Advanced lead-free energy storage ceramics play an indispensable role in next-generation pulse power capacitors market.Here,an ultrahigh energy storage density of~13.8 J cm^(-3)and a large efficiency of~82.4%are achie...Advanced lead-free energy storage ceramics play an indispensable role in next-generation pulse power capacitors market.Here,an ultrahigh energy storage density of~13.8 J cm^(-3)and a large efficiency of~82.4%are achieved in high-entropy lead-free relaxor ferroelectrics by increasing configuration entropy,named high-entropy strategy,realizing nearly ten times growth of energy storage density compared with low-entropy material.Evolution of energy storage performance and domain structure with increasing configuration entropy is systematically revealed for the first time.The achievement of excellent energy storage properties should be attributed to the enhanced random field,decreased nanodomain size,strong multiple local distortions,and improved breakdown field.Furthermore,the excellent frequency and fatigue stability as well as charge/discharge properties with superior thermal stability are also realized.The significantly enhanced comprehensive energy storage performance by increasing configuration entropy demonstrates that high entropy is an effective but convenient strategy to design new high-performance dielectrics,promoting the development of advanced capacitors.展开更多
Inorganic halide double perovskites A_(2)B'B"X_(6) have gained significant interests for their diverse composition,stable physicochemical properties,and potential for photoelectric applications.The influences...Inorganic halide double perovskites A_(2)B'B"X_(6) have gained significant interests for their diverse composition,stable physicochemical properties,and potential for photoelectric applications.The influences of trivalent and monovalent cations on the formation energy,decomposition energy,electronic structure and optical properties of cesium-based lead-free Cs^(+)_(2)B'B"Br_(6) (B'=Na^(+),In^(+)Cu^(+),or Ag^(+);B"=Bi^(3),Sb^(3+),In^(3+)) are systematically studied.In view of the analysis and results of the selected double perovskites,for the double perovskites with different B-site trivalent cation,the band gap increases in the order of Cs_(2)AgInBr_(6),Cs_(2)AgSbBr_(6) and Cs_(2)AgBiBr_(6),with Cs_(2)AgBiBr_(6) possessing the highest thermodynamic stability.Therefore,the Bi-based perovskites are further studied to elucidate the effect of monovalent cation on their stability and electronics.Results show that the thermodynamic stability rises in the sequence of Cs_(2)NaBiBr_(6),Cs_(2)InBiBr_(6),Cs_(2)AgBiBr_(6) and Cs_(2)CuBiBr_(6).Notably,Cs_(2)CuBiBr_(6) exhibits a relatively narrow and appropriate band gap of 1.4634 eV,together with the highest absorption coefficient than other compounds,suggesting that Cs_(2)CuBiBr_(6) is a promising light absorbing material that can be further explored experimentally and be applied to optoelectronic devices.Our research offers theoretical backing for the potential optoelectronic application of cesium-based lead-free halide double perovskites in solar energy conversion.展开更多
To reduce the coercive field of Na_(0.5)Bi_(0.5)TiO_(3),Ba TiO_(3)were added as dopant materials.Then the(1-x)Na_(0.5)Bi_(0.5)TiO_(3)-xBaTiO_(3)ceramic samples were produced in solid synthetic way.The optimum preparat...To reduce the coercive field of Na_(0.5)Bi_(0.5)TiO_(3),Ba TiO_(3)were added as dopant materials.Then the(1-x)Na_(0.5)Bi_(0.5)TiO_(3)-xBaTiO_(3)ceramic samples were produced in solid synthetic way.The optimum preparation condition and piezoelectric properties of the samples were investigated.The XRD results show that the fabric transites from rhombohedral to tetragonal gradually with the substitution of the Ba^(2+).The morphotropic phase boundaries(MPB)exists in the composition range of 0.06.展开更多
Yellow light-emitting diodes(LEDs) as soft light have attracted abundant attention in lithography room, museum and art gallery. However, the development of efficient yellow LEDs lags behind green and blue LEDs, and th...Yellow light-emitting diodes(LEDs) as soft light have attracted abundant attention in lithography room, museum and art gallery. However, the development of efficient yellow LEDs lags behind green and blue LEDs, and the available perovskites yellow LEDs suffer from the instability. Herein, a pressure-assisted cooling method is proposed to grow lead-free CsCu2I3single crystals, which possess uniform surface morphology and enhanced photoluminescence quantum yield(PLQY) stability, with only 10% PLQY losses after being stored in air after 5000 h.Then, the single crystals used for yellow LEDs without encapsulation exhibit a decent Correlated Color Temperature(CCT) of 4290 K, a Commission Internationale de l’Eclairage(CIE) coordinate of(0.38, 0.41), and an excellent 570-h operating stability under heating temperature of 100°C. Finally, the yellow LEDs facilitate the application in wireless visible light communication(VLC), which show a-3 dB bandwidth of 21.5 MHz and a high achievable data rate of 219.2 Mbps by using orthogonal frequency division multiplexing(OFDM) modulation with adaptive bit loading. The present work not only promotes the development of lead-free single crystals, but also inspires the potential of CsCu2I3in the field of yellow illumination and wireless VLC.展开更多
The tensile properties of Sn-9Zn-xAg-ySb;{(x, y) = (0.2, 0.6), (0.2, 0.8), (0.6, 0.2), (0.8, 0.2)} lead-free solders were investigated. All the test samples were annealed at 150°C for 1 hour. The tests are carrie...The tensile properties of Sn-9Zn-xAg-ySb;{(x, y) = (0.2, 0.6), (0.2, 0.8), (0.6, 0.2), (0.8, 0.2)} lead-free solders were investigated. All the test samples were annealed at 150°C for 1 hour. The tests are carried out at room temperature at the strain rate of 4.17 × 10<sup>-3</sup> s<sup>-1</sup>, 20.85 × 10<sup>-3</sup> s<sup>-1</sup>, and 208.5 × 10<sup>-3</sup> s<sup>-1</sup>. It is seen that the tensile strength increases and the ductility decrease with increasing the strain rate over the investigated range. From the strain rate change test results, the strain sensitivity values are found in the range of 0.0831 to 0.1455 due to the addition of different alloying elements.展开更多
Soldering experiments with Sn-3.5Ag-0.5Cu lead-free solder on Au/Ni/Cu pad were carried out by means of diode-laser and IR reflow soldering methods respectively.The influence of different heating methods as well as ou...Soldering experiments with Sn-3.5Ag-0.5Cu lead-free solder on Au/Ni/Cu pad were carried out by means of diode-laser and IR reflow soldering methods respectively.The influence of different heating methods as well as output power of diode-laser on shear force of micro-joints was studied and the relationship between the shear force and microstructures of micro-joints was analyzed.The results indicate that the formation of intermetallic compound Ag3Sn is the key factor to affect the shear force and the fine eutectic network structures of micro-joints as well as the dispersion morphology of fine compound Ag3Sn,in which eutectic network band is responsible for the improvement of the shear force of micro-joints soldered with Sn-Ag-Cu lead-free solder.With the increases of output power of diode-laser,the shear force and the microstructures change obviously.The eutectic network structures of micro-joints soldered with diode-laser soldering method are more homogeneous and the grains of Ag3Sn compounds are finer in the range of near optimal output power than those soldered with IR reflow soldering method,so the shear force is also higher than that using IR reflow soldering method.When the output power value of diode-laser is about 41.0 W,the shear force exhibits the highest value that is 70% higher than that using IR reflow soldering method.展开更多
This article explores tile effects of phosphorus addition on the wettability between Sn-9Zn solder alloy and Cu substrates, the oxidation behavior and the corrosion behavior of Sn-9Zn solder alloy. Spreading test was ...This article explores tile effects of phosphorus addition on the wettability between Sn-9Zn solder alloy and Cu substrates, the oxidation behavior and the corrosion behavior of Sn-9Zn solder alloy. Spreading test was used to characterize the wettability of Sn-9Zn-xP solder alloys to Cu substrates. The oxidation and corrosion behaviors of Sn- 9Zn-xP solder alloys were determined by means of weight gaining, and secondary ion mass spectrometry was used to analyze the oxygen content. The role and mechanism of P in the solder alloys were also discussed. It is found that the addition of P can significantly improve the wettability of the solder alloys. Incorporating P into Sn-9Zn solder alloy obviously decreases the oxygen content and enhances the oxidation and corrosion resistance. Microstructure observations show that an appropriate amount of P can greatly refine coarse rod-like Zn-rich phases in Sn-gZn solder alloy.展开更多
Sensitive and reliable X-ray detectors are essential for medical radiography,industrial inspection and security screening.Lowering the radiation dose allows reduced health risks and increased frequency and fidelity of...Sensitive and reliable X-ray detectors are essential for medical radiography,industrial inspection and security screening.Lowering the radiation dose allows reduced health risks and increased frequency and fidelity of diagnostic technologies for earlier detection of disease and its recurrence.Three-dimensional(3 D)organic-inorganic hybrid lead halide perovskites are promising for direct X-ray detection-they show improved sensitivity compared to conventional X-ray detectors.However,their high and unstable dark current,caused by ion migration and high dark carrier concentration in the 3 D hybrid perovskites,limits their performance and long-term operation stability.Here we report ultrasensitive,stable X-ray detectors made using zero-dimensional(0 D)methylammonium bismuth iodide perovskite(MA3Bi2I9)single crystals.The 0 D crystal structure leads to a high activation energy(Ea)for ion migration(0.46 e V)and is also accompanied by a low dark carrier concentration(~10^6 cm^-3).The X-ray detectors exhibit sensitivity of 10,620μC Gy-1 air cm-2,a limit of detection(Lo D)of 0.62 nG yairs-1,and stable operation even under high applied biases;no deterioration in detection performance was observed following sensing of an integrated X-ray irradiation dose of^23,800 m Gyair,equivalent to>200,000 times the dose required for a single commercial X-ray chest radiograph.Regulating the ion migration channels and decreasing the dark carrier concentration in perovskites provide routes for stable and ultrasensitive X-ray detectors.展开更多
Lead-free piezoelectric ceramics of (Bi1/2Na1/2)TiO3-BaTiO3(BNT-BT) were prepared by the conventional piezoelectric ceramic preparation technique (free air atmosphere sintering). The influence of BaTiO3 additive amoun...Lead-free piezoelectric ceramics of (Bi1/2Na1/2)TiO3-BaTiO3(BNT-BT) were prepared by the conventional piezoelectric ceramic preparation technique (free air atmosphere sintering). The influence of BaTiO3 additive amount and La2O3 additive amount on the properties of BNT-BT lead-free piezoceramics were investigated. The results show that the dielectric constant(ε) and piezoelectric strain constant(d33) of materials start increasing and then decreasing while BaTiO3 additive amount increasing, the ε and d33 of materials have maximum value (ε=1650, d33=120 PC·N-1) while x(BaTiO3)=0.06 mol. The ε and d33 of materials start increasing and then decreasing while La2O3 additive amount increasing, the ε and d33 of materials have maximum value (ε=1684, d33=153 PC·N-1) while w(La2O3)=0.3%. The influence of La2O3 additive amount on the microstructure of BNT-BT piezoelectric ceramics was analysed by SEM(scanning electron microscope). The influence mechanism of La2O3 additive amount on the properties of BNT-BT piezoelectric ceramics was discussed. The BNT-BT ceramics with optimum comprehensive properties were obtained.展开更多
Sn-Ag alloy system has been regarded as one of the most promising lead-free solder to substitute conventional Sn- Pb eutectic solder. But the formation of bulk Ag3Sn intermetallic compounds (IMCs) during reflow and ...Sn-Ag alloy system has been regarded as one of the most promising lead-free solder to substitute conventional Sn- Pb eutectic solder. But the formation of bulk Ag3Sn intermetallic compounds (IMCs) during reflow and post heat treatment significantly influences the performance of the solder joints. With an effort to clarify its microstructural evolution as a function of slow cooling rates, the fraction of bulk IMCs within the slowly solidified Sn-4.0 wt pct Ag solder was investigated by standard metallographic and compared with that detected by thermal analysis. It was found that the bulk IMCs fraction determined by thermal analysis corresponds quite well with the microstructure observation results. In accordance with the conventional solidification theory, the lower the applied cooling rate, the fewer the amount of bulk Ag3Sn IMCs formed in Sn-4.0 wt pct Ag alloy. In addition, Vickers hardness measurement results indicated that the relative coarse eutectic Ag3Sn IMCs distributing in the lamellar eutectic structure favored the improvement of the mechanical performance.展开更多
An orthogonal method was used to evaluate the effects of Ga, Al, Ag, and Ce multi-additions on the wetting characteristics of Sn-9Zn lead-free solders by wetting balance method. The results show that the optimal loadi...An orthogonal method was used to evaluate the effects of Ga, Al, Ag, and Ce multi-additions on the wetting characteristics of Sn-9Zn lead-free solders by wetting balance method. The results show that the optimal loading of Ga, Al, Ag, and Ce was 0.2 wt.%, 0.002 wt.%, 0.25 wt.%, and 0.15 wt.%, respectively. Intermetallic compounds (IMCs) formed at the interface between Sn-9Zn-0.2Ga-0.002Al-0.25Ag- 0.15Ce solder and Cu substrate were investigated by scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) analysis. The SEM images illustrate that the IMCs can be divided into two portions from the substrate side to the solder side: a planar CusZns layer and an additional continuous scallop-like AgZn3 layer. The EDS analysis also shows that Ga segregates in the solder abutting upon the interface. X-ray photoelectron spectroscopy (XPS) and Auger electron spectroscopy (AES) of the surface components of Sn-9Zn-0.2Ga-0.002Al- 0.25Ag-0.15Ce solder indicate that Al aggregates at the surface in the form of Al203 protective fdm, which prevents the further oxidation of the solder surface. On the other hand, Ce aggregates at the subsurface, which may reduce the surface tension of the solder and improve the wettability in consequence.展开更多
Aim The piezoelectric properties and cytotoxicity of a porous lead-free piezoelectric ceramic for use as a direct bone substitute were investigated. Methodology Cold isostatic pressing (CIP) was applied to fabricate...Aim The piezoelectric properties and cytotoxicity of a porous lead-free piezoelectric ceramic for use as a direct bone substitute were investigated. Methodology Cold isostatic pressing (CIP) was applied to fabricate porous lithium sodium potassium niobate (Li0.06Na0.5K0.44) NbO3 specimens using a pore-forming method. The morphologies of the CIP-processed specimens were characterized and compared to those of specimens made by from conventional pressing procedures. The effects of the ceramic on the attachment and proliferation of osteoblasts isolated from the cranium of 1-day-old Sprague- Dawley rats were examined by a scanning electron microscopy (SEM) and metbylthiazol tetrazolium (MTT) assay. Results The results showed that CIP enhanced piezoelectricity and biological performance of the niobate specimen, and also promoted an extracellular matrix-like topography of it. In vitro studies showed that the CIP-enhanced material had positive effects on the attachment and proliferation of osteoblasts. Conclusion Niobate ceramic generated by CIP shows a promise for being a piezoelectric composite bone substitute.展开更多
CuO-doped(Ag0.75Li0.1Na0.1K0.05)NbO3(ALNKN-xCuO, x = 0.2mol%) lead-free piezoelectric ceramics were prepared by the solid-state reaction method in air atmosphere. The effects of CuO addition on the phase structure...CuO-doped(Ag0.75Li0.1Na0.1K0.05)NbO3(ALNKN-xCuO, x = 0.2mol%) lead-free piezoelectric ceramics were prepared by the solid-state reaction method in air atmosphere. The effects of CuO addition on the phase structure, microstructure, and piezoelectric properties of the ceramics were investigated. The experimental results show that the ALNKN ceramics without doping CuO possess rhombohedral phase along with K2NbrO16- type phase and metallic silver phase. For all of the CuO-doped ALNKN ceramics, a pure perovskite structure with the orthorhombic phase was obtained by enclosing the samples in a corundum tube. A homogeneous microstructure with'the grain size of about 1 ~tm was formed for the ceramics with 0.5mo1% CuO. The grain size increases with increasing amount of CuO. The temperature dependence of dielectric properties indicates that the ferroelectric phase of the ALNKN-xCuO ceramics becomes less stable with the addition of CuO. The ceramics with x = lm01% exhibit relatively good electrical properties along with a high Curie temperature. These results will provide a helpful guidance to preparing other AN-based ceramics by solid-state reaction method in air atmosphere.展开更多
Lead-free piezoelectric (K0.5sNa0.5)1-xLixNbO3 (x = 0at%-20at%) ceramics were synthesized by spark plasma sintering (SPS) at low temperature and the effects of LiNbO3 addition on its crystal structure and proper...Lead-free piezoelectric (K0.5sNa0.5)1-xLixNbO3 (x = 0at%-20at%) ceramics were synthesized by spark plasma sintering (SPS) at low temperature and the effects of LiNbO3 addition on its crystal structure and properties were also studied. When the Li content was less than 6at%, a single proveskite phase with the similar structure of (K0.5Na0.5)NbO3 was formed; and a secondary phase with K3Li2Nb5O15 structure was observed in the 6at% 〈 x 〈 20at% compositional range. Furthermore, LiNbO3 existed as the third phase when the Li content was higher than 8at%. The grain sizes increased from 200-500 nm to 5-8 μm when the K3Li2Nb5O15 and LiNbO3 like phases were formed. With increasing Li content, the relative density of the ceramics first decreased from 97% to 93% and then kept constant. The piezoelectric coefficient d33, dielectric constant, and planner electromechanical coupling factor exhibited a decreasing tendency with increasing Li content because of the decrease in density and the formation of the secondary phase such as K3Li2Nb5O15 and LiNbO3. The formation of dense microstructure with a single phase is necessary in improving the properties of the (K0.5Na0.5)1-xLixNbO3 ceramics.展开更多
Ti-Modified (Na0.5K0.5)(TixNb1-x)O3 (NKNT) piezoelectric ceramics were fabricated by double-layer buried powder process at 1020°C for 2 h. The microstructures,and piezoelectric and dielectric properties of the le...Ti-Modified (Na0.5K0.5)(TixNb1-x)O3 (NKNT) piezoelectric ceramics were fabricated by double-layer buried powder process at 1020°C for 2 h. The microstructures,and piezoelectric and dielectric properties of the lead-free NKNT ceramics were investigated. X-ray diffraction re-sults indicated that Ti4+ had diffused into the (Na0.5K0.5)NbO3 lattices to form a solid solution with a perovskite structure. The introducing of Ti into the (Na0.5K0.5)NbO3 solid solution effectively reduced the sintering temperature and densified the microstructure with a decreased grain size. The highest relative density reached more than 90%. The highest piezoelectric dielectric coefficient d33 and planar mode electro-mechanical coupling coefficient kp were 110 pC/N and 19.5%,which were obtained in the NKNT ceramic with 1 mol% Ti. The piezoelectric properties of the NKNT ceramics were enhanced by aging in air for a period of time owing to the compensation of oxygen vacancies.展开更多
A lead-free Sn-3.5Ag solder was prepared by rapid solidification technology. The high solidification rate, obtained by rapid cooling, promotes nucleation, and suppresses the growth of Ag3Sn intermetallic compounds (I...A lead-free Sn-3.5Ag solder was prepared by rapid solidification technology. The high solidification rate, obtained by rapid cooling, promotes nucleation, and suppresses the growth of Ag3Sn intermetallic compounds (IMCs) in Ag-rich zone, yielding fine Ag3Sn nanoparticulates with spherical morphology in the matrix of the solder. The large amount of tough homogeneously-dispersed IMCs helps to improve the surface area per unit volume and obstructs the dislocation lines passing through the solder, which fits with the dispersion-strengthening theory. Hence, the rapidly-solidified Sn-3.5Ag solder exhibits a higher rnicrohardness when compared with a slowly-solidified Sn-3.5Ag solder.展开更多
Emf technique was employed to determine indium activities in the liquid Ag-In-Pd alloys using galvanic cells with yttria-stabilised-zirconia as solid electrolyte according to the scheme: kanthal/rhenium, Ag-In-Pd, In...Emf technique was employed to determine indium activities in the liquid Ag-In-Pd alloys using galvanic cells with yttria-stabilised-zirconia as solid electrolyte according to the scheme: kanthal/rhenium, Ag-In-Pd, In2O3 | YSZ | Ni, NiO, Pt. Composition and temperature measurement ranges were limited, because of very steep liquidus surface; 35 compositions for Xpd up to 0.3 were investigated and at temperatures from near-liquidus up to 1700 K. High temperature experiments required special moly furnace to be constructed with unique automatic gas supply system for fumace winding protective atmosphere. Emf readings were taken and recorded by automatic data acquisition system. Linear dependence of emf on temperature was observed for all compositions investigated, and results were approximated by straight line equa- tions. Then In activities were calculated using well-known relations and taking into account correction for thermoelectric power between kanthal and platinum. Results are to be used along with other existing data to perform assessment of the ternary system under accord.展开更多
A new group of lead-free piezoelectric ceramics,(Bi0.5 Na0.5)1-x(BaaSrb)xTiO3(abbreviated as BNBST[100x-100a/100b],0〈x〈1,a+b=1),was synthesized.The ceramics were prepared by conventional ceramic sintering tec...A new group of lead-free piezoelectric ceramics,(Bi0.5 Na0.5)1-x(BaaSrb)xTiO3(abbreviated as BNBST[100x-100a/100b],0〈x〈1,a+b=1),was synthesized.The ceramics were prepared by conventional ceramic sintering technique,and the ceramics with density of 95% of the theoretical one can be sintered without the atmosphere control during the sintering process.The results of the X-ray diffraction(XRD) data show that the ceramics possess a single perovskite phase.The measurements of dielectric and piezoelectric properties reveal that the ceramics provide relatively high piezoelectric charge constant d33 and high planar electromechanical coupling factor kp.For the BNBST6-95/5 ceramics,d33 is equal to 170pC/N,and kp is equal to 32.0%.The fabrication technique for these ceramics is conventional and stable.展开更多
A lead-free base glaze suitable for pearlescent pigments was prepared by a low-temperature solid-phase reaction with alkali waste.Tests were performed to evaluate the effects of the sintering conditions and alkali was...A lead-free base glaze suitable for pearlescent pigments was prepared by a low-temperature solid-phase reaction with alkali waste.Tests were performed to evaluate the effects of the sintering conditions and alkali waste composition on the prepared base glaze and pearlescent glaze.The experimental results show that partially replacing SiO_(2) with B_(2)O_(3) effectively reduced the sintering temperature and time to form a glass network,but the network structure becomes disconnected as the B_(2)O_(3) content increases.An amorphous base glaze was obtained when soda ash was replaced with a small amount of alkali waste,but increasing the addition of NaCl further was adverse to base glaze formation by resulting in crystallization of the base glaze and a decrease in the bridging oxygen content.The pearlescent pigment was thermally stable in the glaze at 750℃,while higher temperatures caused the crystalline phase of NaAlSiO_(4) to appear and adhere to the surface of pigment granules,which degraded the pearlescent effect of the glaze.展开更多
基金supported by the National Natural Science Foundation of China(Grant Nos.21825102,22235002,52172181,and 22105017)Key R&D Plan of the Ministry of Science and Technology of China(Grant No.2022YFB3204000)。
文摘Advanced lead-free energy storage ceramics play an indispensable role in next-generation pulse power capacitors market.Here,an ultrahigh energy storage density of~13.8 J cm^(-3)and a large efficiency of~82.4%are achieved in high-entropy lead-free relaxor ferroelectrics by increasing configuration entropy,named high-entropy strategy,realizing nearly ten times growth of energy storage density compared with low-entropy material.Evolution of energy storage performance and domain structure with increasing configuration entropy is systematically revealed for the first time.The achievement of excellent energy storage properties should be attributed to the enhanced random field,decreased nanodomain size,strong multiple local distortions,and improved breakdown field.Furthermore,the excellent frequency and fatigue stability as well as charge/discharge properties with superior thermal stability are also realized.The significantly enhanced comprehensive energy storage performance by increasing configuration entropy demonstrates that high entropy is an effective but convenient strategy to design new high-performance dielectrics,promoting the development of advanced capacitors.
基金Funded by the National Natural Science Foundation of China (No.51772228)the Open Fund of Sanya Science and Education Innovation Park (No.2022KF0008)。
文摘Inorganic halide double perovskites A_(2)B'B"X_(6) have gained significant interests for their diverse composition,stable physicochemical properties,and potential for photoelectric applications.The influences of trivalent and monovalent cations on the formation energy,decomposition energy,electronic structure and optical properties of cesium-based lead-free Cs^(+)_(2)B'B"Br_(6) (B'=Na^(+),In^(+)Cu^(+),or Ag^(+);B"=Bi^(3),Sb^(3+),In^(3+)) are systematically studied.In view of the analysis and results of the selected double perovskites,for the double perovskites with different B-site trivalent cation,the band gap increases in the order of Cs_(2)AgInBr_(6),Cs_(2)AgSbBr_(6) and Cs_(2)AgBiBr_(6),with Cs_(2)AgBiBr_(6) possessing the highest thermodynamic stability.Therefore,the Bi-based perovskites are further studied to elucidate the effect of monovalent cation on their stability and electronics.Results show that the thermodynamic stability rises in the sequence of Cs_(2)NaBiBr_(6),Cs_(2)InBiBr_(6),Cs_(2)AgBiBr_(6) and Cs_(2)CuBiBr_(6).Notably,Cs_(2)CuBiBr_(6) exhibits a relatively narrow and appropriate band gap of 1.4634 eV,together with the highest absorption coefficient than other compounds,suggesting that Cs_(2)CuBiBr_(6) is a promising light absorbing material that can be further explored experimentally and be applied to optoelectronic devices.Our research offers theoretical backing for the potential optoelectronic application of cesium-based lead-free halide double perovskites in solar energy conversion.
基金Funded by the National Natural Science Foundation of China (No.61704113)the Shenzhen Science and Technology Program (No.GJHZ20210705141805015)the Scientific Research Project in School-level (SZIIT2019KJ026)。
文摘To reduce the coercive field of Na_(0.5)Bi_(0.5)TiO_(3),Ba TiO_(3)were added as dopant materials.Then the(1-x)Na_(0.5)Bi_(0.5)TiO_(3)-xBaTiO_(3)ceramic samples were produced in solid synthetic way.The optimum preparation condition and piezoelectric properties of the samples were investigated.The XRD results show that the fabric transites from rhombohedral to tetragonal gradually with the substitution of the Ba^(2+).The morphotropic phase boundaries(MPB)exists in the composition range of 0.06.
基金This work is funded by National Natural Science Foundation of China(Nos.61904023,11974063)Fundamental Research Funds for the Cen-tral Universities(2021CDJQY-022)Natural Science Foundation of Chongqing(No.cstc2019jcyj-bshX0078,cstc2020jcyj-jqX0028).
文摘Yellow light-emitting diodes(LEDs) as soft light have attracted abundant attention in lithography room, museum and art gallery. However, the development of efficient yellow LEDs lags behind green and blue LEDs, and the available perovskites yellow LEDs suffer from the instability. Herein, a pressure-assisted cooling method is proposed to grow lead-free CsCu2I3single crystals, which possess uniform surface morphology and enhanced photoluminescence quantum yield(PLQY) stability, with only 10% PLQY losses after being stored in air after 5000 h.Then, the single crystals used for yellow LEDs without encapsulation exhibit a decent Correlated Color Temperature(CCT) of 4290 K, a Commission Internationale de l’Eclairage(CIE) coordinate of(0.38, 0.41), and an excellent 570-h operating stability under heating temperature of 100°C. Finally, the yellow LEDs facilitate the application in wireless visible light communication(VLC), which show a-3 dB bandwidth of 21.5 MHz and a high achievable data rate of 219.2 Mbps by using orthogonal frequency division multiplexing(OFDM) modulation with adaptive bit loading. The present work not only promotes the development of lead-free single crystals, but also inspires the potential of CsCu2I3in the field of yellow illumination and wireless VLC.
文摘The tensile properties of Sn-9Zn-xAg-ySb;{(x, y) = (0.2, 0.6), (0.2, 0.8), (0.6, 0.2), (0.8, 0.2)} lead-free solders were investigated. All the test samples were annealed at 150°C for 1 hour. The tests are carried out at room temperature at the strain rate of 4.17 × 10<sup>-3</sup> s<sup>-1</sup>, 20.85 × 10<sup>-3</sup> s<sup>-1</sup>, and 208.5 × 10<sup>-3</sup> s<sup>-1</sup>. It is seen that the tensile strength increases and the ductility decrease with increasing the strain rate over the investigated range. From the strain rate change test results, the strain sensitivity values are found in the range of 0.0831 to 0.1455 due to the addition of different alloying elements.
文摘Soldering experiments with Sn-3.5Ag-0.5Cu lead-free solder on Au/Ni/Cu pad were carried out by means of diode-laser and IR reflow soldering methods respectively.The influence of different heating methods as well as output power of diode-laser on shear force of micro-joints was studied and the relationship between the shear force and microstructures of micro-joints was analyzed.The results indicate that the formation of intermetallic compound Ag3Sn is the key factor to affect the shear force and the fine eutectic network structures of micro-joints as well as the dispersion morphology of fine compound Ag3Sn,in which eutectic network band is responsible for the improvement of the shear force of micro-joints soldered with Sn-Ag-Cu lead-free solder.With the increases of output power of diode-laser,the shear force and the microstructures change obviously.The eutectic network structures of micro-joints soldered with diode-laser soldering method are more homogeneous and the grains of Ag3Sn compounds are finer in the range of near optimal output power than those soldered with IR reflow soldering method,so the shear force is also higher than that using IR reflow soldering method.When the output power value of diode-laser is about 41.0 W,the shear force exhibits the highest value that is 70% higher than that using IR reflow soldering method.
基金supported by the National Natural Science Foundation of China(No.50904035)
文摘This article explores tile effects of phosphorus addition on the wettability between Sn-9Zn solder alloy and Cu substrates, the oxidation behavior and the corrosion behavior of Sn-9Zn solder alloy. Spreading test was used to characterize the wettability of Sn-9Zn-xP solder alloys to Cu substrates. The oxidation and corrosion behaviors of Sn- 9Zn-xP solder alloys were determined by means of weight gaining, and secondary ion mass spectrometry was used to analyze the oxygen content. The role and mechanism of P in the solder alloys were also discussed. It is found that the addition of P can significantly improve the wettability of the solder alloys. Incorporating P into Sn-9Zn solder alloy obviously decreases the oxygen content and enhances the oxidation and corrosion resistance. Microstructure observations show that an appropriate amount of P can greatly refine coarse rod-like Zn-rich phases in Sn-gZn solder alloy.
基金supported by the National Natural Science Foundation of China(Grant nos.21773218,61974063)the Sichuan Province(Grant no.2018JY0206)the China Academy of Engineering Physics(Grant no.YZJJLX2018007)。
文摘Sensitive and reliable X-ray detectors are essential for medical radiography,industrial inspection and security screening.Lowering the radiation dose allows reduced health risks and increased frequency and fidelity of diagnostic technologies for earlier detection of disease and its recurrence.Three-dimensional(3 D)organic-inorganic hybrid lead halide perovskites are promising for direct X-ray detection-they show improved sensitivity compared to conventional X-ray detectors.However,their high and unstable dark current,caused by ion migration and high dark carrier concentration in the 3 D hybrid perovskites,limits their performance and long-term operation stability.Here we report ultrasensitive,stable X-ray detectors made using zero-dimensional(0 D)methylammonium bismuth iodide perovskite(MA3Bi2I9)single crystals.The 0 D crystal structure leads to a high activation energy(Ea)for ion migration(0.46 e V)and is also accompanied by a low dark carrier concentration(~10^6 cm^-3).The X-ray detectors exhibit sensitivity of 10,620μC Gy-1 air cm-2,a limit of detection(Lo D)of 0.62 nG yairs-1,and stable operation even under high applied biases;no deterioration in detection performance was observed following sensing of an integrated X-ray irradiation dose of^23,800 m Gyair,equivalent to>200,000 times the dose required for a single commercial X-ray chest radiograph.Regulating the ion migration channels and decreasing the dark carrier concentration in perovskites provide routes for stable and ultrasensitive X-ray detectors.
文摘Lead-free piezoelectric ceramics of (Bi1/2Na1/2)TiO3-BaTiO3(BNT-BT) were prepared by the conventional piezoelectric ceramic preparation technique (free air atmosphere sintering). The influence of BaTiO3 additive amount and La2O3 additive amount on the properties of BNT-BT lead-free piezoceramics were investigated. The results show that the dielectric constant(ε) and piezoelectric strain constant(d33) of materials start increasing and then decreasing while BaTiO3 additive amount increasing, the ε and d33 of materials have maximum value (ε=1650, d33=120 PC·N-1) while x(BaTiO3)=0.06 mol. The ε and d33 of materials start increasing and then decreasing while La2O3 additive amount increasing, the ε and d33 of materials have maximum value (ε=1684, d33=153 PC·N-1) while w(La2O3)=0.3%. The influence of La2O3 additive amount on the microstructure of BNT-BT piezoelectric ceramics was analysed by SEM(scanning electron microscope). The influence mechanism of La2O3 additive amount on the properties of BNT-BT piezoelectric ceramics was discussed. The BNT-BT ceramics with optimum comprehensive properties were obtained.
基金the National Natural Science Foundation of China(No.50401033)the Foundation for the Author of National Excellent Doctoral Dissertation of China(No.200335)+1 种基金the Natural Science Foundation of Tianjin City(No.033608811)Scientific Reseaxch Foundation for the Returned 0verseas Chinese Scholaxs,State Education Ministry,for grant and financial support.
文摘Sn-Ag alloy system has been regarded as one of the most promising lead-free solder to substitute conventional Sn- Pb eutectic solder. But the formation of bulk Ag3Sn intermetallic compounds (IMCs) during reflow and post heat treatment significantly influences the performance of the solder joints. With an effort to clarify its microstructural evolution as a function of slow cooling rates, the fraction of bulk IMCs within the slowly solidified Sn-4.0 wt pct Ag solder was investigated by standard metallographic and compared with that detected by thermal analysis. It was found that the bulk IMCs fraction determined by thermal analysis corresponds quite well with the microstructure observation results. In accordance with the conventional solidification theory, the lower the applied cooling rate, the fewer the amount of bulk Ag3Sn IMCs formed in Sn-4.0 wt pct Ag alloy. In addition, Vickers hardness measurement results indicated that the relative coarse eutectic Ag3Sn IMCs distributing in the lamellar eutectic structure favored the improvement of the mechanical performance.
文摘An orthogonal method was used to evaluate the effects of Ga, Al, Ag, and Ce multi-additions on the wetting characteristics of Sn-9Zn lead-free solders by wetting balance method. The results show that the optimal loading of Ga, Al, Ag, and Ce was 0.2 wt.%, 0.002 wt.%, 0.25 wt.%, and 0.15 wt.%, respectively. Intermetallic compounds (IMCs) formed at the interface between Sn-9Zn-0.2Ga-0.002Al-0.25Ag- 0.15Ce solder and Cu substrate were investigated by scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) analysis. The SEM images illustrate that the IMCs can be divided into two portions from the substrate side to the solder side: a planar CusZns layer and an additional continuous scallop-like AgZn3 layer. The EDS analysis also shows that Ga segregates in the solder abutting upon the interface. X-ray photoelectron spectroscopy (XPS) and Auger electron spectroscopy (AES) of the surface components of Sn-9Zn-0.2Ga-0.002Al- 0.25Ag-0.15Ce solder indicate that Al aggregates at the surface in the form of Al203 protective fdm, which prevents the further oxidation of the solder surface. On the other hand, Ce aggregates at the subsurface, which may reduce the surface tension of the solder and improve the wettability in consequence.
基金supported by the National Natural Science Foundation of China (59972020)
文摘Aim The piezoelectric properties and cytotoxicity of a porous lead-free piezoelectric ceramic for use as a direct bone substitute were investigated. Methodology Cold isostatic pressing (CIP) was applied to fabricate porous lithium sodium potassium niobate (Li0.06Na0.5K0.44) NbO3 specimens using a pore-forming method. The morphologies of the CIP-processed specimens were characterized and compared to those of specimens made by from conventional pressing procedures. The effects of the ceramic on the attachment and proliferation of osteoblasts isolated from the cranium of 1-day-old Sprague- Dawley rats were examined by a scanning electron microscopy (SEM) and metbylthiazol tetrazolium (MTT) assay. Results The results showed that CIP enhanced piezoelectricity and biological performance of the niobate specimen, and also promoted an extracellular matrix-like topography of it. In vitro studies showed that the CIP-enhanced material had positive effects on the attachment and proliferation of osteoblasts. Conclusion Niobate ceramic generated by CIP shows a promise for being a piezoelectric composite bone substitute.
基金Funded by the Scientific Research Fund of Sichuan Provincial Education Department(No.11ZB109)
文摘CuO-doped(Ag0.75Li0.1Na0.1K0.05)NbO3(ALNKN-xCuO, x = 0.2mol%) lead-free piezoelectric ceramics were prepared by the solid-state reaction method in air atmosphere. The effects of CuO addition on the phase structure, microstructure, and piezoelectric properties of the ceramics were investigated. The experimental results show that the ALNKN ceramics without doping CuO possess rhombohedral phase along with K2NbrO16- type phase and metallic silver phase. For all of the CuO-doped ALNKN ceramics, a pure perovskite structure with the orthorhombic phase was obtained by enclosing the samples in a corundum tube. A homogeneous microstructure with'the grain size of about 1 ~tm was formed for the ceramics with 0.5mo1% CuO. The grain size increases with increasing amount of CuO. The temperature dependence of dielectric properties indicates that the ferroelectric phase of the ALNKN-xCuO ceramics becomes less stable with the addition of CuO. The ceramics with x = lm01% exhibit relatively good electrical properties along with a high Curie temperature. These results will provide a helpful guidance to preparing other AN-based ceramics by solid-state reaction method in air atmosphere.
文摘Lead-free piezoelectric (K0.5sNa0.5)1-xLixNbO3 (x = 0at%-20at%) ceramics were synthesized by spark plasma sintering (SPS) at low temperature and the effects of LiNbO3 addition on its crystal structure and properties were also studied. When the Li content was less than 6at%, a single proveskite phase with the similar structure of (K0.5Na0.5)NbO3 was formed; and a secondary phase with K3Li2Nb5O15 structure was observed in the 6at% 〈 x 〈 20at% compositional range. Furthermore, LiNbO3 existed as the third phase when the Li content was higher than 8at%. The grain sizes increased from 200-500 nm to 5-8 μm when the K3Li2Nb5O15 and LiNbO3 like phases were formed. With increasing Li content, the relative density of the ceramics first decreased from 97% to 93% and then kept constant. The piezoelectric coefficient d33, dielectric constant, and planner electromechanical coupling factor exhibited a decreasing tendency with increasing Li content because of the decrease in density and the formation of the secondary phase such as K3Li2Nb5O15 and LiNbO3. The formation of dense microstructure with a single phase is necessary in improving the properties of the (K0.5Na0.5)1-xLixNbO3 ceramics.
基金financially supported by the Specialized Research Fund for the Doctoral Program of Higher Education of China(No.20090006110010)Beijing Natural Science Foundation(No.2112028)
基金the National Natural Science Foundation of China (No. 50842028)the National High-Tech Research and Development Program of China (No. 2006AA03Z436).
文摘Ti-Modified (Na0.5K0.5)(TixNb1-x)O3 (NKNT) piezoelectric ceramics were fabricated by double-layer buried powder process at 1020°C for 2 h. The microstructures,and piezoelectric and dielectric properties of the lead-free NKNT ceramics were investigated. X-ray diffraction re-sults indicated that Ti4+ had diffused into the (Na0.5K0.5)NbO3 lattices to form a solid solution with a perovskite structure. The introducing of Ti into the (Na0.5K0.5)NbO3 solid solution effectively reduced the sintering temperature and densified the microstructure with a decreased grain size. The highest relative density reached more than 90%. The highest piezoelectric dielectric coefficient d33 and planar mode electro-mechanical coupling coefficient kp were 110 pC/N and 19.5%,which were obtained in the NKNT ceramic with 1 mol% Ti. The piezoelectric properties of the NKNT ceramics were enhanced by aging in air for a period of time owing to the compensation of oxygen vacancies.
基金This work was financially supported by the National Natural Science Foundation of China (No. 50401003), the Natural Science Foundation of Tianjin City (No. 033608811) and Fok Ying Tong Education Foundation (No. 104015).
文摘A lead-free Sn-3.5Ag solder was prepared by rapid solidification technology. The high solidification rate, obtained by rapid cooling, promotes nucleation, and suppresses the growth of Ag3Sn intermetallic compounds (IMCs) in Ag-rich zone, yielding fine Ag3Sn nanoparticulates with spherical morphology in the matrix of the solder. The large amount of tough homogeneously-dispersed IMCs helps to improve the surface area per unit volume and obstructs the dislocation lines passing through the solder, which fits with the dispersion-strengthening theory. Hence, the rapidly-solidified Sn-3.5Ag solder exhibits a higher rnicrohardness when compared with a slowly-solidified Sn-3.5Ag solder.
基金This work contributes to Group Project No. 4, within the frame of European Project COST "Action 531: Lead-free sol-ders". Financial support from Polish State Committee for Scientific Research under grant No. 62/E - 88/SPB/COST/ T08//DZ 459/2003-2006 is gratefully acknowledged.
文摘Emf technique was employed to determine indium activities in the liquid Ag-In-Pd alloys using galvanic cells with yttria-stabilised-zirconia as solid electrolyte according to the scheme: kanthal/rhenium, Ag-In-Pd, In2O3 | YSZ | Ni, NiO, Pt. Composition and temperature measurement ranges were limited, because of very steep liquidus surface; 35 compositions for Xpd up to 0.3 were investigated and at temperatures from near-liquidus up to 1700 K. High temperature experiments required special moly furnace to be constructed with unique automatic gas supply system for fumace winding protective atmosphere. Emf readings were taken and recorded by automatic data acquisition system. Linear dependence of emf on temperature was observed for all compositions investigated, and results were approximated by straight line equa- tions. Then In activities were calculated using well-known relations and taking into account correction for thermoelectric power between kanthal and platinum. Results are to be used along with other existing data to perform assessment of the ternary system under accord.
文摘A new group of lead-free piezoelectric ceramics,(Bi0.5 Na0.5)1-x(BaaSrb)xTiO3(abbreviated as BNBST[100x-100a/100b],0〈x〈1,a+b=1),was synthesized.The ceramics were prepared by conventional ceramic sintering technique,and the ceramics with density of 95% of the theoretical one can be sintered without the atmosphere control during the sintering process.The results of the X-ray diffraction(XRD) data show that the ceramics possess a single perovskite phase.The measurements of dielectric and piezoelectric properties reveal that the ceramics provide relatively high piezoelectric charge constant d33 and high planar electromechanical coupling factor kp.For the BNBST6-95/5 ceramics,d33 is equal to 170pC/N,and kp is equal to 32.0%.The fabrication technique for these ceramics is conventional and stable.
基金by the National Natural Science Foundation of China(No.51402097)the College Students Innovation and Entrepreneurship Training Program of Hubei University of Technology(No.202010500045)。
文摘A lead-free base glaze suitable for pearlescent pigments was prepared by a low-temperature solid-phase reaction with alkali waste.Tests were performed to evaluate the effects of the sintering conditions and alkali waste composition on the prepared base glaze and pearlescent glaze.The experimental results show that partially replacing SiO_(2) with B_(2)O_(3) effectively reduced the sintering temperature and time to form a glass network,but the network structure becomes disconnected as the B_(2)O_(3) content increases.An amorphous base glaze was obtained when soda ash was replaced with a small amount of alkali waste,but increasing the addition of NaCl further was adverse to base glaze formation by resulting in crystallization of the base glaze and a decrease in the bridging oxygen content.The pearlescent pigment was thermally stable in the glaze at 750℃,while higher temperatures caused the crystalline phase of NaAlSiO_(4) to appear and adhere to the surface of pigment granules,which degraded the pearlescent effect of the glaze.