Purpose: The study investigated the impact of dietary habits, specifically soda, milk kefir, water kefir, almond milk, and distilled water (control) consumption, on the microhardness of gingiva-coloured composite and ...Purpose: The study investigated the impact of dietary habits, specifically soda, milk kefir, water kefir, almond milk, and distilled water (control) consumption, on the microhardness of gingiva-coloured composite and acrylic denture bases. Methods: Materials included gingiva-coloured composite (Fusion Universal G1), acrylic (Imicryl), and subdivided Procryla group. Subgroups comprised 15 and 30-minute heat polymerized (Pro15, Pro30), and 1 wt% (Pro1Z) and 3 wt% (Pro3Z) zirconium added groups. Immersed in beverages for 1, 7, and 14 days, pH and microhardness were assessed. SEM examined random samples. Statistical analysis used repeated measures ANOVA, and post hoc tests (p Results: The gingiva-coloured composites displayed noteworthy time-associated microhardness changes (p 0.05). Despite variable pH levels in beverages, no substantial group interaction effects were observed (p > 0.05). Initial microhardness rankings shifted after a 14-day immersion. Conclusions: Gingiva-coloured composite exhibited the highest microhardness pre- and post-immersion, followed by Procryla30 and Imicryl groups. .展开更多
Ag-In intermetallic alloys were produced by using vacuum arc furnace. Differential Scanning Calorimetry(DSC) and Energy Dispersive X-Ray Spectrometry(EDX) were used to determine the thermal properties and chemical com...Ag-In intermetallic alloys were produced by using vacuum arc furnace. Differential Scanning Calorimetry(DSC) and Energy Dispersive X-Ray Spectrometry(EDX) were used to determine the thermal properties and chemical composition of the phases respectively. Microhardness values of Ag-In intermetallics were calculated with Vickers hardness measurement method. According to the experimental results, Ag-34 wt%In intermetallic system generated the best results of energy saving and storage compared to other intermetallic systems. Also from the microhardness results, it was observed that intermetallic alloys were harder than pure silver and Ag-26 wt%In system had the highest microhardness value with 143.45 kg/mm^(2).展开更多
The influences of cooling rate on the phase constitution,microstructural length scale,and microhardness of directionally solidified Galvalume(Zn-55Al-1.6Si)alloy were investigated by directional solidification experim...The influences of cooling rate on the phase constitution,microstructural length scale,and microhardness of directionally solidified Galvalume(Zn-55Al-1.6Si)alloy were investigated by directional solidification experiments at different withdrawal speeds(5,10,20,50,100,200,and 400μm·s^(-1)).The results show that the microstructure of directionally solidified Galvalume alloys is composed of primary Al dendrites,Si-rich phase and(Zn-Al-Si)ternary eutectics at the withdrawal speed ranging from 5 to 400μm·s^(-1).As the withdrawal speed increases,the segregation of Si element intensifies,resulting in an increase in the area fraction of the Si-rich phase.In addition,the primary Al dendrites show significant refinement with an increase in the withdrawal speed.The relationship between the primary dendrite arm spacing(λ_(1))and the thermal parameters of solidification is obtained:λ_(1)=127.3V^(-0.31).Moreover,as the withdrawal speed increases from 5 to 400μm·s^(-1),the microhardness of the alloy increases from 90 HV to 151 HV.This is a combined effect of grain refinement and second-phase strengthening.展开更多
The evolution of microstructure and local properties near the welding interface is essential for the service safety of dissimilar metal welded joints between nickel-based alloy(NA) and low-alloy steel(LA).In this work...The evolution of microstructure and local properties near the welding interface is essential for the service safety of dissimilar metal welded joints between nickel-based alloy(NA) and low-alloy steel(LA).In this work,NA filler metal was deposited on LA substrate under different heat inputs by tungsten inert gas(TIG) welding.Microstructural characterization and microhardness tests were carried out near the prepared cladding interfaces.Optical and scanning electron microscopes show the lack of evident hardening transition layer along the welding interface.As the heat input increases,the mean hardness of the deposited layer also increases remarkably due to the rising dilution rate.Microstructural characterization shows a significant composition gradient across the cladding interface,but the diffusion gradient is limited to a small range.Under high heat input,a planar grain zone is generated along the interface due to the large temperature gradient across the interface region.展开更多
This study carried out the underwater and in-air wire-feed laser deposition of an aluminium alloy with a thin-walled tubular structure. For both the underwater and in-air deposition layers, both were well-formed and i...This study carried out the underwater and in-air wire-feed laser deposition of an aluminium alloy with a thin-walled tubular structure. For both the underwater and in-air deposition layers, both were well-formed and incomplete fusion, cracks, or other defects did not exist.Compared with the single-track deposition layer in air, the oxidation degree of the underwater single-track deposition layer was slightly higher.In both the underwater and in-air deposition layers, columnar dendrites nucleated close to the fusion line and grew along the direction of the maximum cooling rate in the fusion region(FR), while equiaxed grains formed in the deposited region(DR). As the environment changed from air to water, the width of DR and height of FR decreased, but the deposition angle and height of DR increased. The grain size and ratio of the high-angle boundaries also decreased due to the large cooling rate and low peak temperature in the water environment.Besides, the existence of a water environment benefitted the reduction of magnesium element burning loss in the DR. The microhardness values of the underwater deposition layer were much larger than those of the in-air layer, owing to the fine grains and high magnesium content.展开更多
The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing ...The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing agent-boron nitride (10% of the alloy volume) on the microstructure and microhardness of the alloy after quenching was studied. Depending on the conditions of thermobaric action, structures based on solid solution of the B2 type or mixed phases with structures of the Al, A2 or B2 types are formed in the AlNiCoFeCr alloy, which influences the alloy microhardness that varies in the range of 5 - 12.5 GPa. .展开更多
For joining high Cr,Ni and Mo austenitic stainless steel(AISI 316)by direct drive friction welding(DDFW),with friction weld-ing conditions:rotation speed of 3000 r/min,friction time of 10 s,friction pressure of 130 MP...For joining high Cr,Ni and Mo austenitic stainless steel(AISI 316)by direct drive friction welding(DDFW),with friction weld-ing conditions:rotation speed of 3000 r/min,friction time of 10 s,friction pressure of 130 MPa,forge time of 5 s and forge pressure of 260 MPa.The results of microstructure showed that the temperature at the interface reached 819℃while forge applied between 357-237℃,which subdivided welded joint into four distinct regions of highly plastically deformed zone(HPDZ),thermo-mechanically affected zone(TMAZ),heat affected zone(HAZ)and the base metal,with grain size about 10µm,100µm,90µm and 30µm respectively.These re-gions were created due to dynamic recrystallization(DRX)at the interface and thermo-mechanical deformation with heat diffusion in the neighboring regions.Whereas,high level of microhardness about 300 HV0.1 and hardness roughly 240 Hv10 at the interface due to HPDZ creation while low level of 240 HV0.1 for microhardness and moderately of 205 HV10 for hardness in neighboring regions.展开更多
The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing ...The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing agent-boron nitride (10% of the alloy volume) on the microstructure and microhardness of the alloy after quenching was studied. Depending on the conditions of thermobaric action, structures based on solid solution of the B2 type or mixed phases with structures of the Al, A2 or B2 types are formed in the AlNiCoFeCr alloy, which influences the alloy microhardness that varies in the range of 5 - 12.5 GPa. .展开更多
Laser shock peening is a modernized surface enhancement performed methodically to improve fatigue life, enhance the hardness of the material and make coarse grains flat under the superficial layer. In this current stu...Laser shock peening is a modernized surface enhancement performed methodically to improve fatigue life, enhance the hardness of the material and make coarse grains flat under the superficial layer. In this current study, the effect of varying optimized multiple laser shock peening (LSP) is studied on the surface integrity, microhardness, and mechanical properties. The results show that the LSP-treated specimens have visible signs of valleys, wavy and varying height distribution as well as dimples. However, the presence of non-uniformity and sharp protrusions was detected from the superficiality of the as-received specimen and this was so because of the SiC abrasive material used to polish the superficial layer of the specimen before the test experiment. Prior to LSP, the surface roughness was 2 μm, however, after LSP the roughness increased to 4 μm, 6 μm and 17 μm for 1, 2, and 4 impacts, respectively. High-density dislocation can also be observed close to the grain boundary because the grain boundary prevents the migration of dislocation which could lead to dislocation walls and dislocation tangles. The increase in impacts decrease the average grain size, nevertheless, the micro-strain increased after multiple impacts. Furthermore, coarse grains after LSP were transformed into finer grains. The increase in the number of impacts increases the micro-strain likewise the full-width half maximum (FWHM). Finally, the increase in microhardness increases as the LSP impacts increase.展开更多
The constant need for high-strength materials in the construction industry promotes the research of additives that improve the properties of masonry materials. The use of allophane as an additive in concrete and morta...The constant need for high-strength materials in the construction industry promotes the research of additives that improve the properties of masonry materials. The use of allophane as an additive in concrete and mortar mixtures was implemented to improve their strength and waterproofing, respectively, using compression and water absorption tests according to their corresponding standards (ASTM C1231, ASTM D2938, and ASTM C1585). The samples were evaluated at different concentrations and curing ages. In addition, different sand/cement ratios were considered for the mortar. The results revealed that there was a 9.4% increase in compressive strength in concrete and a 23.7% reduction in water absorption in mortar for the 5:1 ratio. These changes would be the result of the interaction of the nanoporous additive in the atomic crystal structure of the material demonstrating the nanotechnological nature of allophane.展开更多
Code converters are essential in digital nano communication;therefore,a low-complexity optimal QCA layout for a BCD to Excess-3 code converter has been proposed in this paper.A QCA clockphase-based design technique wa...Code converters are essential in digital nano communication;therefore,a low-complexity optimal QCA layout for a BCD to Excess-3 code converter has been proposed in this paper.A QCA clockphase-based design technique was adopted to investigate integration with other complicated circuits.Using a unique XOR gate,the recommended circuit’s cell complexity has been decreased.The findings produced using the QCADesigner-2.0.3,a reliable simulation tool,prove the effectiveness of the current structure over earlier designs by considering the number of cells deployed,the area occupied,and the latency as design metrics.In addition,the popular tool QCAPro was used to estimate the energy dissipation of the proposed design.The proposed technique reduces the occupied space by∼40%,improves cell complexity by∼20%,and reduces energy dissipation by∼1.8 times(atγ=1.5EK)compared to the current scalable designs.This paper also studied the suggested structure’s energy dissipation and compared it to existing works for a better performance evaluation.展开更多
In line with recent studies,where it has been shown that nanofluids containing graphene have a stronger capacity to boost the heat transfer coefficient with respect to ordinary nanofluids,experiments have been conducted ...In line with recent studies,where it has been shown that nanofluids containing graphene have a stronger capacity to boost the heat transfer coefficient with respect to ordinary nanofluids,experiments have been conducted using water with cobalt ferrite/graphene nanoparticles.In particular,a circular channel made of copper subjected to a constant heatflux has been considered.As nanoparticles are sensitive to the presence of a magneticfield,different conditions have been examined,allowing both the strength and the frequency of such afield to span relatively wide ranges and assuming different concentrations of nanoparticles.According to thefindings,the addition of nanoparticles to thefluid causes its rotation speed to increase by a factor of two,whereas ultraviolet radiation plays a negligible role.The amount of time required to attain the maximum rotation speed of the nanofluid and the Nusselt number have been measured under both constant and alternating magneticfields for a ferrofluid with a concentration of 0.5%and atflow Reynolds number of 550 and 1750.展开更多
Nanorubber/epoxy composites containing 0,2,6 and 10 wt%nanorubber are subjected to uniaxial compression over a wide range of strain rate from 8×10^(-4) s^(-1) to~2×10^(4) s^(-1).Unexpectedly,their strain rat...Nanorubber/epoxy composites containing 0,2,6 and 10 wt%nanorubber are subjected to uniaxial compression over a wide range of strain rate from 8×10^(-4) s^(-1) to~2×10^(4) s^(-1).Unexpectedly,their strain rate sensitivity and strain hardening index increase with increasing nanorubber content.Potential mechanisms are proposed based on numerical simulations using a unit cell model.An increase in the strain rate sensitivity with increasing nanorubber content results from the fact that the nanorubber becomes less incompressible at high strain,generating a higher hydro-static pressure.Adiabatic shear localization starts to occur in the epoxy under a strain rate of 22,000 s^(-1) when the strain exceeds 0.35.The presence of nanorubber in the epoxy reduces adiabatic shear localization by preventing it from propagating.展开更多
WC-Co nanocrystalline nitrogen-containing cemented carbides were prepared by vacuum sintering and low pressure sintering.The sintering processes of Cr_(2)(C,N)doped nano WC-Co powders were studied by using thermogravi...WC-Co nanocrystalline nitrogen-containing cemented carbides were prepared by vacuum sintering and low pressure sintering.The sintering processes of Cr_(2)(C,N)doped nano WC-Co powders were studied by using thermogravimetric analysis(TGA)and differential scanning calorimetry(DSC).The effect of sintering temperature on the microstructure and mechanical properties of nanocrystalline cemented carbide was studied by scanning electron microscope(SEM),high resolution transmission electron microscope(HRTEM)and mechanical property test.The results showed that the nano WC grains began to grow in the solid phase sintering stage.A high-performance nano-nitrogen-containing cemented carbide with uniform microstructure and good interfacial bonding can be obtained by increasing the sintering temperature to 1380℃.It has a transverse rupture strength(TRS)of 5057 MPa and a hardness of 1956 HV30.展开更多
文摘Purpose: The study investigated the impact of dietary habits, specifically soda, milk kefir, water kefir, almond milk, and distilled water (control) consumption, on the microhardness of gingiva-coloured composite and acrylic denture bases. Methods: Materials included gingiva-coloured composite (Fusion Universal G1), acrylic (Imicryl), and subdivided Procryla group. Subgroups comprised 15 and 30-minute heat polymerized (Pro15, Pro30), and 1 wt% (Pro1Z) and 3 wt% (Pro3Z) zirconium added groups. Immersed in beverages for 1, 7, and 14 days, pH and microhardness were assessed. SEM examined random samples. Statistical analysis used repeated measures ANOVA, and post hoc tests (p Results: The gingiva-coloured composites displayed noteworthy time-associated microhardness changes (p 0.05). Despite variable pH levels in beverages, no substantial group interaction effects were observed (p > 0.05). Initial microhardness rankings shifted after a 14-day immersion. Conclusions: Gingiva-coloured composite exhibited the highest microhardness pre- and post-immersion, followed by Procryla30 and Imicryl groups. .
基金Nev?ehir Hac?Bekta?Veli Runiversity Scientific Research Projects Coordination Unit (No. NEüLüP16/2F3)。
文摘Ag-In intermetallic alloys were produced by using vacuum arc furnace. Differential Scanning Calorimetry(DSC) and Energy Dispersive X-Ray Spectrometry(EDX) were used to determine the thermal properties and chemical composition of the phases respectively. Microhardness values of Ag-In intermetallics were calculated with Vickers hardness measurement method. According to the experimental results, Ag-34 wt%In intermetallic system generated the best results of energy saving and storage compared to other intermetallic systems. Also from the microhardness results, it was observed that intermetallic alloys were harder than pure silver and Ag-26 wt%In system had the highest microhardness value with 143.45 kg/mm^(2).
基金supported by the Key Science and Technology Projects of Gansu Province(Grant No.22ZD6GB019)Gansu Key Research and Development Project(Grant No.23YFGA0003)+2 种基金Gansu Provincial Joint Research Fund(Grant No.23JRRC0004)Fundamental Research Funds for the Central Universities(Grant No.lzujbky-2022-ey15)the State Key Laboratory of Solidification Processing in NPU(Grant No.SKLSP202204).
文摘The influences of cooling rate on the phase constitution,microstructural length scale,and microhardness of directionally solidified Galvalume(Zn-55Al-1.6Si)alloy were investigated by directional solidification experiments at different withdrawal speeds(5,10,20,50,100,200,and 400μm·s^(-1)).The results show that the microstructure of directionally solidified Galvalume alloys is composed of primary Al dendrites,Si-rich phase and(Zn-Al-Si)ternary eutectics at the withdrawal speed ranging from 5 to 400μm·s^(-1).As the withdrawal speed increases,the segregation of Si element intensifies,resulting in an increase in the area fraction of the Si-rich phase.In addition,the primary Al dendrites show significant refinement with an increase in the withdrawal speed.The relationship between the primary dendrite arm spacing(λ_(1))and the thermal parameters of solidification is obtained:λ_(1)=127.3V^(-0.31).Moreover,as the withdrawal speed increases from 5 to 400μm·s^(-1),the microhardness of the alloy increases from 90 HV to 151 HV.This is a combined effect of grain refinement and second-phase strengthening.
文摘The evolution of microstructure and local properties near the welding interface is essential for the service safety of dissimilar metal welded joints between nickel-based alloy(NA) and low-alloy steel(LA).In this work,NA filler metal was deposited on LA substrate under different heat inputs by tungsten inert gas(TIG) welding.Microstructural characterization and microhardness tests were carried out near the prepared cladding interfaces.Optical and scanning electron microscopes show the lack of evident hardening transition layer along the welding interface.As the heat input increases,the mean hardness of the deposited layer also increases remarkably due to the rising dilution rate.Microstructural characterization shows a significant composition gradient across the cladding interface,but the diffusion gradient is limited to a small range.Under high heat input,a planar grain zone is generated along the interface due to the large temperature gradient across the interface region.
基金financially supported by the Fundamental Research Funds for the Central Universities (No. HIT.OCEF.2021036)。
文摘This study carried out the underwater and in-air wire-feed laser deposition of an aluminium alloy with a thin-walled tubular structure. For both the underwater and in-air deposition layers, both were well-formed and incomplete fusion, cracks, or other defects did not exist.Compared with the single-track deposition layer in air, the oxidation degree of the underwater single-track deposition layer was slightly higher.In both the underwater and in-air deposition layers, columnar dendrites nucleated close to the fusion line and grew along the direction of the maximum cooling rate in the fusion region(FR), while equiaxed grains formed in the deposited region(DR). As the environment changed from air to water, the width of DR and height of FR decreased, but the deposition angle and height of DR increased. The grain size and ratio of the high-angle boundaries also decreased due to the large cooling rate and low peak temperature in the water environment.Besides, the existence of a water environment benefitted the reduction of magnesium element burning loss in the DR. The microhardness values of the underwater deposition layer were much larger than those of the in-air layer, owing to the fine grains and high magnesium content.
文摘The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing agent-boron nitride (10% of the alloy volume) on the microstructure and microhardness of the alloy after quenching was studied. Depending on the conditions of thermobaric action, structures based on solid solution of the B2 type or mixed phases with structures of the Al, A2 or B2 types are formed in the AlNiCoFeCr alloy, which influences the alloy microhardness that varies in the range of 5 - 12.5 GPa. .
文摘For joining high Cr,Ni and Mo austenitic stainless steel(AISI 316)by direct drive friction welding(DDFW),with friction weld-ing conditions:rotation speed of 3000 r/min,friction time of 10 s,friction pressure of 130 MPa,forge time of 5 s and forge pressure of 260 MPa.The results of microstructure showed that the temperature at the interface reached 819℃while forge applied between 357-237℃,which subdivided welded joint into four distinct regions of highly plastically deformed zone(HPDZ),thermo-mechanically affected zone(TMAZ),heat affected zone(HAZ)and the base metal,with grain size about 10µm,100µm,90µm and 30µm respectively.These re-gions were created due to dynamic recrystallization(DRX)at the interface and thermo-mechanical deformation with heat diffusion in the neighboring regions.Whereas,high level of microhardness about 300 HV0.1 and hardness roughly 240 Hv10 at the interface due to HPDZ creation while low level of 240 HV0.1 for microhardness and moderately of 205 HV10 for hardness in neighboring regions.
文摘The structure of equiatomic high-entropy AlNiCoFeCr alloy obtained by arc melting was investigated. The influence of high pressures (5, 8 and 11 GPa), quenching temperature (1650?C) and small additions of reinforcing agent-boron nitride (10% of the alloy volume) on the microstructure and microhardness of the alloy after quenching was studied. Depending on the conditions of thermobaric action, structures based on solid solution of the B2 type or mixed phases with structures of the Al, A2 or B2 types are formed in the AlNiCoFeCr alloy, which influences the alloy microhardness that varies in the range of 5 - 12.5 GPa. .
文摘Laser shock peening is a modernized surface enhancement performed methodically to improve fatigue life, enhance the hardness of the material and make coarse grains flat under the superficial layer. In this current study, the effect of varying optimized multiple laser shock peening (LSP) is studied on the surface integrity, microhardness, and mechanical properties. The results show that the LSP-treated specimens have visible signs of valleys, wavy and varying height distribution as well as dimples. However, the presence of non-uniformity and sharp protrusions was detected from the superficiality of the as-received specimen and this was so because of the SiC abrasive material used to polish the superficial layer of the specimen before the test experiment. Prior to LSP, the surface roughness was 2 μm, however, after LSP the roughness increased to 4 μm, 6 μm and 17 μm for 1, 2, and 4 impacts, respectively. High-density dislocation can also be observed close to the grain boundary because the grain boundary prevents the migration of dislocation which could lead to dislocation walls and dislocation tangles. The increase in impacts decrease the average grain size, nevertheless, the micro-strain increased after multiple impacts. Furthermore, coarse grains after LSP were transformed into finer grains. The increase in the number of impacts increases the micro-strain likewise the full-width half maximum (FWHM). Finally, the increase in microhardness increases as the LSP impacts increase.
文摘The constant need for high-strength materials in the construction industry promotes the research of additives that improve the properties of masonry materials. The use of allophane as an additive in concrete and mortar mixtures was implemented to improve their strength and waterproofing, respectively, using compression and water absorption tests according to their corresponding standards (ASTM C1231, ASTM D2938, and ASTM C1585). The samples were evaluated at different concentrations and curing ages. In addition, different sand/cement ratios were considered for the mortar. The results revealed that there was a 9.4% increase in compressive strength in concrete and a 23.7% reduction in water absorption in mortar for the 5:1 ratio. These changes would be the result of the interaction of the nanoporous additive in the atomic crystal structure of the material demonstrating the nanotechnological nature of allophane.
文摘Code converters are essential in digital nano communication;therefore,a low-complexity optimal QCA layout for a BCD to Excess-3 code converter has been proposed in this paper.A QCA clockphase-based design technique was adopted to investigate integration with other complicated circuits.Using a unique XOR gate,the recommended circuit’s cell complexity has been decreased.The findings produced using the QCADesigner-2.0.3,a reliable simulation tool,prove the effectiveness of the current structure over earlier designs by considering the number of cells deployed,the area occupied,and the latency as design metrics.In addition,the popular tool QCAPro was used to estimate the energy dissipation of the proposed design.The proposed technique reduces the occupied space by∼40%,improves cell complexity by∼20%,and reduces energy dissipation by∼1.8 times(atγ=1.5EK)compared to the current scalable designs.This paper also studied the suggested structure’s energy dissipation and compared it to existing works for a better performance evaluation.
文摘In line with recent studies,where it has been shown that nanofluids containing graphene have a stronger capacity to boost the heat transfer coefficient with respect to ordinary nanofluids,experiments have been conducted using water with cobalt ferrite/graphene nanoparticles.In particular,a circular channel made of copper subjected to a constant heatflux has been considered.As nanoparticles are sensitive to the presence of a magneticfield,different conditions have been examined,allowing both the strength and the frequency of such afield to span relatively wide ranges and assuming different concentrations of nanoparticles.According to thefindings,the addition of nanoparticles to thefluid causes its rotation speed to increase by a factor of two,whereas ultraviolet radiation plays a negligible role.The amount of time required to attain the maximum rotation speed of the nanofluid and the Nusselt number have been measured under both constant and alternating magneticfields for a ferrofluid with a concentration of 0.5%and atflow Reynolds number of 550 and 1750.
基金supported by the Key Research and Development Plan of Shaanxi Province (2023-GHZD-12)the Opening Fund of State Key Laboratory for Strength and Vibration of Mechanical Structures (SVL2021-KF-12)+1 种基金Fundamental Research Funds for the Central Universities (G2020KY05112)the 111 Project (BP0719007)
文摘Nanorubber/epoxy composites containing 0,2,6 and 10 wt%nanorubber are subjected to uniaxial compression over a wide range of strain rate from 8×10^(-4) s^(-1) to~2×10^(4) s^(-1).Unexpectedly,their strain rate sensitivity and strain hardening index increase with increasing nanorubber content.Potential mechanisms are proposed based on numerical simulations using a unit cell model.An increase in the strain rate sensitivity with increasing nanorubber content results from the fact that the nanorubber becomes less incompressible at high strain,generating a higher hydro-static pressure.Adiabatic shear localization starts to occur in the epoxy under a strain rate of 22,000 s^(-1) when the strain exceeds 0.35.The presence of nanorubber in the epoxy reduces adiabatic shear localization by preventing it from propagating.
基金Funded by the National Key Research and Development Plan of China(No.2017YFB0305900)。
文摘WC-Co nanocrystalline nitrogen-containing cemented carbides were prepared by vacuum sintering and low pressure sintering.The sintering processes of Cr_(2)(C,N)doped nano WC-Co powders were studied by using thermogravimetric analysis(TGA)and differential scanning calorimetry(DSC).The effect of sintering temperature on the microstructure and mechanical properties of nanocrystalline cemented carbide was studied by scanning electron microscope(SEM),high resolution transmission electron microscope(HRTEM)and mechanical property test.The results showed that the nano WC grains began to grow in the solid phase sintering stage.A high-performance nano-nitrogen-containing cemented carbide with uniform microstructure and good interfacial bonding can be obtained by increasing the sintering temperature to 1380℃.It has a transverse rupture strength(TRS)of 5057 MPa and a hardness of 1956 HV30.