[Objective] The study aimed to extract fulvic acid from brown coal using N-Mn-TiO2 as a catalyst and H2O2 or HNO3 as an oxidizer. [Method] The effects of catalyst N-Mn-TiO2 on the yield and structure of fuMc acid were...[Objective] The study aimed to extract fulvic acid from brown coal using N-Mn-TiO2 as a catalyst and H2O2 or HNO3 as an oxidizer. [Method] The effects of catalyst N-Mn-TiO2 on the yield and structure of fuMc acid were studied, and the content of functional groups in fulvic acid was analyzed qualitatively and quantitatively. [ Reselt] Two catalysts could improved the yield of fulvic acid, that is, catalyst 1 (N: Mn: 13 = 16: 0.001:1, roasting temperature was 400 ℃) and catalyst 2 (N: Mn: Ti = 16: 0.001:1, roasting temperature was 100 ℃) increased OFA yield by 10.69% and 32.17% and NFA by 8.61% and 7.49% respectively. After the addition of catalysts, the content of total acid radicals in OFA changed little, and carboxyi content increased slightly, but phenolic hydroxyl content decreased. When HNO3 was used as an oxidizer, the content of total acid radicals and phenolic hydroxyl in NFA decreased. In addition, the structure of OFA was different from that of NFA. [Condusion] The research could provide scientific references for the development and application of brown coal in future.展开更多
基金Supported by the Bidding Project of Qujing Normal University(2011ZB005)
文摘[Objective] The study aimed to extract fulvic acid from brown coal using N-Mn-TiO2 as a catalyst and H2O2 or HNO3 as an oxidizer. [Method] The effects of catalyst N-Mn-TiO2 on the yield and structure of fuMc acid were studied, and the content of functional groups in fulvic acid was analyzed qualitatively and quantitatively. [ Reselt] Two catalysts could improved the yield of fulvic acid, that is, catalyst 1 (N: Mn: 13 = 16: 0.001:1, roasting temperature was 400 ℃) and catalyst 2 (N: Mn: Ti = 16: 0.001:1, roasting temperature was 100 ℃) increased OFA yield by 10.69% and 32.17% and NFA by 8.61% and 7.49% respectively. After the addition of catalysts, the content of total acid radicals in OFA changed little, and carboxyi content increased slightly, but phenolic hydroxyl content decreased. When HNO3 was used as an oxidizer, the content of total acid radicals and phenolic hydroxyl in NFA decreased. In addition, the structure of OFA was different from that of NFA. [Condusion] The research could provide scientific references for the development and application of brown coal in future.