Corrosion of Y, Fe and Fe-15Y in H_2-H_2S Mixture under 10^(-3)Pa S_2 at 600~800℃ 被引量:1
1
作者 Yan NIU Weitao WU and Chaoliu ZENG (State Key Lab. for Corrosion and Protection, Institute of Corrosion and Protection of Metals,Chinese Academy of Sciences, Shenyang 110015, China)F. Gesmundo and F. Viani (Instituto di Chimica, Facolta di Ingegneria, Un 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 1996年第5期321-328,共8页
The corrosion of an Fe-based alloy containing 15 wt pct Y in H2-H2S mixtures under 10-3 Pa S2 was studied at 600~800℃ in an attempt to find materials with improved sulphidation resistance with respect to pure Fe. The... The corrosion of an Fe-based alloy containing 15 wt pct Y in H2-H2S mixtures under 10-3 Pa S2 was studied at 600~800℃ in an attempt to find materials with improved sulphidation resistance with respect to pure Fe. The presence of Y has been shown to be beneflcial, but not sufficient to the level expected. In fact, the alloy is able to form at all tested temperatures an external FeS layer, beneath which a zone containing a mixture of the two sulphides is also present. Thus,Fe can still diffuse through this region to form the outer FeS layer with non-negligible rate. The corrosion rate of Fe is considerably reduced by the Y addition. but the alloy corrodes still much more rapidly than Y. The sulphidation kinetics is generally rather irregular for both the pure metals, while the corrosion rate of the alloy decreases with time and tends to become parabolic after an initial period of 12~17 h. The sulphidation behaviour of the alloys is discussed by taking into account the presence of an intermetallic compound Fe17Y2 and the limited solubility of Y in Fe 展开更多
关键词 Fe and fe-15y in H2-H2S Mixture under 10 Met OO Pa S2 at 600 Corrosion of y
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部