Experimental and numerical investigations of interface properties of Ti6Al4V/CP-Ti/Copper composite plate prepared by explosive welding 被引量:3
1
作者 Yasir Mahmood Peng-wan Chen +1 位作者 I.A.Bataev Xin Gao 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2021年第5期1592-1601,共10页
Explosive welding technique is widely used in many industries.This technique is useful to weld different kinds of metal alloys that are not easily welded by any other welding methods.Interlayer plays an important role... Explosive welding technique is widely used in many industries.This technique is useful to weld different kinds of metal alloys that are not easily welded by any other welding methods.Interlayer plays an important role to improve the welding quality and control energy loss during the collision process.In this paper,the Ti6Al4V plate was welded with a copper plate in the presence of a commercially pure titanium interlayer.Microstructure details of welded composite plate were observed through optical and scanning electron microscope.Interlayer-base plate interface morphology showed a wavy structure with solid melted regions inside the vortices.Moreover,the energy dispersive spectroscopy analysis in the interlayer-base interface reveals that there are some identified regions of different kinds of chemical equilibrium phases of CueTi,i.e.CuTi,Cu_(2)Ti,CuTi_(2),Cu_(4)Ti,etc.To study the mechanical properties of composite plates,mechanical tests were conducted,including the tensile test,bending test,shear test and Vickers hardness test.Numerical simulation of explosive welding process was performed with coupled Smooth Particle Hydrodynamic method,Euler and Arbitrary Lagrangian-Eulerian method.The multi-physics process of explosive welding,including detonation,jetting and interface morphology,was observed with simulation.Moreover,simulated plastic strain,temperature and pressure profiles were analysed to understand the welding conditions.Simulated results show that the interlayer base plate interface was created due to the high plastic deformation and localized melting of the parent plates.At the collision point,both alloys behave like fluids,resulting in the formation of a wavy morphology with vortices,which is in good agreement with the experimental results. 展开更多
关键词 Explosive welding Ti6Al4V/cp-ti/Cu Smooth particle hydrodynamic(SPH) Microstructure Mechanical properties
下载PDF
溢料槽形状对使用外部工具摩擦焊接的CP-Ti管与304L不锈钢管板的接头性能的影响(英文)
2
作者 C.MAXWELL REJIL C.SHARAN +1 位作者 S.MUTHUKUMARAN M.VASUDEVAN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2016年第8期2067-2078,共12页
通过使用外部工具的管子与管板摩擦焊(FWTPET)来焊接钛管和不锈钢管板。铜被用作连接不同材料的夹层,同时用来减小在接头界面形成的金属间化合物的影响。控制FWTPET过程的工艺参数包括切入速率、旋转速度、切入深度、轴向载荷和溢料槽... 通过使用外部工具的管子与管板摩擦焊(FWTPET)来焊接钛管和不锈钢管板。铜被用作连接不同材料的夹层,同时用来减小在接头界面形成的金属间化合物的影响。控制FWTPET过程的工艺参数包括切入速率、旋转速度、切入深度、轴向载荷和溢料槽形状。其中,管的溢料槽形状对接头完整性具有很大的影响。在焊接到不锈钢管板的钛管上制作了各种溢料槽形状,如垂直槽、洞、曲折洞和花瓣型。宏观和微观研究表明接头没有缺陷。X射线衍射(XRD)、扫描电镜(SEM)和能谱(EDS)分析表明了铜层和金属间化合物的存在。研究横向和纵向焊接界面的显微硬度。使用一种新的测试程序称为"切入剪切试验"来检测焊接接头的性能。具有花瓣型溢料槽形状的试样具有最高的剪切断裂载荷(31.58 k N)。使用SEM进一步表征剪切面。 展开更多
关键词 304L不锈钢管板 cp-ti 摩擦焊 接头性能 溢料槽 外部工具
下载PDF
烧结方法对CP-Ti粉末烧结块显微组织和力学性能的影响(英文)
3
作者 Je-ha SHON Jong-moon PARK +3 位作者 Kyeong-sik CHO Jae-keun HONG Nho-kwang PARK Myung-hoon OH 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第S1期59-67,共9页
研究不同烧结方法,包括放电等离子体烧结(SPS)、热压(HP)和电阻烧结(ERS),对商用纯钛(CP-Ti)粉末固结后显微组织和力学性能的影响。选用的粉末粒度分别为【147μm,【74μm和【43μm,粉末粒度越小,其致密化过程越快。在850°C、30 MP... 研究不同烧结方法,包括放电等离子体烧结(SPS)、热压(HP)和电阻烧结(ERS),对商用纯钛(CP-Ti)粉末固结后显微组织和力学性能的影响。选用的粉末粒度分别为【147μm,【74μm和【43μm,粉末粒度越小,其致密化过程越快。在850°C、30 MPa条件下进行SPS和HP,获得烧结体的相对密度高达99%。而通过ERS,则在950°C、30 MPa条件下才发生CP-Ti粉末的致密化。在850~950°C获得烧结钛的显微组织由等轴晶构成。对于粒度【43μm粉末,在850°C、30 MPa条件下通过SPS制备烧结体,其屈服强度为868 MPa。随着小尺寸颗粒含量的升高,通过SPS和HP制备烧结体的屈服强度得到提高。然而在950°C、30MPa条件下,通过ERS制备样品的最高屈服强度仅为441 MPa,比SPS和HP样品的低。与SPS和HP相比,ERS需要较短的烧结时间,但较高的烧结温度导致材料的脆性断裂,使其强度和伸长率降低。 展开更多
关键词 cp-ti粉末 烧结方法 放电等离子体烧结 热压 电阻烧结
下载PDF
CP-Ti激光焊接接头组织与性能研究
4
作者 黄忠宝 王鹏飞 +2 位作者 尚立宝 陈永亮 刘登邦 《电焊机》 2018年第12期13-16,共4页
采用光学显微镜等观察和测试CP-Ti激光焊接头组织和硬度,对比接头在酸性、中性和碱性环境中的耐腐蚀性能。结果表明:接头各区域组织均为α相,其中焊缝中的α晶呈针状、锯齿状和板条状3种形貌,在热影响区则为锯齿状。硬度测试表明,焊缝... 采用光学显微镜等观察和测试CP-Ti激光焊接头组织和硬度,对比接头在酸性、中性和碱性环境中的耐腐蚀性能。结果表明:接头各区域组织均为α相,其中焊缝中的α晶呈针状、锯齿状和板条状3种形貌,在热影响区则为锯齿状。硬度测试表明,焊缝为接头硬度值最高区域,显微硬度达到210 HV,热影响区次之,约为165 HV。接头在酸性环境中的耐蚀性最差,表现为其电流密度、腐蚀速率均高于碱性和中性环境中的。 展开更多
关键词 cp-ti 晶粒 显微硬度 电流密度 耐蚀性
下载PDF
CP-Ti在含氟离子硝酸中电化学腐蚀行为 被引量:1
5
作者 徐建平 苏航标 +4 位作者 郭荻子 王晓 赵永庆 许并社 周廉 《钛工业进展》 CAS 北大核心 2019年第1期30-34,共5页
采用开路电位(OCP)、动电位极化曲线(PPC)、电化学阻抗谱(EIS) 3种电化学测试手段对工业纯钛(CP-Ti)在含氟离子硝酸溶液中的电化学腐蚀行为进行研究。结果表明:随着硝酸溶液中氟离子浓度的增加,CP-Ti耐蚀性变差;影响CP-Ti耐蚀性转变的... 采用开路电位(OCP)、动电位极化曲线(PPC)、电化学阻抗谱(EIS) 3种电化学测试手段对工业纯钛(CP-Ti)在含氟离子硝酸溶液中的电化学腐蚀行为进行研究。结果表明:随着硝酸溶液中氟离子浓度的增加,CP-Ti耐蚀性变差;影响CP-Ti耐蚀性转变的临界氟离子浓度为1. 25 mmol/L;氟离子与CP-Ti表面的氧化膜发生反应,致使均匀、致密的氧化膜溶解转变为多孔膜,降低了CP-Ti的耐蚀性。 展开更多
关键词 工业纯钛 电化学腐蚀 氟离子 硝酸
下载PDF
CP-Ti棒材加热拉压不对称变形研究
6
作者 张晓丽 严思梁 《内燃机与配件》 2019年第9期104-105,共2页
近年来,随着国民经济的发展和国防工业建设的突飞猛进,高性能、轻量化高端精密构件的技术性需求日益增加。CP-Ti是一种新型结构材料,具有密度小、比强度高、抗蚀抗疲劳等优异的综合性能,能够满足新型飞机研制对机身减重、提高飞行机动... 近年来,随着国民经济的发展和国防工业建设的突飞猛进,高性能、轻量化高端精密构件的技术性需求日益增加。CP-Ti是一种新型结构材料,具有密度小、比强度高、抗蚀抗疲劳等优异的综合性能,能够满足新型飞机研制对机身减重、提高飞行机动性等方面的需求,在航空、航天、汽车、造船等行业获得日益广泛的应用,其中钛产量中约70%用于航空宇航工业。然而CP-Ti在室温下塑性变形过程中存在变形抗力大、延伸率很低、材料流动性差以及成形质量差等问题,如何提高CP-Ti的塑性成形能力成为其塑性变形过程研究中亟待解决的问题。本文选取CP-Ti棒材,通过对棒材试样进行不同温度、速率的单向拉压试验,获得其真应力-真应变曲线,并分析其在拉压加载下的硬化关系。 展开更多
关键词 cp-ti 塑形变形 加工硬化
下载PDF
室温动态等径角挤压CP-Ti的变形孪晶研究 被引量:3
7
作者 冯永智 卢磊 钟政烨 《有色金属工程》 CAS 北大核心 2020年第7期20-25,39,共7页
室温下运用动态等径角挤压(D-ECAP)技术实现了工业纯钛(CP-Ti)在L型模具内的高应变率剪切变形,结合电子背散射衍射(EBSD)技术研究了CP-Ti动态剧烈塑性变形过程中的孪生行为。结果表明,D-ECAP变形在CP-Ti中激发了大量的一次{1122}和{1012... 室温下运用动态等径角挤压(D-ECAP)技术实现了工业纯钛(CP-Ti)在L型模具内的高应变率剪切变形,结合电子背散射衍射(EBSD)技术研究了CP-Ti动态剧烈塑性变形过程中的孪生行为。结果表明,D-ECAP变形在CP-Ti中激发了大量的一次{1122}和{1012}孪晶,同时生成了少量的一次{1121}、{1011}、{1123}和{1124}孪晶。在单个晶粒内部,一次{1122}压缩孪晶和一次{1012}拉伸孪晶分别存在四种和两种孪晶变体,以一次{1122}压缩孪晶和一次{1012}拉伸孪晶为基体可进一步激发二次{1122}-{1121}、{1122}-{1012}和{1012}-{1122}孪晶以及三次{1122}-{1012}-{1122}和{1012}-{1122}-{1012}孪晶,其中二次{1122}-{1012}和{1012}-{1122}孪晶均存在两种孪晶变体。 展开更多
关键词 动态等径角挤压变形 工业纯钛 变形孪晶
下载PDF
Microstructural Evolution of Infrared Brazed CP-Ti Using Ti-Cu-Ni Brazes 被引量:2
8
作者 C.T.Chang T.Y.Yeh +1 位作者 R.K.Shiue C.S.Chang 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2011年第2期131-138,共8页
关键词 Infrared Brazing cp-ti Ti-Cu-Ni fillers MICROSTRUCTURE
原文传递
The Effects of Aging Time on the Structural and Electrochemical Properties of Composite Coatings on CP-Ti Substrate 被引量:1
9
作者 Onur Comakli Mustafa Yazici +2 位作者 Tuba Yetim Ali Fatih Yetim Ayhan Celik 《Journal of Bionic Engineering》 SCIE EI CSCD 2017年第3期532-539,共8页
TiO2-SiO2 composite films were produced on commercially pure titanium (CP-Ti) substrate by a sol-gel method to in- vestigate the behavior of sol aging time and its potential effects on the structural and electrochem... TiO2-SiO2 composite films were produced on commercially pure titanium (CP-Ti) substrate by a sol-gel method to in- vestigate the behavior of sol aging time and its potential effects on the structural and electrochemical properties of composite coatings. Anatase-TiO2 and quartz-SiO2 peaks were observed on all composite coated samples according to XRD results. It was observed that the average grain size increased with sol aging time. Also, the average smallest grain size was seen at composite coatings prepared from unaged sol according to the width of the peaks. Electrochemical behavior of coated samples was mainly investigated by potentiodynamic polarization and Electrochemical Impedance Spectroscopy (EIS) in Simulated Body Fluid (SBF) solution. In corrosion tests, the composite coatings showed better anti-corrosion behavior than that of uncoated samples. In addition, the corrosion properties of the composite films were considerably affected by sol aging time. Corrosion resistance of coatings decreased with increasing aging time and the best result was obtained from composite coatings prepared from unaged sol. 展开更多
关键词 bioinspired TiO2-SiO2 coatings cp-ti substrate electrochemical properties SOL-GEL
原文传递
Design and performance evaluation of additively manufactured composite lattice structures of commercially pure Ti(CP-Ti) 被引量:2
10
作者 Wei Xu Aihua Yu +7 位作者 Xin Lu Maryam Tamaddon Mengdi Wang Jiazhen Zhang Jianliang Zhang Xuanhui Qu Chaozong Liu Bo Su 《Bioactive Materials》 SCIE 2021年第5期1215-1222,共8页
Ti alloys with lattice structures are garnering more and more attention in the field of bone repair or regeneration due to their superior structural,mechanical,and biological properties.In this study,six types of comp... Ti alloys with lattice structures are garnering more and more attention in the field of bone repair or regeneration due to their superior structural,mechanical,and biological properties.In this study,six types of composite lattice structures with different strut radius that consist of simple cubic(structure A),body-centered cubic(structure B),and edge-centered cubic(structure C)unit cells are designed.The designed structures are firstly simulated and analysed by the finite element(FE)method.Commercially pure Ti(CP-Ti)lattice structures with optimized unit cells and strut radius are then fabricated by selective laser melting(SLM),and the dimensions,microtopography,and mechanical properties are characterised.The results show that among the six types of composite lattice structures,combined BA,CA,and CB structures exhibit smaller maximum von-Mises stress,indicating that these structures have higher strength.Based on the fitting curves of stress/specific surface area versus strut radius,the optimized strut radius of BA,CA,and CB structures is 0.28,0.23,and 0.30 mm respectively.Their corresponding compressive yield strength and compressive modulus are 42.28,30.11,and 176.96 MPa,and 4.13,2.16,and 7.84 GPa,respectively.The CP-Ti with CB unit structure presents a similar strength and compressive modulus to the cortical bone,which makes it a potential candidate for subchondral bone restorations. 展开更多
关键词 Composite lattice structure Finite element modelling Selective laser melting(SLM) cp-ti
原文传递
多维度立体塑型Ti-CP术对颅骨缺损患者应用研究
11
作者 张卿云 《现代科学仪器》 2024年第2期98-102,共5页
目的:探究多维度立体塑型Ti-CP术在颅骨缺损患者的应用。方法:选取2020年1月至2023年6月住院行颅骨修补术的60例患者作为研究对象。观察组行多维度立体塑型技术进行颅骨修补;对照组应用传统的钛网进行颅骨修补。比较两组患者术中出血量... 目的:探究多维度立体塑型Ti-CP术在颅骨缺损患者的应用。方法:选取2020年1月至2023年6月住院行颅骨修补术的60例患者作为研究对象。观察组行多维度立体塑型技术进行颅骨修补;对照组应用传统的钛网进行颅骨修补。比较两组患者术中出血量、手术持续时间、住院时间,术前及术后行NIHSS评分、GCS评分,统计术后并发症情况。结果:观察组术中出血量、手术时间、住院时间均较低(P<0.05);干预前两组NIHSS、GCS评分无差异(P>0.05);干预后观察组NIHSS评分降低,GCS评分升高(P<0.05);两组患者并发症的总发生率为18.00%、4.00%(P<0.05)。结论:多维度立体塑型改进下Ti-CP术可达到颅骨生理解剖修复,可缩短治疗时间,改善神经功能,降低并发症。 展开更多
关键词 颅骨缺损 多维度立体塑型技术 Ti-CP术 神经功能 并发症
下载PDF
CP-Ti在含氟离子硝酸中表面附着物形成研究
12
作者 徐建平 苏航标 +3 位作者 郭荻子 赵永庆 许并社 周廉 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2019年第11期3615-3620,共6页
钛具有优良的耐蚀性能,可长期工作在高浓度的沸腾硝酸介质中,是商业后处理较为理想的设备用材。采用SEM、EDS、XRD、XPS等表征手段对CP-Ti在含氟离子硝酸中试样表面出现的白色附着物进行分析,并解释其形成机理。结果表明:氟离子浓度在50... 钛具有优良的耐蚀性能,可长期工作在高浓度的沸腾硝酸介质中,是商业后处理较为理想的设备用材。采用SEM、EDS、XRD、XPS等表征手段对CP-Ti在含氟离子硝酸中试样表面出现的白色附着物进行分析,并解释其形成机理。结果表明:氟离子浓度在50μL/L以下时,CP-Ti腐蚀速率呈现由大到小并趋于稳定的规律;氟离子浓度在50μL/L及以上时,腐蚀速率呈现由大到小再变大的“v”型规律。试样表面的白色附着物的物相为TiO2,其形成机理为:先是试样表面多孔膜的形成;其次是TiO2以多孔膜上的孔为基点进行生长、脱落。 展开更多
关键词 工业纯钛 氟离子 TIO2 多孔膜 硝酸
原文传递
工业纯钛在120°模具中的多道次ECAP室温变形组织与性能(英文) 被引量:22
13
作者 杨西荣 赵西成 付文杰 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2009年第6期955-957,共3页
在室温,采用通道夹角为120°的变形模具对工业纯钛(Commercial Pure Titanium,CP-Ti)以Bc方式实施四道次ECAP(Equal Channel Angular Pressing)挤压变形,成功获得表面光滑无裂纹的变形试样。文中主要研究了工业纯钛在室温下进行ECA... 在室温,采用通道夹角为120°的变形模具对工业纯钛(Commercial Pure Titanium,CP-Ti)以Bc方式实施四道次ECAP(Equal Channel Angular Pressing)挤压变形,成功获得表面光滑无裂纹的变形试样。文中主要研究了工业纯钛在室温下进行ECAP多道次变形的组织结构演变,并测试了变形试样的力学性能。微观结构显示工业纯钛在室温下进行多道次ECAP变形时,只在前两道次产生了大量的变形孪晶,且随道次增加变形孪晶逐渐消失。最终获得的试样晶粒平均尺寸由最初的约28μm细化到约250nm,试样断裂强度和显微硬度分别提高到773和2486MPa,而试样仍保持较好的延伸率(可达16.8%)。 展开更多
关键词 等径弯曲通道变形(ECAP) 工业纯钛(cp-ti) 组织结构 机械性能
下载PDF
ZrCuNi中间层瞬间液相焊扩散连接纯钛TA2工艺研究
14
作者 杨浩哲 裴夤崟 +3 位作者 沈元勋 秦建 李秀朋 刘德运 《电焊机》 2023年第4期81-89,共9页
使用Cu、Ni纯金属箔厚度为0.01 mm,Zr纯金属箔厚度分别为0.01 mm、0.02 mm和0.03 mm的ZrCuNi中间层在880℃×30 min工艺条件下对TA2纯钛进行瞬间液相焊连接试验,研究了接头界面组织演化机理、中间层元素扩散作用及接头的力学性能。... 使用Cu、Ni纯金属箔厚度为0.01 mm,Zr纯金属箔厚度分别为0.01 mm、0.02 mm和0.03 mm的ZrCuNi中间层在880℃×30 min工艺条件下对TA2纯钛进行瞬间液相焊连接试验,研究了接头界面组织演化机理、中间层元素扩散作用及接头的力学性能。结果表明,接头界面组织由焊缝中心化合物层和两侧共析组织构成,在中间层Zr箔厚度为0.01 mm时,焊缝中心形成了厚度约10μm的连续带状(Ti,Zr)_(2)(Cu,Ni)金属间化合物,当Zr箔厚度提高到0.02 mm、0.03 mm时,焊缝中心形成含有(Ti,Zr)_(2)(Cu,Ni)化合物的共晶组织,共晶组织厚度先增加到80μm后降低到37μm。焊缝中(Ti,Zr)_(2)(Cu,Ni)化合物层维氏硬度在500 HV0.1以上,其厚度减小有助于提高接头强度,中间层Zr箔为0.01 mm时接头的剪切强度最高,平均值为207 MPa,裂纹沿焊缝中心化合物层和两侧共析组织扩展,断口具有韧窝特征和河流状花样,为韧性-脆性复合断裂模式,Zr箔厚度提高到0.02 mm、0.03 mm时,接头剪切强度分别为92 MPa和135 MPa,裂纹沿焊缝中心共晶组织扩展延伸,断口形貌显示的小平面解理特征是(Ti,Zr)_(2)(Cu,Ni)化合物断口的典型形貌。 展开更多
关键词 纯钛 瞬间液相焊 ZrCuNi中间层 显微组织 力学性能
下载PDF
工业纯钛室温一道次ECAP加工后的组织和硬度 被引量:2
15
作者 雷娜 赵西成 +1 位作者 杨西荣 赵健 《热加工工艺》 CSCD 北大核心 2011年第12期13-15,59,共4页
室温下,分别采用90°模具和120°模具对工业纯钛(CP-Ti)进行一道次等径弯曲通道变形(Equal ChannelAngular Pressing,简称ECAP),研究了其组织和硬度的变化情况。结果表明,工业纯钛经一道次ECAP变形后都形成板条状组织,硬度显著... 室温下,分别采用90°模具和120°模具对工业纯钛(CP-Ti)进行一道次等径弯曲通道变形(Equal ChannelAngular Pressing,简称ECAP),研究了其组织和硬度的变化情况。结果表明,工业纯钛经一道次ECAP变形后都形成板条状组织,硬度显著提高。90°模具挤压后试样上、下表面的硬度值稍低于试样中间的硬度值,而120°模具挤压后试样表面硬度分布较均匀。 展开更多
关键词 工业纯钛(cp-ti) 等径弯曲通道变形 硬度
下载PDF
剧烈塑性变形条件下工业纯钛晶粒细化机理研究 被引量:7
16
作者 何晓梅 朱晓雅 +1 位作者 董洁 刘晓燕 《热加工工艺》 CSCD 北大核心 2009年第22期56-58,63,共4页
通过对工业纯钛表面机械研磨(SMAT)这种变形方式的结果和微观组织变化的研究,分析了工业纯钛的晶粒细化机制,讨论了其他剧烈塑性变形技术无法制备出晶粒尺寸更小的纳米晶的原因。结果表明:对于工业纯钛,SMAT这种具有高的应变速率和多方... 通过对工业纯钛表面机械研磨(SMAT)这种变形方式的结果和微观组织变化的研究,分析了工业纯钛的晶粒细化机制,讨论了其他剧烈塑性变形技术无法制备出晶粒尺寸更小的纳米晶的原因。结果表明:对于工业纯钛,SMAT这种具有高的应变速率和多方向载荷的变形方式,有利于形成细小的纳米晶;同时高应变速率增加了位错滑移的临界分切应力。 展开更多
关键词 工业纯钛 表面机械研磨(SMAT) 剧烈塑性变形 晶粒细化机制
下载PDF
轧制变形超细晶纯钛的电化学腐蚀行为 被引量:5
17
作者 江鸿 雷君相 谢超英 《塑性工程学报》 CAS CSCD 北大核心 2016年第6期187-193,共7页
工业纯钛经过8道次等通道弯角挤压处理后,在室温或液氮温度下进行轧制。随后以林格式人工模拟体液为腐蚀介质,对两步大变形前后纯钛的电化学腐蚀行为进行了研究。结果表明,8道次ECAE处理后获得的超细晶纯钛,较退火粗晶态具有更好的轧制... 工业纯钛经过8道次等通道弯角挤压处理后,在室温或液氮温度下进行轧制。随后以林格式人工模拟体液为腐蚀介质,对两步大变形前后纯钛的电化学腐蚀行为进行了研究。结果表明,8道次ECAE处理后获得的超细晶纯钛,较退火粗晶态具有更好的轧制变形能力。两步大变形制备超细晶纯钛不仅表现出良好的综合力学性能,而且具备优异的耐腐蚀性能。8道次ECAE处理的纯钛在室温冷轧后的耐腐蚀性较液氮温度冷轧后好,主要因为不同温度轧制织构组分改变使得平行于样品表面的晶面变为密排面或低指数晶面,比高指数晶面难溶解,呈现更优的耐腐蚀性能。 展开更多
关键词 纯钛 等通道弯角挤压 轧制 电化学行为 动电位极化 织构
下载PDF
120°模具室温ECAP制备工业纯钛的压缩变形本构关系 被引量:4
18
作者 刘晓燕 赵西成 +1 位作者 杨西荣 王成 《中国有色金属学报》 EI CAS CSCD 北大核心 2012年第5期1292-1297,共6页
在Gleeble-1500热模拟机上对120°模具室温Bc方式ECAP变形8道次制备的平均晶粒尺寸约为200 nm的工业纯钛进行等温变速压缩实验,研究超细晶工业纯钛在变形温度为298~673 K和应变速率为1×10-4~1×100s-1条件下的流变应力行... 在Gleeble-1500热模拟机上对120°模具室温Bc方式ECAP变形8道次制备的平均晶粒尺寸约为200 nm的工业纯钛进行等温变速压缩实验,研究超细晶工业纯钛在变形温度为298~673 K和应变速率为1×10-4~1×100s-1条件下的流变应力行为。结果表明:变形温度和应变速率均对流变应力具有显著影响,峰值应力随变形温度的升高和应变速率的降低而降低;流变应力在变形初期随应变的增加而增大,出现峰值后逐渐趋于平稳,呈现稳态流变特征。采用双曲正弦模型确定了超细晶工业纯钛的变形激活能Q=104.46 kJ/mol和应力指数n=23,建立了相应的变形本构关系。 展开更多
关键词 超细晶工业纯钛 热压缩变形 流变应力 本构关系 变形激活能
下载PDF
反复熔铸对纯钛烤瓷合金力学性能的影响 被引量:3
19
作者 杨松 程辉 +3 位作者 李秀容 吴维青 郑明 王颖卉 《上海口腔医学》 CAS CSCD 北大核心 2014年第6期651-653,共3页
目的 :探讨反复熔铸对纯钛烤瓷合金力学性能的影响。方法 :纯钛经过1-3次单纯反复熔铸后,采用拉伸实验、弯曲实验、硬度实验对各代试件的力学性能进行测试。采用SPSS13.0软件包对数据进行统计学分析。结果:经不同次数熔铸的纯钛烤瓷... 目的 :探讨反复熔铸对纯钛烤瓷合金力学性能的影响。方法 :纯钛经过1-3次单纯反复熔铸后,采用拉伸实验、弯曲实验、硬度实验对各代试件的力学性能进行测试。采用SPSS13.0软件包对数据进行统计学分析。结果:经不同次数熔铸的纯钛烤瓷合金试件,其弯曲强度无显著差异。经过2次、3次熔铸的纯钛烤瓷合金试件,其弯曲模量较1次熔铸的纯钛烤瓷合金显著升高(P〈0.05)。拉伸强度、0.2%屈服强度随着熔铸次数的增加而升高(P〈0.05)。经过3次熔铸的纯钛烤瓷合金试件,其延伸率较经过1次、2次熔铸的纯钛烤瓷合金显著降低(P〈0.05)。经过3次熔铸的纯钛烤瓷合金试件,其显微硬度较经过1次、2次熔铸的纯钛烤瓷合金显著升高(P〈0.05)。结论:纯钛烤瓷合金经1~3次单纯反复熔铸后,弯曲性能、显微硬度未下降,但拉伸性能下降。 展开更多
关键词 纯钛烤瓷合金 反复熔铸 力学性能
下载PDF
表面机械研磨工业纯钛表面纳米化研究 被引量:9
20
作者 张聪惠 何晓梅 《稀有金属》 EI CAS CSCD 北大核心 2009年第6期769-773,共5页
表面机械研磨处理可以使工业纯钛形成纳米表面层,通过扫描电镜、透射电镜和高分辨电镜观察SMAT处理后的工业纯钛表层组织,并研究了工业纯钛表面纳米化机制。工业纯钛表面纳米化机制为:孪晶的形成和孪晶的交割使得原始晶粒尺寸减小,同时... 表面机械研磨处理可以使工业纯钛形成纳米表面层,通过扫描电镜、透射电镜和高分辨电镜观察SMAT处理后的工业纯钛表层组织,并研究了工业纯钛表面纳米化机制。工业纯钛表面纳米化机制为:孪晶的形成和孪晶的交割使得原始晶粒尺寸减小,同时使晶格取向发生改变,有利于位错滑移;孪晶通过自身交割,以及位错密度增加及其相互作用,形成了细小的孪晶与胞状组织;胞状组织转变为多边形亚晶;亚晶不断吸收位错形成大角度晶界,亚晶以及取向不同的细小孪晶逐渐转变为随机取向的纳米晶。 展开更多