The infrared emissivity of conducting polymers in 8—20μm and at 50—150℃ in the direction of normal line has been measured as a function of wavelength, conductivity at room temperature, counterion, doping levels, m...The infrared emissivity of conducting polymers in 8—20μm and at 50—150℃ in the direction of normal line has been measured as a function of wavelength, conductivity at room temperature, counterion, doping levels, measuring temperature and thickness of sample.展开更多
文摘The infrared emissivity of conducting polymers in 8—20μm and at 50—150℃ in the direction of normal line has been measured as a function of wavelength, conductivity at room temperature, counterion, doping levels, measuring temperature and thickness of sample.