Brazeability evaluation of Ti-Zr-Cu-Ni-Co-Mo filler for vacuum brazing TiAl-based alloy 被引量:10
1
作者 Li LI Xiao-qiang LI +2 位作者 Ke HU Bo-lin HE Hua MAN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2019年第4期754-763,共10页
Ti-47Al-2Nb-2Cr-0.15B(mole fraction,%)alloy was vacuum brazed with amorphous and crystalline Ti.25Zr-12.5Cu-12.5Ni-3.0Co-2.0Mo(mass fraction,%)filler alloys,and the melting,spreading and gap filling behaviors of the a... Ti-47Al-2Nb-2Cr-0.15B(mole fraction,%)alloy was vacuum brazed with amorphous and crystalline Ti.25Zr-12.5Cu-12.5Ni-3.0Co-2.0Mo(mass fraction,%)filler alloys,and the melting,spreading and gap filling behaviors of the amorphous and crystalline filler alloys as well as the joints brazed with them were investigated in details.Results showed that the amorphous filler alloy possessed narrower melting temperature interval,lower liquidus temperature and melting active energy compared with the crystalline filler alloy,and it also exhibited better brazeability on the surface of the Ti.47Al.2Nb.2Cr.0.15B alloy.The TiAl joints brazed with crystalline and amorphous filler alloys were composed of two interfacial reaction layers and a central brazed layer.Under the same conditions,the tensile strength of the joint brazed with the amorphous filler alloy was always higher than that with the crystalline filler alloy.The maxmium tensile strength of the joint brazed at 1273 K with the amorphous filler alloy reached 254 MPa. 展开更多
关键词 vacuum brazing Ti.47Al.2Nb.2Cr.0.15B alloy amorphous Ti-25Zr-12.5cu-12.5ni-3.0Co-2.0Mo filler alloy tensile strength interfacial microstructure brazeability
下载PDF
热处理工艺对Cu-Ni-Si合金组织与性能的影响 被引量:4
2
作者 张龙 汪明朴 +3 位作者 贾延琳 陈畅 董琦祎 易将 《粉末冶金材料科学与工程》 EI 北大核心 2014年第6期928-934,共7页
采用3种不同的工艺(直接在450℃下进行时效处理;80%冷轧,然后在450℃下进行时效处理;600℃/8 h高温预时效+80%冷轧+780℃/2 min+450℃/16 h终时效)对固溶处理后的Cu-2.0Ni-0.34Si-Mg合金进行形变热处理,研究形变热处理工艺对该合金的组... 采用3种不同的工艺(直接在450℃下进行时效处理;80%冷轧,然后在450℃下进行时效处理;600℃/8 h高温预时效+80%冷轧+780℃/2 min+450℃/16 h终时效)对固溶处理后的Cu-2.0Ni-0.34Si-Mg合金进行形变热处理,研究形变热处理工艺对该合金的组织与硬度及电导率的影响。结果表明:采用第3种工艺对合金进行形变热处理,由于其中的短时高温预处理可以获得溶质原子充分固溶的过饱和固溶体,因此终时效后的合金具有最佳的综合性能,显微硬度为180 HV,相对电导率为49.8%IACS,伸长率为13%。合金的平均晶粒尺寸约为20μm,主要析出强化相为δ-Ni2Si。 展开更多
关键词 cu-2.0ni-0.34si-mg合金 显微组织 显微硬度 电导率