Carbon nanotubes (CNTs) were prepared by decomposition of C2H2 over newly developed LaCu0.2Ni0.8Ox in the temperature range from 600 to 850℃. The effect of the reaction temperature on the yield of CNTs was investiga...Carbon nanotubes (CNTs) were prepared by decomposition of C2H2 over newly developed LaCu0.2Ni0.8Ox in the temperature range from 600 to 850℃. The effect of the reaction temperature on the yield of CNTs was investigated in detail. At 680℃,the yield of CNTs reaches 17 g/g.catal. or so. The morphology of CNTs was examined by TEM. The diameter of CNTs rangs from 9 nm to 14 nm.展开更多
文摘Carbon nanotubes (CNTs) were prepared by decomposition of C2H2 over newly developed LaCu0.2Ni0.8Ox in the temperature range from 600 to 850℃. The effect of the reaction temperature on the yield of CNTs was investigated in detail. At 680℃,the yield of CNTs reaches 17 g/g.catal. or so. The morphology of CNTs was examined by TEM. The diameter of CNTs rangs from 9 nm to 14 nm.