Erosion Effect of Molten Steel on Carbon Containing Refractories for Continuous Casting
1
作者 LI Hongxia YANG Bin LIU Guoqi CHENG Hepeng 《China's Refractories》 CAS 2007年第2期3-10,共8页
关键词 carbon containing refractories Continuous casting EROSION Decarbonization
下载PDF
Recent Progress of Carbon Nanotubes Reinforced MgO-C and Al_2O_3-C Refractories 被引量:1
2
作者 WANG Junkai DENG Xiangong +2 位作者 LI Faliang ZHANG Haijun ZHANG Shaowei 《China's Refractories》 CAS 2014年第4期16-21,共6页
Carbon nanotubes (CNTs) have been extensively studied over the last two decades since they possess excellent properties.CNTs have been considered as new promising reinforcements for carbon containing refractories (... Carbon nanotubes (CNTs) have been extensively studied over the last two decades since they possess excellent properties.CNTs have been considered as new promising reinforcements for carbon containing refractories (CCRs).Current research progress of the CNT-reinforced MgO-C and Al2O3-C refractories was summarized in this mini-review,and the CNT-reinforced CCRs possess remarkable mechanical properties and superior thermal shock resistance compared to CCRs without CNTs. 展开更多
关键词 carbon nanotubes carbon containing refractories magnesia-carbon refractory alumina-carbon refractory
下载PDF
Microstructure Study on Oxidation of Zirconium Diboride
3
作者 GAO Zhenxin LIU Cheng 《China's Refractories》 CAS 2019年第4期1-6,共6页
The oxidation behaviors of fused zirconium diboride and chemosynthetic zirconium diboride as well as morphology and composition of their oxidation products were researched by FESEM-EDS and XRD.The two kinds of zirconi... The oxidation behaviors of fused zirconium diboride and chemosynthetic zirconium diboride as well as morphology and composition of their oxidation products were researched by FESEM-EDS and XRD.The two kinds of zirconium diboride were heated at 700℃,900℃,1100℃and 1300℃for 3 h in air,respectively.The results show that Zr02 and B203(Ⅰ)are generated from the chemosynthetic zirconium diboride oxidized at 700℃for 3 h or the fused zirconium diboride oxidized at 800℃for 24 h;B203(Ⅰ)dissolves into water and then H3B03 crystallizes. 展开更多
关键词 zirconium diboride GRAPHITE carbon containing refractories anti-oxidation agent ZIRCONIA boron oxide