蒸发干燥法制备LiNi_(0.5)Mn_(1.5)O_(4)正极材料
1
作者 董怡辰 王振波 《蓄电池》 CAS 2024年第4期151-155,共5页
以LiNO_(3)、Ni(NO_(3))_(2)·6H_(2)O和Mn(CH_(3)COO)_(2)·4H_(2)O为原料,采用蒸发干燥法制备锂电池用LiNi_(0.5)Mn_(1.5)O_(4)正极材料。将原料在玛瑙研钵中研磨后置于100℃水浴盆中。待固体物料溶解后,在混合物中加入的无... 以LiNO_(3)、Ni(NO_(3))_(2)·6H_(2)O和Mn(CH_(3)COO)_(2)·4H_(2)O为原料,采用蒸发干燥法制备锂电池用LiNi_(0.5)Mn_(1.5)O_(4)正极材料。将原料在玛瑙研钵中研磨后置于100℃水浴盆中。待固体物料溶解后,在混合物中加入的无水乙醇和浓度为15.0 mol·L^(-1)的氨水,伴随机械搅拌。将混合物置于120℃的真空干燥室中,干燥2 h(始终在真空氛围中)以获得前驱体。把前驱体放在400℃空气中煅烧4 h,分解硝酸盐和醋酸盐,接着在不同温度的氧气中煅烧6 h,合成LiNi_(0.5)Mn_(1.5)O_(4)材料。将合成的LiNi_(0.5)Mn_(1.5)O_(4)材料放在600℃氧气氛围中退火氧化2 h,再冷却至室温。通过电化学测试得到,在烧结温度800℃,烧结时间6 h的条件下合成的LiNi_(0.5)Mn_(1.5)O_(4)正极材料具有较高的锂插层容量和良好的循环稳定性。 展开更多
关键词 LiNO_(3) Ni(NO_(3))_(2)·6H_(2)O Mn(CH_(3)COO)_(2)·4H_(2)O LiNi_(0.5)Mn_(1.5)O_(4) 锂电池 正极材料 插层容量 蒸发干燥法
下载PDF
锰氧化膜包覆沸石的制备及其处理含锰水特性研究
2
作者 金星 傅金祥 +1 位作者 张黎 何祥 《硅酸盐通报》 CAS 北大核心 2023年第9期3295-3305,共11页
净水厂广泛采用石英砂或锰砂滤池,但在接触氧化法除锰过程中存在滤料吸附性能差、“锰质活性滤膜”成熟期长等问题。针对这一现象,以沸石为基质材料,高锰酸钾和硫酸锰生成锰氧化物沉积在沸石表面,制备锰氧化膜包覆沸石(MOMCZ),MOMCZ结... 净水厂广泛采用石英砂或锰砂滤池,但在接触氧化法除锰过程中存在滤料吸附性能差、“锰质活性滤膜”成熟期长等问题。针对这一现象,以沸石为基质材料,高锰酸钾和硫酸锰生成锰氧化物沉积在沸石表面,制备锰氧化膜包覆沸石(MOMCZ),MOMCZ结合了沸石的吸附性能和锰氧化物的催化氧化特性。采用SEM、EDS、XPS、XRD、BET、Zeta电位等分析表征方法研究MOMCZ的表面形态、化学组成等特性,通过响应曲面模型分析MOMCZ对锰离子的吸附性能。结果表明:MOMCZ表面的锰氧化膜呈现立体复杂的网状结构,Mn元素存在形式及摩尔分数分别为Mn(Ⅲ)51.28%,Mn(Ⅳ)48.72%,锰氧化膜主要成分为Na0.55Mn_(2)O_(4)(H_(2)O)1.5;MOMCZ比表面积为38.76 m^(2)/g,孔径分布集中在3~40 nm,等电点pH=2.36;MOMCZ吸附锰离子的四项影响因素关系顺序为:pH值>负荷>吸附时间>吸附温度;通过模型优化发现当负荷为0.8 mg/g、pH=8.5、吸附温度为23.40℃、吸附时间为6.58 min时,锰离子去除率达到最大值70.82%;试验模型预测值和实际数据值相对误差均小于2.5%。MOMCZ吸附锰离子响应曲面模型拟合程度高、预测准确,具有较高的可行性和参考价值。 展开更多
关键词 沸石 锰氧化膜 Na_(0.55)Mn_(2)O_(4)(H_(2)O)_(1.5) 吸附 响应曲面
下载PDF
固体氧化物燃料电池Ce_(0.8)Sm_(0.2)O_2电解质与Mn_(1.5)Co_(1.5)O_4的稳定性 被引量:2
3
作者 王军 李成新 刘晶歌 《材料科学与工程学报》 CAS CSCD 北大核心 2017年第2期269-273,共5页
本文面向管状固体氧化物燃料单电池串联中连接极与电解质界面稳定性展开研究,以氧化钐掺杂氧化铈(Ce_(0.8)Sm_(0.2)O_2,SDC)和Mn_(1.5)Co_(1.5)O_4(MCO)为原料,采用XRD、SEM和EDS来表征、探讨了SDC和MCO两种材料在不同运行和制备温度下... 本文面向管状固体氧化物燃料单电池串联中连接极与电解质界面稳定性展开研究,以氧化钐掺杂氧化铈(Ce_(0.8)Sm_(0.2)O_2,SDC)和Mn_(1.5)Co_(1.5)O_4(MCO)为原料,采用XRD、SEM和EDS来表征、探讨了SDC和MCO两种材料在不同运行和制备温度下的化学稳定性和结构稳定性。研究结果表明,SDC和MCO两种材料具有良好的化学相容性。当烧结温度低于1000℃时,难以获得致密的复合材料,而当处理温度为1400℃时,由于热力学温度过高,将导致颗粒迅速长大。 展开更多
关键词 固体氧化物燃料电池 SDC mn1.5co1.5o4 稳定性
下载PDF
5V锂离子电池尖晶石正极材料LiM_(0.5)Mn_(1.5)O_4的研究评述 被引量:26
4
作者 伊廷锋 胡信国 +1 位作者 霍慧彬 高昆 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2006年第9期1350-1353,共4页
评述了锂离子电池锰酸锂正极材料的重要性,介绍了3d-过渡金属离子(Cr3+,Ni2+,Cu2+,Fe3+)掺杂在锰酸锂正极材料中的应用。研究了3d-过渡金属离子掺杂对锰酸锂正极材料结构和电化学性能的影响,并提出了其影响锂离子电池充放电和循环性能... 评述了锂离子电池锰酸锂正极材料的重要性,介绍了3d-过渡金属离子(Cr3+,Ni2+,Cu2+,Fe3+)掺杂在锰酸锂正极材料中的应用。研究了3d-过渡金属离子掺杂对锰酸锂正极材料结构和电化学性能的影响,并提出了其影响锂离子电池充放电和循环性能的机制。展望了3d-过渡金属离子掺杂在锂离子电池锰酸锂正极材料中的发展前景,并指出LiNi0.5Mn1.5O4是非常有应用前景的5V锂离子电池正极材料。 展开更多
关键词 锂离子电池 尖晶石 正极材料 LiM0.5Mn1.5O4
下载PDF
正极材料LiNi_(0.5)Mn_(1.5)O_4的合成及性能 被引量:13
5
作者 季勇 王志兴 +3 位作者 尹周澜 郭华军 彭文杰 李新海 《无机化学学报》 SCIE CAS CSCD 北大核心 2007年第4期597-601,共5页
采用低温固相法制备镍锰复合草酸盐,煅烧后生成的镍锰复合氧化物与Li2CO3混合,在空气中于700℃反应12h,得到LiNi0.5Mn1.5O4。通过XRD,SEM和恒电流充放电测试对样品进行了表征。XRD结果表明:复合草酸盐经390℃煅烧3h,生成了多相氧化物;... 采用低温固相法制备镍锰复合草酸盐,煅烧后生成的镍锰复合氧化物与Li2CO3混合,在空气中于700℃反应12h,得到LiNi0.5Mn1.5O4。通过XRD,SEM和恒电流充放电测试对样品进行了表征。XRD结果表明:复合草酸盐经390℃煅烧3h,生成了多相氧化物;合成的LiNi0.5Mn1.5O4为纯相,具有立方尖晶石结构。电化学测试结果表明,合成的样品在室温和高温(55℃)下,具有较好的电化学性能;大电流充放电时,具有良好的循环性能。 展开更多
关键词 锂离子电池 正极材料 LINI0.5MN1.5O4 倍率性能
下载PDF
5V正极材料LiNi0.5Mn1.5O4的自蔓延燃烧合成及性能 被引量:14
6
作者 范未峰 瞿美臻 +1 位作者 彭工厂 于作龙 《无机化学学报》 SCIE CAS CSCD 北大核心 2009年第1期124-128,共5页
通过自蔓延燃烧方法合成了性能优良的高电位5V锂离子电池正极材料LiNi0.5Mn1.5O4,利用傅立叶红外光谱(FTIR)、热分析(DSC/TG)、X射线衍射(XRD)、透射电镜(TEM)等方法对前驱物及样品的结构和物化性质等进行了分析和表征,考察了材料的电... 通过自蔓延燃烧方法合成了性能优良的高电位5V锂离子电池正极材料LiNi0.5Mn1.5O4,利用傅立叶红外光谱(FTIR)、热分析(DSC/TG)、X射线衍射(XRD)、透射电镜(TEM)等方法对前驱物及样品的结构和物化性质等进行了分析和表征,考察了材料的电化学性能。结果表明,所制备样品具有单一的尖晶石相结构,具有4.7V充放电平台;在3.5V到5.2V之间进行充放电性能测试具有131mAh·g-1以上的可逆容量;在2C倍率下循环100次后的容量保持率为96%以上。 展开更多
关键词 锂离子电池 5V正极材料 LINI0.5MN1.5O4 溶胶-凝胶法 自蔓延燃烧法
下载PDF
凝胶燃烧法合成5V级正极材料LiNi_(0.5)Mn_(1.5)O_4及其高倍率放电性能 被引量:15
7
作者 代克化 毛景 翟玉春 《物理化学学报》 SCIE CAS CSCD 北大核心 2010年第8期2130-2134,共5页
采用聚乙烯吡咯烷酮(PVP)作为络合剂和燃料以凝胶燃烧法制备了具有优异高倍率放电性能的亚微米LiNi0.5Mn1.5O4材料.用热重/差热分析(TG/DTA)研究了凝胶的燃烧过程,用X射线衍射(XRD)、扫描电镜(SEM)和循环伏安(CV)研究了LiNi0.5Mn1.5O4... 采用聚乙烯吡咯烷酮(PVP)作为络合剂和燃料以凝胶燃烧法制备了具有优异高倍率放电性能的亚微米LiNi0.5Mn1.5O4材料.用热重/差热分析(TG/DTA)研究了凝胶的燃烧过程,用X射线衍射(XRD)、扫描电镜(SEM)和循环伏安(CV)研究了LiNi0.5Mn1.5O4材料的结构和形貌.结果表明材料为结晶良好的纯尖晶石相结构,由5μm左右的二次颗粒组成,颗粒大小分布均匀,一次晶粒发育良好,粒径在500nm左右.充放电测试表明材料的倍率性能和循环性能十分优异.在3.5至4.9V进行充放电测试,0.5C、1C、4C、8C和10C倍率下放电容量分别为131.9、127.6、123.4、118.4和113.7mAh·g-1.在10C大倍率放电条件下循环100、500和1000次的容量保持率分别为91.4%、80.9%和73.5%. 展开更多
关键词 锂离子电池 正极材料 LINI0.5MN1.5O4 凝胶燃烧法 聚乙烯吡咯烷酮
下载PDF
5V锂离子电池正极材料LiNi0.5Mn1.5O4的合成与Li^+在材料中的扩散性能 被引量:6
8
作者 卢华权 吴锋 +3 位作者 苏岳锋 李宁 陈实 包丽颖 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2011年第4期946-951,共6页
采用草酸盐共沉淀法合成了5 V正极材料LiNi0.5Mn1.5O4,研究了不同温度下合成材料的结构形貌与电化学性能之间的关系.结果表明,在900℃下合成样品的电化学性能最好,首次放电容量达到133.0mA.h/g,经30周循环后,容量仍然保持在132.2 mA.h/g... 采用草酸盐共沉淀法合成了5 V正极材料LiNi0.5Mn1.5O4,研究了不同温度下合成材料的结构形貌与电化学性能之间的关系.结果表明,在900℃下合成样品的电化学性能最好,首次放电容量达到133.0mA.h/g,经30周循环后,容量仍然保持在132.2 mA.h/g,容量保持率高达99.4%.采用恒电位间歇滴定法(PITT)和电化学阻抗谱法(EIS)测定了锂离子在LiNi0.5 Mn1.5 O4材料中的扩散系数.结果表明,在LiNi0.5Mn1.5O4材料放电过程中,在不同的电位下,锂离子扩散系数在10-10~10-11 cm2/s范围内变化. 展开更多
关键词 锂离子电池 正极材料 草酸盐共沉淀 LINI0.5MN1.5O4 扩散系数
下载PDF
LiNi_(0.5)Mn_(1.5)O_4/Ag复合材料的制备及其电化学性能 被引量:6
9
作者 何则强 熊利芝 +1 位作者 梁凯 卢彪 《中国有色金属学报》 EI CAS CSCD 北大核心 2010年第4期801-806,共6页
采用流变相法合成LiNi0.5Mn1.5O4粉末。以甲醛为还原剂,采用化学镀法制备LiNi0.5Mn1.5O4/Ag复合材料。通过X射线衍射分析、扫描电镜分析以及电化学测试等手段对LiNi0.5Mn1.5O4/Ag的微观结构、表面形貌和电化学性能进行研究。结果表明:在... 采用流变相法合成LiNi0.5Mn1.5O4粉末。以甲醛为还原剂,采用化学镀法制备LiNi0.5Mn1.5O4/Ag复合材料。通过X射线衍射分析、扫描电镜分析以及电化学测试等手段对LiNi0.5Mn1.5O4/Ag的微观结构、表面形貌和电化学性能进行研究。结果表明:在LiNi0.5Mn1.5O4/Ag中,LiNi0.5Mn1.5O4表面被包覆一层分散均匀且颗粒大小均匀的Ag,Ag颗粒的大小为200~300nm。Ag颗粒的存在增加LiNi0.5Mn1.5O4颗粒之间的电子导电性,降低电池的极化作用,减少锰的溶解,使得LiNi0.5Mn1.5O4/Ag具有比LiNi0.5Mn1.5O4更高的可逆容量、更稳定的循环性能和更好的倍率性能。以0.2C放电时,LiNi0.5Mn1.5O4/Ag的首次放电容量达到143.8mA·h/g;而经100次循环后,以0.2C和2.0C放电时,LiNi0.5Mn1.5O4/Ag的容量保持率分别达到99.2%和86.8%。 展开更多
关键词 锂离子电池 LINI0.5MN1.5O4 包覆 化学镀
下载PDF
LiNi_(0.5)Mn_(1.5)O_4高电压正极材料的制备及性能研究 被引量:6
10
作者 颜群轩 王志兴 +2 位作者 吴晶 李新海 谭群英 《功能材料》 EI CAS CSCD 北大核心 2009年第6期933-935,939,共4页
采用液相共沉淀法制备镍锰复合碳酸盐前驱体,650℃煅烧后生成的镍锰复合氧化物与Li2CO3混合,在空气中于750~900℃下煅烧10h,600℃退火10h得到LiNi0.5Mn1.5O4。采用XRD、SEM和恒电流充放电测试等对样品进行了表征。SEM结果表明,合成温度... 采用液相共沉淀法制备镍锰复合碳酸盐前驱体,650℃煅烧后生成的镍锰复合氧化物与Li2CO3混合,在空气中于750~900℃下煅烧10h,600℃退火10h得到LiNi0.5Mn1.5O4。采用XRD、SEM和恒电流充放电测试等对样品进行了表征。SEM结果表明,合成温度对LiNi0.5Mn1.5O4的表面形貌及粒径有较大影响;XRD结果表明,合成的样品均为纯的立方尖晶石结构。电化学测试结果表明,800℃合成的样品在室温下具有较好的电化学性能:0.1、1、2、4C首次放电容量分别130.24、129.47、115.5、108.05mAh/g,且大倍率下具有较好的循环性能。 展开更多
关键词 LINI0.5MN1.5O4 高电压 正极材料
下载PDF
Li_2CO_3、NiO和电解MnO_2合成高容量LiNi_(0.5)Mn_(1.5)O_4及其表征(英文) 被引量:6
11
作者 方海升 王志兴 +3 位作者 李新海 尹周澜 郭华军 彭文杰 《无机化学学报》 SCIE CAS CSCD 北大核心 2006年第2期311-315,共5页
Well-developed crystalline LiNi0.5Mn1.5O4 was prepared by solid-state reaction using Li2CO3, NiO and electrolytic MnO2 at high heating and cooling rate. X-ray diffraction (XRD) patterns and scanning electron microscop... Well-developed crystalline LiNi0.5Mn1.5O4 was prepared by solid-state reaction using Li2CO3, NiO and electrolytic MnO2 at high heating and cooling rate. X-ray diffraction (XRD) patterns and scanning electron microscopic (SEM) images showed that LiNi0.5Mn1.5O4 synthesized at 900 ℃ and 950 ℃ had cubic spinel structure with clearly defined shape. LiNi0.5Mn1.5O4 spinel phase decomposed at 1 000 ℃ accompanying with structural and morphological degradation. TG measurement revealed that the weight loss during heating process could be mostly gained in cooling process, and the upward tendency of weight loss during heating process decreased, while that of irreversible weight loss rapidly increased with the increase of temperature. LiNi0.5Mn1.5O4 powders prepared at 900 ℃ for 12 h delivered the maximum discharge capacity of 134 mAh·g-1 with good cyclic performance at 2/7 C. In addition, by adjusting the calcination time at 900 ℃, the capacity and cycling performance of LiNi0.5Mn1.5O4 were further enhanced. 展开更多
关键词 锂离子电池 LiNin5Mn1.5O4 固相法
下载PDF
Li-Ni-Mn-O锂离子电池正极材料研究进展 被引量:6
12
作者 卢华权 李宁 +4 位作者 吴锋 苏岳锋 陈实 包丽颖 汪鑫 《有色金属(冶炼部分)》 CAS 北大核心 2011年第7期48-55,共8页
Li-Ni-Mn-O正极材料由于具有比容量高、资源丰富、价格便宜、污染少等优点,而被视为最具发展潜力的锂离子电池的正极材料之一,近年来受到广泛关注。综述锂离子电池正极材料Li-Ni-Mn-O的研究进展,阐述其结构特征、制备方法及电化学性能... Li-Ni-Mn-O正极材料由于具有比容量高、资源丰富、价格便宜、污染少等优点,而被视为最具发展潜力的锂离子电池的正极材料之一,近年来受到广泛关注。综述锂离子电池正极材料Li-Ni-Mn-O的研究进展,阐述其结构特征、制备方法及电化学性能。指出这些材料目前存在的主要问题并介绍解决方法,最后指出Li-Ni-Mn-O正极材料的发展前景和今后的研究方向。 展开更多
关键词 无机非金属材料 Li-Ni-Mn-O 综述 锂离子电池 正极材料 LINI0.5MN0.5O2 LINI0.5MN1.5O4 固溶体
下载PDF
锂离子电池镍掺杂尖晶石LiMn2O4正极材料的电子结构 被引量:4
13
作者 伊廷锋 朱彦荣 +1 位作者 诸荣孙 胡信国 《无机化学学报》 SCIE CAS CSCD 北大核心 2008年第10期1576-1581,共6页
采用密度泛函平面波赝势方法对LiMn2O4和LiNi0.5Mn1.5O4的几何结构进行了优化,并计算了相应的电子结构。计算的结果表明:在Li+脱嵌前后,LiMn2O4和LiNi0.5Mn1.5O4均为导体,且锂元素主要以离子形式存在于两种材料中,O2p轨道与Mn(Ni)的3d... 采用密度泛函平面波赝势方法对LiMn2O4和LiNi0.5Mn1.5O4的几何结构进行了优化,并计算了相应的电子结构。计算的结果表明:在Li+脱嵌前后,LiMn2O4和LiNi0.5Mn1.5O4均为导体,且锂元素主要以离子形式存在于两种材料中,O2p轨道与Mn(Ni)的3d轨道形成了较强的共价键。Li+嵌入导致Mn(Ni)3d轨道的态密度峰发生移动。Ni的掺杂导致Mn(Ni)和O2p轨道的成键作用得以加强,电子在Mn(Ni)3d轨道的填充发生变化,从而提高了电池的充放电电压。 展开更多
关键词 正极材料 尖晶石 LIMN2O4 LINI0.5MN1.5O4 电子结构 密度泛函理论
下载PDF
碳包覆对LiNi_(0.5)Mn_(1.5)O_4电化学性能的影响 被引量:4
14
作者 何则强 熊利芝 +1 位作者 梁凯 李菊香 《精细化工》 EI CAS CSCD 北大核心 2009年第12期1145-1148,1214,共5页
以蔗糖为碳源,采用溶液沉积-真空热解法制备了LiNi_(0.5)Mn_(1.5)O_4/C复合材料。用热重与差热分析、X射线衍射分析、扫描电镜分析及电化学测试等手段对LiNi_(0.5)Mn_(1.5)O_4/C的微观结构、表面形貌和电化学性能进行了研究。结果表明,... 以蔗糖为碳源,采用溶液沉积-真空热解法制备了LiNi_(0.5)Mn_(1.5)O_4/C复合材料。用热重与差热分析、X射线衍射分析、扫描电镜分析及电化学测试等手段对LiNi_(0.5)Mn_(1.5)O_4/C的微观结构、表面形貌和电化学性能进行了研究。结果表明,蔗糖热分解后在LiNi_(0.5)Mn_(1.5)O_4颗粒的表面包覆形成了一层无定形碳。无定形碳可以有效阻止LiNi_(0.5)Mn_(1.5)O_4颗粒的聚集,增加电极的导电面积,降低电池极化,从而改善LiNi_(0.5)Mn_(1.5)O_4的电化学性能。与未包覆的LiNi_(0.5)Mn_(1.5)O_4粉末相比,LiNi_(0.5)Mn_(1.5)O_4/C复合材料具有更高的可逆容量、更稳定的循环性能和更好的倍率性能。0.2C放电时,LiNi_(0.5)Mn_(1.5)O_4/C复合材料的首次放电容量达到144.8mA.h.g-1,经60次循环后平均每次循环的容量损失仅为0.0081%。而1.0C和2.0C放电时,LiNi_(0.5)Mn_(1.5)O_4/C复合材料的首次放电容量分别保持在131.9mA.h.g-1和122.4mA.h.g-1。 展开更多
关键词 LINI0.5MN1.5O4 蔗糖 包覆 溶液沉积 真空热解 功能材料
下载PDF
锂离子导体包覆镍锰酸锂正极材料的制备及其电化学性能 被引量:6
15
作者 熊利芝 刘文萍 +1 位作者 吴玉先 何则强 《中国有色金属学报》 EI CAS CSCD 北大核心 2015年第7期1911-1919,共9页
采用原位包覆法制备表面包覆Li1.3Al0.3Ti1.7(PO4)3(LATP)的Li Ni0.5Mn1.5O4(LNMO),即LNMO@LATP正极材料。采用X-射线衍射(XRD)、扫描电镜(SEM)、透射电镜(TEM)及电化学测试等手段对其物相结构、表面形貌及电化学性能进行研究。结果表明... 采用原位包覆法制备表面包覆Li1.3Al0.3Ti1.7(PO4)3(LATP)的Li Ni0.5Mn1.5O4(LNMO),即LNMO@LATP正极材料。采用X-射线衍射(XRD)、扫描电镜(SEM)、透射电镜(TEM)及电化学测试等手段对其物相结构、表面形貌及电化学性能进行研究。结果表明:LATP以无定型态紧密包覆于Li Ni0.5Mn1.5O4的表面,包覆层厚度约为5 nm。由于LATP包覆层具有保护电极材料表面和提高锂离子导电的双重作用,减少了电极过程的副反应,降低了电化学极化,提供了更多的锂离子扩散通道,导致LNMO@LATP具有比LNMO更稳定的循环性能和更好的倍率性能,特别是在高温的情况下。室温下在0.2C放电时,LNMO@LATP和LNMO的首次放电容量分别为141.5和142.6m A·h/g,经80次循环后,二者放电容量保持率分别达到99.2%和98.0%;而在10.0C放电时,LNMO@LATP和LNMO的首次放电容量分别为93.5和70.6 m A·h/g,经80次循环后,二者放电容量保持率分别达到66.1%和49.5%。当循环温度提高到55℃时,LNMO@LATP和LNMO在0.2C循环80次后的放电容量保持率分别为95.5%和79.2%;而在10.0C放电循环80次后,放电容量保持率分别为88.0%和51.0%。 展开更多
关键词 Li Ni0.5Mn1.5O4 Li1.3Al0.3Ti1.7(PO4)3 高电压正极 表面包覆 电化学性能
下载PDF
锂离子电池正极材料LiNi_(0.5)Mn_(1.5)O_4的研究现状 被引量:5
16
作者 杨杰 杨建文 +2 位作者 石阳 李丹 李蕾 《化工新型材料》 CAS CSCD 北大核心 2012年第3期9-11,37,共4页
锂离子二次电池的研究不断深入,高电位正极材料的研究正日益受到重视。新型锂离子电池正极材料LiNi0.5Mn1.5O4嵌锂电位高达4.7V,能量效率高,循环性能好,在电动汽车、航空航天等领域具有良好的发展前景。综述了LiNi0.5Mn1.5O4的制备方法... 锂离子二次电池的研究不断深入,高电位正极材料的研究正日益受到重视。新型锂离子电池正极材料LiNi0.5Mn1.5O4嵌锂电位高达4.7V,能量效率高,循环性能好,在电动汽车、航空航天等领域具有良好的发展前景。综述了LiNi0.5Mn1.5O4的制备方法及近年来在提高其电化学性能方面的研究进展。 展开更多
关键词 锂离子电池 正极材料 LINI0.5MN1.5O4 高电压
下载PDF
高电压镍锰酸锂动力电池正极材料研究进展 被引量:11
17
作者 宋植彦 谢凯 郑春满 《电源技术》 CAS CSCD 北大核心 2012年第9期1405-1409,共5页
新能源电动汽车的发展使动力锂离子电池的研究受到广泛关注,不断改善和提高现有正极材料的功率性能,开发新型正极材料已成为动力电池研究的热点。首先简述了锰酸锂作为动力电池材料存在的主要问题及改性产物镍锰酸锂的研究、镍锰酸锂正... 新能源电动汽车的发展使动力锂离子电池的研究受到广泛关注,不断改善和提高现有正极材料的功率性能,开发新型正极材料已成为动力电池研究的热点。首先简述了锰酸锂作为动力电池材料存在的主要问题及改性产物镍锰酸锂的研究、镍锰酸锂正极材料的结构与嵌脱锂机理,然后从研究的角度详细综述了镍锰酸锂的合成方法和针对材料循环性能的问题进行的离子掺杂和表面包覆,分析了镍锰酸锂正极材料研究中存在的问题,展望了镍锰酸锂动力电池用于高功率型正极材料的发展趋势和应用前景。 展开更多
关键词 动力电池 正极材料 高功率 LINI0.5MN1.5O4
下载PDF
5V锂离子电池正极材料LiNi_(0.5)Mn_(1.5)O_4的研究进展 被引量:8
18
作者 唐致远 胡冉 王雷 《化工进展》 EI CAS CSCD 北大核心 2006年第1期31-34,共4页
用3d过渡金属元素部分取代锂离子正极材料的尖晶石型锂锰氧化物中的Mn,可使电极获得接近5V的电压平台,5V电池的好处是可以获得高的功率密度。本文综述了近年来制备5V正极材料LiNi0.5Mn1.5O4的方法以及通过这些方法制备出的材料的电化学... 用3d过渡金属元素部分取代锂离子正极材料的尖晶石型锂锰氧化物中的Mn,可使电极获得接近5V的电压平台,5V电池的好处是可以获得高的功率密度。本文综述了近年来制备5V正极材料LiNi0.5Mn1.5O4的方法以及通过这些方法制备出的材料的电化学性能的优劣性。 展开更多
关键词 尖晶石型LiNi0.5Mn1.5O4 正极材料 电压平台 锂离子电池
下载PDF
NTC陶瓷材料Co_(1.5)Mn_(1.5-X)Ni_XO_4中阳离子分布与导电性间的关系 被引量:4
19
作者 张惠敏 常爱民 +4 位作者 王伟 赵青 彭昌文 陈爱香 姚金城 《无机化学学报》 SCIE CAS CSCD 北大核心 2010年第5期781-786,共6页
本文通过溶胶-凝胶法制备三元系Co1.5Mn1.5-XNiXO4(X=0,0.1,0.3,0.5,0.7,1.0)NTC热敏电阻粉体材料,采用激光粒度分析、X射线衍射分析、红外光谱分析、电阻测量等手段,表征了煅烧材料的颗粒尺寸、烧结体的物相、红外吸收光谱以及陶瓷材... 本文通过溶胶-凝胶法制备三元系Co1.5Mn1.5-XNiXO4(X=0,0.1,0.3,0.5,0.7,1.0)NTC热敏电阻粉体材料,采用激光粒度分析、X射线衍射分析、红外光谱分析、电阻测量等手段,表征了煅烧材料的颗粒尺寸、烧结体的物相、红外吸收光谱以及陶瓷材料的电学特性。结合XRD、IR的分析结果,探讨了阳离子分布与热敏电阻电性能之间的关系,为解决热敏电阻材料高精度、高可靠性方面提供了依据。结果表明:随着Ni离子的增加,所得热敏材料的电阻率呈U型变化,材料常数B值从4427减小到2429K,该系列的电阻率、B25/50值调整范围较大,是一种具有实际应用价值的NTC热敏电阻。 展开更多
关键词 Co1.5Mn1.5-XNiXO4 NTC热敏电阻 阳离子分布 溶胶-凝胶法
下载PDF
LiMg_xNi_(0.5-x)Mn_(1.5)O_4的制备和电化学性能 被引量:5
20
作者 张胜利 李良玉 +1 位作者 宋延华 杨胜杰 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2010年第3期515-518,共4页
为改善LiNi0.5Mn1.5O4的电化学性能,采用流变相法合成掺镁的锂离子电池正极材料LiMgxNi0.5-xMn1.5O4(x=0,0.05,0.1)。XRD测试结果表明所得材料仍为尖晶石结构。电化学性能测试结果显示:当x取值0.1,在3.5~4.9V电压范围内进行充放电循环... 为改善LiNi0.5Mn1.5O4的电化学性能,采用流变相法合成掺镁的锂离子电池正极材料LiMgxNi0.5-xMn1.5O4(x=0,0.05,0.1)。XRD测试结果表明所得材料仍为尖晶石结构。电化学性能测试结果显示:当x取值0.1,在3.5~4.9V电压范围内进行充放电循环时,材料LiMg0.1Ni0.4Mn1.5O4具有较好的循环性能,1C充放电时,初始放电比容量可达110.22mAh/g,30次循环后容量衰减率仅为7.7%。 展开更多
关键词 锂离子电池 LiMgxNi0.5-xMn1.5O4 流变相法 掺杂
下载PDF