The ballistic resistance and failure pattern of a bi-layer alumina 99.5%-aluminium alloy 1100-H12 target against steel 4340 ogival nosed projectile has been explored in the present experimental cum numerical study.In ...The ballistic resistance and failure pattern of a bi-layer alumina 99.5%-aluminium alloy 1100-H12 target against steel 4340 ogival nosed projectile has been explored in the present experimental cum numerical study.In the experimental investigation,damage induced in the ceramic layer has been quantified in terms of number of cracks developed and failure zone dimensions.The resultant damage in the backing layer has been studied with variation in the bulge and perforation hole in the backing layer with the varying incidence velocity.The discussion of the experimental results has been further followed by three dimensional finite element computations using ABAQUS/Explicit finite code to investigate the behaviour of different types of bi-layer targets under multi-hit projectile impact.The JH-2 constitutive model has been used to reproduce the behaviour of alumina 99.5%and JC constitutive model has been used for steel 4340 and aluminium alloy 1100-H12.The total energy dissipation has been noted to be of lesser magnitude in case of sub-sequential impact in comparison to simultaneous impact of two projectiles.The distance between the impact points of two projectiles also effected the ballistic resistance of bi-layer target.The ballistic resistance of single tile ceramic front layer and four tile ceramic of equivalent area found to be dependent upon the boundary conditions provided to the target.展开更多
A solid-state sodium metal battery has cut a striking figure in next-generation large-scale energy storage technology on account of high safety,high energy density,and low cost.Nevertheless,the large interfacial resis...A solid-state sodium metal battery has cut a striking figure in next-generation large-scale energy storage technology on account of high safety,high energy density,and low cost.Nevertheless,the large interfacial resistance and sodium dendrite growth originating from the poor interface contact seriously hinder its practical application.Herein,a modified ultrasound welding was proposed to atomically bond Na anodes and Au-metalized Na_(3)Zr_(2)Si_(2)PO_(12) electrolytes associated with the in situ formation of Na–Au alloy interlayers.Thereupon,intimate Na_(3)Zr_(2)Si_(2)PO_(12)-Au/Na interfaces with a low interfacial resistance(~23Ωcm^(2))and a strong dendrite inhibition ability were constructed.The optimized Na symmetric battery can cycle steadily for more than 900 h at 0.3 mA cm^(-2) under a low overpotential(<50 mV)of Na electroplating/stripping and deliver a high critical current density of 0.8 mAcm^(-2) at room temperature.By incorporating the above interface into the solid-state Na metal battery,taking three-dimensional Na_(3)V_(2)(PO_(4))_(3) as the cathode,the full battery offers a high energy density of 291 Wh kg^(-1) at a high power density of 1860Wkg^(-1).A pouch-type solid-state sodium metal full battery based on a ceramic electrolyte was assembled for the first time,and it lit a 3 V LED lamp.Such a strategy of the ultrasound welding metalized solid-state electrolyte/Na interface by engineering the Na-Au interlayer would pave a new pathway to engineer a low-resistance and highly stable interface for high-energy/density solid-state sodium metal batteries.展开更多
Electric-spark deposition (ESD) was adopted for depositing a Ti( CN) -based ceramic coating on the TC4 titanium alloy substrate using a laboratory-developed electric-spark deposition system, a nitrogen-sealed atmo...Electric-spark deposition (ESD) was adopted for depositing a Ti( CN) -based ceramic coating on the TC4 titanium alloy substrate using a laboratory-developed electric-spark deposition system, a nitrogen-sealed atmosphere and graphite electrode. The surface morphology, microstructure, interfacial behavior between the coatings and substrate, phase and element composition of the coatings were investigated by scanning electron microscope ( SEM ) , X-ray diffraction ( XRD ) , X-ray photoelectron spectroscopy ( XPS ) and Auger electron spectroscopy ( AES ) . Microhardness profile was measured with a Vickers microhardness tester. The results show that metallurgical bond between the coating and substrate is realized and the phase of coatings are made up of Ti( CN ) spherocrystal and dendritic crystal, TiV and C. Ti( CN) ceramic particles, which is in-situ synthesized by the reaction among titanium from the substrate, carbon from the graphite electrode and nitrogen from the shielding nitrogen gas, is about 600 mn and distributes dispersively among the coatings. Microharduess profile falls off with the coatings thickness increasing and the highest microhardness values of the superficial coating could be up to 1 496HV, which is six times more than that of the substrate.展开更多
Based on ANSYS FEM software, the distribution of residual stress in the diffusion bonding joints between Ti( C,N) metallic ceramic/interlayer/4OCr steel was calculated and experimentally ver^ed. The results showed t...Based on ANSYS FEM software, the distribution of residual stress in the diffusion bonding joints between Ti( C,N) metallic ceramic/interlayer/4OCr steel was calculated and experimentally ver^ed. The results showed that the trend on the distribution of residual stress field in the joints was not changed with the use of interlayer. The maximum residual stress was always located in metallic ceramic with area ranging from 1 mm to 4 mm to the interlayer. The maximum residual stress in the joints was also affected by diffusion temperature. The satellite pulse current during the initial stage on diffusion bonding can promote the formation of liquid film at the interface, by which diffusion temperature and loading pressure can be greatly decreased. The crack initiation was easily produced at the corner of Ti ( C, N) metallic ceramic close to the interlayer. If a higher residual stress produced in the joints, the crack was propagated into the whole ceramic.展开更多
Numerical simulation for the dynamic response of ceramic/metal armours impacted by deformable projectile is carried out with LS-DYNA3D.The simulated penetration processes are shown. The mushrooming of the projectile i...Numerical simulation for the dynamic response of ceramic/metal armours impacted by deformable projectile is carried out with LS-DYNA3D.The simulated penetration processes are shown. The mushrooming of the projectile is displayed. A distinct conoid shaped zone of fragmented ceramic is observed. A significant bending of the backing plate is revealed. Simulation results match fairly well with the experimental values and the theoretical analysis results. The accuracy of the numerical simulation is validated.展开更多
With Al2O3, Dy2O3, and SiO2 as starting materials, the basic glass of Al2O3-Dy2O3-SiO2 system was prepared by conventional melting technology, and their thermal expansion coefficients (TECs) at different anneal time...With Al2O3, Dy2O3, and SiO2 as starting materials, the basic glass of Al2O3-Dy2O3-SiO2 system was prepared by conventional melting technology, and their thermal expansion coefficients (TECs) at different anneal time were investigated. TECs of the basic glass, which were heat-treated under different temperature, were also investigated. The result showed that TECs of the basic glass gradually approached a fixed value as the anneal time was extended, which suggested that most of the inner stress had been eliminated. After heat treatment, the contents of Dy2O3, Dy2Si2O7, and a new crystal increased up to 1200 ℃ and decreased below 1250 ℃, which was consistent with the TEC change of crystallized samples. This suggests that the crystal has a direct effect on TECs of the crystallized samples.展开更多
A design of the sandwich joint,steel/ ceramic/steel,was made for direct comparison be- tween tensile and flexural strength of ceramic/metal joint.The flexural strength is about twice as high as the tensile strength fo...A design of the sandwich joint,steel/ ceramic/steel,was made for direct comparison be- tween tensile and flexural strength of ceramic/metal joint.The flexural strength is about twice as high as the tensile strength for the same joint.The results also showed that the flexural test is more excellent than tensile test for joint with a high interracial bond strength.展开更多
A new analytical model was established to describe the complex behavior of ceramic/metal armor under impact of deformable projectile by assuming some hypotheses. Three aspects were taken into account: the mushrooming...A new analytical model was established to describe the complex behavior of ceramic/metal armor under impact of deformable projectile by assuming some hypotheses. Three aspects were taken into account: the mushrooming deformation of the projectile, the fragment of ceramic tile and the formation and change of ceramic conoid and the deformation of the metal backup plate. Solving the set of equations, all the variables were obtained for the different impact velocities: the extent and particle velocity in rigid zone; the extent, cross-section area and particle velocity in plastic zone; the velocity and depth of penetration of projectile to the target; the reduction in volume and compressive strength of the fractured ceramic conoid; the displacement and movement velocity of the effective zone of backup plate. Agreement observed among analytical result, numerical simulation and experimental result confirms the validity of the model, suggesting the model developed can be a useful tool for ceramic/metal armor design.展开更多
Due to the wide application of ceramics in electronic device packaging,the performance of ceramic metallization layer directly determines the performance of the whole package device.This paper introduces the main prep...Due to the wide application of ceramics in electronic device packaging,the performance of ceramic metallization layer directly determines the performance of the whole package device.This paper introduces the main preparation methods of ceramic metallization,discusses the influence of Mo powder size,metallization formula,sintering temperature and other factors on the performance of ceramic metallization layer prepared by activated Mo-Mn method,and introduces several kinds of methods that can be tested to test the performance of ceramic metallized sealing samples.A new research direction of Ceramic Metallization Technology in the advanced field is put forward.展开更多
The injection molding products with different volume ratios of ZrO2 ceramic powder to 316L stainless steel powder were prepared. Properties and structure of the products were characterized by X-ray diffraction(XRD),...The injection molding products with different volume ratios of ZrO2 ceramic powder to 316L stainless steel powder were prepared. Properties and structure of the products were characterized by X-ray diffraction(XRD), scanning electron microscope(SEM) and transmission electron microscope (TEM). The results show that the compressive stress exists in the products and the bend strength reaches 300MPa. ZrO2 phase and stainless steel phase are uniform in samples. The toughness of ceramic increases with the increasing the content of stainless steel. Through TEM study of the interface, some crystalline orientation relationships are determined.展开更多
Thin metallic layers (~ 2 μm) of Ni were deposited on polycrystalline Al2O3. ZrO2 and (Ce-TZP)+Al2O3 ceramic substrates. and further irradiated with pulsed excimer (Xeno chloride) laser pulses. The laser energy densi...Thin metallic layers (~ 2 μm) of Ni were deposited on polycrystalline Al2O3. ZrO2 and (Ce-TZP)+Al2O3 ceramic substrates. and further irradiated with pulsed excimer (Xeno chloride) laser pulses. The laser energy density was varied from 0.21 to 0.81 J / cm2 to optimize bending strength. For ZrO2 ceramic, it was found that the strength increases from 530 to 753 MPa at 0.51 J / cm2 irradiation. For Al2O3 and (Ce-TZP)+ Al2O3 the fracture strength also increases in varying degree. The causes of strength increment were discussed.展开更多
The Al_2O_3-(W,Ti)C composites with Ni and Mo additions varying from 0vol% to 12vol% were prepared via hot pressing sintering under 30 MPa. The microstructure was investigated via X-ray diffraction(XRD) and scanni...The Al_2O_3-(W,Ti)C composites with Ni and Mo additions varying from 0vol% to 12vol% were prepared via hot pressing sintering under 30 MPa. The microstructure was investigated via X-ray diffraction(XRD) and scanning electron microscopy(SEM) equipped with energy dispersive spectrometry(EDS). Mechanical properties such as flexural strength, fracture toughness, and Vickers hardness were also measured. Results show that the main phases A12O3 and(W,Ti)C were detected by XRD. Compound Mo Ni also existed in sintered nanocomposites. The fracture modes of the nanocomposites were both intergranular and transgranular fractures. The plastic deformation of metal particles and crack bridging were the main toughening mechanisms. The maximum flexural strength and fracture toughness were obtained for 9vol% and 12vol% additions of Ni and Mo, respectively. The hardness of the composites reduced gradually with increasing content of metals Ni and Mo.展开更多
The performances of mixed ceramic and sialon ceramic tools in machining nickel based alloy are tested.The negative cutting edge inclination and small tool lead angle are recommended for reducing ceramic tool failure....The performances of mixed ceramic and sialon ceramic tools in machining nickel based alloy are tested.The negative cutting edge inclination and small tool lead angle are recommended for reducing ceramic tool failure. So called“notching at depth of cut”is not actually at the depth of cutting line, but out of cutting area。 The real reason of notching is caused by shocking of “sawtooth”on sawtooth- shaped burr and fin- shaped edges of chip展开更多
Through systematic cutting experiments, characteristics of the cutting performance of Ti(C, N) based cermets is identified. The experiments were designed to study their resistance,toughness, cutting force, tool-chip f...Through systematic cutting experiments, characteristics of the cutting performance of Ti(C, N) based cermets is identified. The experiments were designed to study their resistance,toughness, cutting force, tool-chip friction coefficient and machining quality by comparing them with those of WC based cemented carbides. The cutting data and the regressed empirical formulae would be useful to promote proper application of cermet cutting tool materials.展开更多
The interface structure, work of adhesion, and bonding character of the polar TiC/Ti interface have been examined by the first-principles density functional plane-wave pseudopotential calculations. Both Ti- and C-term...The interface structure, work of adhesion, and bonding character of the polar TiC/Ti interface have been examined by the first-principles density functional plane-wave pseudopotential calculations. Both Ti- and C-terminated interfaces including six different interface structures were calculated, which present quite different features. For the Ti-terminated interface, the interfacial Ti-Ti bond has a strong metallic and weak covalent character; while for the C-terminated interface, the interfacial bond is a strong polar covalent interaction between the Ti-3d and C-2p orbital. The work of adhesion of C-terminated interface is nearly 9 J/m2 stronger than that of the Ti-terminated. It is found that each termination has relatively large work of adhesion, which is consistent with other polar interfaces.展开更多
Employing Dy2O3, Al2O3, and SiO2 as starting materials, several series of Dy2O3-Al2O3-SiO2 sealing glass were prepared. The relationship between their coefficients of thermal expansion and the contents of Dy2O3, Al2O3...Employing Dy2O3, Al2O3, and SiO2 as starting materials, several series of Dy2O3-Al2O3-SiO2 sealing glass were prepared. The relationship between their coefficients of thermal expansion and the contents of Dy2O3, Al2O3, and SiO2 were studied respectively. Experimental results showed that Dy2O3 and Al2O3 had a positive effect on the coefficient of thermal expansion of glass, whereas, SiO2 had a negative effect. The coefficient of thermal expansion of glass showed an apparent linear relation to the contents of these three raw materials, from which an estimation model was built, to calculate the coefficient of thermal expansion of sealing glass. Relative errors of the calculating results to testing results were no more than 2%, which suggested that the estimation model was reasonable. This study provides a good theory reference for the practical utilizing of this sealing material, through which a proper glass composition for good sealing could be easily found.展开更多
In this paper first-principles calculations of Ni(111)/α-Al2O3(0001) interfaces have been performed, and are compared with the preceding results of the Cu (111)/α-Al2O3(0001) interface [2004 Phil. Mag. Left....In this paper first-principles calculations of Ni(111)/α-Al2O3(0001) interfaces have been performed, and are compared with the preceding results of the Cu (111)/α-Al2O3(0001) interface [2004 Phil. Mag. Left. 84 425]. The AI- terminated and O-terminated interfaces have quite different adhesion mechanisms, which are similar to the Cu(111)/α Al2O3(0001) interface. For the O-terminated interface, the adhesion is caused by the strong O-2p/Ni-3d orbital hybridization and ionic interactions. On the other hand, the adhesion nature of the Al-terminated interface is the image-like electrostatic and Ni-Al hybridization interactions, the latter is substantial and cannot be neglected. Charge transfer occurs from Al2O3 to Ni, which is opposite to that in the O=terminated interface. The charge transfer direction for the Al-terminated and O-terminated Ni(111)/α-A1203(0001) interfaces is similar to that in the corresponding Cu(111)/α- Al2O3(0001) interface, but there exist the larger charge transfer quantity and consequent stronger adhesion nature, respectively.展开更多
SiC composites and 40 Cr Steels were joined with Ag-Cu-Ti solder in order to develop a new method of joining ceramics to metal. Effects of solder component and process parameters on the joining strength were investiga...SiC composites and 40 Cr Steels were joined with Ag-Cu-Ti solder in order to develop a new method of joining ceramics to metal. Effects of solder component and process parameters on the joining strength were investigated. The results show that some chemical reactions occur on the jointing interface between ceramics and metal. Higher joining strength is achieved when titanium is 0.2% (mass fraction) in the solder. The thickness of solder also affects the joining characteristics, and 0.2-0.3 mm. thickness of solder is the most suitable.展开更多
As a structural and functional material with excellent properties,ceramics play an extremely important role in a wide range of industries,including life and production.To expand the range of applications for ceramic m...As a structural and functional material with excellent properties,ceramics play an extremely important role in a wide range of industries,including life and production.To expand the range of applications for ceramic materials,ceramics are often joined to metals and then used.Among the physical and chemical joining methods of ceramics to metals,the AMB method is efficient and simple,suitable for industrial applications,and has been a hot topic of research.However,due to the problems of residual stresses caused by the large difference in thermal expansion coefficients between ceramic and metal brazing,composite fillers have become a very worthwhile solution by regulating the physical properties of the brazing material and improving the weld structure.This review describes the wetting principle and application of Ag‒Cu‒Ti active metal filler in the field of ceramic joining,with emphasis on the current stage of composite filler,and discusses the influence on the former brazing properties and organization after the introduction of dissimilar materials.展开更多
文摘The ballistic resistance and failure pattern of a bi-layer alumina 99.5%-aluminium alloy 1100-H12 target against steel 4340 ogival nosed projectile has been explored in the present experimental cum numerical study.In the experimental investigation,damage induced in the ceramic layer has been quantified in terms of number of cracks developed and failure zone dimensions.The resultant damage in the backing layer has been studied with variation in the bulge and perforation hole in the backing layer with the varying incidence velocity.The discussion of the experimental results has been further followed by three dimensional finite element computations using ABAQUS/Explicit finite code to investigate the behaviour of different types of bi-layer targets under multi-hit projectile impact.The JH-2 constitutive model has been used to reproduce the behaviour of alumina 99.5%and JC constitutive model has been used for steel 4340 and aluminium alloy 1100-H12.The total energy dissipation has been noted to be of lesser magnitude in case of sub-sequential impact in comparison to simultaneous impact of two projectiles.The distance between the impact points of two projectiles also effected the ballistic resistance of bi-layer target.The ballistic resistance of single tile ceramic front layer and four tile ceramic of equivalent area found to be dependent upon the boundary conditions provided to the target.
基金Scientific Developing Foundation of Tianjin Education Commission,Grant/Award Number:2018ZD09National Natural Science Foundation of China,Grant/Award Numbers:51777138,52202282。
文摘A solid-state sodium metal battery has cut a striking figure in next-generation large-scale energy storage technology on account of high safety,high energy density,and low cost.Nevertheless,the large interfacial resistance and sodium dendrite growth originating from the poor interface contact seriously hinder its practical application.Herein,a modified ultrasound welding was proposed to atomically bond Na anodes and Au-metalized Na_(3)Zr_(2)Si_(2)PO_(12) electrolytes associated with the in situ formation of Na–Au alloy interlayers.Thereupon,intimate Na_(3)Zr_(2)Si_(2)PO_(12)-Au/Na interfaces with a low interfacial resistance(~23Ωcm^(2))and a strong dendrite inhibition ability were constructed.The optimized Na symmetric battery can cycle steadily for more than 900 h at 0.3 mA cm^(-2) under a low overpotential(<50 mV)of Na electroplating/stripping and deliver a high critical current density of 0.8 mAcm^(-2) at room temperature.By incorporating the above interface into the solid-state Na metal battery,taking three-dimensional Na_(3)V_(2)(PO_(4))_(3) as the cathode,the full battery offers a high energy density of 291 Wh kg^(-1) at a high power density of 1860Wkg^(-1).A pouch-type solid-state sodium metal full battery based on a ceramic electrolyte was assembled for the first time,and it lit a 3 V LED lamp.Such a strategy of the ultrasound welding metalized solid-state electrolyte/Na interface by engineering the Na-Au interlayer would pave a new pathway to engineer a low-resistance and highly stable interface for high-energy/density solid-state sodium metal batteries.
基金The work was supported by the Natural Science Foundation of Hebei Province of China under Grant No. E2007000566.
文摘Electric-spark deposition (ESD) was adopted for depositing a Ti( CN) -based ceramic coating on the TC4 titanium alloy substrate using a laboratory-developed electric-spark deposition system, a nitrogen-sealed atmosphere and graphite electrode. The surface morphology, microstructure, interfacial behavior between the coatings and substrate, phase and element composition of the coatings were investigated by scanning electron microscope ( SEM ) , X-ray diffraction ( XRD ) , X-ray photoelectron spectroscopy ( XPS ) and Auger electron spectroscopy ( AES ) . Microhardness profile was measured with a Vickers microhardness tester. The results show that metallurgical bond between the coating and substrate is realized and the phase of coatings are made up of Ti( CN ) spherocrystal and dendritic crystal, TiV and C. Ti( CN) ceramic particles, which is in-situ synthesized by the reaction among titanium from the substrate, carbon from the graphite electrode and nitrogen from the shielding nitrogen gas, is about 600 mn and distributes dispersively among the coatings. Microharduess profile falls off with the coatings thickness increasing and the highest microhardness values of the superficial coating could be up to 1 496HV, which is six times more than that of the substrate.
基金The authors are grateful to the financial support for this research from National Natural Science Foundation of China (Grant No. 51175259) , Jiangsu Science and Technology Planning Project (No. BK2011494) and University Science Research Project of Jiangsu Province ( 11KJAd30005 ).
文摘Based on ANSYS FEM software, the distribution of residual stress in the diffusion bonding joints between Ti( C,N) metallic ceramic/interlayer/4OCr steel was calculated and experimentally ver^ed. The results showed that the trend on the distribution of residual stress field in the joints was not changed with the use of interlayer. The maximum residual stress was always located in metallic ceramic with area ranging from 1 mm to 4 mm to the interlayer. The maximum residual stress in the joints was also affected by diffusion temperature. The satellite pulse current during the initial stage on diffusion bonding can promote the formation of liquid film at the interface, by which diffusion temperature and loading pressure can be greatly decreased. The crack initiation was easily produced at the corner of Ti ( C, N) metallic ceramic close to the interlayer. If a higher residual stress produced in the joints, the crack was propagated into the whole ceramic.
基金National Natural Science Foundation of China(10172063)
文摘Numerical simulation for the dynamic response of ceramic/metal armours impacted by deformable projectile is carried out with LS-DYNA3D.The simulated penetration processes are shown. The mushrooming of the projectile is displayed. A distinct conoid shaped zone of fragmented ceramic is observed. A significant bending of the backing plate is revealed. Simulation results match fairly well with the experimental values and the theoretical analysis results. The accuracy of the numerical simulation is validated.
基金Project supported by the Ministry of Science and Technology of China (2006CB601104)
文摘With Al2O3, Dy2O3, and SiO2 as starting materials, the basic glass of Al2O3-Dy2O3-SiO2 system was prepared by conventional melting technology, and their thermal expansion coefficients (TECs) at different anneal time were investigated. TECs of the basic glass, which were heat-treated under different temperature, were also investigated. The result showed that TECs of the basic glass gradually approached a fixed value as the anneal time was extended, which suggested that most of the inner stress had been eliminated. After heat treatment, the contents of Dy2O3, Dy2Si2O7, and a new crystal increased up to 1200 ℃ and decreased below 1250 ℃, which was consistent with the TEC change of crystallized samples. This suggests that the crystal has a direct effect on TECs of the crystallized samples.
文摘A design of the sandwich joint,steel/ ceramic/steel,was made for direct comparison be- tween tensile and flexural strength of ceramic/metal joint.The flexural strength is about twice as high as the tensile strength for the same joint.The results also showed that the flexural test is more excellent than tensile test for joint with a high interracial bond strength.
基金Project supported by the National Natural Science Foundation of China (No.10472033)the Natural Science Foundation of Guangdong Province (No.05300134)
文摘A new analytical model was established to describe the complex behavior of ceramic/metal armor under impact of deformable projectile by assuming some hypotheses. Three aspects were taken into account: the mushrooming deformation of the projectile, the fragment of ceramic tile and the formation and change of ceramic conoid and the deformation of the metal backup plate. Solving the set of equations, all the variables were obtained for the different impact velocities: the extent and particle velocity in rigid zone; the extent, cross-section area and particle velocity in plastic zone; the velocity and depth of penetration of projectile to the target; the reduction in volume and compressive strength of the fractured ceramic conoid; the displacement and movement velocity of the effective zone of backup plate. Agreement observed among analytical result, numerical simulation and experimental result confirms the validity of the model, suggesting the model developed can be a useful tool for ceramic/metal armor design.
基金The authors are grateful to National Science Foundation of China(51602347)Hunan Natural Science Foundation(2019JJ50282)for financial support.The authors are also grateful to Aid Program for Innovative Group of National University of Defense Technology and Aid Program for Science and Technology Innovative Research Team in Higher Educational Institutions of Hunan Province.
文摘Due to the wide application of ceramics in electronic device packaging,the performance of ceramic metallization layer directly determines the performance of the whole package device.This paper introduces the main preparation methods of ceramic metallization,discusses the influence of Mo powder size,metallization formula,sintering temperature and other factors on the performance of ceramic metallization layer prepared by activated Mo-Mn method,and introduces several kinds of methods that can be tested to test the performance of ceramic metallized sealing samples.A new research direction of Ceramic Metallization Technology in the advanced field is put forward.
文摘The injection molding products with different volume ratios of ZrO2 ceramic powder to 316L stainless steel powder were prepared. Properties and structure of the products were characterized by X-ray diffraction(XRD), scanning electron microscope(SEM) and transmission electron microscope (TEM). The results show that the compressive stress exists in the products and the bend strength reaches 300MPa. ZrO2 phase and stainless steel phase are uniform in samples. The toughness of ceramic increases with the increasing the content of stainless steel. Through TEM study of the interface, some crystalline orientation relationships are determined.
文摘Thin metallic layers (~ 2 μm) of Ni were deposited on polycrystalline Al2O3. ZrO2 and (Ce-TZP)+Al2O3 ceramic substrates. and further irradiated with pulsed excimer (Xeno chloride) laser pulses. The laser energy density was varied from 0.21 to 0.81 J / cm2 to optimize bending strength. For ZrO2 ceramic, it was found that the strength increases from 530 to 753 MPa at 0.51 J / cm2 irradiation. For Al2O3 and (Ce-TZP)+ Al2O3 the fracture strength also increases in varying degree. The causes of strength increment were discussed.
基金financially supported by the National Natural Science Foundation of China (No. 51475273)
文摘The Al_2O_3-(W,Ti)C composites with Ni and Mo additions varying from 0vol% to 12vol% were prepared via hot pressing sintering under 30 MPa. The microstructure was investigated via X-ray diffraction(XRD) and scanning electron microscopy(SEM) equipped with energy dispersive spectrometry(EDS). Mechanical properties such as flexural strength, fracture toughness, and Vickers hardness were also measured. Results show that the main phases A12O3 and(W,Ti)C were detected by XRD. Compound Mo Ni also existed in sintered nanocomposites. The fracture modes of the nanocomposites were both intergranular and transgranular fractures. The plastic deformation of metal particles and crack bridging were the main toughening mechanisms. The maximum flexural strength and fracture toughness were obtained for 9vol% and 12vol% additions of Ni and Mo, respectively. The hardness of the composites reduced gradually with increasing content of metals Ni and Mo.
文摘The performances of mixed ceramic and sialon ceramic tools in machining nickel based alloy are tested.The negative cutting edge inclination and small tool lead angle are recommended for reducing ceramic tool failure. So called“notching at depth of cut”is not actually at the depth of cutting line, but out of cutting area。 The real reason of notching is caused by shocking of “sawtooth”on sawtooth- shaped burr and fin- shaped edges of chip
文摘Through systematic cutting experiments, characteristics of the cutting performance of Ti(C, N) based cermets is identified. The experiments were designed to study their resistance,toughness, cutting force, tool-chip friction coefficient and machining quality by comparing them with those of WC based cemented carbides. The cutting data and the regressed empirical formulae would be useful to promote proper application of cermet cutting tool materials.
基金This work was supported by the special Funds for Major State Basic Research Projects of China(No G2000067104).
文摘The interface structure, work of adhesion, and bonding character of the polar TiC/Ti interface have been examined by the first-principles density functional plane-wave pseudopotential calculations. Both Ti- and C-terminated interfaces including six different interface structures were calculated, which present quite different features. For the Ti-terminated interface, the interfacial Ti-Ti bond has a strong metallic and weak covalent character; while for the C-terminated interface, the interfacial bond is a strong polar covalent interaction between the Ti-3d and C-2p orbital. The work of adhesion of C-terminated interface is nearly 9 J/m2 stronger than that of the Ti-terminated. It is found that each termination has relatively large work of adhesion, which is consistent with other polar interfaces.
基金Project supported by the Ministry of Science and Technology of China (2006CB601104)
文摘Employing Dy2O3, Al2O3, and SiO2 as starting materials, several series of Dy2O3-Al2O3-SiO2 sealing glass were prepared. The relationship between their coefficients of thermal expansion and the contents of Dy2O3, Al2O3, and SiO2 were studied respectively. Experimental results showed that Dy2O3 and Al2O3 had a positive effect on the coefficient of thermal expansion of glass, whereas, SiO2 had a negative effect. The coefficient of thermal expansion of glass showed an apparent linear relation to the contents of these three raw materials, from which an estimation model was built, to calculate the coefficient of thermal expansion of sealing glass. Relative errors of the calculating results to testing results were no more than 2%, which suggested that the estimation model was reasonable. This study provides a good theory reference for the practical utilizing of this sealing material, through which a proper glass composition for good sealing could be easily found.
基金supported by Qianjiang Talent Project of Zhejiang Province of China (Grant No 2007R10028)the Science Foundation of Zhejiang Sci-Tech University (ZSTU) in China (Grant No 0613271-Y)Science Foundation of Zhejiang Province of China(Grant No Y407188)
文摘In this paper first-principles calculations of Ni(111)/α-Al2O3(0001) interfaces have been performed, and are compared with the preceding results of the Cu (111)/α-Al2O3(0001) interface [2004 Phil. Mag. Left. 84 425]. The AI- terminated and O-terminated interfaces have quite different adhesion mechanisms, which are similar to the Cu(111)/α Al2O3(0001) interface. For the O-terminated interface, the adhesion is caused by the strong O-2p/Ni-3d orbital hybridization and ionic interactions. On the other hand, the adhesion nature of the Al-terminated interface is the image-like electrostatic and Ni-Al hybridization interactions, the latter is substantial and cannot be neglected. Charge transfer occurs from Al2O3 to Ni, which is opposite to that in the O=terminated interface. The charge transfer direction for the Al-terminated and O-terminated Ni(111)/α-A1203(0001) interfaces is similar to that in the corresponding Cu(111)/α- Al2O3(0001) interface, but there exist the larger charge transfer quantity and consequent stronger adhesion nature, respectively.
文摘SiC composites and 40 Cr Steels were joined with Ag-Cu-Ti solder in order to develop a new method of joining ceramics to metal. Effects of solder component and process parameters on the joining strength were investigated. The results show that some chemical reactions occur on the jointing interface between ceramics and metal. Higher joining strength is achieved when titanium is 0.2% (mass fraction) in the solder. The thickness of solder also affects the joining characteristics, and 0.2-0.3 mm. thickness of solder is the most suitable.
基金the National Natural Science Foundation of China(Grant Nos.51971204 and 52171081)the Zhejiang Provincial Natural Science Foundation of China(Grant Nos.LY19E010006 and LY21E010005).
文摘As a structural and functional material with excellent properties,ceramics play an extremely important role in a wide range of industries,including life and production.To expand the range of applications for ceramic materials,ceramics are often joined to metals and then used.Among the physical and chemical joining methods of ceramics to metals,the AMB method is efficient and simple,suitable for industrial applications,and has been a hot topic of research.However,due to the problems of residual stresses caused by the large difference in thermal expansion coefficients between ceramic and metal brazing,composite fillers have become a very worthwhile solution by regulating the physical properties of the brazing material and improving the weld structure.This review describes the wetting principle and application of Ag‒Cu‒Ti active metal filler in the field of ceramic joining,with emphasis on the current stage of composite filler,and discusses the influence on the former brazing properties and organization after the introduction of dissimilar materials.