Ultrasound-assisted pretreatment under mild operating conditions has been investigated for intensification of delignification to facilitate the obtaining of ethyl levulinate from biomass. The effect of pH (2 - 12), te...Ultrasound-assisted pretreatment under mild operating conditions has been investigated for intensification of delignification to facilitate the obtaining of ethyl levulinate from biomass. The effect of pH (2 - 12), temperature (30°C - 70°C) and pretreatment time (0 - 120 minutes) has been studied for different biomass samples. The most favorable conditions were basic pH, temperature of 70°C and pretreatment time of 2 h, obtaining values of delignification near 80 percent. The ethyl levulinate is obtained in microwave directly via from samples before and after delignification and analyzed for GC-MS. The results evidenced better yields for the delignified samples.展开更多
The chemical composition of n-hexane extractives from lignocellulose residual contained in different agroindustrial wastes was studied. The n-hexane extract, which accounted for 1.6% of total lignocellulose residual w...The chemical composition of n-hexane extractives from lignocellulose residual contained in different agroindustrial wastes was studied. The n-hexane extract, which accounted for 1.6% of total lignocellulose residual weight, was analysed by 1H-NMR and gas chromatography/mass spectrometry. The most predominant compounds identified were aliphatic hydrocarbons (lineal alkanes, branched alkanes, alkenes). Additionally, terpenes, ketones, fatty alcohols, fatty acids and steroids were also found together in minor amounts. The lipophilic compounds in n-hexane extracts in three lignocellulosic wastes, which is highly valuable information for a more complete industrial utilization of these lignocellulosic materials.展开更多
文摘Ultrasound-assisted pretreatment under mild operating conditions has been investigated for intensification of delignification to facilitate the obtaining of ethyl levulinate from biomass. The effect of pH (2 - 12), temperature (30°C - 70°C) and pretreatment time (0 - 120 minutes) has been studied for different biomass samples. The most favorable conditions were basic pH, temperature of 70°C and pretreatment time of 2 h, obtaining values of delignification near 80 percent. The ethyl levulinate is obtained in microwave directly via from samples before and after delignification and analyzed for GC-MS. The results evidenced better yields for the delignified samples.
基金To the National Council of Science and Technology(Conacyt)for the financing of the project.
文摘The chemical composition of n-hexane extractives from lignocellulose residual contained in different agroindustrial wastes was studied. The n-hexane extract, which accounted for 1.6% of total lignocellulose residual weight, was analysed by 1H-NMR and gas chromatography/mass spectrometry. The most predominant compounds identified were aliphatic hydrocarbons (lineal alkanes, branched alkanes, alkenes). Additionally, terpenes, ketones, fatty alcohols, fatty acids and steroids were also found together in minor amounts. The lipophilic compounds in n-hexane extracts in three lignocellulosic wastes, which is highly valuable information for a more complete industrial utilization of these lignocellulosic materials.