Influence of refining process and utilization of different slags on inclusions, titanium yield and total oxygen content of Ti-stabilized 321 stainless steel 被引量:2
1
作者 Xing-run Chen Guo-guang Cheng +2 位作者 Yu-yang Hou Jing-yu Li Ji-xiang Pan 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2020年第8期913-921,共9页
Ti-stabilized 321 stainless steel was prepared using an electric arc furnace, argon oxygen decarburization (AOD) furnace, ladle furnace (LF), and continuous casting processes. In addition, the effect of refining proce... Ti-stabilized 321 stainless steel was prepared using an electric arc furnace, argon oxygen decarburization (AOD) furnace, ladle furnace (LF), and continuous casting processes. In addition, the effect of refining process and utilization of different slags on the evolution of inclusions, titanium yield, and oxygen content was systematically investigated by experimental and thermodynamic analysis. The results reveal that the total oxygen content (TO) and inclusion density decreased during the refining process. The spherical CaO–SiO2–Al2O3–MgO inclusions existed in the 321 stainless steel after the AOD process. Moreover, prior to the Ti addition, the spherical CaO–Al2O3–MgO–SiO2 inclusions were observed during LF refining pro-cess. However, Ti addition resulted in multilayer CaO–Al2O3–MgO–TiOx inclusions. Two different samples were prepared by conventional CaO–Al2O3-based slag (Heat-1) and -TiO2-rich CaO–Al2O3-based slag (Heat-2). The statistical analysis revealed that the density of inclusions and the -TiOx content in CaO–Al2O3–MgO–TiOx inclusions found in Heat-2 sample are much lower than those in the Heat-1 sample. Furthermore, the TO content and Ti yield during the LF refining process were controlled by using -TiO2-rich calcium aluminate synthetic slag. These results were consistent with the ion–molecule coexist-ence theory and FactSage?7.2 software calculations. When -TiO2-rich CaO–Al2O3-based slag was used, the -TiO2 activity of the slag increased, and the equilibrium oxygen content significantly decreased from the AOD to LF processes. Therefore, the higher -TiO2 activity of slag and lower equilibrium oxygen content suppressed the undesirable reactions between Ti and O. 展开更多
关键词 321 Austenitic stainless steel Oxygen content INCLUSION TiO2-rich CaO–Al2O3-based slag Ladle furnace(lf)refining process Ion–molecule coexistence theory
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部