Enhanced Photocatalytic Denitrification Rhodamine Bover In2O3/Bi24O31Br10 Nanocomposites under Visible Light Irradiation 被引量:3
1
作者 黄继涛 崔春娜 +1 位作者 颜桂炀 邢永雷 《Chinese Journal of Structural Chemistry》 SCIE CAS CSCD 2018年第4期611-616,共6页
A novel In203/Bi24O31Br10 composite photocatalyst, where In2O3 nanoparticleswith the diameter of about 5-10 nm were tightly attached on the surface of Bi24O31Br10 plates, wasprepared by using hydrolysis, impregnation ... A novel In203/Bi24O31Br10 composite photocatalyst, where In2O3 nanoparticleswith the diameter of about 5-10 nm were tightly attached on the surface of Bi24O31Br10 plates, wasprepared by using hydrolysis, impregnation method and post-thermal process. Photocatalyticactivity was evaluated by the degradation of Rhodamine B under the visible light irradiation.Effects of the contents of In203 nanoparticles on the optical property and photocatalytic activity of In203/Bi24O31Br10 composite were also investigated. Compared with neat In203 and Bi24O31Brlomaterials, 15In203/Bi24O31Br10 composite exhibits the best photocatalytic activity owing to theefficient separation of photogenerated electron and hole pairs, which is evidenced byphotoluminence spectra. More than 95% of Rhodamine B solution can be degraded by15In203/Bi24O31Brlo sample in 30 min. 展开更多
关键词 PHoTocatalyst In2o3/bi24o31Br10 composite photocatalytic activity rhodamine B
下载PDF
Laser Cladding Al-Si/Al_2O_3-TiO_2 Composite Coatings on AZ31B Magnesium Alloy 被引量:1
2
作者 崔泽琴 YANG Hongwei +2 位作者 王文先 WU Hongliang XU Bingshe 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2012年第6期1042-1047,共6页
To improve the wear resistance and corrosion resistance of magnesium alloys, a 5 kW continuous wave CO2 laser was used to investigate the laser surface cladding on AZ31 B magnesium alloys with Al-Si/Al2O3-TiO2 composi... To improve the wear resistance and corrosion resistance of magnesium alloys, a 5 kW continuous wave CO2 laser was used to investigate the laser surface cladding on AZ31 B magnesium alloys with Al-Si/Al2O3-TiO2 composite powders. A detailed microstructure, chemical composition, and phase analysis of the composite coatings were studied by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and X-ray diffraction (XRD). The laser cladding shows good metallurgical bonding with the substrate. The composite coatings are composed of Mgl7Al12, Al3Mg2, Mg2Si, Al2O3, and TiO2 phases. Compared to the average microhardness (50HV0.05) of the AZ3 1 B substrate, that of the composite coatings (230HV0.05) is improved significantly. The wear resistances of the surface layers were evaluated in detail. The results demonstrate that the wear resistances of the laser surface-modified samples are considerably improved compared to the substrate. It also show that the composite coatings exhibit better corrosion resistance than that of the substrate in 3.5wt% NaCI solution. 展开更多
关键词 AZ31B magnesium alloy laser cladding Al-Si/Al2o3-tio2 composite coating wear resistance corrosion resistance
下载PDF
Bi_2O_3-TiO_2的制备及其光催化性能研究 被引量:2
3
作者 孙伟 刘炎 赵瑜 《安徽农学通报》 2016年第19期32-34,共3页
该文以四氯化钛和硝酸铋为原料,通过共沉淀法制备Bi_2O_3-TiO_2复合氧化物,以罗丹明B模拟有机污染物,在太阳光照射研究Bi_2O_3-TiO_2复合氧化物催化剂的光降解性能。考察了不同的沉淀剂、Ti∶Bi的配比及焙烧温度等制备条件对光催化性能... 该文以四氯化钛和硝酸铋为原料,通过共沉淀法制备Bi_2O_3-TiO_2复合氧化物,以罗丹明B模拟有机污染物,在太阳光照射研究Bi_2O_3-TiO_2复合氧化物催化剂的光降解性能。考察了不同的沉淀剂、Ti∶Bi的配比及焙烧温度等制备条件对光催化性能的影响。结果表明,Bi_2O_3-TiO_2复合氧化物催化剂的光降解率明显高于单一氧化物Bi_2O_3、TiO_2的光降解率;以Na OH为沉淀剂、Ti∶Bi的配比为1∶10、焙烧温度500℃时制得的Bi_2O_3-TiO_2复合氧化物催化剂具有很好的光催化降解效果。 展开更多
关键词 bi2o3-tio2 负载型催化剂 光催化降解 罗丹明B
下载PDF
PREPARATION,CHARACTERIZATION AND HYDROGENATION PROPERTY OF POLYMER-SUPPORTED Pd-Fe_2O_3 COMPOSITE CATALYSTS
4
作者 ZHANG Shengmin HU Weibing ZHANG Manzheng Wuhan University of Technology Hubei Research Institute of Chemistry 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 1999年第4期48-52,共5页
A series of polymer- supported Pd -Fe2O3 composite catalysts were prepared and their hydrogenation property mas investigated. It was found that the above catalysts have good catalytic hydrogenation activity for carbon... A series of polymer- supported Pd -Fe2O3 composite catalysts were prepared and their hydrogenation property mas investigated. It was found that the above catalysts have good catalytic hydrogenation activity for carbon - carbon double bonds systems and reusability. Furthermore, XPS and IR spectra shouted that active component in the composite catalysts is atomic Pd(0). An addition of a small amount of Fe2O3 has a promotive action upon hydrogenation activity of the catalysts, which indicated that there are some strong interactions (electron transfer) between Pd(0) and Fe(Ⅲ) species. Based on these results, a possible catalytic hydrogenation mechanism was also suggested. 展开更多
关键词 functional material polymet-sup- ported catalyst composite Pd - F2o3/polystyrene HYDRoGENATIoN mechanism
下载PDF
Preparation of Al_2O_3-SiO_2-TiO_2-ZrO_2 Composite Ceramic Membranes by Sol-Gel Method
5
作者 吴建锋 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2005年第1期42-45,共4页
Al 2O 3-SiO 2-TiO 2-ZrO 2 supported membranes were prepar ed by Sol-Gel method. These composite ceramic membranes are level, even and no macro crack. There exist several crystalline phases such as Al 2O 3, TiO... Al 2O 3-SiO 2-TiO 2-ZrO 2 supported membranes were prepar ed by Sol-Gel method. These composite ceramic membranes are level, even and no macro crack. There exist several crystalline phases such as Al 2O 3, TiO 2(a natase), Al 2SiO 5, and ZrO 2 in these membranes. Changing the molar ratio of Al∶Si∶Ti∶Zr,the kinds and content of crystal phases of composite membranes could be different, which may lead to a variety of microstructure of membranes. The surface nanoscale topography and microstructure of membranes were investiga ted by XRD,SEM,AFM,EPMA. The effects of additives and heat treatments on the sur face nanoscale topography and microstructure of composite ceramic membranes were also analyzed. 展开更多
关键词 sol-gel method Al 2o 3-Sio 2-tio 2-Zro 2 composite ceramic membranes surface nanoscale topography microstructure
下载PDF
Composite CoFe2O4/Bi3.1La0.9Ti3O12 Structures with Multiferroic Properties
6
作者 Amanda Charris-Hemandez Arun Kumar Maharaj Tomar 《Journal of Chemistry and Chemical Engineering》 2014年第8期767-771,共5页
Chemical solution route was used to synthesize Bi3.1La0.9Ti3O12 and CoFe2O4. Alternate CoFe2O4/Bi3.1La0.9Ti3O12 layers were deposited on Pt substrate (Pt/TiO2/SiO2/Si) by spin coating. X-ray diffraction and SEM (sc... Chemical solution route was used to synthesize Bi3.1La0.9Ti3O12 and CoFe2O4. Alternate CoFe2O4/Bi3.1La0.9Ti3O12 layers were deposited on Pt substrate (Pt/TiO2/SiO2/Si) by spin coating. X-ray diffraction and SEM (scanning electron microscopy) studies show composite-like polycrystalline films. Films were studied for leakage current, dielectric response, ferroelectric and ferromagnetic properties. Leakage current was low (〈 10^-8 A) in electric field below 120 kV/cm, and the dielectric response shows relaxation. Dielectric loss (tan 8) reduces 〈 3% at 10^6 Hz. Two and four layer structures showed room temperature FE (ferroelectric) and FM (ferromagnetic) responses with FE Pr (polarization) 〉 25℃/cm2 and ferromagnetic Mr (memory) 〉 52 emu/cm3. Co-existence of FE and FM can be attributed to stress due to different crystal structures of the material involved in composite film structure. 展开更多
关键词 MULTIFERRoIC CoFe2o4/bi3.1La0.9Ti3o12 composite chemical route.
下载PDF
Mass Production of Bi3NbO7/Bi2Zn(2/3)Nb(4/3)O7 Composites and Their Visible-light Photocatalytic Activity
7
作者 彭代江 ZOU Zhengguang +3 位作者 HE Jinyun 龙飞 MO Shuyi ZHOU Huanfu 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2017年第2期403-407,共5页
Series Bi3NbO7/Bi2Zn(2/3)Nb(4/3)O7 (BN/BZN) composites were synthesized through a facile solid state reaction method. The products were characterized by X-ray diffraction(XRD), field emission scanning electron... Series Bi3NbO7/Bi2Zn(2/3)Nb(4/3)O7 (BN/BZN) composites were synthesized through a facile solid state reaction method. The products were characterized by X-ray diffraction(XRD), field emission scanning electron microscopy(FE-SEM) and UV-vis diffuse reflectance spectroscopy(DRS). When BN: BZN=0.1 mole ratio, the BN/BZN composite showed the best visible-light-driven photocatalytic performance, which decomposed nearly 100% of Rh B(10 ppm, p H=3-4) within 40 min. The results demonstrated that in-situ solid state synthesis of BN/BZN composites could be an efficient strategy to develop new photocatalyst for environmental remediation. 展开更多
关键词 visible-light-driven photocatalyst bi3Nbo7/bi2Zn(2/3)Nb(4/3)o7 composites solid state reaction method
下载PDF
复合纳米材料Bi_2O_3-TiO_2的制备与表征 被引量:1
8
作者 丁鹏 《长春师范学院学报(自然科学版)》 2009年第3期29-31,共3页
采用均匀沉淀法,以硫酸钛为前驱体,制备了Bi2O3-TiO2复合纳米粉体材料,利用XPS、XRD、UV-Vis等现代化技术手段对复合纳米材料的结构和性质进行了表征。研究结果表明,TiO2的加入阻碍了Bi2O3晶粒的生长,导致复合纳米材料粒径的减小;而光... 采用均匀沉淀法,以硫酸钛为前驱体,制备了Bi2O3-TiO2复合纳米粉体材料,利用XPS、XRD、UV-Vis等现代化技术手段对复合纳米材料的结构和性质进行了表征。研究结果表明,TiO2的加入阻碍了Bi2O3晶粒的生长,导致复合纳米材料粒径的减小;而光生电子产生于Bi2O3并迁移到TiO2表面,所需的激发光频率变低,从而使复合纳米材料的吸光波长向可见光区域扩展。 展开更多
关键词 bi2o3-tio2 制备 表征
下载PDF
A Decisive Study on Dielectric Response of Bi2O3/Polystyrene &Bi2O3/PVDF Composite as Flexible Electrodes for Energy Storage
9
作者 Dinesh Kumar Yadav Anju Yadav +2 位作者 Sushil Kumar Jain Narendra Jakhar Balram Tripathi 《Open Journal of Composite Materials》 CAS 2023年第1期1-11,共11页
In this manuscript a comparative study on Bi<sub>2</sub>O<sub>3</sub>/polystyrene and Bi<sub>2</sub>O<sub>3</sub>/PVDF composites has been executed via analysis of struc... In this manuscript a comparative study on Bi<sub>2</sub>O<sub>3</sub>/polystyrene and Bi<sub>2</sub>O<sub>3</sub>/PVDF composites has been executed via analysis of structural, bonding, surface morphology and dielectric response of composites for energy storage. The composites have been synthesized using solution cast method by varying concentrations of Bi<sub>2</sub>O<sub>3</sub> (BO = 1 - 5 mw%) into polystyrene (PS) and polyvinylidene fluoride (PVDF) polymers respectively. X-ray diffraction confirms the generation of crystallinity, Fourier transform infrared (FT-IR) spectroscopy confirms bonding behavior and scanning electron microscopy (SEM) confirms uniform distribution of Bi<sub>2</sub>O<sub>3</sub> (BO) in PS and PVDF polymers. Impedance spectroscopy has been employed for determination of dielectric response of the fabricated composites. The dielectric constant has been found to be increased as 1.4 times of pristine PS to BO<sub>5%</sub>PS<sub>95%</sub> composites and 1.8 times of pristine PVDF to BO<sub>5%</sub>PVDF<sub>95%</sub> composites respectively. These high dielectric composite electrodes are useful for flexible energy storage devices. 展开更多
关键词 bismuth oxide (bi2o3) Polymer composites Surface Morphology Dielectric Constant Energy Storage
下载PDF
Nd掺杂Bi_2O_3-TiO_2纳米复合材料的制备、表征与模拟太阳光催化活性 被引量:1
10
作者 刘攀 邹浩 +3 位作者 宋绵新 边亮 张继黎 张帅 《科技创新与应用》 2016年第21期38-40,共3页
采用溶胶-凝胶法制备了Nd掺杂Bi2O3-Ti O2纳米复合材料,利用X射线衍射(XRD)、拉曼光谱(Raman)、透射电子显微镜(TEM)、高分辨透射电子显微镜(HRTEM)、紫外-可见漫反射吸收光谱(UV-vis DRS)等分析测试手段对样品的微观结构和吸光性能等... 采用溶胶-凝胶法制备了Nd掺杂Bi2O3-Ti O2纳米复合材料,利用X射线衍射(XRD)、拉曼光谱(Raman)、透射电子显微镜(TEM)、高分辨透射电子显微镜(HRTEM)、紫外-可见漫反射吸收光谱(UV-vis DRS)等分析测试手段对样品的微观结构和吸光性能等进行了表征,并以甲基橙溶液的降解作为探针反应,考察了样品的模拟太阳光催化性能。结果表明:所有S-X样品均呈锐钛矿结构;Nd以氧化物的形式附着在Bi2O3-Ti O2纳米复合材料表面;Nd具有敏化Bi2O3-Ti O2纳米复合材料的作用;S-0.250样品的光催化活性最好,当其用量为2.5g/L时,25mg/L的甲基橙溶液在模拟太阳光下照射5h后,脱色率可达到99.3%。 展开更多
关键词 bi2o3-tio2纳米复合材料 ND掺杂 模拟太阳光 光催化活性 甲基橙
下载PDF
Preparation and characterization of Fe_2O_3-CeO_2-TiO_2/γ-Al_2O_3 catalyst for degradation dye wastewater 被引量:5
11
作者 LIU Yan SUN De-zhi CHENG Lin LI Yan-ping 《Journal of Environmental Sciences》 SCIE EI CAS CSCD 2006年第6期1189-1192,共4页
In order to develop a catalyst with high activity for catalytic wet oxidation (CWO) process at room temperature and atmospheric pressure, Fe2O3-CeO2-TiO2/γ-Al2O3 catalyst was prepared by consecutive impregnation me... In order to develop a catalyst with high activity for catalytic wet oxidation (CWO) process at room temperature and atmospheric pressure, Fe2O3-CeO2-TiO2/γ-Al2O3 catalyst was prepared by consecutive impregnation method and the prepared parameters were optimized. The structure of the catalyst was characterized by BET, XRF, SEM and XPS technologies, and the actual wastewater was used to investigate the catalytic activity of Fe2O3-CeO2-TiO2/γ-Al2O3 in CWO process. The experimental results showed that the prepared catalyst exhibited good catalytic activity when the doping amount of Ti was 1.0 wt% (the weight ratio of Ti to carriers), and the middle product, Fe2O3-CeO2-TiO2/γ-Al2O3, was calcined in 450℃ for 2 h. The CWO experiment for treating actual dye wastewater indicated that the COD, color and TOC of actual wastewater were decreased by 62.23%, 50.12% and 41.26% in 3 h, respectively, and the ratio of BOD5/COD was increased from 0.19 to 0.30. 展开更多
关键词 catalytic wet oxidation (CWo Fe2o3-Ceo2-tio2/γ-Al2o3 catalyst dye wastewater treatment
下载PDF
BBZS掺杂对BaO-Sm2O3-TiO2系微波介质陶瓷性能的影响 被引量:5
12
作者 刘维良 唐春宝 +1 位作者 胡元云 李月明 《人工晶体学报》 EI CAS CSCD 北大核心 2008年第4期986-990,共5页
利用固相法制备BaO-Sm2O3-TiO2系微波介质陶瓷。通过复合添加氧化物ZnO、CuO和玻璃料Bi2O3-B2O3-ZnO-SiO2(BBZS),系统的烧结温度降至900℃。研究了玻璃料的添加量对介电性能的影响。按BaSm2Ti4O12+1wt%ZnO+1wt%CuO+xwt%BBZS(0<x≤30... 利用固相法制备BaO-Sm2O3-TiO2系微波介质陶瓷。通过复合添加氧化物ZnO、CuO和玻璃料Bi2O3-B2O3-ZnO-SiO2(BBZS),系统的烧结温度降至900℃。研究了玻璃料的添加量对介电性能的影响。按BaSm2Ti4O12+1wt%ZnO+1wt%CuO+xwt%BBZS(0<x≤30)配方,当x=25,预烧温度为1100℃和烧结温度为900℃时,有以下的微波特性:其介电常数为εr为60.51,Qf=2256 GHz,τf=1.502×10-5/℃,这种陶瓷材料有望与纯Ag电极共烧,应用到LTCC领域。 展开更多
关键词 微波介质陶瓷 Bao—Sm2o3-tio2系统 bi2o3-B2o3-Zno-Sio2(BBZS)
下载PDF
低温烧结BaO-Sm2O3-TiO2系微波介质陶瓷材料的研究
13
作者 刘维良 唐春宝 +1 位作者 胡元云 李月明 《功能材料》 EI CAS CSCD 北大核心 2007年第A02期834-837,共4页
利用传统的固相法制备BaO-Sm2O3-TiO2系陶瓷。通过复合添加氧化物ZnO、CuO和玻璃料Bi2O3-B2O3-ZnO-SiO2(BBZS),系统的烧结温度降至900℃。研究了玻璃料的添加量对介电性能的影响。按BaSm2Ti4O12+1%(质量分数)ZnO+1%(质量分数... 利用传统的固相法制备BaO-Sm2O3-TiO2系陶瓷。通过复合添加氧化物ZnO、CuO和玻璃料Bi2O3-B2O3-ZnO-SiO2(BBZS),系统的烧结温度降至900℃。研究了玻璃料的添加量对介电性能的影响。按BaSm2Ti4O12+1%(质量分数)ZnO+1%(质量分数)CuO+x%(质量分数)BBZS(0<x≤30)配方,当x=25,预烧温度为1100℃和烧结温度为900℃时,有以下的微波特性:εr=60.51,Qf=2256GHz,τf=15.02×10^-6/℃,该陶瓷材料有望与纯Ag电极共烧,应用到LTCC领域。 展开更多
关键词 微波介质陶瓷 Bao-Sm2o3-tio2系统 低温烧结 介电性能 bi2o3-B2o3-Zno-Sio2(BBZS)
下载PDF
SO_4^(2-)/Bi_2O_3-TiO_2制备及对罗丹明-B可见光活性研究
14
作者 刘世宇 赵隋欣 +3 位作者 万顺鑫 丁鹏 李春实 李佳 《内蒙古科技与经济》 2018年第13期89-91,共3页
利用溶胶凝胶法制备了SO_4^(2-)/Bi_2O_3-TiO_2光催化剂,样品结构经过X-射线粉末衍射仪(XRD)、扫描电子显微镜(SEM)、红外光谱仪(IR)、热重分析仪(TGA)等测试手段进行了表征,以罗丹明-B作为目标污染物,在可见光照射下测试了该光催化剂... 利用溶胶凝胶法制备了SO_4^(2-)/Bi_2O_3-TiO_2光催化剂,样品结构经过X-射线粉末衍射仪(XRD)、扫描电子显微镜(SEM)、红外光谱仪(IR)、热重分析仪(TGA)等测试手段进行了表征,以罗丹明-B作为目标污染物,在可见光照射下测试了该光催化剂的光催化活性,结果表明:该光催化剂主要由锐钛矿TiO2和四方体的Bi2O3组成,SO_4^(2-)主要以螯合双配位方式结合在Bi_2O_3-TiO_2表面,并在500℃焙烧的光催化剂具有更高的脱色效率,在罗丹明-B初始浓度为8mg/L和催化剂用量为600mg/L时,脱色效率可达97.89%,该光催化剂可以应用于有色废水的净化处理中。 展开更多
关键词 So42-/bi2o3-tio2 可见光 光催化 罗丹明-B 废水
下载PDF
低温烧结Bi_6Ti_5TeO_(22)和Bi_2Ti_3TeO_(12)陶瓷及其微波介电性能
15
作者 王洪恩 李勃 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2009年第A02期613-616,共4页
采用固相烧结法,研究了不同温度和配方Bi2O3-TiO2-TeO2体系陶瓷的低温烧结情况,研究了产物物相、微观结构和微波介电性能。研究表明,配方A(Bi2O3:TiO2:TeO2=1:3:1)在800℃以上煅烧可制备出较纯净的Bi6Ti5TeO22,配方B(Bi2O3:TiO2:TeO2=1.... 采用固相烧结法,研究了不同温度和配方Bi2O3-TiO2-TeO2体系陶瓷的低温烧结情况,研究了产物物相、微观结构和微波介电性能。研究表明,配方A(Bi2O3:TiO2:TeO2=1:3:1)在800℃以上煅烧可制备出较纯净的Bi6Ti5TeO22,配方B(Bi2O3:TiO2:TeO2=1.025:3:1)在700℃以上煅烧可制备纯净的Bi2Ti3TeO12粉末。所得Bi6Ti5TeO22和Bi2Ti3TeO12粉末都能在750~900℃度实现低温烧结。配方B在750℃烧结的介电性能较好,εr=32.5,介电损失为0.20%(100MHz)。 展开更多
关键词 低温共烧陶瓷 bi2o3-tio2-Teo2体系 微波介电性能
下载PDF
低温烧结BaO-Nd_2O_3-TiO_2陶瓷介质材料的研制 被引量:1
16
作者 莫方策 付振晓 +1 位作者 张火光 李娟 《电子元件与材料》 CAS CSCD 北大核心 2011年第10期8-10,共3页
采用固相法制备了BaO-Nd2O3-TiO2(BNT)陶瓷,研究了Bi2O3-SiO2-ZnO-CaO(BSZC)玻璃添加量对所制BNT陶瓷介电性能的影响。结果表明:添加质量分数7%~9%的BSZC玻璃,可使BNT陶瓷在960℃下烧结致密,匹配10Pd/90Ag内电极,获得相对介电常数εr≈... 采用固相法制备了BaO-Nd2O3-TiO2(BNT)陶瓷,研究了Bi2O3-SiO2-ZnO-CaO(BSZC)玻璃添加量对所制BNT陶瓷介电性能的影响。结果表明:添加质量分数7%~9%的BSZC玻璃,可使BNT陶瓷在960℃下烧结致密,匹配10Pd/90Ag内电极,获得相对介电常数εr≈88,介质损耗tanδ=6×10–4,电容温度系数αc≈0的高频MLCC陶瓷介质材料。 展开更多
关键词 多层陶瓷电容器 低温烧结 Bao-Nd2o3-tio2陶瓷 bi2o3-Sio2-Zno-Cao玻璃
下载PDF
新型复合光催化剂Cu_(2)O/Ag/Ag_(3)PO_(4)光催化降解甲基橙
17
作者 李丽丽 姜珂 +4 位作者 孙雅丽 李佳奇 杨振东 高天乐 王阳 《化工科技》 CAS 2022年第2期1-5,37,共6页
采用简单液相法制备Cu_(2)O/Ag/Ag_(3)PO_(4)三元复合光催化材料,并通过XRD、SEM、UV方法进行表征。结果表明,与纯Cu_(2)O相比,三元复合材料Cu_(2)O/Ag/Ag_(3)PO_(4)催化效果明显提高,30 min可以催化70%的污染物。浸泡次数直接影响催化... 采用简单液相法制备Cu_(2)O/Ag/Ag_(3)PO_(4)三元复合光催化材料,并通过XRD、SEM、UV方法进行表征。结果表明,与纯Cu_(2)O相比,三元复合材料Cu_(2)O/Ag/Ag_(3)PO_(4)催化效果明显提高,30 min可以催化70%的污染物。浸泡次数直接影响催化效果,浸泡20次降解90%的甲基橙需要约50 min,远高于浸泡5次和10次的时间。该催化剂为同类光催化复合材料的制备提供了新思路。 展开更多
关键词 Cu_(2)o/Ag/Ag_(3)Po_(4) 复合催化剂 催化活性 合成
下载PDF
γ-Al_2O_3预处理方式对γ-Al_2O_3/SAPO-34复合催化剂物化性质及催化性能的影响
18
作者 王冠超 刘飞 +1 位作者 罗兰 曹建新 《人工晶体学报》 EI CAS CSCD 北大核心 2018年第8期1535-1541,共7页
采用水热包覆法制备了γ-Al_2O_3/SAPO-34复合催化剂,考察了γ-Al_2O_3预处理方式对复合催化剂物化性质和MTO反应催化性能的影响。采用X射线衍射(XRD)、傅里叶红外(FT-IR)、扫描电子显微镜(SEM)、NH3程序升温脱附(NH3-TPD)、N2吸附脱附(... 采用水热包覆法制备了γ-Al_2O_3/SAPO-34复合催化剂,考察了γ-Al_2O_3预处理方式对复合催化剂物化性质和MTO反应催化性能的影响。采用X射线衍射(XRD)、傅里叶红外(FT-IR)、扫描电子显微镜(SEM)、NH3程序升温脱附(NH3-TPD)、N2吸附脱附(BET)等手段对几种复合催化剂进行了分析表征。结果表明,γ-Al_2O_3预处理方式对复合催化剂物化性质和MTO催化性能影响较大。添加拟勃姆石和电位改性γ-Al_2O_3制得复合催化剂未形成包覆复合相结构,比表面积较小,表现出较短催化寿命,仅分别为360 min和450 min;添加γ-Al_2O_3制得复合催化剂形成了包覆相结构和微-介复合孔结构(微孔比表面积123.49 m2·g-1、介孔比表面积122.68 m2·g-1,总比表面积为246.17 m2·g-1,总孔容0.29 cm3·g-1),总酸量较大(0.30 mmol·g-1);在常压、反应温度380℃、进料空速2 h-1反应条件下,复合催化剂催化性能优越,稳定性良好,具有较长的催化寿命,甲醇转化率为100%,低碳烯烃选择性为88.10%,催化寿命达990 min。 展开更多
关键词 γ-Al2o3/SAPo-34 复合催化剂 γ-Al2o3预处理 催化寿命 MTo反应
下载PDF
Fabrication of Bi_2O_3/TiO_2nanocomposites and their applications to the degradation of pollutants in air and water under visible-light 被引量:7
19
作者 Ashok Kumar Chakraborty Md Emran Hossain +1 位作者 Md Masudur Rhaman K M A Sobahan 《Journal of Environmental Sciences》 SCIE EI CAS CSCD 2014年第2期458-465,共8页
A nanoheterojunction composite photocatalyst Bi2O3/TiO2 working under visible-light (λ≥ 420 nm) was prepared by combining two semiconductors Bi2O3 and TiO2 varying the Bi2O3/TiO2 molar ratio. Maleic acid was emplo... A nanoheterojunction composite photocatalyst Bi2O3/TiO2 working under visible-light (λ≥ 420 nm) was prepared by combining two semiconductors Bi2O3 and TiO2 varying the Bi2O3/TiO2 molar ratio. Maleic acid was employed as an organic binder to unite Bi2O3 and TiO2 nanoparticles. The SEM, TEM, XRD and diffuse reflectance spectra were utilized to characterize the prepared Bi2O3/TiO2 nanoheterojunction. The nanocomposite exhibited unusual high photocatalytic activity in decomposing 2-propanol in gas phase and phenol in aqueous phase and, evolution of CO2 under visible light irradiation while the end members exhibited low photocatalytic activity. The composite was optimized to 5 mol% Bi2O3/TiO2. The remarkable high photocatalytic efficiency originates from the unique relative energy band position of Bi2O3 and TiO2 as well as the absorption of visible light by Bi2O3. 展开更多
关键词 nanoheterojunction bi2o3/Tio2 composite photocatalyst pollutants visible-light
原文传递
Bi_2O_3-TiO_2复合光催化剂协同处理铬-邻苯二甲酸酯复合污染 被引量:5
20
作者 刘星辰 胡芸 +1 位作者 刁习 韦朝海 《环境科学学报》 CAS CSCD 北大核心 2016年第11期3994-4000,共7页
以硝酸铋和钛酸丁酯为前驱体,采用水热法制备了Bi_2O_3-TiO_2复合半导体材料,并利用X射线衍射(XRD)、紫外-可见吸收光谱(UVVis)、能谱分析(EDS)、X射线光电子能谱(XPS)等手段对复合材料的结构进行了表征.同时,考察了Bi_2O_3-TiO_2复合... 以硝酸铋和钛酸丁酯为前驱体,采用水热法制备了Bi_2O_3-TiO_2复合半导体材料,并利用X射线衍射(XRD)、紫外-可见吸收光谱(UVVis)、能谱分析(EDS)、X射线光电子能谱(XPS)等手段对复合材料的结构进行了表征.同时,考察了Bi_2O_3-TiO_2复合材料对重金属Cr(Ⅵ)和难降解邻苯二甲酸二丁酯(DBP)复合污染的处理性能,并探讨了复合催化剂协同处理复合污染的作用机制.结果表明:该复合催化剂在可见光下能同时降低重金属Cr(Ⅵ)和有机物DBP的浓度,抑制电子和空穴复合,表现出比对单一Cr(Ⅵ)及DBP污染物更高的处理效率.当Bi_2O_3含量为4%时,复合催化剂表现出最佳的光催化活性. 展开更多
关键词 bi2o3-tio2复合催化剂 重金属 难降解有机物 复合污染 协同处理
原文传递