0.1)O_(3-α)固体氧化物燃料电池电极极化性能的研究 被引量:1
3
作者 石慧 马桂林 +2 位作者 贾定先 仇立干 陈蓉 《苏州大学学报(自然科学版)》 CAS 2002年第2期90-95,共6页
以BaCe0.9Y0.1O3-α氧化物陶瓷为固体电解质,以多孔性Pt为电极材料,组成氢-空气燃料电池,用电流遮断法分别测定了600℃~1000℃范围燃料电池输出电流时的欧姆电位降和正负极的电极极化 结果表明,该燃料电池的优良性能与Pt电极很小的极... 以BaCe0.9Y0.1O3-α氧化物陶瓷为固体电解质,以多孔性Pt为电极材料,组成氢-空气燃料电池,用电流遮断法分别测定了600℃~1000℃范围燃料电池输出电流时的欧姆电位降和正负极的电极极化 结果表明,该燃料电池的优良性能与Pt电极很小的极化作用密切相关,正负极的电极极化皆随着温度的升高而变小。 展开更多
关键词 极化性能 bace0.9Y0.1o3 固体氧化物 燃料电池 质子导体 放电性能 电流遮断法 -空气燃料电池
下载PDF
BaCe_(0.5)Zr_(0.4)Y_(0.1)O_(3-α)的溶胶-凝胶法制备及其电性能 被引量:2
4
作者 汪洁 丁伟中 +2 位作者 方建慧 朱冬冬 吴敏艳 《中国稀土学报》 CAS CSCD 北大核心 2005年第4期449-454,共6页
采用溶胶-凝胶法,以低于固相合成法150~250℃的温度进行烧结,分别制备了BaCe0.9Y0.1O3-α和BaCe0.5Zr0.4Y0.1O3-α固体电解质。应用AUTOLABPGSTA30型电化学工作站测定了两种电解质在不同温度下的阻抗谱,在350~800℃范围内电导率分别为1.... 采用溶胶-凝胶法,以低于固相合成法150~250℃的温度进行烧结,分别制备了BaCe0.9Y0.1O3-α和BaCe0.5Zr0.4Y0.1O3-α固体电解质。应用AUTOLABPGSTA30型电化学工作站测定了两种电解质在不同温度下的阻抗谱,在350~800℃范围内电导率分别为1.62×10-4~6.43×10-3S.cm-1,2.52×10-5~3.73×10-3S.cm-1,电导激活能分别为0.54和0.84eV。同时用高温固相合成法合成了BaCe0.9Y0.1O3-α质子导体,在相同条件下其电导率为1×10-4~4×10-3S.cm-1,激活能为0.50eV。实验结果表明:用溶胶-凝胶法得到的材料在烧结温度低于固相合成法150~250℃的情况下,制备出的样品电导率高;对于同一质子导体BaCe0.9Y0.1O3-α,用Zr代替部分Ce,固体电解质的电导率明显降低。 展开更多
关键词 bace0.9-xzrxy0.1o3-α 固体电解质 溶胶-凝胶法 电导率 激活能 固相合成法 稀土
下载PDF
纳米粉体(CeO_2)_(0.9-x)(GdO_(1.5))_x(Sm_2O_3)_(0.1)的溶胶-凝胶低温燃烧合成 被引量:19
5
作者 黎大兵 胡建东 +4 位作者 连建设 张秀燕 陈积伟 郭作兴 王红颖 《硅酸盐学报》 EI CAS CSCD 北大核心 2001年第4期340-343,共4页
采用溶胶 -凝胶法与低温燃烧法相结合 ,合成了 (CeO2 ) 0 .9-x(GdO1 .5 ) x(Sm2 O3) 0 .1 系列粉体 .结果表明 :由硝酸盐与柠檬酸混合形成的凝胶 ,可在较低温度 (2 0 0~ 3 0 0℃ )点火并燃烧 ,其火焰温度达 90 0℃以上 .经TEM ,XRD测... 采用溶胶 -凝胶法与低温燃烧法相结合 ,合成了 (CeO2 ) 0 .9-x(GdO1 .5 ) x(Sm2 O3) 0 .1 系列粉体 .结果表明 :由硝酸盐与柠檬酸混合形成的凝胶 ,可在较低温度 (2 0 0~ 3 0 0℃ )点火并燃烧 ,其火焰温度达 90 0℃以上 .经TEM ,XRD测试 ,燃烧后即直接形成了粒径为 2 0~ 3 0nm ,具有萤石结构的单相粉体 ,由该粉体制备的固体电解质在中温下电导率为 5 .8× 10 - 2 S/cm ,组装的单个H2 -O2 燃料电池最大功率密度达 70mW 展开更多
关键词 溶胶-凝胶法 低温燃烧 氧化铈 固体电解质 纳米粉体 合成 (Ceo2)0.9-x(Gdo1.5)x(Sm2o3)0.1
下载PDF
CuO掺杂SrFe_(0.9)Sn_(0.1)O_(3-δ)负温度系数厚膜热敏电阻的电学性能 被引量:3
6
作者 袁昌来 巫秀芳 +4 位作者 刘心宇 黄静月 李擘 梁梅芳 莫崇贵 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2011年第4期387-392,共6页
采用印刷法制备了CuO掺杂SrFe0.9Sn0.1O3-δ(CSFS)厚膜负温度系数(NTC)热敏电阻(掺杂量为20mol%~50mol%).对其微观结构及电性能研究发现:随着CuO掺杂含量的增加,厚膜表面变得更加致密,室温电阻逐渐降低至0.46 M?,而热敏常数基... 采用印刷法制备了CuO掺杂SrFe0.9Sn0.1O3-δ(CSFS)厚膜负温度系数(NTC)热敏电阻(掺杂量为20mol%~50mol%).对其微观结构及电性能研究发现:随着CuO掺杂含量的增加,厚膜表面变得更加致密,室温电阻逐渐降低至0.46 M?,而热敏常数基本保持在3300K附近.CuO的加入导致SrFe0.9Sn0.1O3-δ分裂成多种铁含量更低的SrFe1-xSnxO3-δ物相(0. 展开更多
关键词 SrFe0.9Sn0.1o3-δ 厚膜NTC热敏电阻 CUo 阻抗分析
下载PDF
中温SOFCLa_(0.9)Sr_(0.1)Ga_(0.8)Mg_(0.2)O_(3-δ)固体电解质的电性能研究 被引量:4
7
作者 张乃庆 孙克宁 +1 位作者 吴宁宁 周德瑞 《人工晶体学报》 EI CAS CSCD 北大核心 2004年第3期354-357,共4页
采用固相反应法制备了La0 .9Sr0 .1Ga0 .8Mg0 .2 O3 -δ(LSGM)固体电解质 ,XRD测试表明 ,经 15 0 0℃煅烧 2 4h后得到LSGM单相结构 ,采用交流阻抗测试技术对La0 .9Sr0 .1Ga0 .8Mg0 .2 O3 -δ的电性能进行了研究 ,结果表明La0 .9Sr0 .1Ga... 采用固相反应法制备了La0 .9Sr0 .1Ga0 .8Mg0 .2 O3 -δ(LSGM)固体电解质 ,XRD测试表明 ,经 15 0 0℃煅烧 2 4h后得到LSGM单相结构 ,采用交流阻抗测试技术对La0 .9Sr0 .1Ga0 .8Mg0 .2 O3 -δ的电性能进行了研究 ,结果表明La0 .9Sr0 .1Ga0 .8Mg0 .2 O3 -δ低温区电导率主要取决于晶界电导 ;而在高温区电导率主要取决于晶粒电导。低温下导电率激活能较高为 1.0 9eV ,高温的激活能较低为 0 .8eV。 展开更多
关键词 固体电解质 电性能 SoFCLa0.9Sr0.1Ga0.8Mg0.2o3-δ 固相反应法 燃料电池
下载PDF
Ba_(0.98)Ce_(0.9)Y_(0.1)O_(3-α)固体电解质的离子导电性 被引量:5
8
作者 马桂林 陈蓉 仇立干 《功能材料》 EI CAS CSCD 北大核心 2002年第4期418-419,421,共3页
用高温固相反应法制备了非化学计量性固体电解质Ba0 .98Ce0 .9Y0 .1O3 -α,分别用氢浓差电池及氧浓差电池方法研究了在 60 0~ 10 0 0℃范围Ba0 .98Ce0 .9Y0 .1O3 -α的离子导电特性。结果表明 ,Ba0 .98Ce0 .9Y0 .1O3 -α固体电解质在... 用高温固相反应法制备了非化学计量性固体电解质Ba0 .98Ce0 .9Y0 .1O3 -α,分别用氢浓差电池及氧浓差电池方法研究了在 60 0~ 10 0 0℃范围Ba0 .98Ce0 .9Y0 .1O3 -α的离子导电特性。结果表明 ,Ba0 .98Ce0 .9Y0 .1O3 -α固体电解质在氢气气氛中几乎为纯质子导体 。 展开更多
关键词 Ba0.98Ce0.9Y0.1o3 固体电解质 离子导电性 钙钛矿型氧化物 质子导体
下载PDF
La_(0.7)Sr_(0.3-x)Ca_xCo_(0.9)Fe_(0.1)O_(3-δ)的柠檬酸盐法制备和性能 被引量:4
9
作者 于洪浩 高文元 孙俊才 《稀土》 EI CAS CSCD 北大核心 2005年第4期1-5,9,共6页
采用柠檬酸盐法合成了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-δ(LSCCF,x=0.05,0.1,0.15和0.2)粉料。TG-DSC分析表明,凝胶在320℃~558℃分解为相应的氧化物。XRD测试表明:产物前躯体在800℃下热处理3h就可制备出具有畸变钙钛矿结构的LSCCF粉料。... 采用柠檬酸盐法合成了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-δ(LSCCF,x=0.05,0.1,0.15和0.2)粉料。TG-DSC分析表明,凝胶在320℃~558℃分解为相应的氧化物。XRD测试表明:产物前躯体在800℃下热处理3h就可制备出具有畸变钙钛矿结构的LSCCF粉料。电导率测试表明,随着烧结温度的升高和Sr2+含量的增加,样品电导率变大,其导电活化能变小。在600℃~800℃范围内,LSCCF样品的电导率为102S/cm^103S/cm,能够满足中温固体氧化物燃料电池阴极材料的要求。LSCCF粉料与Ce0.8Sm0.2O2电解质在800℃下烧结10h后没有新相生成,表明LSCCF粉料与Ce0.8Sm0.2O2电解质具有良好的化学相容性。 展开更多
关键词 La0.7Sr0.3-xCaxCo0.9Fe0.1o3-δ 柠檬酸盐法 阴极材料 电导率
下载PDF
Ba_(0.95)Ce_(0.9)Y_(0.1)O_(3-α)固体氧化物的离子导电性及其燃料电池性能 被引量:3
10
作者 马桂林 贾定先 +2 位作者 仇立干 石慧 陈蓉 《电化学》 CAS CSCD 2002年第3期321-326,共6页
以Ba0 .95Ce0 .9Y0 .1O3-α氧化物陶瓷为固体电解质 ,以多孔性Pt为电极材料 ,分别组成氢、氧浓差电池和氢_空气燃料电池 ,测定了 6 0 0~ 10 0 0℃范围内的浓差电池电动势 ,燃料电池的放电性能和电极极化性能 .结果表明 ,Ba0 .95Ce0 .9Y... 以Ba0 .95Ce0 .9Y0 .1O3-α氧化物陶瓷为固体电解质 ,以多孔性Pt为电极材料 ,分别组成氢、氧浓差电池和氢_空气燃料电池 ,测定了 6 0 0~ 10 0 0℃范围内的浓差电池电动势 ,燃料电池的放电性能和电极极化性能 .结果表明 ,Ba0 .95Ce0 .9Y0 .1O3-α在氢气氛中几乎是一个纯质子导体 ,在氧气氛中是氧离子与电子空穴的混合导体 ,氧离子迁移数在 0 .3~ 0 .5之间 ,在氢_空气燃料电池条件下显示出混合离子 (质子 +氧离子 )导电性 ,总离子迁移数大于 0 .9.该燃料电池性能良好 ,Pt电极极化性能很小 ,最大输出电流密度为 6 80mA·cm- 2 (10 0 0℃ ) ,最大输出功率密度为 16 0mW·cm- 2 (10 0 0℃ ) . 展开更多
关键词 离子导电性 性能 复合氧化物 Ba0.95Ce0.9Y0.1o3 固体氧化物燃料电池 质子导体 氧化物陶瓷 电极材料
下载PDF
共沉淀法合成La_(0.7)Sr_(0.3-x)Ca_xCo_(0.9)Fe_(0.1)O_(3-)及其性能表征 被引量:5
11
作者 于洪浩 高文元 孙俊才 《电源技术》 CAS CSCD 北大核心 2005年第8期496-498,522,共4页
以金属硝酸盐、氨水为沉淀剂,采用化学共沉淀法合成了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-"(简称LSCCF,x=0.05,0.10,0.15,0.20)粉料。借助差示扫描量热法-热重分析法(DSC-TG)、X射线衍射法(XRD)和扫描电子显微镜法(SEM)对600℃,800℃,100... 以金属硝酸盐、氨水为沉淀剂,采用化学共沉淀法合成了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-"(简称LSCCF,x=0.05,0.10,0.15,0.20)粉料。借助差示扫描量热法-热重分析法(DSC-TG)、X射线衍射法(XRD)和扫描电子显微镜法(SEM)对600℃,800℃,1000℃热处理4h后LSCCF粉料的形成过程、晶体结构和粒度形貌进行了研究。实验结果表明,LSCCF粉料的形成过程分为4个阶段——脱水阶段、分解阶段、LaCoO3基氧化物形成阶段和LSCCF固溶体形成阶段;适宜热处理制度为800℃下保温4h,且制备出的LSCCF粉料为均一的钙钛矿结构。使用直流四极探针法测定了LSCCF样品在空气气氛下的电导率,发现该体系材料在600~800℃范围的电导率都超过了250S·cm-1,其导电机制符合p型小极化子绝热孔隙理论,且能够满足中温固体氧化物燃料电池(ITSOFC)阴极材料的要求。 展开更多
关键词 中温固体氧化物燃料电池 阴极材料 La0.7Sr0.3-aCo0.9Fe0.1o3-δ 化学共沉淀法 电导率
下载PDF
SrTi_(0.9)M_(0.1)O_(3-δ)钙钛矿型氧化物催化剂甲烷氧化偶联反应性能的研究 被引量:2
12
作者 缪建文 范以宁 +1 位作者 金永漱 陈懿 《无机化学学报》 SCIE CAS CSCD 北大核心 2003年第11期1257-1260,共4页
The structure and catalytic properties of SrTi0.9M0.1O3- δ (M=Mg,Al, Zr) perovskite type catalysts for oxidative coupling of methane (OCM) have been studied by using X ray diffraction (XRD),X ray photoelectron spectr... The structure and catalytic properties of SrTi0.9M0.1O3- δ (M=Mg,Al, Zr) perovskite type catalysts for oxidative coupling of methane (OCM) have been studied by using X ray diffraction (XRD),X ray photoelectron spectroscopy (XPS) and temperature programmed desorption of oxygen(O2 TPD) methods. It has been shown that doping the cations of lower valence (e.g. Mg2+ , Al3+ ) to the B site of SrTi0.9M0.1O3- δ perovskite type catalysts results in the higher content of adsorbed oxygen species on the surface of catalysts and thus higher C2 selectivity for OCM reaction. It is suggested that the oxygen vacancies of SrTi0.9M0.1O3- δ (M=Mg, Al, Zr) perovskite type catalysts are the sites responsible for oxygen activation, and the adsorbed oxygen species on the surface of SrTi0.9M0.1O3- δ catalysts are the main active species for OCM reaction. 展开更多
关键词 SrTi0.9M0.1o3-δ 钙钛矿型氧化物 催化剂 甲烷 氧化偶联反应 性能 氧空位 吸附氧
下载PDF
共沉淀和低温燃烧法制备Sr_(0.9)Ce_(0.9)Y_(0.1)O_(3-δ)陶瓷粉及性能 被引量:3
13
作者 孟波 谭小耀 孟秀霞 《硅酸盐通报》 CAS CSCD 北大核心 2007年第6期1129-1135,共7页
分别采用基于Pechini法的溶胶低温燃烧法和共沉淀法制备了Sr_(0.9)Ce_(0.9)Y_(0.1)O_(3-δ)(SCY)超细陶瓷粉。应用X射线衍射、扫描电镜、能量散射谱和激光粒度分析仪对陶瓷粉体的结构和组成进行了表征,并研究了两种方法制备的粉体的烧... 分别采用基于Pechini法的溶胶低温燃烧法和共沉淀法制备了Sr_(0.9)Ce_(0.9)Y_(0.1)O_(3-δ)(SCY)超细陶瓷粉。应用X射线衍射、扫描电镜、能量散射谱和激光粒度分析仪对陶瓷粉体的结构和组成进行了表征,并研究了两种方法制备的粉体的烧结性能。结果表明:用溶胶低温燃烧法制备的SCY粉体为近似球形、粒径小于50nm,粒度分布范围窄,在1250℃烧结致密;用共沉淀法制备的粉体具有钙钛矿结构,粒径小于0.25μm、粒度分布窄,在1300℃烧结致密。此外,SCY致密膜具有一定的透氢作用,850℃氢渗速率在2×10-3mL.cm-2.min-1左右。 展开更多
关键词 固体电解质 Sr0.9Ce0.9V0.1o3-δ 陶瓷粉 透氢
下载PDF
微波固相烧结制备La_(0.7)Sr_(0.3-x)Ca_xCo_(0.9)Fe_(0.1)O_(3-δ)阴极材料及性能表征 被引量:3
14
作者 高文元 孙俊才 于洪浩 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2005年第11期1738-1742,共5页
以碳酸盐和氧化物为原料,采用微波固相烧结法制备了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-δ(简称:LSCCF,x=0.05,0.10,0.15和0.20)粉料.用XRD和SEM对LSCCF粉料的晶体结构和颗粒形貌进行了研究.结果表明:微波固相反应在1200℃下烧结0.5 h便可以... 以碳酸盐和氧化物为原料,采用微波固相烧结法制备了La0.7Sr0.3-xCaxCo0.9Fe0.1O3-δ(简称:LSCCF,x=0.05,0.10,0.15和0.20)粉料.用XRD和SEM对LSCCF粉料的晶体结构和颗粒形貌进行了研究.结果表明:微波固相反应在1200℃下烧结0.5 h便可以形成密度为5.366 g/cm3,晶粒尺寸小于500 nm钙钛矿结构的粉料.而常规固相反应法在1300℃下烧结7 h只形成了密度为3.426 g/cm3,晶粒尺寸小于2000 nm钙钛矿结构的粉料.电导率测量结果表明:随着烧结温度的升高和Sr2+含量的增加,LSCCF样品的电导率变大,600℃~800℃范围内微波烧结制备的La0.7Sr0.15Ca0.15Co0.9Fe0.1O3-δ样品的电导率最小值为672 S/cm,且高于常规固相烧结制备的相同组成样品的电导率最小值425 S/cm.LSCCF粉料与Ce0.8Sm0.2O2电解质的混合物在800℃下烧结10 h后没有新相生成,表明LSCCF粉料与Ce0.8Sm0.2O2电解质具有良好的化学相容性. 展开更多
关键词 微波固相烧结 La0.7Sr0.3-xCaxCo0.9Fe0.1o3-δ 电导率 化学相容性
下载PDF
Ta掺杂对BaCe_(0.8)In_(0.1)Y_(0.1)O_(3-δ)电解质材料性能的影响 被引量:2
15
作者 苏金瑞 南怡晨 +1 位作者 何豪 赵莹莹 《郑州大学学报(工学版)》 CAS 北大核心 2017年第3期30-34,共5页
采用柠檬酸盐燃烧法和固相反应相结合的方法制备BaCe_(0.8)In_(0.1)Y_(0.1)O_(3-δ)(BCIY)和掺杂Ta的BaCe_(0.7)Ta_(0.1)In_(0.1)Y_(0.1)O_(3-δ)(BCTIY)电解质粉体,在200 MPa压力下干压成型后在不同温度下烧结成电解质片,并使用X射线... 采用柠檬酸盐燃烧法和固相反应相结合的方法制备BaCe_(0.8)In_(0.1)Y_(0.1)O_(3-δ)(BCIY)和掺杂Ta的BaCe_(0.7)Ta_(0.1)In_(0.1)Y_(0.1)O_(3-δ)(BCTIY)电解质粉体,在200 MPa压力下干压成型后在不同温度下烧结成电解质片,并使用X射线衍射仪(XRD)、扫描电子显微镜(SEM)和电化学工作站分别对样品的物相、微观结构和电导率进行了表征.XRD结果显示,1 000℃煅烧5 h的BCIY和BCTIY均表现出单一的钙钛矿相.收缩率和SEM结果显示,BCIY在1 250℃下就可以烧结致密,掺杂Ta的BCTIY在1 350℃下也可以烧结致密.在空气和湿润的H_2气氛下BCTIY的电导率比BCIY的略有降低.在CO_2和沸水环境下,BCTIY比BCIY明显表现出较好的化学稳定性.研究结果表明:BCTIY有望成为中低温固体氧化物燃料电池稳定的电解质材料. 展开更多
关键词 质子导体 固体氧化物燃料电池 bace0.8In0.1Y0.1o3-δ bace0.7Ta0.1In0.1Y0.1o3-δ 烧结活性 化学稳定性 电导率
下载PDF
高温质子导体Ba(Ce_(0.8)Zr_(0.2))_(0.9)Y_(0.1)O_(3-δ)的合成与性能 被引量:3
16
作者 庞兆宝 孟波 谭小耀 《中国有色金属学报》 EI CAS CSCD 北大核心 2006年第5期858-861,共4页
采用低温燃烧法合成掺Zr的新型高温质子导体Ba(Ce0.8Zr0.2)0.9Y0.1O3-δ陶瓷粉体。运用X射线衍射仪、扫描电子显微镜以及激光粒度仪分别对粉体的晶型、微观形貌和粒度分布进行分析。通过控制柠檬酸用量与金属离子摩尔总量的比,直接制备... 采用低温燃烧法合成掺Zr的新型高温质子导体Ba(Ce0.8Zr0.2)0.9Y0.1O3-δ陶瓷粉体。运用X射线衍射仪、扫描电子显微镜以及激光粒度仪分别对粉体的晶型、微观形貌和粒度分布进行分析。通过控制柠檬酸用量与金属离子摩尔总量的比,直接制备出具有斜方晶钙钛矿结构的纯Ba(Ce0.8Zr0.2)0.9Y0.1O3-δ超细粉体,且粉体粒度分布均匀,平均粒径为5.55μm。粉体烧结性能实验结果表明,粉体在1 200℃发生烧结,在1 300℃下烧结致密,相对密度达到94.32%。 展开更多
关键词 高温质子导体 Ba(Ce0.8 Zr0.2)0.9Y0.1o3-δ陶瓷粉体 低温燃烧 钙钛矿
下载PDF
BaCe_(0.5)Zr_(0.4)Y_(0.1)O_(3-δ)粉体的溶胶-凝胶法和高温固相法制备及性能表征 被引量:1
17
作者 张翠娟 赵海雷 +2 位作者 王治峰 李雪 沈薇 《中国稀土学报》 CAS CSCD 北大核心 2008年第4期409-415,共7页
分别通过溶胶-凝胶法和高温固相反应法制备了BaCe0.5Zr0.4Y0.1O3-δ粉体。采用热重-差热分析(TG-DTA),粉末X射线衍射(XRD),扫描电子显微镜(SEM),傅立叶红外衍射(FT-IR),N2吸附-脱附等方法对所制备的粉体进行了表征。结果表明:用溶胶-凝... 分别通过溶胶-凝胶法和高温固相反应法制备了BaCe0.5Zr0.4Y0.1O3-δ粉体。采用热重-差热分析(TG-DTA),粉末X射线衍射(XRD),扫描电子显微镜(SEM),傅立叶红外衍射(FT-IR),N2吸附-脱附等方法对所制备的粉体进行了表征。结果表明:用溶胶-凝胶法在1200℃×10 h可以合成纯的BaCe0.5Zr0.4Y0.1O3-δ粉体,合成温度比传统的高温固相反应法降低400℃左右;溶胶-凝胶法合成粉体具有多孔结构特征,与固相法合成粉体相比具有较高的比表面积。但致密化试验表明:溶胶-凝胶法合成粉体与固相法合成粉体相比具有较低的烧结活性。溶胶-凝胶法合成粉体颗粒表面残余的有机基团和颗粒内部的大量微孔将在致密化过程中产生空间位阻,从而影响高温下原子的迁移,阻碍材料的致密化过程。 展开更多
关键词 高温质子导体 bace0.5Zr0.4Y0.1o3-δ 溶胶-凝胶法 高温固相反应法 稀土
下载PDF
水基凝胶注模成型工艺制备0.9Al2O3-0.1TiO2陶瓷的微波介电性能(英文) 被引量:1
18
作者 吴甲民 吕文中 +1 位作者 梁军 汪小红 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2011年第1期102-106,共5页
采用水基凝胶注模成型工艺制备了0.9Al_2O_3-0.1TiO_2陶瓷.研究了烧结后的0.9Al_2O_3-0.1TiO_2陶瓷的微结构、相组成以及微波介电性能.通过采用合适的预烧温度(1200℃)和连续、缓慢的降温工艺来退火,成功消除了Al_2TiO_5第二相.和传统... 采用水基凝胶注模成型工艺制备了0.9Al_2O_3-0.1TiO_2陶瓷.研究了烧结后的0.9Al_2O_3-0.1TiO_2陶瓷的微结构、相组成以及微波介电性能.通过采用合适的预烧温度(1200℃)和连续、缓慢的降温工艺来退火,成功消除了Al_2TiO_5第二相.和传统干压法相比,用水基凝胶注模成型工艺制备的0.9Al_2O_3-0.1TiO_2陶瓷具有较大的晶粒,较少的气孔和更加均匀的微结构.因此,用水基凝胶注模成型工艺制备的0.9Al_2O_3-0.1TiO_2陶瓷拥有更好的微波介电性能:ε_r=10.71,Q×f=20421GHz,τ_f=1.3×10^(-6)/℃,而用传统干压法制备的0.9Al_2O_3-0.1TiO_2陶瓷的微波介电性能为ε_r=10.89,Q×f=11938GHz,τ_f=1.4×10^(-6)/℃. 展开更多
关键词 陶瓷 介电性能 微结构 0.9Al2o3-0.1Tio2 水基凝胶注模成型工艺
下载PDF
BaCe0.7Zr0.2La0.1O3-α陶瓷的制备和导电性 被引量:1
19
作者 王茂元 仇立干 马桂林 《无机化学学报》 SCIE CAS CSCD 北大核心 2008年第3期357-362,共6页
以高温固相反应法合成了BaCe_0.7Zr_0.2La_0.1O_(3-α)陶瓷。粉末XRD结果表明,该陶瓷材料为单一钙钛矿型BaCeO3斜方晶结构。以陶瓷材料为固体电解质、多孔性铂为电极,采用交流阻抗谱技术和气体浓差电池方法分别测定了材料在500~900℃下... 以高温固相反应法合成了BaCe_0.7Zr_0.2La_0.1O_(3-α)陶瓷。粉末XRD结果表明,该陶瓷材料为单一钙钛矿型BaCeO3斜方晶结构。以陶瓷材料为固体电解质、多孔性铂为电极,采用交流阻抗谱技术和气体浓差电池方法分别测定了材料在500~900℃下,干燥空气、湿润空气和湿润氢气中的电导率以及离子迁移数,研究了材料的离子导电特性。结果表明,在500~900℃下干燥空气中,陶瓷材料的最大电导率为1.8mS·cm-1,氧离子迁移数为0.14~0.04,是一个氧离子与电子空穴的混合导体。在湿润空气中,陶瓷材料的最大电导率为2.0mS·cm-1,质子迁移数为0.48~0,氧离子迁移数为0.25~0.10,是质子、氧离子和电子空穴的混合导体。在湿润氢气中,陶瓷材料的最大电导率为3.6mS·cm-1。在500~700℃温度范围内,陶瓷材料的质子迁移数为1,是纯的质子导体;而在800~900℃温度范围内,陶瓷材料的质子迁移数为0.93~0.91,是质子与电子的混合导体,质子电导占主导。 展开更多
关键词 bace0.7Zr0.2La0.1o3 阻抗谱 气体浓差电池 离子导电性
下载PDF
Ba_(0.9)La_(0.1)Ce_(0.7)Zr_(0.2)Nd_(0.1)O_(3-α)陶瓷的化学稳定性和离子导电性 被引量:1
20
作者 仇立干 王茂元 曹旭 《无机化学学报》 SCIE CAS CSCD 北大核心 2011年第1期145-151,共7页
用高温固相反应法制备了Ba0.9La0.1Ce0.7Zr0.2Nd0.1O3-α陶瓷。粉末X-射线衍射(XRD)结果表明,该材料为单一钙钛矿型BaCeO3斜方晶结构,在高温下、CO2或水蒸气气氛中具有较高的稳定性。在500~900℃温度范围内,分别用交流阻抗谱技术和气... 用高温固相反应法制备了Ba0.9La0.1Ce0.7Zr0.2Nd0.1O3-α陶瓷。粉末X-射线衍射(XRD)结果表明,该材料为单一钙钛矿型BaCeO3斜方晶结构,在高温下、CO2或水蒸气气氛中具有较高的稳定性。在500~900℃温度范围内,分别用交流阻抗谱技术和气体浓差电池方法研究了材料在不同气体气氛中的离子导电特性,并与Ba0.9Ca0.1Ce0.9Nd0.1O3-α材料的导电特性进行了比较。结果表明,在500~900℃温度范围内,干燥和湿润的氢气、氮气、空气和氧气气氛中,材料的电导率均随着温度升高和氧分压增加而增加,且材料在湿润气氛中的电导率稍高于相应的干燥气氛中的电导率(氢气气氛中则相反)。在湿润氢气中,材料的质子迁移数为1,是一个纯的质子导体;在干燥空气中,材料的氧离子迁移数为0.087~0.155,是一个氧离子与电子空穴的混合导体;在湿润空气中,材料的质子迁移数为0.001~0.004,氧离子迁移数为0.160~0.198,是一个质子、氧离子和电子空穴的混合导体。材料在干燥和湿润空气中的氧离子电导率均高于相同条件下Ba0.9Ca0.1Ce0.9Nd0.1O3-α材料的氧离子电导率。 展开更多
关键词 Ba0.9La0.1Ce0.7Zr0.2Nd0.1o3 化学稳定性 质子导电性 阻抗谱 气体浓差电池
下载PDF