期刊文献+
共找到103篇文章
< 1 2 6 >
每页显示 20 50 100
(Cr,La)_(2)(C,N)添加对Ti(C,N)基金属陶瓷结构与性能的影响
1
作者 龙航飞 叶金文 曹之南 《粉末冶金技术》 CAS CSCD 北大核心 2024年第1期45-52,共8页
在开放体系下采用高温碳管炉制备了(Cr,La)_(2)(C,N)粉末,并将其作为添加剂制备Ti(C,N)基金属陶瓷。利用X射线衍射仪、扫描电镜、万能力学试验机及维氏硬度计等设备研究了(Cr,La)_(2)(C,N)添加对Ti(C,N)基金属陶瓷微观组织和力学性能的... 在开放体系下采用高温碳管炉制备了(Cr,La)_(2)(C,N)粉末,并将其作为添加剂制备Ti(C,N)基金属陶瓷。利用X射线衍射仪、扫描电镜、万能力学试验机及维氏硬度计等设备研究了(Cr,La)_(2)(C,N)添加对Ti(C,N)基金属陶瓷微观组织和力学性能的影响。结果表明,(Cr,La)_(2)(C,N)的添加能够有效细化Ti(C,N)基金属陶瓷的硬质相晶粒,其中Cr、La元素主要固溶于粘结相,La元素促进了硬质相的溶解–析出过程,金属陶瓷的抗弯强度、硬度以及断裂韧性等力学性能得到明显改善。当添加(Cr,La)_(2)(C,N)的质量分数为5.0%时,Ti(C,N)基金属陶瓷的综合力学性能达到最佳,抗弯强度为2002 MPa,维氏硬度为1643 MPa,断裂韧性为11.22 MPa·m^(1/2)。 展开更多
关键词 TI(C n)基金属陶瓷 (cr La)_(2)(C n) 微观组织 力学性能 断裂韧性
下载PDF
CO_(2)驱油井环境下N80钢与3Cr13钢的电偶腐蚀行为 被引量:1
2
作者 齐宏伟 《材料保护》 CAS CSCD 2024年第3期93-97,共5页
N80钢与3Cr13钢常作为油管和水力锚等的材料使用,在CO_(2)驱油井环境中不可避免偶接使用易产生电偶腐蚀。为此,通过开展CO_(2)环境下N80钢和3Cr13钢的腐蚀速率试验和电偶腐蚀试验,明确了CO_(2)含量、温度、压力和矿化度等因素作用下2种... N80钢与3Cr13钢常作为油管和水力锚等的材料使用,在CO_(2)驱油井环境中不可避免偶接使用易产生电偶腐蚀。为此,通过开展CO_(2)环境下N80钢和3Cr13钢的腐蚀速率试验和电偶腐蚀试验,明确了CO_(2)含量、温度、压力和矿化度等因素作用下2种钢的电偶腐蚀规律。结果表明:CO_(2)驱油井中2种钢产生电偶腐蚀,3Cr13钢为阴极,且不受电偶腐蚀影响,N80钢为阳极,电偶腐蚀速率增大;且N80钢的电偶腐蚀速率随CO_(2)含量、温度、压力和矿化度的增大而增大;电偶腐蚀敏感因子随CO_(2)含量和压力增大而减小,当CO_(2)含量达到20.0%时电偶腐蚀敏感因子为负值,随温度升高先减小后增大,随矿化度增加而增大,电偶腐蚀速率最大可高于常规腐蚀69%。 展开更多
关键词 CO_(2)驱油井 n80钢 3cr13钢 电偶腐蚀 腐蚀速率 电偶腐蚀敏感因子
下载PDF
Effect of(Cr,V)_(2)(C,N)on the Microstructure and Mechanical Properties of WC-10Co Cemented Carbides
3
作者 LI Xiangkun WANG Lu YE Jinwen 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2024年第5期1138-1148,共11页
WC-10Co cemented carbides with finer WC and narrower grain size distributions are produced by using(Cr,V)_(2)(C,N)as grain growth inhibitors.As a result,with the increase of(Cr_(0.9),V_(0.1))_(2)(C,N)and(V_(0.9),Cr_(0... WC-10Co cemented carbides with finer WC and narrower grain size distributions are produced by using(Cr,V)_(2)(C,N)as grain growth inhibitors.As a result,with the increase of(Cr_(0.9),V_(0.1))_(2)(C,N)and(V_(0.9),Cr_(0.1))_(2)(C,N),the grains size of WC and mean free path of Co phase decrease,and adjacency of WC increases.Refinement and homogenization of grains enhance the transverse rupture strength(TRS)and the hardness.Meanwhile,the deflection and bridging of cracks keep the fracture toughness at a respectable level.The WC-10Co-0.6(Cr_(0.9),V_(0.1))_(2)(C,N)-0.025(V_(0.9),Cr_(0.1))_(2)(C,N)cemented carbides exhibit excellent comprehensive mechanical properties with the TRS of 4602.6 MPa,hardness of 1835 kg/mm^(2),and fracture toughness of 10.39 MPa·m^(1/2),respectively.However,the large pores are caused by excess N larger than 0.03 wt%and deteriorates the mechanical properties.We provide a new approach to WC-Co cemented carbides preparation with a narrow grain size distribution by adding novel grain growth inhibitors. 展开更多
关键词 (cr V)_(2)(C n) nutrient content WC grains size microstructure mechanical properties
下载PDF
高强无磁不锈钢Cr21Ni13Mn5Mo2N的热加工特性
4
作者 嵇爽 韩彦光 +3 位作者 陈文 赵英利 马瑞楠 周文慧 《河北冶金》 2024年第5期56-61,共6页
利用Gleeble 3800热模拟机对奥氏体不锈钢Cr21Ni13Mn5Mo2N进行热压缩实验,研究该钢种的高温变形与应变速率以及温度的关系,建立了双曲正弦本构方程,最终得到其热激活能为679.58 kJ/mol,应变速率因子Z=εexp(679580/R T)。实验结果表明,... 利用Gleeble 3800热模拟机对奥氏体不锈钢Cr21Ni13Mn5Mo2N进行热压缩实验,研究该钢种的高温变形与应变速率以及温度的关系,建立了双曲正弦本构方程,最终得到其热激活能为679.58 kJ/mol,应变速率因子Z=εexp(679580/R T)。实验结果表明,在950~1200℃,0.01~10 s^(-1)条件内,材料变形过程均发生动态再结晶,在950℃,应变速率为0.1 s^(-1)条件下,再结晶开始的变形量为10%。流变应力随温度升高及应变速率降低呈现明显下降趋势,由950℃、10 s^(-1)时的326 MPa降低至1200℃、0.01 s^(-1)时的75 MPa。结合微观组织分析及锻造试验,对压缩试样开裂问题进行深入探究,结果表明晶界处碳、氧化物的聚集恶化晶界塑性,导致热变形过程中在该处形成裂纹源并逐步扩展。通过热处理和热变形试验,确定Cr21Ni13Mn5Mo2N电渣锭在1170℃固溶6 h后晶界碳、氧化物消除,电渣锭晶界处结合力明显提升,成功消除锻造开裂问题,实现锻造成材率大幅提升。 展开更多
关键词 不锈钢cr21ni13Mn5Mo2n 压缩热模拟 本构方程 热加工塑性
下载PDF
Structure and mechanical properties of thick Cr/Cr_2N/CrN multilayer coating deposited by multi-arc ion plating 被引量:7
5
作者 单磊 王永欣 +3 位作者 李金龙 李赫 鲁侠 陈建敏 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2015年第4期1135-1143,共9页
A Cr/Cr2N/CrN multilayer coating with a thickness of 24.4 μm was deposited by multi-arc ion plating. The coating was systematically characterized by field emission scanning electron microscopy(FESEM), X-ray photoelec... A Cr/Cr2N/CrN multilayer coating with a thickness of 24.4 μm was deposited by multi-arc ion plating. The coating was systematically characterized by field emission scanning electron microscopy(FESEM), X-ray photoelectron spectrometry(XPS), energy dispersive spectroscopy(EDS), X-ray diffraction(XRD) and transmission electron microscopy(TEM). Hardness and adhesion were tested by nanoindentation and scratch tester, respectively. The friction properties were investigated by a reciprocating UMT-3MT ball-on-disk tribometer in air and seawater. The results showed that the multilayer coating consisted of three different layers, with Cr,Cr2N and CrN phases, respectively. Compared with CrN single layer coating, the adhesion of the multilayer coating was improved significantly, the hardness of the multilayer coating was(21±2) GPa. The corrosion resistance of the multilayer coating was also improved in artificial seawater. The friction coefficient of multilayer coating was lower than that of CrN single layer coating both in air and seawater. 展开更多
关键词 cr/cr2n/crn multilayer coating microstructure mechanical properties corrosion resistance FRICTIOn
下载PDF
纯铁表面三价镀铬/渗氮复合处理制备CrN/Cr_2N涂层 被引量:1
6
作者 焦东玲 黄海滨 +1 位作者 丁红珍 邱万奇 《材料热处理学报》 EI CAS CSCD 北大核心 2017年第5期129-133,共5页
采用预三价镀铬再穿透气体渗氮的方法,在纯铁表面制备CrN/Cr_2N涂层。研究不同镀铬层厚度、渗氮温度和时间所形成涂层的微观结构和相组成变化规律。随渗氮温度从540℃提高到700℃,镀铬层相结构变化为:Cr→CrN/Cr_2N(具有超点阵结构的Cr_... 采用预三价镀铬再穿透气体渗氮的方法,在纯铁表面制备CrN/Cr_2N涂层。研究不同镀铬层厚度、渗氮温度和时间所形成涂层的微观结构和相组成变化规律。随渗氮温度从540℃提高到700℃,镀铬层相结构变化为:Cr→CrN/Cr_2N(具有超点阵结构的Cr_2N)→CrN/Cr_2N。在同一温度(640℃)渗氮,随时间延长,Cr→CrN/Cr_2N,形成大量具有超点阵结构的Cr_2N相。SEM/EPMA测试结果表明,采用该复合处理制备的氮化铬层与基体间可形成互扩散的冶金结合,实现氮化铬层与基体间在组织结构上的平缓过渡,有利于提高涂层性能。 展开更多
关键词 氮化铬 渗氮 镀铬 crn cr2n
下载PDF
冷轧变形量对00Cr17Ni13Mo2N不锈钢组织和硬度的影响
7
作者 刘波 赵会娟 靳峰峰 《热加工工艺》 北大核心 2023年第5期108-110,共3页
对固溶态00Cr17Ni13Mo2N不锈钢进行了不同变形量的冷轧试验,采用OM、XRD、硬度测试等研究了不同冷轧变形量对不锈钢组织与硬度的影响。结果表明:固溶态00Cr17Ni13Mo2N钢组织为单一奥氏体组织。经不同变形量冷轧后钢发生了形变诱导马氏... 对固溶态00Cr17Ni13Mo2N不锈钢进行了不同变形量的冷轧试验,采用OM、XRD、硬度测试等研究了不同冷轧变形量对不锈钢组织与硬度的影响。结果表明:固溶态00Cr17Ni13Mo2N钢组织为单一奥氏体组织。经不同变形量冷轧后钢发生了形变诱导马氏体相变,随着冷轧变形量的增加,钢中α’-马氏体体积分数逐渐增加,钢的硬度逐渐提高。轧制变形量80%的钢中α’-马氏体体积分数达到了70.6%,硬度达到421 HV,比固溶态试验钢硬度提高了152.1%。 展开更多
关键词 00cr17ni13Mo2n不锈钢 冷轧变形量 显微组织 硬度
下载PDF
辐射接枝制备聚甲基丙烯酸N,N-二甲氨基乙酯-TiO_(2)光催化剂及其对Cr(Ⅵ)的吸附还原性能
8
作者 王亚洋 王亦凡 +2 位作者 张彬 杨小洁 李月生 《辐射研究与辐射工艺学报》 CAS CSCD 2023年第1期33-41,共9页
以二氧化钛(TiO_(2))为基材,甲基丙烯酸二甲氨基乙酯(DMAEMA)为单体,采用共辐射接枝法成功合成了聚甲基丙烯酸N,N-二甲氨基乙酯-TiO_(2)(TiO_(2)-g-PDMAEMA)吸附-光催化剂。同时探究了单体浓度和吸收剂量对重金属离子吸附作用的影响。... 以二氧化钛(TiO_(2))为基材,甲基丙烯酸二甲氨基乙酯(DMAEMA)为单体,采用共辐射接枝法成功合成了聚甲基丙烯酸N,N-二甲氨基乙酯-TiO_(2)(TiO_(2)-g-PDMAEMA)吸附-光催化剂。同时探究了单体浓度和吸收剂量对重金属离子吸附作用的影响。利用扫描电镜、X射线衍射仪、傅里叶红外光谱分析仪、热重分析仪、X射线光电子能谱、接触角等表征手段,证实了电子束共辐射接枝法成功将DMAEMA单体接枝到TiO_(2)表面。在吸收剂量为60 kGy、单体浓度为20%时,TiO_(2)-g-PDMAEMA对10 mg/L Cr(Ⅵ)具有较佳的吸附能力,吸附容量可达10.75 mg/g。在可见光诱导下,吸收剂量为60 kGy、单体浓度为10%时,制备的TiO_(2)-g-PDMAEMA具有最佳的吸附-光催化还原能力,对10 mg/L Cr(Ⅵ)的去除率达85.56%。该新型光催化剂上的吸附-光催化协同效应可以满足去除水中Cr(Ⅵ)污染的要求。 展开更多
关键词 二氧化钛 甲基丙烯酸二甲氨基乙酯 辐射接枝 光催化 cr(Ⅵ) 吸附-光催化还原
下载PDF
Effect of VC/Cr_3C_2 on microstructure and mechanical properties of Ti(C,N)-based cermets 被引量:5
9
作者 詹斌 刘宁 +2 位作者 金之铂 李其龙 石锦罡 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2012年第5期1096-1105,共10页
Effects of VC/Cr3C2 on the microstructure and mechanical properties of Ti(C,N)-based cermets were studied. The microstructure was investigated by means of optical microscopy, X-ray diffractometry as well as scanning... Effects of VC/Cr3C2 on the microstructure and mechanical properties of Ti(C,N)-based cermets were studied. The microstructure was investigated by means of optical microscopy, X-ray diffractometry as well as scanning electron microscopy in combination with energy dispersive spectrometry. Mechanical properties, such as transverse rupture strength, hardness and fracture toughness, were measured. The results show that there are black core-grey rim structure and white core-grey rim structure in the microstructure. The grains become fine due to the VC/Cr3C2, and the grains of cermet added with 0.75VC/0.25Cr3C2 are refined most remarkably. The black core becomes finer with the increase of VC addition and rim phase becomes thicker with the decrease of Cr3C2 addition. The porosity increases with the increase of VC addition in VC/Cr3C2. Compared with the cermet free of VC/Cr3C2, the transverse rupture strength and hardness of cermets with VC/Cr3C2 are both improved, and the maximum values are both found for the cermet with 0.25VC/0.75Cr3C2. The fracture toughness can be effectively promoted by adding VC/Cr3C2 with an appropriate ratio of VC to Cr3C2, and the maximum value is found for the cermet with 0.5VC/0.5Cr3C2. 展开更多
关键词 Ti(C n)-based cermet VC cr3C2 microstructure mechanical properties
下载PDF
Cr2N/CrN多层复合涂层的生长和性能
10
作者 彭补之 《材料保护》 CAS CSCD 北大核心 2002年第9期69-69,共1页
关键词 cr2n/crn多层复合涂层 性能 磁控溅射技术 硅基体 沉积单层 多层氮化铬涂层 沉积温度
下载PDF
N,Cr共掺锐钛矿TiO_2电子结构和光学性质的第一性原理研究 被引量:4
11
作者 孙凌涛 郭朝中 +1 位作者 伏春平 石东平 《功能材料》 EI CAS CSCD 北大核心 2015年第23期23075-23079,共5页
采用第一性原理的平面波赝势方法研究了N、Cr单一掺杂及共掺杂锐钛矿TiO_2的能带结构、态密度和光学性质。结果表明,N单一掺杂体系中N2p杂质轨道交叠在费米能级上;Cr单一掺杂体系中杂质能级主要由O2p和Cr3d轨道杂化贡献;N、Cr共掺杂致... 采用第一性原理的平面波赝势方法研究了N、Cr单一掺杂及共掺杂锐钛矿TiO_2的能带结构、态密度和光学性质。结果表明,N单一掺杂体系中N2p杂质轨道交叠在费米能级上;Cr单一掺杂体系中杂质能级主要由O2p和Cr3d轨道杂化贡献;N、Cr共掺杂致使导带及价带相对费米能级明显下降,同时在原禁带基础上形成了新的杂质能级、禁带宽度减小,锐钛矿TiO_2的光吸收带红移,其吸收系数增大、能量损失缩小,有效增强了锐钛矿TiO_2的光催化效率。 展开更多
关键词 锐钛矿TIO2 n+cr共掺杂 电子结构 光学性质
下载PDF
Y_2O_3薄膜处理对3Cr25Ni7N合金的抗高温氧化性能的影响 被引量:5
12
作者 马静 何业东 +1 位作者 王俊 孙宝德 《中国稀土学报》 CAS CSCD 北大核心 2007年第6期765-768,共4页
采用电沉积-热解法在3Cr25Ni7N合金表面制备了Y2O3薄膜,并研究了薄膜处理对合金在1000℃空气中的抗高温氧化性能的影响。氧化动力学曲线、SEM及XRD分析结果表明,Y2O3薄膜处理使合金表面氧化膜以尖晶石结构为主,氧化膜致密,有效地抑制了C... 采用电沉积-热解法在3Cr25Ni7N合金表面制备了Y2O3薄膜,并研究了薄膜处理对合金在1000℃空气中的抗高温氧化性能的影响。氧化动力学曲线、SEM及XRD分析结果表明,Y2O3薄膜处理使合金表面氧化膜以尖晶石结构为主,氧化膜致密,有效地抑制了Cr2O3的挥发反应,且氧化膜与基体的附着性好,因此合金在高温下的抗氧化性能得到提高,这与氧化钇薄膜在较低温度下抗高温氧化性能提高的机制是不同的。在不同温度下,Y2O3薄膜处理均可以有效提高合金的抗高温氧化性能。 展开更多
关键词 Y2O3薄膜 抗高温氧化 3cr25ni7n合金 电沉积-热解法 稀土
下载PDF
1Cr17Mn6Ni5N不锈钢电沉积PbO_2的机理 被引量:3
13
作者 陈阵 廖登辉 +4 位作者 陆丽芳 杜重麟 司云森 郭忠诚 丁龙 《材料保护》 CAS CSCD 北大核心 2012年第8期10-13,44,共5页
目前,有关PbO2电极制备机理的研究还不够成熟。采用恒电流法在1Cr17Mn6Ni5N不锈钢基体上电沉积PbO2制成电极,采用循环伏安法对PbO2的沉积过程进行了研究,并用X射线衍射仪(XRD)对沉积层物相进行了表征。结果表明:PbO2的沉积过程分为Pb的... 目前,有关PbO2电极制备机理的研究还不够成熟。采用恒电流法在1Cr17Mn6Ni5N不锈钢基体上电沉积PbO2制成电极,采用循环伏安法对PbO2的沉积过程进行了研究,并用X射线衍射仪(XRD)对沉积层物相进行了表征。结果表明:PbO2的沉积过程分为Pb的低价氧化物PbO的生成、α-PbO2的生成和β-PbO2的生成3步;沉积的PbO2主要为β-PbO2和少量的α-PbO2。 展开更多
关键词 PbO2电沉积 1cr17Mn6ni5n不锈钢 循环伏安 沉积机理
下载PDF
靶电流密度对热丝增强等离子磁控溅射制备Cr_2N薄膜结构与性能的影响 被引量:2
14
作者 张鑫 王晓明 +3 位作者 高健波 郭媛媛 解志文 周艳文 《功能材料》 EI CAS CSCD 北大核心 2018年第3期3070-3075,共6页
采用等离子体增强平衡磁控溅射技术在316L奥氏体不锈钢基体表面制备了不同靶电流密度条件下的Cr_2N薄膜,并检测分析了靶电流密度对薄膜表面形貌、相结构、力学性能、膜基结合力和摩擦磨损性能的影响。结果表明,薄膜呈致密柱状结构,以Cr_... 采用等离子体增强平衡磁控溅射技术在316L奥氏体不锈钢基体表面制备了不同靶电流密度条件下的Cr_2N薄膜,并检测分析了靶电流密度对薄膜表面形貌、相结构、力学性能、膜基结合力和摩擦磨损性能的影响。结果表明,薄膜呈致密柱状结构,以Cr_2N(111)择优取向为主。当靶电流密度为0.132 mA/mm^2时,WN相与Cr_2N并存;随着靶电流密度的增加,薄膜厚度逐渐增加,硬度、弹性模量略有下降,膜基结合增强。薄膜与基体结合处呈脆性失效。靶电流密度0.132 mA/mm^2时,最高薄膜硬度及模量分别为33及480GPa,且磨损量最小。靶电流密度0.264mA/mm^2时,最大膜机结合力为36.6N。经过镀Cr_2N薄膜后,试样表面硬度、耐磨性明显提高。 展开更多
关键词 等离子体增强磁控溅射 cr2n薄膜 靶电流密度 结构 性能
下载PDF
XS-1型缓蚀剂对2Cr13钢和N80钢缓蚀性能的影响 被引量:4
15
作者 毕凤琴 徐岩 +3 位作者 朱峰 梁柱 张旭昀 王勇 《化工机械》 CAS 2019年第6期646-650,共5页
利用失重法,借助高温高压H2S/CO2腐蚀反应釜,研究了XS-1型耐高温新型抗氧缓蚀剂在NaCl介质中的缓蚀性能。通过正交实验法,分析了介质温度、Cl^-浓度、缓蚀剂浓度对2Cr13不锈钢和N80套管钢腐蚀行为的影响。结果表明:Cl^-浓度是影响两种... 利用失重法,借助高温高压H2S/CO2腐蚀反应釜,研究了XS-1型耐高温新型抗氧缓蚀剂在NaCl介质中的缓蚀性能。通过正交实验法,分析了介质温度、Cl^-浓度、缓蚀剂浓度对2Cr13不锈钢和N80套管钢腐蚀行为的影响。结果表明:Cl^-浓度是影响两种钢腐蚀的主要因素,缓蚀剂浓度的影响力度略小于Cl^-浓度的影响力度。XS-1型缓蚀剂适用于Cl^-浓度高、酸化程度高和温度高的地层液中。 展开更多
关键词 缓蚀剂 缓蚀性能 2cr13不锈钢 n80套管钢 正交实验法 失重法
下载PDF
Cr2O3催化氮化制备Si3N4/SiC耐火材料及其性能 被引量:2
16
作者 韩磊 赵万国 +3 位作者 李发亮 张俊 曾渊 张海军 《机械工程材料》 CAS CSCD 北大核心 2018年第10期72-76,共5页
以SiC粉和硅粉为原料,原位合成的Cr_2O_3为催化剂,采用催化氮化法制备了Si_3N_4/SiC耐火材料,研究了催化剂用量及氮化温度对耐火材料物相组成、微观形貌、物理性能和力学性能的影响。结果表明:当氮化温度为1 673K,Cr_2O_3含量(与硅粉质... 以SiC粉和硅粉为原料,原位合成的Cr_2O_3为催化剂,采用催化氮化法制备了Si_3N_4/SiC耐火材料,研究了催化剂用量及氮化温度对耐火材料物相组成、微观形貌、物理性能和力学性能的影响。结果表明:当氮化温度为1 673K,Cr_2O_3含量(与硅粉质量之比,下同)为3%时,硅粉完全氮化,耐火材料主要由颗粒状SiC和晶须状α-Si_3N_4、β-Si_3N_4等组成;随着Cr_2O_3含量的增加,Si_3N_4晶须的数量增多,长度增大,耐火材料变得致密;随氮化温度的升高,耐火材料的抗折强度和耐压强度均增大,当氮化温度为1 673K、Cr_2O_3含量为3%时,抗折强度和耐压强度均最大,分别为34MPa和132MPa。 展开更多
关键词 Si3n4/SiC耐火材料 cr2O3催化氮化 Si3n4晶须 力学性能
下载PDF
N80和Cr13钢在含CO_2油田采出液中缓蚀性能研究 被引量:1
17
作者 毕凤琴 张伟东 +3 位作者 王妍 赵红梅 张旭昀 王勇 《兵器材料科学与工程》 CAS CSCD 北大核心 2016年第1期37-40,共4页
利用电化学工作站测试N80和Cr13两种钢在饱和CO_2油田采出液中添加不同浓度的ZK缓蚀剂的腐蚀行为,分析缓蚀剂用量对其腐蚀行为的影响规律,用高温高压反应釜借助失重法和腐蚀形貌观察确定最佳缓蚀剂用量下两种钢的缓蚀性能。结果表明:静... 利用电化学工作站测试N80和Cr13两种钢在饱和CO_2油田采出液中添加不同浓度的ZK缓蚀剂的腐蚀行为,分析缓蚀剂用量对其腐蚀行为的影响规律,用高温高压反应釜借助失重法和腐蚀形貌观察确定最佳缓蚀剂用量下两种钢的缓蚀性能。结果表明:静态时,N80和Cr13钢在饱和CO_2油田采出液中分别呈现活化和钝化特征,N80钢的ZK缓蚀剂最佳用量为500 m L/L,而Cr13钢则为1 000 m L/L;动态时,N80钢缓蚀效率达97.95%,而Cr13钢则为95.20%。 展开更多
关键词 n80钢 cr13钢 缓蚀剂 CO2腐蚀
下载PDF
热处理对0Cr17Mn14Mo2N双相不锈钢性能的影响 被引量:2
18
作者 毛萍莉 苏国跃 杨柯 《材料研究学报》 EI CAS CSCD 北大核心 2002年第1期88-92,共5页
研究了热处理对0Cr17Mn14Mo2N双相不锈钢铸态组织中δ-铁素体的含量、形态以及双相不锈钢性能的影响.结果表明,在1050~1200℃之间加热时,组织为奥氏体基体上分布着的球化的及长条形的δ-铁素体,且加热温度... 研究了热处理对0Cr17Mn14Mo2N双相不锈钢铸态组织中δ-铁素体的含量、形态以及双相不锈钢性能的影响.结果表明,在1050~1200℃之间加热时,组织为奥氏体基体上分布着的球化的及长条形的δ-铁素体,且加热温度越高保温时间越长铁素体的球化率越高.在1250℃加热时,组织为粗大的铁素体等轴晶,其中铁素体以球状均匀分布的0Cr17Mn14Mo2N双相不锈钢的拉伸性能最好. 展开更多
关键词 热处理 0cr17Mn14Mo2n双相不锈钢 Δ-铁素体 形态 拉伸性能
下载PDF
03Cr16Mn14Mo2N奥氏体不锈钢的热疲劳行为 被引量:1
19
作者 徐桂芳 严羽 +2 位作者 徐文慧 程晓农 李冬升 《机械工程材料》 CAS CSCD 北大核心 2016年第12期99-102,共4页
对新型高氮低镍03Cr16Mn14Mo2N奥氏体不锈钢进行了不同上限温度下的热疲劳试验,通过光学显微镜观察了热疲劳裂纹的萌生及扩展,研究了其热疲劳行为。结果表明:热疲劳裂纹的孕育期随上限温度的升高而缩短,其扩展速率随着循环次数的增加呈... 对新型高氮低镍03Cr16Mn14Mo2N奥氏体不锈钢进行了不同上限温度下的热疲劳试验,通过光学显微镜观察了热疲劳裂纹的萌生及扩展,研究了其热疲劳行为。结果表明:热疲劳裂纹的孕育期随上限温度的升高而缩短,其扩展速率随着循环次数的增加呈先增大后减小的变化趋势;随着上限温度的升高,试验钢V型缺口处的裂纹扩展至0.5mm时所需的热疲劳循环次数显著降低;热疲劳裂纹在V型缺口处优先萌生,随着热循环次数的增加,晶界和孪晶界也成为裂纹源,裂纹主要沿晶界扩展。 展开更多
关键词 03cr16Mn14Mo2n 热疲劳裂纹 萌生 扩展
下载PDF
5Cr21 Mn9Ni4N耐热钢高温运行条件下组织性能的变化 被引量:1
20
作者 许晓磊 于志伟 +2 位作者 鲍翔 常宝坤 吉连瑜 《机械工程材料》 CAS CSCD 北大核心 2003年第12期49-51,共3页
利用XRD、SEM研究了5Cr21Mn9Ni4N(21 4N)耐热钢在高温(600~800℃)运行过程中组织结构的变化及其对性能的影响。结果表明,高温运行条件下基体组织发生胞状分解,形成M23C6+γ组成的层状组织是排气门盘部断裂失效的主要原因。原始组织状... 利用XRD、SEM研究了5Cr21Mn9Ni4N(21 4N)耐热钢在高温(600~800℃)运行过程中组织结构的变化及其对性能的影响。结果表明,高温运行条件下基体组织发生胞状分解,形成M23C6+γ组成的层状组织是排气门盘部断裂失效的主要原因。原始组织状态决定了高温运行条件下21 4N钢的组织稳定性。 展开更多
关键词 21—4n耐热钢 层状组织 断裂失效 5cr2lMn9ni4n 高温运行 组织结构 力学性能 断裂失效
下载PDF
上一页 1 2 6 下一页 到第
使用帮助 返回顶部