Zirconia-loaded sulfuric acid (SO2-/ZrO2) catalysts were prepared by impregnation method, molded by punch tablet machine and characterized by X-ray diffraction. SO4^2-/ZrO2 catalyst was used to obtain glycerol triac...Zirconia-loaded sulfuric acid (SO2-/ZrO2) catalysts were prepared by impregnation method, molded by punch tablet machine and characterized by X-ray diffraction. SO4^2-/ZrO2 catalyst was used to obtain glycerol triacetate (GTA) directly from glycerin. The effect of some factors, such as different temperatures of calcination and catalysts molded or not, on the reusable times of catalysts and the yield of GTA were investigated. The optimum reaction conditions were shown as follows: the reaction temperature was 403 K; the reaction time continued for 8 h; the amount of molded catalysts was 5 wt% of glycerin and the molar ratio of glycerin to acetic acid was 1 : 8. The yield of GTA was 97.93% under the optimum condition.展开更多
基金supported by the National High Technology Research and Development Program of China (No. 2009AA03Z222 and No. 2009AA05Z437)the "Six Talents Pinnacle Program" of Jiangsu Province of China (No. 2008028)
文摘Zirconia-loaded sulfuric acid (SO2-/ZrO2) catalysts were prepared by impregnation method, molded by punch tablet machine and characterized by X-ray diffraction. SO4^2-/ZrO2 catalyst was used to obtain glycerol triacetate (GTA) directly from glycerin. The effect of some factors, such as different temperatures of calcination and catalysts molded or not, on the reusable times of catalysts and the yield of GTA were investigated. The optimum reaction conditions were shown as follows: the reaction temperature was 403 K; the reaction time continued for 8 h; the amount of molded catalysts was 5 wt% of glycerin and the molar ratio of glycerin to acetic acid was 1 : 8. The yield of GTA was 97.93% under the optimum condition.