The decomposed process of bastnaesite, monazite and mixed rare earth concentrate in CaO-CaCl-CaCl2 was studied by means of TG-DTA method. The relationship among decomposition ratio, roasting temperature, and CaO-NaCl ...The decomposed process of bastnaesite, monazite and mixed rare earth concentrate in CaO-CaCl-CaCl2 was studied by means of TG-DTA method. The relationship among decomposition ratio, roasting temperature, and CaO-NaCl addition was studied by the quadratic regression orthogonal analysis, and then the regression equation was obtained. Through analysis, the optimum process conditions of mixed rare earth concentrate decomposed by CaO-CaCl-CaCl2 were obtained as follows: roasting temperature: 700℃, CaO addition: 15%, NaCl-CaCl2 addition: 10%, roasting time: 60 min, the decomposition ratio: 91.3%.展开更多
GC technology was used to study escaping fluorine in calcined process of mixed rare earth concentrate. The mixed rare earth concentrate and it adding assistant of CaO-NaCl-CaCl2 were calcined at 400~750 ℃ for 30~12...GC technology was used to study escaping fluorine in calcined process of mixed rare earth concentrate. The mixed rare earth concentrate and it adding assistant of CaO-NaCl-CaCl2 were calcined at 400~750 ℃ for 30~120 min, and then total amount of fluorine, exhausting ratio of fluorine, decomposition ratio and the component were determined. The results showed that adding CaO-NaCl-CaCl2 the decomposition ratio was up to 90% at 700 ℃ in 1 h, and the escaping ratio of fluorine decreased from 29.52% to 0.948%. The average inhabitation ratio was 98.39%. This method supplied basis for low energy and clean decomposition of mixed rare earth concentrate.展开更多
Scheelite and scheelite-wolframite mixed concentrates with different grades were decomposed by caustic soda digestion, and the effects of caustic soda(NaOH) dosage, the ratio of water to ore and the stirring rate on...Scheelite and scheelite-wolframite mixed concentrates with different grades were decomposed by caustic soda digestion, and the effects of caustic soda(NaOH) dosage, the ratio of water to ore and the stirring rate on tungsten recovery were studied. The results show that under the conditions that the ratio of water to ore is (0.8,) stirring rate is 500 r·min-1 and the heating time is 2.0 h at (160 ℃,) the recovery of tungsten reaches 98% for scheelite (w(WO3) is (65.04%)) and wolframite containing high proportion of calcium (w(WO3) is 65.58%, w(Ca) is (7.53%),) when caustic soda dosage is 2.2 and 2.0 times of theoretical value, respectively; the recovery of tungsten can be more than 98%,98% and 96% respectively for low-grade scheelite-wolframite mixed concentrate with (55.78%,) 45.32% and 25.21% WO3, when caustic soda dosage is 2.6,3.2 and 5.5 times of theoretical value, respectively.展开更多
[Objective] This paper was to study effects of pelleted total mixed ration with different concentrate-roughage ratios on production performance and serum biochemical parameters of fattening Hainan black goats.[Method]...[Objective] This paper was to study effects of pelleted total mixed ration with different concentrate-roughage ratios on production performance and serum biochemical parameters of fattening Hainan black goats.[Method] Thirty-six fattening Hainan black goats with the same genetic background and similar initial weight of(14.08±0.13) kg were randomly assigned into three treatments. Goats were fed with Juncao + concentrate(control group), pelleted total mixed ration I(concentrate: roughage 50 ∶50, group Ⅰ) and Ⅱ(concentrate: roughage 45∶55, group Ⅱ), respectively. The test lasted 45 d.[Result] The final weight, daily gain and feed intake of rams in experimental group Ⅰ were significantly higher than those of control group and experimental group Ⅱ(P<0.05);the final weight and daily gain of rams in experimental group Ⅰ were also markedly higher than those of experimental group Ⅱ(P<0.05);the feed/gain of rams in experimental group Ⅰ was significantly lower than those in control group and experimental group Ⅱ(P<0.05). The feed gain cost of rams in experimental group Ⅰ was markedly lower than that in experimental group Ⅱ( P<0.05), but was significantly higher than that in experimental group Ⅰ(P<0.05);the gross profit of rams in experimental group Ⅰ was significantly higher than those in control group and experimental group Ⅱ(P<0.05). Compared with control group and experimental group Ⅱ, the serum total protein and glucose lev-els in experimental group Ⅱ increased significantly(P<0.05), but the urea nitrogen content reduced(P>0.05).[Conclusion] When the concentrateroughage ratio of pelleted total mixed ration was 50∶50, the fattening effect of Hainan black goat was better, and the serum total protein and glucose levels were evidently improved.展开更多
The application of the response surface methodology and the central composite design(CCD) technique for modeling and optimization of the influence of some operating variables on copper,molybdenum and rhenium recover...The application of the response surface methodology and the central composite design(CCD) technique for modeling and optimization of the influence of some operating variables on copper,molybdenum and rhenium recoveries in a bioleaching process was investigated.Three main bioleaching parameters,namely pH,solid concentration and inoculum percent,were changed during the bioleaching tests based on CCD.The ranges of the bioleaching process variables used in the design were as follows:pH1.46-2.14,solid concentration 0.95%-11.05%,and inoculum percent 1.59%-18.41%.A total of 20 bioleaching tests were carried out by the CCD method according to software-based designed matrix.Empirical model equations were developed according to the copper,molybdenum and rhenium recoveries obtained with these three parameters.Model equations of responses at the base of parameters were achieved by using statistical software.The model equations were then individually optimized by using quadratic programming to maximize copper,molybdenum and rhenium recoveries individually within the experimental range.The optimum conditions for copper recovery were pH 1.68,solid concentration 0.95% and the inoculum 18.41%(v/v),while molybdenum and rhenium recoveries were 2.18% and 24.41%,respectively.The predicted values for copper,molybdenum and rhenium recoveries were found to be in good agreement with the experimental values.Also jarosite formation during bioleaching tests was also investigated.展开更多
The loss of rare earths(REs)takes place during the pre-decalcification process of mixed rare earth concentrate.In an effort to reduce such RE loss,a novel idea to improve the leaching selectivity of Ca to REs by apply...The loss of rare earths(REs)takes place during the pre-decalcification process of mixed rare earth concentrate.In an effort to reduce such RE loss,a novel idea to improve the leaching selectivity of Ca to REs by applying selective mechanical activation was proposed.First,regarding the key minerals affecting the leaching selectivity of Ca to REs,the differences in the mechanical activation behaviors of CaF_(2) and REFCO_(3) were studied,and we find that the lattice strain of CaF_(2) increases from 0.21%to 0.42%,whereas that of REFCO_(3) increases from 0.31%to 0.40%.Notably,CaF_(2) demonstrates a larger lattice strain than REFCO_(3),indicating greater mechanical activation energy storage and higher leaching activity.Next,the HCl leaching process was studied.A significant leaching selectivity of Ca to REs,from 21.6 to 35.1,is achieved through mechanical activation.The Ca leaching rate reaches 80.7%when the RE loss is 2.3%in the activated sample.This study provides an novel approach for achieving selective extraction of specific components via mechanical activation pretreatment.展开更多
In recent years,a new process for leaching scheelite concentrates with sulfur-phosphorus mixed acid has been successfully industrialized.This process suffers from the elimination of the retarding effect of calcium sul...In recent years,a new process for leaching scheelite concentrates with sulfur-phosphorus mixed acid has been successfully industrialized.This process suffers from the elimination of the retarding effect of calcium sulfate,the selective extraction of tungsten from the H_(3)PW_(12)O_(40)-H_(2)SO_(4)-H_(3)PO_(4)mixture solution,and the removal of introduced phosphorus.Therefore,in this paper,we investigated the inhibition measures of a calcium sulfate-blocking membrane,the selective extraction of tungsten by ion exchange,and the removal of phosphorus by the magnesium ammonium salt method.The results showed that the addition of calcium sulfate whisker seeds and a higher H_(3)PO_(4)concentration inhibited spontaneous diffuse nucleation,promoted crystal growth,and avoided the formation of a dense blocking film.About 98 wt.%of the scheelite concentrate was digested by H_(2)SO_(4)-H_(3)PO_(4).The selective adsorption of PW_(12)O_(40)^(3-)was realized using D301 resin,and the extraction efficiency of tungsten exceeded 99.9%.After desorption with ammonia water,PW_(12)O_(40)^(3-)was depolymerized into WO_(4)^(2-)and PO_(4)^(3-).99.9 wt.%of phosphorus was removed in the form of MgNH_(4)PO_(4)by the magnesium ammonium salt method,and the residual phosphorus concentration in the solution was lower than 10 mg·L^(-1).After purification,the highest-grade ammonium paratungstate product was prepared by evaporative crystallization.展开更多
The decomposition reactions of monazite and bastnaesite mixed rare earth minerals calcined by CaO-NaCl-CaCl2 were studied by means of TG-DTA and XRD. The results show that the process of the minerals decomposed by CaO...The decomposition reactions of monazite and bastnaesite mixed rare earth minerals calcined by CaO-NaCl-CaCl2 were studied by means of TG-DTA and XRD. The results show that the process of the minerals decomposed by CaO involves two steps. The first step occurs in the temperature range of 425-540 ℃, and the main reactions are bastnaesite decomposition, i.e. REOF reacts with CaO to produce RE2O3 and CaF2, and Ce2O3 is oxidized to CeO2. During this step, CaCO3 is formed at about 500 ℃. The second step takes place in the temperature range of 610-700 ℃, and the reactions are monazite decomposition into RE2O3, Ca5F(PO4)3 and Ca3(PO4)2 by CaO and CaF2. In this process, the decomposition ability is improved because CaO from CaCO3 decomposing has high chemical activity. In calcining process, the new formed Ca5F(PO4)3 restrains fluorine that can escape in form of gaseous compound. The decomposition ratio of the mixed rare earth minerals reaches 90.8% at 700 ℃.展开更多
BaCe0.8Pr0.2O3-α ceramic was synthesized by high temperature solid-state reaction. The structural characteristics and the phase purity of the crystal were determined using powder X-ray diffraction analysis. By using ...BaCe0.8Pr0.2O3-α ceramic was synthesized by high temperature solid-state reaction. The structural characteristics and the phase purity of the crystal were determined using powder X-ray diffraction analysis. By using the methods of AC impedance spectroscopy, gas concentration cell and electrochemical pumping of hydrogen, the conductivity and ionic transport number of BaCe0.8Pr0.2O3-α were measured, and the electrical conduction behavior of the material was investigated in different gases in the temperature range of 500-900℃. The results indicate that the material was of a single perovskite-type orthorhombic phase. From 500℃ to 900 ℃, electronic-hole conduction was dominant in dry and wet oxygen, air or nitrogen, and the total conductivity of the material increased slightly with increasing oxygen partial pressure in the oxygen partial pressure range studied. Ionic conduction was dominant in wet hydrogen, and the total conductivity was about one or two orders of magnitude higher than that in hydrogen-free atmosphere (oxygen, air or nitrogen)展开更多
<span style="font-family:Verdana;">Coordination compounds of 2-amino-3-methylbutanoic acid were synthesized with chromium(III) and oxovanadium(IV) ions. M:L;1:2. Adducts of these complexes using 1,10-p...<span style="font-family:Verdana;">Coordination compounds of 2-amino-3-methylbutanoic acid were synthesized with chromium(III) and oxovanadium(IV) ions. M:L;1:2. Adducts of these complexes using 1,10-phenantroline and ethylenediamine were further synthesized, M:L, (1:2). These compounds were characterized using electronic, infra-red spectrophotometry, magnetic susceptibility measurement and percentage metal analyses. The zones of inhibition and minimum inhibitory concentrations of the compounds against eight microbes were studied. The results obtained indicated an octahedral geometry for the Cr(III) complexes, indicative of additional coordination of two water molecules. On the other hand a square pyramid geometry was obtained for the binary oxovanadium complex and its 1,10-phenantroline adduct. However</span><span style="font-family:Verdana;"><span style="font-family:Verdana;"><span style="font-family:Verdana;">,</span></span></span><span style="font-family:Verdana;"><span style="font-family:Verdana;"><span style="font-family:Verdana;"> for the oxovanadium ethylenediamine adduct a distorted octahedral geometry was proposed. The result for the antibacterial studies indicated that both mixed ligand complexes of 1,10-phenantroline exhibited good antibacterial activity, and in some cases better activity than the standard, streptomycin.</span></span></span>展开更多
As a significant index to evaluate the mixing efficiency,studying the concentration distribution is directly related to the intensity of segregation(I_(s)).In this work,the I_(s) of the mixture composed of NaCl soluti...As a significant index to evaluate the mixing efficiency,studying the concentration distribution is directly related to the intensity of segregation(I_(s)).In this work,the I_(s) of the mixture composed of NaCl solutionwater was investigated experimentally in a rotating bar reactor(RBR)by the conductivity method.The results showed that the mixing efficiency was improved along the axial direction from the bottom to the top in the RBR.The concentration distribution at the bottom section was more uneven,and I_(s) was higher compared with the top section,which decreased from 6.53×10^(-5)to 1.57×10^(-7).With the increase of rotational speed from 0 to 700 r·min^(-1),I_s at the bottom and top sections decreased from 4.27×10^(-3)to 7.10×10^(-5)and from 1.93×10^(-3)to 7.29×10^(-7),respectively.The increases flow rate of solution A,and the decreases of concentration of NaCl and flow rate of solution B gave rise to the reduction of I_(s),signifying an improved mixing efficiency.The results revealed that the conductivity method used in this paper has high efficiency and low cost to measure the I_(s),which indicates a promising prospect for estimating reactors'mixing performance.展开更多
The element iron limitation is one of the crucial factors contributing to high nutrient low chlorophyll in the Southern Ocean(SO).Mixed layer dynamics regulate the availability of iron to phytoplankton.In this paper,w...The element iron limitation is one of the crucial factors contributing to high nutrient low chlorophyll in the Southern Ocean(SO).Mixed layer dynamics regulate the availability of iron to phytoplankton.In this paper,we investigate the influence of surface iron supplementation triggered by the mixed layer depth(MLD)variation on chlorophyll-a(Chl-a)concentration in the SO on seasonal and interannual timescales.This analysis is based on the Biogeochemical Southern Ocean State Estimate for the period from 2013 to 2021.We provide a comprehensive and systematic mapping of the regions within the SO,where Chl-a is affected by iron input related to MLD deepening.The relationship between the MLD and the Chl-a varies with the latitude on the seasonal time scale.Both the MLD and sea ice melting affect the distribution of Chl-a.On the interannual scale,iron supply due to MLD deepening occurs primarily north of 60°S.Horizontal advection-induced entrainment enhances the surface iron input during the austral summer,which favors Chl-a increase.In addition to the MLD,the melting of sea ice and cooling of the sea surface can also alter iron input and subsequently affect Chl-a distribution in the austral summer.During the austral winter,entrainment can boost iron stocks,stimulating a subsequent spring increase of Chl-a in the SO.Furthermore,sea surface temperature declines during the austral winter,promoting an increased iron supply and creating favorable conditions for the subsequent spring Chl-a increase in the SO.展开更多
基金Project supported by the National Natural Science Foundation of China (50574031)Scientific Research Special Foundation of Doctor Subject of Chinese University (20030145015)
文摘The decomposed process of bastnaesite, monazite and mixed rare earth concentrate in CaO-CaCl-CaCl2 was studied by means of TG-DTA method. The relationship among decomposition ratio, roasting temperature, and CaO-NaCl addition was studied by the quadratic regression orthogonal analysis, and then the regression equation was obtained. Through analysis, the optimum process conditions of mixed rare earth concentrate decomposed by CaO-CaCl-CaCl2 were obtained as follows: roasting temperature: 700℃, CaO addition: 15%, NaCl-CaCl2 addition: 10%, roasting time: 60 min, the decomposition ratio: 91.3%.
基金National Natural Science Foundation of China (50574031)
文摘GC technology was used to study escaping fluorine in calcined process of mixed rare earth concentrate. The mixed rare earth concentrate and it adding assistant of CaO-NaCl-CaCl2 were calcined at 400~750 ℃ for 30~120 min, and then total amount of fluorine, exhausting ratio of fluorine, decomposition ratio and the component were determined. The results showed that adding CaO-NaCl-CaCl2 the decomposition ratio was up to 90% at 700 ℃ in 1 h, and the escaping ratio of fluorine decreased from 29.52% to 0.948%. The average inhabitation ratio was 98.39%. This method supplied basis for low energy and clean decomposition of mixed rare earth concentrate.
文摘Scheelite and scheelite-wolframite mixed concentrates with different grades were decomposed by caustic soda digestion, and the effects of caustic soda(NaOH) dosage, the ratio of water to ore and the stirring rate on tungsten recovery were studied. The results show that under the conditions that the ratio of water to ore is (0.8,) stirring rate is 500 r·min-1 and the heating time is 2.0 h at (160 ℃,) the recovery of tungsten reaches 98% for scheelite (w(WO3) is (65.04%)) and wolframite containing high proportion of calcium (w(WO3) is 65.58%, w(Ca) is (7.53%),) when caustic soda dosage is 2.2 and 2.0 times of theoretical value, respectively; the recovery of tungsten can be more than 98%,98% and 96% respectively for low-grade scheelite-wolframite mixed concentrate with (55.78%,) 45.32% and 25.21% WO3, when caustic soda dosage is 2.6,3.2 and 5.5 times of theoretical value, respectively.
基金Supported by Major Science and Technology Program of Hainan Province(ZDKJ2016017-01,ZDKJ2016017-03)Youth Science and Technology Talents Innovation Project of Hainan Science&Technology Association(QCXM201802)
文摘[Objective] This paper was to study effects of pelleted total mixed ration with different concentrate-roughage ratios on production performance and serum biochemical parameters of fattening Hainan black goats.[Method] Thirty-six fattening Hainan black goats with the same genetic background and similar initial weight of(14.08±0.13) kg were randomly assigned into three treatments. Goats were fed with Juncao + concentrate(control group), pelleted total mixed ration I(concentrate: roughage 50 ∶50, group Ⅰ) and Ⅱ(concentrate: roughage 45∶55, group Ⅱ), respectively. The test lasted 45 d.[Result] The final weight, daily gain and feed intake of rams in experimental group Ⅰ were significantly higher than those of control group and experimental group Ⅱ(P<0.05);the final weight and daily gain of rams in experimental group Ⅰ were also markedly higher than those of experimental group Ⅱ(P<0.05);the feed/gain of rams in experimental group Ⅰ was significantly lower than those in control group and experimental group Ⅱ(P<0.05). The feed gain cost of rams in experimental group Ⅰ was markedly lower than that in experimental group Ⅱ( P<0.05), but was significantly higher than that in experimental group Ⅰ(P<0.05);the gross profit of rams in experimental group Ⅰ was significantly higher than those in control group and experimental group Ⅱ(P<0.05). Compared with control group and experimental group Ⅱ, the serum total protein and glucose lev-els in experimental group Ⅱ increased significantly(P<0.05), but the urea nitrogen content reduced(P>0.05).[Conclusion] When the concentrateroughage ratio of pelleted total mixed ration was 50∶50, the fattening effect of Hainan black goat was better, and the serum total protein and glucose levels were evidently improved.
基金supported by the National Iranian Copper Industry Co. and Geological Survey of Iran
文摘The application of the response surface methodology and the central composite design(CCD) technique for modeling and optimization of the influence of some operating variables on copper,molybdenum and rhenium recoveries in a bioleaching process was investigated.Three main bioleaching parameters,namely pH,solid concentration and inoculum percent,were changed during the bioleaching tests based on CCD.The ranges of the bioleaching process variables used in the design were as follows:pH1.46-2.14,solid concentration 0.95%-11.05%,and inoculum percent 1.59%-18.41%.A total of 20 bioleaching tests were carried out by the CCD method according to software-based designed matrix.Empirical model equations were developed according to the copper,molybdenum and rhenium recoveries obtained with these three parameters.Model equations of responses at the base of parameters were achieved by using statistical software.The model equations were then individually optimized by using quadratic programming to maximize copper,molybdenum and rhenium recoveries individually within the experimental range.The optimum conditions for copper recovery were pH 1.68,solid concentration 0.95% and the inoculum 18.41%(v/v),while molybdenum and rhenium recoveries were 2.18% and 24.41%,respectively.The predicted values for copper,molybdenum and rhenium recoveries were found to be in good agreement with the experimental values.Also jarosite formation during bioleaching tests was also investigated.
基金Project supported by the National Natural Science Foundation of China(52004252)Natural Science Foundation ofHenan Province(222300420548)Strategic Research and Consulting Project of Chinese Academy of Engineering(2022-XBZD-07)。
文摘The loss of rare earths(REs)takes place during the pre-decalcification process of mixed rare earth concentrate.In an effort to reduce such RE loss,a novel idea to improve the leaching selectivity of Ca to REs by applying selective mechanical activation was proposed.First,regarding the key minerals affecting the leaching selectivity of Ca to REs,the differences in the mechanical activation behaviors of CaF_(2) and REFCO_(3) were studied,and we find that the lattice strain of CaF_(2) increases from 0.21%to 0.42%,whereas that of REFCO_(3) increases from 0.31%to 0.40%.Notably,CaF_(2) demonstrates a larger lattice strain than REFCO_(3),indicating greater mechanical activation energy storage and higher leaching activity.Next,the HCl leaching process was studied.A significant leaching selectivity of Ca to REs,from 21.6 to 35.1,is achieved through mechanical activation.The Ca leaching rate reaches 80.7%when the RE loss is 2.3%in the activated sample.This study provides an novel approach for achieving selective extraction of specific components via mechanical activation pretreatment.
基金jointly supported by the National Natural Science Foundation of China(No.51334008)the Basic Science Center of the National Natural Science Foundation of China(72088101)the National Key Research and Development Program of China(No.2022YFC2904505)。
文摘In recent years,a new process for leaching scheelite concentrates with sulfur-phosphorus mixed acid has been successfully industrialized.This process suffers from the elimination of the retarding effect of calcium sulfate,the selective extraction of tungsten from the H_(3)PW_(12)O_(40)-H_(2)SO_(4)-H_(3)PO_(4)mixture solution,and the removal of introduced phosphorus.Therefore,in this paper,we investigated the inhibition measures of a calcium sulfate-blocking membrane,the selective extraction of tungsten by ion exchange,and the removal of phosphorus by the magnesium ammonium salt method.The results showed that the addition of calcium sulfate whisker seeds and a higher H_(3)PO_(4)concentration inhibited spontaneous diffuse nucleation,promoted crystal growth,and avoided the formation of a dense blocking film.About 98 wt.%of the scheelite concentrate was digested by H_(2)SO_(4)-H_(3)PO_(4).The selective adsorption of PW_(12)O_(40)^(3-)was realized using D301 resin,and the extraction efficiency of tungsten exceeded 99.9%.After desorption with ammonia water,PW_(12)O_(40)^(3-)was depolymerized into WO_(4)^(2-)and PO_(4)^(3-).99.9 wt.%of phosphorus was removed in the form of MgNH_(4)PO_(4)by the magnesium ammonium salt method,and the residual phosphorus concentration in the solution was lower than 10 mg·L^(-1).After purification,the highest-grade ammonium paratungstate product was prepared by evaporative crystallization.
基金Project(50574031) supported by the National Natural Science Foundation of ChinaProject(20030145015) supported by the Scientific Research Special Foundation of Doctoral Subject of Chinese University
文摘The decomposition reactions of monazite and bastnaesite mixed rare earth minerals calcined by CaO-NaCl-CaCl2 were studied by means of TG-DTA and XRD. The results show that the process of the minerals decomposed by CaO involves two steps. The first step occurs in the temperature range of 425-540 ℃, and the main reactions are bastnaesite decomposition, i.e. REOF reacts with CaO to produce RE2O3 and CaF2, and Ce2O3 is oxidized to CeO2. During this step, CaCO3 is formed at about 500 ℃. The second step takes place in the temperature range of 610-700 ℃, and the reactions are monazite decomposition into RE2O3, Ca5F(PO4)3 and Ca3(PO4)2 by CaO and CaF2. In this process, the decomposition ability is improved because CaO from CaCO3 decomposing has high chemical activity. In calcining process, the new formed Ca5F(PO4)3 restrains fluorine that can escape in form of gaseous compound. The decomposition ratio of the mixed rare earth minerals reaches 90.8% at 700 ℃.
基金This work was supported by the National Natural Science Foundation of China (No.20771079) and the Natural Science Foundation of Education Department of Jiangsu Province (No.07KJB150126).
文摘BaCe0.8Pr0.2O3-α ceramic was synthesized by high temperature solid-state reaction. The structural characteristics and the phase purity of the crystal were determined using powder X-ray diffraction analysis. By using the methods of AC impedance spectroscopy, gas concentration cell and electrochemical pumping of hydrogen, the conductivity and ionic transport number of BaCe0.8Pr0.2O3-α were measured, and the electrical conduction behavior of the material was investigated in different gases in the temperature range of 500-900℃. The results indicate that the material was of a single perovskite-type orthorhombic phase. From 500℃ to 900 ℃, electronic-hole conduction was dominant in dry and wet oxygen, air or nitrogen, and the total conductivity of the material increased slightly with increasing oxygen partial pressure in the oxygen partial pressure range studied. Ionic conduction was dominant in wet hydrogen, and the total conductivity was about one or two orders of magnitude higher than that in hydrogen-free atmosphere (oxygen, air or nitrogen)
文摘<span style="font-family:Verdana;">Coordination compounds of 2-amino-3-methylbutanoic acid were synthesized with chromium(III) and oxovanadium(IV) ions. M:L;1:2. Adducts of these complexes using 1,10-phenantroline and ethylenediamine were further synthesized, M:L, (1:2). These compounds were characterized using electronic, infra-red spectrophotometry, magnetic susceptibility measurement and percentage metal analyses. The zones of inhibition and minimum inhibitory concentrations of the compounds against eight microbes were studied. The results obtained indicated an octahedral geometry for the Cr(III) complexes, indicative of additional coordination of two water molecules. On the other hand a square pyramid geometry was obtained for the binary oxovanadium complex and its 1,10-phenantroline adduct. However</span><span style="font-family:Verdana;"><span style="font-family:Verdana;"><span style="font-family:Verdana;">,</span></span></span><span style="font-family:Verdana;"><span style="font-family:Verdana;"><span style="font-family:Verdana;"> for the oxovanadium ethylenediamine adduct a distorted octahedral geometry was proposed. The result for the antibacterial studies indicated that both mixed ligand complexes of 1,10-phenantroline exhibited good antibacterial activity, and in some cases better activity than the standard, streptomycin.</span></span></span>
基金supported by the National Natural Science Foundation of China(21725601)。
文摘As a significant index to evaluate the mixing efficiency,studying the concentration distribution is directly related to the intensity of segregation(I_(s)).In this work,the I_(s) of the mixture composed of NaCl solutionwater was investigated experimentally in a rotating bar reactor(RBR)by the conductivity method.The results showed that the mixing efficiency was improved along the axial direction from the bottom to the top in the RBR.The concentration distribution at the bottom section was more uneven,and I_(s) was higher compared with the top section,which decreased from 6.53×10^(-5)to 1.57×10^(-7).With the increase of rotational speed from 0 to 700 r·min^(-1),I_s at the bottom and top sections decreased from 4.27×10^(-3)to 7.10×10^(-5)and from 1.93×10^(-3)to 7.29×10^(-7),respectively.The increases flow rate of solution A,and the decreases of concentration of NaCl and flow rate of solution B gave rise to the reduction of I_(s),signifying an improved mixing efficiency.The results revealed that the conductivity method used in this paper has high efficiency and low cost to measure the I_(s),which indicates a promising prospect for estimating reactors'mixing performance.
基金The fund from Ministry of Science and Technology of the People’s Republic of China under contract No.2023YFF0805204the Natural Science Foundation of Yunnan Province under contract No.202302AN360006the National Natural Science Foundation of China under contract No.41776019.
文摘The element iron limitation is one of the crucial factors contributing to high nutrient low chlorophyll in the Southern Ocean(SO).Mixed layer dynamics regulate the availability of iron to phytoplankton.In this paper,we investigate the influence of surface iron supplementation triggered by the mixed layer depth(MLD)variation on chlorophyll-a(Chl-a)concentration in the SO on seasonal and interannual timescales.This analysis is based on the Biogeochemical Southern Ocean State Estimate for the period from 2013 to 2021.We provide a comprehensive and systematic mapping of the regions within the SO,where Chl-a is affected by iron input related to MLD deepening.The relationship between the MLD and the Chl-a varies with the latitude on the seasonal time scale.Both the MLD and sea ice melting affect the distribution of Chl-a.On the interannual scale,iron supply due to MLD deepening occurs primarily north of 60°S.Horizontal advection-induced entrainment enhances the surface iron input during the austral summer,which favors Chl-a increase.In addition to the MLD,the melting of sea ice and cooling of the sea surface can also alter iron input and subsequently affect Chl-a distribution in the austral summer.During the austral winter,entrainment can boost iron stocks,stimulating a subsequent spring increase of Chl-a in the SO.Furthermore,sea surface temperature declines during the austral winter,promoting an increased iron supply and creating favorable conditions for the subsequent spring Chl-a increase in the SO.