Interface behavior study of WC92-Co8 coating produced by electrospark deposition 被引量:6
1
作者 汪瑞军 钱乙余 刘军 《China Welding》 EI CAS 2004年第1期61-64,共4页
ESD (electrospark deposition) is a promising process to produce hard and wear-resisting coatings on metallic substrates. In this paper microstructure and interfacial characteristics of the WC92-Co8 coated on titanium ... ESD (electrospark deposition) is a promising process to produce hard and wear-resisting coatings on metallic substrates. In this paper microstructure and interfacial characteristics of the WC92-Co8 coated on titanium and carbon steel are presented. A metallurgical bonding between the coating and substrate is obtained. The Ti element was found to distribute in WC92-Co8 at the metal pool, as well as the interface by diffusion. Some new phases were produced in the coating layer due to the chemical reaction during the ESD process. Experimental observation and thermodynamic analysis were utilized to study the mechanism of ESD. 展开更多
关键词 electrospark deposition interface behavior WC92-Co8
下载PDF
Interface behavior of chalcopyrite during flotation from cyanide tailings 被引量:1
2
作者 Xuemin Qiu Hongying Yang +3 位作者 Guobao Chen Linlin Tong Zhenan Jin Qin Zhang 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2022年第3期439-445,共7页
The interface characteristics of cyanide tailings are different from those of the raw ore. In this study, valuable elements could not be thoroughly recovered via the flotation of cyanide tailings from Shandong, China.... The interface characteristics of cyanide tailings are different from those of the raw ore. In this study, valuable elements could not be thoroughly recovered via the flotation of cyanide tailings from Shandong, China. The interface and floatability of these tailings were investig- ated by phase analysis and flotation tests. The chalcopyrite in the cyanide tailings was fine and had a porous surface. The floatability of 68% chalcopyrite was similar to that of galena in the presence of a collector. A layer of fine galena particles compactly wrapped the chalcopyrite. The chalcopyrite recovery sharply decreased as the nonpolar oil residue in cyanide tailings was extracted using alcohol;however, this removal had no effect on the galena. The remaining chalcopyrite in the flotation tailings was covered with an oxidation layer consisting of O, Fe, S, Pb, Cu, Zn, and Si. 展开更多
关键词 cyanide tailings interface behavior CHALCOPYRITE FLOTATION surface wrapped layer
下载PDF
Comparison of the interface reaction behaviors of CaO–V_(2)O_(5) and MnO_(2)–V_(2)O_(5) solid-state systems based on the diffusion couple method 被引量:3
3
作者 Jing Wen Hongyan Sun +3 位作者 Tao Jiang Bojian Chen Fangfang Li Mengxia Liu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2023年第5期834-843,共10页
The formation mechanism of calcium vanadate and manganese vanadate and the difference between calcium and manganese in the reaction with vanadium are basic issues in the calcification roasting and manganese roasting p... The formation mechanism of calcium vanadate and manganese vanadate and the difference between calcium and manganese in the reaction with vanadium are basic issues in the calcification roasting and manganese roasting process with vanadium slag.In this work,CaO–V_(2)O_(5) and MnO_(2)–V_(2)O_(5) diffusion couples were prepared and roasted for different time periods to illustrate and compare the diffusion reaction mechanisms.Then,the changes in the diffusion product and diffusion coefficient were investigated and calculated based on scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS) analysis.Results show that with the extension of the roasting time,the diffusion reaction gradually proceeds among the CaO–V_(2)O_(5) and MnO_(2)–V_(2)O_(5) diffusion couples.The regional boundaries of calcium and vanadium are easily identifiable for the CaO–V_(2)O_(5) diffusion couple.Meanwhile,for the MnO_(2)–V_(2)O_(5) diffusion couple,MnO_(2) gradually decomposes to form Mn_(2)O_(3),and vanadium diffuses into the interior of Mn_(2)O_(3).Only a part of vanadium combines with manganese to form the diffusion production layer.CaV_(2)O_(6) and MnV_(2)O_(6) are the interfacial reaction products of the CaO–V_(2)O_(5) and MnO_(2)–V_(2)O_(5) diffusion couples,respectively,whose thicknesses are 39.85 and 32.13μm when roasted for 16 h.After 16 h,both diffusion couples reach the reaction equilibrium due to the limitation of diffusion.The diffusion coefficient of the CaO–V_(2)O_(5) diffusion couple is higher than that of the MnO_(2)–V_(2)O_(5) diffusion couple for the same roasting time,and the diffusion reaction between vanadium and calcium is easier than that between vanadium and manganese. 展开更多
关键词 solid-state reaction reaction regularity of calcium and vanadium reaction regularity of manganese and vanadium diffusion couple method interface reaction behavior
下载PDF
Interface Mechanical Behavior of Flexible Piles Under Lateral Loads in OWT Systems
4
作者 LI Xiao-juan ZHU Ming-xing +2 位作者 DAI Guo-liang WANG Li-yan LIU Jing 《China Ocean Engineering》 SCIE EI CSCD 2023年第3期484-494,共11页
This paper investigates the interface mechanical behavior of flexible piles with L_p/D>10 under lateral load and an overturning moment in monotonic loading conditions.To modify the beam-on-Winkler-foundation model ... This paper investigates the interface mechanical behavior of flexible piles with L_p/D>10 under lateral load and an overturning moment in monotonic loading conditions.To modify the beam-on-Winkler-foundation model of piles in offshore wind farms,the energy-based variational method is used.The soil is treated as a multi-layered elastic continuum with the assumption of three-dimensional displacements,the pile modeled as an Euler-Bernoulli beam.A series of cases using MATLAB programming was conducted to investigate the simplified equations of initial stiffness.The results indicated that the interaction between soil layers and the applied force position should be taken into account in calculating the horizontal soil resistance.Additionally,the distributed moment had a limiting effect on the lateral capacity of a flexible pile.Moreover,to account for the more realistic conditions of OWT systems,field data from the Donghai Bridge offshore wind farm were used. 展开更多
关键词 flexible piles interface mechanical behavior initial stiffness p-y curves offshore wind turbine systems
下载PDF
Interface Behavior of Copper and Steel by Plasma-MIG Hybrid Arc Welding 被引量:2
5
作者 Tao YANG Hongming GAO +1 位作者 Shenghu ZHANG Lin WU 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2013年第3期328-332,共5页
Plasma-MIG hybrid arc welding is a hybrid heating source welding method which is composed of plasma arc and MIG arc. During Plasma-MIG hybrid arc welding process, the interface behavior of copper and steel dissimilar ... Plasma-MIG hybrid arc welding is a hybrid heating source welding method which is composed of plasma arc and MIG arc. During Plasma-MIG hybrid arc welding process, the interface behavior of copper and steel dissimilar alloy is investigated. The results show that electromagnetic stirring effect decreases and the heat input increases with the increase of outer plasma current in the hybrid arc welding process. The interface diffusion and interface thickness is controlled by the tradeoff of electromagnetic stirring effect degradation and heat input increase. The interface diffusion and interface thickness are controlled by decreasing the electromagnetic stirring force and increasing the heat input with the increase of plasma current in Cu/Fe plasma-MIG hybrid arc welding process. 展开更多
关键词 Plasma-MIG hybrid arc Copper-steel dissimilar alloy interface behavior
原文传递
Insightful understanding of three-phase interface behaviors in 1T-2H MoS_(2)/CFP electrode for hydrogen evolution improvement 被引量:1
6
作者 Jiamu Cao Jing Zhou +3 位作者 Mingxue Li Junyu Chen Yufeng Zhang Xiaowei Liu 《Chinese Chemical Letters》 SCIE CAS CSCD 2022年第8期3745-3751,共7页
Hydrogen evolution reaction(HER)catalytic electrodes under actual working conditions show interesting mass transfer behaviors at solid(electrode)/liquid(electrolyte)/gas(hydrogen)three-phase interfaces.These behaviors... Hydrogen evolution reaction(HER)catalytic electrodes under actual working conditions show interesting mass transfer behaviors at solid(electrode)/liquid(electrolyte)/gas(hydrogen)three-phase interfaces.These behaviors are essential for forming a continuous and effective physical contact region between the electrolyte and the electrode and require further detailed understanding.Here,a case study on 1 T-2 H phase molybdenum disulfide(Mo S_(2))/carbon fiber paper(CFP)catalytic electrodes is performed.Rapid gas-liquid mass transfer at the interface for enhancing the working area stability and capillarity for increasing the electrode working area is found.The real scenario,wherein the energy utilization efficiency of the as-prepared non-noble metal catalytic electrode exceeds that of the noble metal catalytic electrode,is disclosed.Specifically,a fluid dynamics model is developed to investigate the behavior mechanism of hydrogen bubbles from generation to desorption on the catalytic electrode surface with different hydrophilic and hydrophobic properties.These new insights and theoretical evidence on the non-negligible three-phase interface behaviors will identify opportunities and motivate future research in high-efficiency,stability,and low-cost HER catalytic electrode development. 展开更多
关键词 Hydrogen evolution reaction Three-phase interface behavior Catalytic electrode Fluid dynamics 1T-2H MoS_(2)
原文传递
Experimental study on the shear behavior of the interface between cushion materials and the concrete raft 被引量:1
7
作者 Li Yaokun Han Xiaolei +1 位作者 Khaled Galal Ji Jing 《Earthquake Engineering and Engineering Vibration》 SCIE EI CSCD 2018年第1期165-178,共14页
Cushion is a layer of granular materials between the raft and the ground. The shear behavior of the interface between the cushion and the raft may influence the seismic performance of the superstructure. In order to q... Cushion is a layer of granular materials between the raft and the ground. The shear behavior of the interface between the cushion and the raft may influence the seismic performance of the superstructure. In order to quantify such influences, horizontal shear tests on the interfaces between different cushion materials and concrete raft under monotonic and cyclic loading were carried out. The vertical pressure P_v, material type and cushion thickness h_c were taken as variables. Conclusions include: 1) under monotonic loading, P_v is the most significant factor; the shear resistance P_(hmax) increases as P_v increases, but the normalized factor of resistance μ_n has an opposite tendency; 2) for the materials used in this study, μ_n varies from 0.40 to 0.70, the interface friction angle δ_s varies from 20° to 35°, while u_(max) varies from 3 mm to 15 mm; 3) under cyclic loading, the interface behavior can be abstracted as a "three-segment" back-bone curve, the main parameters include μ_n, the displacement u_1 and stiffness K_1 of the elastic stage, the displacement u_2 and stiffness K_2 of the plastic stage; 4) by observation and statistical analysis, the significance of different factors, together with values of K_1, K_2 and μ_n have been obtained. 展开更多
关键词 cushion/raft interface shear behavior monotonic test cyclic test "three-segment" back-bone curve
下载PDF
The Numerical Analysis of Strain Behavior at Solder Joint and Interface of Flip Chip Package
8
作者 S C Chen Y C Lin 《厦门大学学报(自然科学版)》 CAS CSCD 北大核心 2002年第S1期186-188,共3页
The flip chip package is a kind of advanced electri ca l packages. Due to the requirement of miniaturization, lower weight, higher dens ity and higher performance in the advanced electric package, it is expected that ... The flip chip package is a kind of advanced electri ca l packages. Due to the requirement of miniaturization, lower weight, higher dens ity and higher performance in the advanced electric package, it is expected that flip chip package will soon be a mainstream technology. The silicon chip is dir ectly connected to printing circuit substrate by SnPb solder joints. Also, the u nderfill, a composite of polymer and silica particles, is filled in the gap betw een the chip and substrate around the solder joints to improve the reliabili ty of solder joints. When flip chip package specimen is tested with thermal cycl ing, the cyclic stress/strain response that exists at the underfill interfaces and solder joints may result in interfacial crack initiation and propagation. Therefore, the chip cracking and the interfacial delamination between underfill and chip corner have been investigated in many studies. Also, most researches h ave focused on the effect of fatigue and creep properties of solder joint induce d by the plastic strain alternation and accumulation. The nuderfill must have lo w viscosity in the liquid state and good adhesion to the interface after solidif ying. Also, the mechanical behavior of such epoxy material has much dependen ce on temperature in its glass transition temperature range that is usually cove red by the temperature range of thermal cycling test. Therefore, the materia l behavior of underfill exists a significant non-linearity and the assumption o f linear elastic can lack for accuracy in numerical analysis. Through numerical analysis, this study had some comparisons about the effect of linear and non -linear properties of underfill on strain behaviors around the interface of fli p chip assembly. Especially, the deformation tendency inside solder bumps could be predicted. Also, it is worthily mentioned that we have pointed out which comp onent of plastic strain, thus, either normal or shear, has dominant influence to the fatigue and creep of solder bump, which have not brought up before. About the numerical analysis to the thermal plastic strain occurs in flip chip i nterconnection during thermal cycling test, a commercial finite element software , namely, ANSYS, was employed to simulate the thermal cycling test obeyed by MIL-STD-883C. The temperatures of thermal cycling ranged from -55 ℃ to 125 ℃ with ramp rate of 36 ℃/min and a dwell time of 25 min at peak temperature. T he schematic drawing of diagonal cross-section of flip chip package composed of FR-4 substrate, silicon chip, underfill and solder bump was shown as Fig.1. Th e numerical model was two-dimensional (2-D) with plane strain assumption and o nly one half of the cross-section was modeled due to geometry symmetry. The dim ensions and boundary conditions of numerical model were shown in Fig.2. The symm etric boundary conditions were applied along the left edge of the model, and the left bottom corner was additional constrained in vertical direction to prevent body motion. The finite element meshes of overall and local numerical model was shown as Fig.3. In this study, two cases of material model were used to describe the material behavior of the underfill: the case1 was linear elastic model that assumed Young’s Modulus (E) and thermal expansion coefficient (CTE) were consta nt during thermal cycling; the case2 was MKIN model (in ANSYS) that had nonlinea r temperature-dependent stress-strain relationship and temperature-dependent CTE. The material model applied to the solder bump was ANAND model (in ANSYS) th at described time-dependent plasticity phenomenon of viscoplastic material. Bot h the FR-4 substrate and silicon chip were assumed as temperature-independent elastic material; moreover, FR-4 substrate is orthotropic while silicon chip is isotropic. From the comparison between numerical results of linear and nonlinear material a ssumption of underfill, (i.e. case1 and case2), the quantities of plastic strain around the interconnection from case1 are higher than that in case2. Thus, the linear 展开更多
关键词 The Numerical Analysis of Strain behavior at Solder Joint and interface of Flip Chip Package
下载PDF
THE INTERFACIAL BEHAVIORS OF ALUMINUM MATRIX COMPOSITE IN DIFFERENT WELDING METHODS 被引量:5
9
作者 W.Guo J.T.Niu +2 位作者 J.F.Zhai G.T.Zhou M.Z.Wang 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2004年第1期55-60,共6页
Non-interlayer liquid phase diffusion welding (China Patent) and laser welding methods for aluminum matrix composite are mainly described in this paper. In the non-interlayer liquid phase diffusion welding, the key pr... Non-interlayer liquid phase diffusion welding (China Patent) and laser welding methods for aluminum matrix composite are mainly described in this paper. In the non-interlayer liquid phase diffusion welding, the key processing parameters affecting the strength of joint is welding temperature. When temperature rises beyond solidus temperature, the bonded line vanishes. The strength of joint reaches the maximum and becomes constant when welding temperature is close to liquid phase temperature. Oxide film in the interface is no longer detected by SEM in the welded joint. With this kind of technique, particle reinforced aluminum matrix composite Al2 O3p/6061Al is welded successfully, and the joint strength is about 80% of the strength of composite (as-casted). In the laser welding, results indicate that because of the huge specific surface area of the reinforcement, the interfacial reaction between the matrix and the reinforcement is restrained intensively at certain laser power and pulsed laser beam. The laser pulse frequency directly affects the reinforcement segregation and the reinforcement distribution in the weld, so that the weldability of the composite could be improved by increasing the laser pulse frequency. The maximum strength of the weld can reach 70% of the strength of the parent. 展开更多
关键词 non-interlayer liquid phase diffusion welding Al2O3p/6061 Alaluminum matrix composite laser welding interface behavior REINFORCEMENT
下载PDF
Friction Characteristics Between Marine Clay and Construction Materials
10
作者 KOU Hailei HUANG Jiaming CHENG Yang 《Journal of Ocean University of China》 CAS CSCD 2024年第2期427-437,共11页
Structure-soil interface friction characteristics is of importance to investigate the interaction between engineering structures and soils,especially for offshore structures.The interface friction behavior between mar... Structure-soil interface friction characteristics is of importance to investigate the interaction between engineering structures and soils,especially for offshore structures.The interface friction behavior between marine clay and structural materials with different roughness was studied in this paper by using 3D optical scanning tests,a modified direct shear device and numerical simulation.Relationships between the surface roughness of structures,water content and interface friction angle were presented by model tests.The increase of water contents decreased the interface friction angles.For interfaces with different roughness,the interface friction angles will be smaller than that of the soil when the water content exceeds a certain value.The roughness of the interface and the water content of the soil are mutually coupled to influence the coefficient of friction(COF).This paper proposed a Finite Element Method(FEM)to simulate the interface direct shear tests of structures with different roughness.The surface models with different roughness are established based on the structure data obtained by 3D scanning.The Coupled Eulerian-Lagrangian(CEL)approach was employed to analyse soils sheared by irregular surfaces.The interface behavior for interfaces with different roughness under cyclic shear stresses was analyzed by FEM. 展开更多
关键词 marine clay construction material interface friction behavior surface roughness Finite Element Method
下载PDF
A Simplified Method for Estimating the Initial Stiffness of Monopile-Soil Interaction Under Lateral Loads in Offshore Wind Turbine Systems
11
作者 LI Xiao-juan DAI Guo-liang +2 位作者 ZHU Ming-xing WANG Li-yan LIU Hong-yuan 《China Ocean Engineering》 SCIE EI CSCD 2023年第1期165-174,共10页
The interface mechanical behavior of a monopile is an important component of the overall offshore wind turbine structure design.Understanding the soil-structure interaction,particularly the initial soil-structure stif... The interface mechanical behavior of a monopile is an important component of the overall offshore wind turbine structure design.Understanding the soil-structure interaction,particularly the initial soil-structure stiffness,has a significant impact on the study of natural frequency and dynamic response of the monopile.In this paper,a simplified method for estimating the interface mechanical behavior of monopiles under initial lateral loads is proposed.Depending on the principle of minimum potential energy and virtual work theory,the functions of soil reaction components at the interface of monopiles are derived;MATLAB programming has been used to simplify the functions of the initial stiffness by fitting a large number of examples;then the functions are validated against the field test data and FDM results.This method can modify the modulus of the subgrade reaction in the p-y curve method for the monopile-supported offshore wind turbine system. 展开更多
关键词 theoretical analysis pile−soil interaction interface mechanical behavior offshore wind turbine systems
下载PDF
Laser brazing with filler wire for galvanized steel sheets 被引量:2
12
作者 封小松 李俐群 +1 位作者 陈彦宾 周善宝 《China Welding》 EI CAS 2005年第1期9-14,共6页
The process properties and interface behavior of CO_2 laser brazing with automatic wire feed for galvanized steel sheets were investigated, in which the brazing filler metal was CuSi3 and no flux was used. As to the a... The process properties and interface behavior of CO_2 laser brazing with automatic wire feed for galvanized steel sheets were investigated, in which the brazing filler metal was CuSi3 and no flux was used. As to the appearance quality of the brazing seams, the roles of the processing parameters, such as brazing speed, wire feeding rate, inclination and feeding direction of the wire, laser power, spot diameter and heating position, were assessed. The further investigation indicates that the behavior of the active elements Si, Mn and Zn are significantly influenced by energy input. At the interface, the microstructure of the base metal was composed of columnar crystals and the acicular α solid solution was found on the filler metal side. 展开更多
关键词 galvanized steel sheets laser brazing with filler wire interface behavior
下载PDF
Interfacial Microstructure between WC-Based Cermet and Cu Alloy 被引量:1
13
作者 Xinhong WANG, Zengda ZOU, Sili SONG and Shiyao QUSchool of Materials Science and Engineering, Shandong University, Jinan 250061, China 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2004年第6期731-734,共4页
A WC-TiC-Co/CuZnNi composite layer was produced on 1045 steel substrate by means of inside-furnace brazing technique. The microstructure, phase constituent and interfacial diffusion behavior between cermet and CuZnNi ... A WC-TiC-Co/CuZnNi composite layer was produced on 1045 steel substrate by means of inside-furnace brazing technique. The microstructure, phase constituent and interfacial diffusion behavior between cermet and CuZnNi alloy were investigated by means of scanning electron microscopy (SEM), transmission electron microscope (TEM), electron probe microanalyzer (EPMA) and X-ray diffraction. The results showed that microstructure of matrix was α and β phases. Cermet particies were surrounded by the α+β phases in the composite layer and their sizes were almost similar to those in original state. The interfacial zone was formed by the mutual diffusion of elements under the condition of high temperature. The interface consists of WC, TiC, CuZn, and CuNi phases, and there are no microcracks and inclusions near the interface. 展开更多
关键词 Cu-base alloy WC-based cermet interface behavior Microstructure
下载PDF
STUDIES ON THE INTERFACIAL ADHESION BETWEEN FUNCTIONALIZED POLYPROPYLENE AND POLYAMIDE 1010
14
作者 Xiao-min Zhang Zhihui Yin +1 位作者 Yongxian Song Jinghua Yin Polymer Physics Laboratory, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, China 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 1999年第3期237-244,共8页
The interface behavior of polyamide 1010 (PA1010) and polypropylene (PP) was studied. In order to improve their interfacial adhesion, functional PP was prepared by means of grafting glycidyl methacrylate (GMA) on PP m... The interface behavior of polyamide 1010 (PA1010) and polypropylene (PP) was studied. In order to improve their interfacial adhesion, functional PP was prepared by means of grafting glycidyl methacrylate (GMA) on PP main chains and used instead of plain PP. Several technological characterizations were performed here on their interfaces. ESCA was used to confirm that some kind of reaction occurred between end groups of PA1010 and epoxy species of PP-g-GMA. The peel test was adopted to measure interfacial adhesion. It was found that the fracture energy of interfaces between PA1010 and PP-g-GMA was dramatically increased with the content of GMA. Their interfaces were observed as being blurred by using SEM and TEM and a crack that could be seen in the case of the interfaces of the PA1010 and the plain PP disappeared. 展开更多
关键词 polyamide 1010 polypropylene-g-GMA interface behavior ADHESION
下载PDF
Bearing mechanism of a tunnel-type anchorage in a railway suspension bridge 被引量:3
15
作者 JIANG Nan WANG Duo +2 位作者 FENG Jun ZHANG Sheng-liang HUANG Lin 《Journal of Mountain Science》 SCIE CSCD 2021年第8期2143-2158,共16页
A tunnel-type anchorage(TTA)is one of the main components in suspension bridges:the bearing mechanism is a key problem.Investigating the deformation characteristics,development law,and failure phenomenon of a TTA unde... A tunnel-type anchorage(TTA)is one of the main components in suspension bridges:the bearing mechanism is a key problem.Investigating the deformation characteristics,development law,and failure phenomenon of a TTA under load can provide the theoretical basis for a robust design.Utilizing the TTA of the Jinsha River suspension bridge at Lijiang Shangri-La railway as a prototype,a laboratory model test of the TTA was carried out for three different contact conditions between the anchorage body and the surrounding rock.The stress and deformation distribution law of the anchorage body and its surrounding rock were studied,and the ultimate bearing capacity and failure mode of the TTA were analyzed.The test results show that the compressive stress level is highest at the rear part of the anchorage body.Moving away from the rear portion of the body,the stress decays in a negative exponential function.Based on the load transfer curve,the calculation formula for the shear stress on the contact surface between the anchorage body and the surrounding rock was derived,which shows that the distribution of the shear stress along the axial direction of the anchorage body is not uniform.The distance from the maximum value to the loading surface is approximately 1/3 of the length of the anchorage body,and the stress decreases as the distance from the loading surface increases.Furthermore,the contact condition between the anchorage body and surrounding rock has a great influence on the bearing capacity of the TTA.The increase in the anti-skid tooth ridge and radial anchor bolt can improve the cooperative working capacity of the anchorage body and the surrounding rock,which is approximately 50%higher than that of the flat contact condition.The main function of the anchor bolt is to increase the overall rigidity of the TTA.The contact condition between the anchorage body and the surrounding rock will lead to a change in the failure mode of the TTA.With an increase in the degree of contact,the failure mode will change from shear sliding along the interface to trumpet-shaped inverted cone-shaped failure extending into the surrounding rock. 展开更多
关键词 Tunnel anchorage Model test Load transfer curve interface mechanical behavior
下载PDF
Diffusion behavior and reactions between Al and Ca in Mg alloys by diffusion couples
16
作者 Jiahong Dai Hong Xiao +6 位作者 Bin Jiang Hongmei Xie Cheng Peng Zhongtao Jiang Qin Zou Qingshan Yang Fusheng Pan 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2018年第2期291-298,共8页
The diffusion behavior and reactions between AI and Ca in Mg alloys by diffusion couple method were investigated. Results demonstrate that Al2Ca is the only phase existing in the diffusion reaction layers. The volume ... The diffusion behavior and reactions between AI and Ca in Mg alloys by diffusion couple method were investigated. Results demonstrate that Al2Ca is the only phase existing in the diffusion reaction layers. The volume fraction of Al2Ca in diffusion reaction layers increases linearly with temperature. The standard enthalpy of formation for intermetallic compounds was rationalized on the basis of the Miedema model. Al-Ca intermetallic compounds were preferable to form in the Mg-Al-Ca ternary system under the same conditions. Over the range of 350-400℃, the structure of Al2Ca is more stable than that of Al4Ca, Al14Ca13and Al3Ca8, The growth constants of the layer I, layer II and entire diffusion reaction layers were determined. The activation energies for the growth of the layer I, layer II and entire diffusion reaction layers were (80.74 ± 3.01 ) kJ/mol, (93.45 ±2.12) kJ/mol and (83.52 ±1.50) kJ/mot, respectively. In layer I and II, AI has higher integrated interdiffusion coefficients D^i^Int,layer layer than Ca. The average effective interdiffusion coefficients D^Al^eff values are higher than D^Ca^eff in the layer I and II. 展开更多
关键词 Magnesium alloys Diffusion behavior interface lntermetallic compounds
原文传递
Ta_(4)HfC_(5)-Si_(2)BC_(3)N复相陶瓷的界面结构和晶粒生长行为
17
作者 关景怡 李达鑫 +6 位作者 周国相 段文久 杨治华 贾德昌 Ralf Riedel 秦少华 周玉 《Science China Materials》 SCIE EI CAS CSCD 2023年第11期4306-4316,共11页
超高温陶瓷(UHTC)Ta_(4)HfC_(5)因其优异的热物理和热机械性能而成为适用于高超音速飞行器最有前途的候选材料之一.然而,较差的烧结能力限制了其潜在的使用.为了克服该障碍,采用Si_(2)BC_(3)N陶瓷对钽-铪碳化物固溶体进行了致密化处理.... 超高温陶瓷(UHTC)Ta_(4)HfC_(5)因其优异的热物理和热机械性能而成为适用于高超音速飞行器最有前途的候选材料之一.然而,较差的烧结能力限制了其潜在的使用.为了克服该障碍,采用Si_(2)BC_(3)N陶瓷对钽-铪碳化物固溶体进行了致密化处理.通过热压烧结合成了致密的Ta_(4)HfC_(5)-Si_(2)BC_(3)N陶瓷,所得复相陶瓷由Ta_(4)HfC_(5),SiC和BN(C)相组成.在2100℃下,随着晶粒的快速生长,陶瓷内形成了“蝌蚪”状的SiC和BN(C)连接相,断裂韧性提高到3.47±0.12 MPa m^(1/2).随着烧结温度的升高,Ta_(4)HfC_(5)晶粒的生长活化能从112.4 kJ mol^(−1)增加到250.7±29.3 kJ mol^(−1). 展开更多
关键词 Ta_(4)HfC_(5)-Si_(2)BC_(3)N ceramic interface behavior growth kinetics mechanical properties