Enrichment of schist mined in Morocco resulted in an extract essentially made of andalusite, quartz and muscovite, which was investigated with the aim to synthesize mullite refractory materials. X-ray diffraction anal...Enrichment of schist mined in Morocco resulted in an extract essentially made of andalusite, quartz and muscovite, which was investigated with the aim to synthesize mullite refractory materials. X-ray diffraction analysis was used to assess phase transformations upon heating at different temperatures. Mullite formation starts as early as 1200℃ and seems almost total at 1450℃. This process correlates with a weak shrinkage (3.5% at 1450℃) and the formation of an important glass phase. Green compacts obtained by unidirectional pressing the extract powder were heated under air in the temperature range 1200℃ - 1600℃. Chemical and mechanical properties of these materials were investigated and correlated with their microstructure.展开更多
In order to restrain cement kiln shell' s thermal loss and potential safety hazards,composite design was employed of working layer,thermal preservation layer and thermal insulation layer.Thermal preservation layer' ...In order to restrain cement kiln shell' s thermal loss and potential safety hazards,composite design was employed of working layer,thermal preservation layer and thermal insulation layer.Thermal preservation layer' s boundary and strain were analyzed and the overall thermal conductivity was calculated.The result shows that the sinusoidal curve boundary combination is adopted between the working layer and thermal preservation layer,and the slope-shape with angle of 135 degrees between the thermal preservation layer and thermal insulation layer could relieve the strain concentration.Comprehensive thermal conductivity of the composite mullite brick decreases from the working layer 2.74 W·m^(-1)·K^(-1) to1.54 W·m^(-1)·K^(-1).When applying the composite bricks in cement kilns,the kiln shell temperature is from50 ℃ to 70 ℃ lower than using normal bricks.展开更多
基金the Centre d’Etude et de Re-cherche des Phosphates Mineraux(Cerphos,Morocco)for their collaboration and financial support.
文摘Enrichment of schist mined in Morocco resulted in an extract essentially made of andalusite, quartz and muscovite, which was investigated with the aim to synthesize mullite refractory materials. X-ray diffraction analysis was used to assess phase transformations upon heating at different temperatures. Mullite formation starts as early as 1200℃ and seems almost total at 1450℃. This process correlates with a weak shrinkage (3.5% at 1450℃) and the formation of an important glass phase. Green compacts obtained by unidirectional pressing the extract powder were heated under air in the temperature range 1200℃ - 1600℃. Chemical and mechanical properties of these materials were investigated and correlated with their microstructure.
基金National Key Technology Research and Development Program of China during the "12~(th) Five-Year Plan"(No. 2013BAE03B01-10)
文摘In order to restrain cement kiln shell' s thermal loss and potential safety hazards,composite design was employed of working layer,thermal preservation layer and thermal insulation layer.Thermal preservation layer' s boundary and strain were analyzed and the overall thermal conductivity was calculated.The result shows that the sinusoidal curve boundary combination is adopted between the working layer and thermal preservation layer,and the slope-shape with angle of 135 degrees between the thermal preservation layer and thermal insulation layer could relieve the strain concentration.Comprehensive thermal conductivity of the composite mullite brick decreases from the working layer 2.74 W·m^(-1)·K^(-1) to1.54 W·m^(-1)·K^(-1).When applying the composite bricks in cement kilns,the kiln shell temperature is from50 ℃ to 70 ℃ lower than using normal bricks.