Comparative investigation of microstructure and high-temperature oxidation resistance of high-velocity oxy-fuel sprayed CoNiCrAlY/nano-Al_(2)O_(3) composite coatings using satellited powders 被引量:2
1
作者 Pejman Zamani Zia Valefi 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2023年第9期1779-1791,共13页
Satellited CoNiCrAlY–Al_(2)O_(3)feedstocks with 2wt%, 4wt%, and 6wt% oxide nanoparticles and pure CoNiCrAlY powder were deposited by the high-velocity oxy fuel process on an Inconel738 superalloy substrate. The oxida... Satellited CoNiCrAlY–Al_(2)O_(3)feedstocks with 2wt%, 4wt%, and 6wt% oxide nanoparticles and pure CoNiCrAlY powder were deposited by the high-velocity oxy fuel process on an Inconel738 superalloy substrate. The oxidation test was performed at 1050℃ for 5, 50, 100,150, 200, and 400 h. The microstructure and phase composition of powders and coatings were characterized by scanning electron microscopy and X-ray diffraction, respectively. The bonding strength of the coatings was also evaluated. The results proved that with the increase in the percentage of nanoparticles(from 2wt% to 6wt%), the amount of porosity(from 1vol% to 4.7vol%), unmelted particles, and roughness of the coatings(from 4.8 to 8.8 μm) increased, and the bonding strength decreased from 71 to 48 MPa. The thicknesses of the thermally grown oxide layer of pure and composite coatings(2wt%, 4wt%, and 6wt%) after 400 h oxidation were measured as 6.5, 5.5, 7.6, and 8.1 μm, respectively.The CoNiCrAlY–2wt% Al_(2)O_(3)coating showed the highest oxidation resistance due to the diffusion barrier effect of well-dispersed nanoparticles. The CoNiCrAlY–6wt% Al_(2)O_(3)coating had the lowest oxidation resistance due to its rough surface morphology and porous microstructure. 展开更多
关键词 MCrAlY coating CoNiCrAlY-Al_(2)O_(3)composite satellited feedstock MICROSTRUCTURE high-temperature oxidation high-velocity oxy-fuel spraying
下载PDF
Two-Dimensional Co_(2)(OH)1,4-Benzenedicarboxylate-Halloysite Nanotube Nanocomposite-Epoxy Coating with High Corrosion Resistance
2
作者 Zhao Huarong Zhang Yueshuang Cheng Zhilin 《China Petroleum Processing & Petrochemical Technology》 SCIE CAS CSCD 2023年第1期44-53,共10页
Introducing inorganic nanomaterials into a polymer matrix greatly improves the anticorrosion performance of epoxy coatings(EP);however,poor compatibility between the materials can limit the improvement in properties.I... Introducing inorganic nanomaterials into a polymer matrix greatly improves the anticorrosion performance of epoxy coatings(EP);however,poor compatibility between the materials can limit the improvement in properties.In this work,based on the high interface compatibility of two-dimensional(2D)Co_(2)(OH)_(2)BDC(BDC=1,4-benzenedicarboxylate)in the epoxy coating that we reported in previous work,we fabricated a 2D Co_(2)(OH)_(2)BDC-halloysite nanotube(HNT)nanocomposite have a structure consisting of alternating of nanosheets and nanotube by in situ synthesis.The nanocomposite was characterized by Fourier transform infrared spectroscopy,X-ray diffraction,and scanning electron microscopy.The mechanical and anticorrosion performance of the 2D Co_(2)(OH)_(2)BDC-HNT/EP coating was evaluated by mechanical tests and electrochemical impedance spectroscopy spectra.Compared with a conventional unreinforced epoxy coating,the 2D Co_(2)(OH)_(2)BDC-HNT/EP coating had higher mechanical strength and toughness,and the low-frequency impedance modulus of 2D Co_(2)(OH)_(2)BDC-HNT/EP coating was increased by three orders of magnitude,demonstrating the high corrosion resistance of our reinforced coating. 展开更多
关键词 composite materials 2D Co_(2)(OH)1 4-Benzenedicarboxylate-Halloysite Nanotube halloysite nanotube epoxy coatings corrosion resistance
下载PDF
Preparation and oxidation property of ZrB_2-MoSi_2/SiC coating on carbon/carbon composites 被引量:14
3
作者 张武装 曾毅 +2 位作者 GBOLOGAH Lemuel 熊翔 黄伯云 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第7期1538-1544,共7页
To improve the oxidation resistance of carbon/carbon composites,ZrB2-MoSi2/SiC coating on the carbon/carbon substrate was prepared.The inner coating of SiC was prepared by pack cementation and the outer coating of ZrB... To improve the oxidation resistance of carbon/carbon composites,ZrB2-MoSi2/SiC coating on the carbon/carbon substrate was prepared.The inner coating of SiC was prepared by pack cementation and the outer coating of ZrB2-MoSi2 was prepared by slurry painting.The phase compositions and microstructures of the coating were characterized by XRD and SEM,respectively.The preparation and the high temperature oxidation property of the coated composites were investigated.The results show that the outer coating of carbon/carbon composites is composed of ZrB2,MoSi2 and SiC phases.The mass losses of the ZrB2-MoSi2/SiC coated samples with SiC nano-whiskers after 30 h and 10 h of oxidation at 1 273 K and 1 773 K were,respectively,5.3% and 3.0%.The ZrB2-MoSi2/SiC coated samples exhibit self-sealing performance and good oxidation resistance at high temperature. 展开更多
关键词 carbon/carbon composites ZrB2-MoSi2 SIC coating OXIDATION
下载PDF
Anti-oxidation properties of ZrB_2 modified silicon-based multilayer coating for carbon/carbon composites at high temperatures 被引量:7
4
作者 李贺军 姚西媛 +2 位作者 张雨雷 姚栋嘉 王少龙 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第7期2094-2099,共6页
To improve the anti-oxidation ability of silicon-based coating for carbon/carbon (C/C) composites at high temperatures, a ZrB2 modified silicon-based multilayer oxidation protective coating was prepared by pack ceme... To improve the anti-oxidation ability of silicon-based coating for carbon/carbon (C/C) composites at high temperatures, a ZrB2 modified silicon-based multilayer oxidation protective coating was prepared by pack cementation. The phase composition, microstructure and oxidation resistance at 1773, 1873 and 1953 K in air were investigated. The prepared coating exhibits dense structure and good oxidation protective ability. Due to the formation of stable ZrSiO4-SiO2 compound, the coating can effectively protect C/C composites from oxidation at 1773 K for more than 550 h. The anti-oxidation performance decreases with the increase of oxidation temperature. The mass loss of coated sample is 2.44% after oxidation at 1953 K for 50 h, which is attributed to the decomposition of ZrSiO4 and the volatilization of SiO2 protection layer. 展开更多
关键词 C/C composites coating ZRB2 anti-oxidation properties
下载PDF
SiC-MoSi_2/ZrO_2-MoSi_2 coating to protect C/C composites against oxidation 被引量:7
5
作者 付前刚 张佳平 +2 位作者 张正中 李贺军 孙粲 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第7期2113-2117,共5页
To improve the oxidation resistance of carbon/carbon (C/C) composites in air at high temperatures, a SiC- MoSi2/ZrO2-MoSi2 coating was prepared on the surface of C/C composites by pack cementation and slurry method.... To improve the oxidation resistance of carbon/carbon (C/C) composites in air at high temperatures, a SiC- MoSi2/ZrO2-MoSi2 coating was prepared on the surface of C/C composites by pack cementation and slurry method. The microstructures and phase compositions of the coated C/C composites were analyzed by scanning electron microscopy and X-ray diffraction, respectively. The result shows that the SiC-MoSi2/ZrO2-MoSi2 coating is dense and crack-free with a thickness of 250-300 μm. The preparation and the high temperature oxidation property of the coated composites were investigated. The as-received coating has excellent oxidation protection ability and can protect C/C composites from oxidation for 260 h at 1773 K in air. The excellent anti-oxidation performance of the coating is considered to come from the formation of ZrSiO4, which improves the stability of the coating at high temperatures. 展开更多
关键词 carbon/carbon composites SiC-MoSi2/ZrO2-MoSi2 coating oxidation resistance
下载PDF
Tribological properties of nanostructured Al_2O_3-40%TiO_2 multiphase ceramic particles reinforced Ni-based alloy composite coatings 被引量:9
6
作者 何龙 谭业发 +2 位作者 谭华 周春华 高立 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第9期2618-2627,共10页
The Ni-based alloy composite coatings reinforced by nanostructured Al2O3-40%TiO2 multiphase ceramic particles were prepared on the surface of 7005 aluminum alloy by plasma spray technology. The microstructure and trib... The Ni-based alloy composite coatings reinforced by nanostructured Al2O3-40%TiO2 multiphase ceramic particles were prepared on the surface of 7005 aluminum alloy by plasma spray technology. The microstructure and tribological properties of the composite coatings were researched. The results show that the composite coatings mainly consist of γ-Ni, α-Al2O3, γ-Al2O3 and rutile-TiO2 etc, and exhibit lower friction coefficients and wear losses than the Ni-based alloy coatings at different loads and speeds. The composite coating bears low contact stress at 3 N and its wear mechanism is micro-cutting wear. As loads increase to 6-12 N, the contact stress is higher than the elastic limit stress of worn surface, and the wear mechanisms change into multi-plastic deformation wear, micro-brittle fracture wear and abrasive wear. With the increase of speeds, the contact temperature of worn surface increases. The composite coating experiences multi-plastic deformation wear, fatigue wear and adhesive wear. 展开更多
关键词 nanostructured A1203-TiO2 multiphase ceramic particles Ni-based alloy composite coating plasma spray friction wear
下载PDF
C/SiC/MoSi_2-SiC-Si multilayer coating for oxidation protection of carbon/carbon composites 被引量:5
7
作者 张雨雷 李贺军 +2 位作者 胡志雄 李克智 张磊磊 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第7期2118-2122,共5页
C/SiC/MoSi2-SiC-Si oxidation protective multilayer coating for carbon/carbon (C/C) composites was prepared by pack cementation and slurry method. The microstructure, element distribution and phase composition of the... C/SiC/MoSi2-SiC-Si oxidation protective multilayer coating for carbon/carbon (C/C) composites was prepared by pack cementation and slurry method. The microstructure, element distribution and phase composition of the as-received coating were analyzed by scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction (XRD). The results show that the multilayer coating was composed of MoSi2, SiC and Si. It could effectively protect C/C composites against oxidation for 200 h with the mass loss of 3.25% at 1873 K in static air. The mass loss of the coated C/C composites results from the volatilization of SiO2 and the formation of cracks and bubble holes in the coating. 展开更多
关键词 C/C composites C/SIC MOSI2 SiC MULTILAYER coating OXIDATION
下载PDF
Tribological behavior and mechanisms of graphite/CaF_2/TiC/Ni-base alloy composite coatings 被引量:4
8
作者 蔡滨 谭业发 +2 位作者 何龙 谭华 王小龙 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第2期392-399,共8页
In order to reduce the friction coefficients and improve the wear resistance of mechanical parts, which work in the severe friction and wear conditions at heavy loads, the graphite/CaFg/TiC/Ni-base alloy composite coa... In order to reduce the friction coefficients and improve the wear resistance of mechanical parts, which work in the severe friction and wear conditions at heavy loads, the graphite/CaFg/TiC/Ni-base alloy composite coatings were prepared by plasma spray and their tribological behavior and mechanisms were investigated. The results show that the friction coefficients of the composite coatings are in the range of 0.22-0.288, which are reduced by 25.9% to 53% compared with those of the pure Ni-base alloy coatings, and the wear rates of the former are 18.6%-70.1% less than those of the latter. When wear against GCr15 steel balls, a transferred layer mainly composed of ferric oxides, graphite and CaF2 may gradually develop on the worn surface of the composite coatings, which made the friction and wear between GCr15 steel ball and the composite coatings change into that between the former and the transferred layer. So the friction coefficients and the wear lubrication effect of the transferred layer. The main wear layer in friction process. rates of the composite coatings are greatly reduced because of the solid mechanism of the composite coatings is delamination of the transferred 展开更多
关键词 plasma spray composite coatings Ni-base alloy GRAPHITE TIC CAF2 TRIBOLOGY
下载PDF
Oxidation behavior of C/C composites with SiC/ZrSiO_4-SiO_2 coating 被引量:3
9
作者 李杨 肖鹏 +2 位作者 李专 罗威 周伟 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2017年第2期397-405,共9页
A SiC/ZrSiO4?SiO2 (SZS) coating was successfully fabricated on the carbon/carbon (C/C) composites by pack cementation, slurry painting and sintering to improve the anti-oxidation property and thermal shock r... A SiC/ZrSiO4?SiO2 (SZS) coating was successfully fabricated on the carbon/carbon (C/C) composites by pack cementation, slurry painting and sintering to improve the anti-oxidation property and thermal shock resistance. The anti-oxidation properties under different oxygen partial pressures (OPP) and thermal shock resistance of the SZS coating were investigated. The results show that the SZS coated sample under low OPP, corresponding to the ambient air, during isothermal oxidation was 0.54% in mass gain after 111 h oxidation at 1500 ° C and less than 0.03% in mass loss after 50 h oxidation in high OPP, corresponding to the air flow rate of 36 L/h. Additionally, the residual compressive strengths (RCS) of the SZS coated samples after oxidation for 50 h in high OPP and 80 h in low OPP remain about 70% and 72.5% of those of original C/C samples, respectively. Moreover, the mass loss of SZS coated samples subjected to the thermal cycle from 1500 ° C in high OPP to boiling water for 30 times was merely 1.61%. 展开更多
关键词 C/C composite SiC/ZrSiO4-SiO2 coating oxygen partial pressure ANTI-OXIDATION thermal shock residual compressive strength
下载PDF
Tribological behavior and mechanism of NiCrBSi-Y_2O_3 composite coatings 被引量:1
10
作者 蔡滨 谭业发 +2 位作者 谭华 敬奇锋 张中威 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第7期2002-2010,共9页
The NiCrBSi-Y2O3 composite coatings were prepared on the surface of 45 carbon steel by plasma spray, the microstructure and tribological properties of the coatings were investigated. The results show that the NiCrBSi-... The NiCrBSi-Y2O3 composite coatings were prepared on the surface of 45 carbon steel by plasma spray, the microstructure and tribological properties of the coatings were investigated. The results show that the NiCrBSi-Y2O3 composite coatings are mainly composed of γ-Ni, CrB, Cr7C3 and Y2O3. With addition of Y2O3, hard phases such as CrB, Cr7C3 emerge in composite coating, and the density of the composite coatings also increases. The NiCrBSi-0.5Y2O3 composite coating presents excellent tribological properties. Its friction coefficient is 0.175, which is about 37% of that of the pure NiCrBSi coating. The mass wear loss is 1.2 mg, which is reduced by 43% compared with the pure NiCrBSi coating. When the loads are 6-10 N, the NiCrBSi-0.5Y2O3 composite coating suffers from slight wear and the wear mechanisms are mainly adhesive wear accompany with slight micro-cutting wear and micro-fracture wear. As the load increases to 12 N, the wear mechanisms are adhesive wear and severe micro-cutting wear. 展开更多
关键词 plasma spray composite coating NICRBSI Y2O3 friction WEAR
下载PDF
Preparation of Al_2O_3/Au nano-laminated composite coatings and their oxidation resistance on stainless steel 被引量:1
11
作者 高俊国 陆峰 +2 位作者 汤智慧 王长亮 何业东 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2012年第10期2491-2497,共7页
Al2O3/Au nano-laminated composite coatings were prepared by means of magnetron sputtering. The coating was compact and comprised of nano-laminated Al2O3 and Au layers. High temperature cyclic oxidation test was employ... Al2O3/Au nano-laminated composite coatings were prepared by means of magnetron sputtering. The coating was compact and comprised of nano-laminated Al2O3 and Au layers. High temperature cyclic oxidation test was employed to investigate the oxidation resistance of the composite coatings. The results revealed that the applied Al2O3/Au nano-laminated composite coatings improved the oxidation and spallation resistance of the stainless steel substrate significantly. The mechanism accounting for oxidation resistance was related with the suppression of inward oxygen diffusion and selective oxidation of Cr in the substrate. The mechanism accounting for spallation resistance was attributed to the relaxation of thermal stress by the nano-laminated structure. 展开更多
关键词 Al2O3/Au composite coatings magnetron sputtering oxidation resistance spallation resistance
下载PDF
Microstructure and properties of induction brazing nickel base/WC composite coating 被引量:2
12
作者 秦建 杨骄 +4 位作者 刘攀 刘大双 卢洪波 廖清泉 常云峰 《China Welding》 CAS 2023年第1期27-34,共8页
BNi-2/WC composite wear-resisting coating was prepared on carbon steel by the method of induction brazing.The microstructure and phase composition of the composite coating were analyzed,and the bonding strength and we... BNi-2/WC composite wear-resisting coating was prepared on carbon steel by the method of induction brazing.The microstructure and phase composition of the composite coating were analyzed,and the bonding strength and wear-resisting performance of the coating were tested.During the process of induction brazing,the tungsten carbide partially dissolves and reacts with the filler metal alloy to form NiW compound phase,which realizes the metallurgical combination of tungsten carbide and filler metal alloy.The matrix of the filler metal alloy consists of Ni solid solution and Ni_(3)B/Ni_(3)Si eutectic phase,and the metallurgical diffusion reaction occurs between the filler metal alloy and the steel matrix.The mechanical analysis results show that the self-strength of the composite coating reaches 140 MPa and the bonding strength of the filler metal alloy to the steel matrix reaches 360 MPa.The dry sand rubber wheel wear testing machine showed that the coating weight loss was only 0.2824 g,which was only 1/5 of the weight loss of 65 Mn matrix under the same conditions. 展开更多
关键词 composite coating induction brazing tungsten carbide BNI-2 wear resistance
下载PDF
Electrical resistivity of TiB_2/C composite cathode coating for aluminum electrolysis 被引量:6
13
作者 李劼 吕晓军 +2 位作者 李庆余 赖延清 杨建红 《Journal of Central South University of Technology》 EI 2006年第3期209-213,共5页
The electrical resistivity of TiB2/C cathode composite coating at different temperatures was measured with the electrical conductivity test device; the effects of TiB2 content and kinds of carbonaceous fillers as well... The electrical resistivity of TiB2/C cathode composite coating at different temperatures was measured with the electrical conductivity test device; the effects of TiB2 content and kinds of carbonaceous fillers as well as their mean particle size on their electrical resistivities were investigated. The results show that electrical resistivity of the coating decreases with the increase of TiB2 content and the decrease of its mean particle size. When the mass fraction of TiB2 increases from 30% to 60%, the electrical resistivity of the coating at room temperature decreases from 31.2μΩ·m to 23.8μΩ·m. The electrical resistivity of the coating at 960℃ lowers from 76.1μΩ· m to 38.4μΩ·m with the decrease of TiB2 mean particle size from 12μm to 1μm. The kinds of carbonaceous fillers have great influence on the electrical resistivity of TiB2/C composite coating at 960℃, when the graphite, petroleum coke and anthracite are used as fillers, the electrical resistivities of the coating are 20.3μΩ·m, 53.7μΩ·m and 87.2μΩ·m, respectively. For the coating with petroleum coke filler, its electrical resistivity decreases with the increase of the mean particle size of petroleum coke filler. The electrical resistivity at 960℃ decreases from 56.2μΩ·m to 48.2μΩ·m with the mean particle size of petroleum coke increasing from 44μm to 1200μm. However, too big carbonaceous particle size has adverse influence on the abrasion resistance of coating. Its proper mean particle size is 420μm. 展开更多
关键词 aluminum electrolysis composite material TiB2 coating electrical resistivity
下载PDF
Effect of MoSi_2 content on dielectric and mechanical properties of MoSi_2/Al_2O_3 composite coatings 被引量:5
14
作者 WU Zhi-hong ZHOU Wan-cheng +1 位作者 LUO Fa ZHU Dong-mei 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2012年第1期111-116,共6页
Molybdenum disilicide (MoSi2) sheath and aluminum oxide (Al2O3) core blended powders were fabricated by spray drying. A derived coating material was produced for the application as microwave absorbers using the as... Molybdenum disilicide (MoSi2) sheath and aluminum oxide (Al2O3) core blended powders were fabricated by spray drying. A derived coating material was produced for the application as microwave absorbers using the as prepared powders by atmospheric plasma spray (APS) technology. The effects of MoSi2/Al2O3 mass ratio on the dielectric and physical mechanical properties of the composite coatings were investigated. When the MoSi2 content of the composites increases from 0 to 45%, the flexure strength and fracture toughness improve from 198 to 324 MPa and 3.05 to 4.82 MPa-m1/2 then decline to 310 MPa and 4.67 MPa-m1/2, respectively. The dielectric loss tangent increases with increasing MoSi2 content, and the real part of permittivity decreases conversely over the frequency range of 8.2-12.4 GHz. These effects are due to the agglomeration of early molten MoSi2 particles and the increase of the electrical conductivity with increasing MoSi2 content. 展开更多
关键词 MoSi2/Al2O3 composite coating atmospheric plasma spraying mechanical properties dielectric properties
下载PDF
ELECTROPLATED Zn-Ni-SiO_(2) COMPOSITE COATINGS TREATED WITH A SILANE COUPLING AGENT TO REPLACE CHROMATING 被引量:4
15
作者 M.Hino M.Hiramatsu +2 位作者 K.Murakami A.Saijo T.Kanadani 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2005年第3期416-422,共7页
The fixing of a silane coupling agent to Zn-Ni-silica(SiO_(2))composite coatings was studied for the purpose of developing a coating process as an alternative to chromating.The corrosion resistance of Zn-Ni-silica com... The fixing of a silane coupling agent to Zn-Ni-silica(SiO_(2))composite coatings was studied for the purpose of developing a coating process as an alternative to chromating.The corrosion resistance of Zn-Ni-silica composite coatings was rem arkably improved by the silica nanoparticles in the composite,which were disper sed in the surface of this film.The silane coupling agent formed chemical bonds with the inorganic silica particles during the silane coupling treatment on the se composite coatings.The treatment suppressed the formation of white corrosion products to the same extent as chromating,as measured in salt spray tests.It is concluded that treating Zn-Ni-silica composite coatings with silane coupling agents is a viable alternative technique to chromating. 展开更多
关键词 ELECTRODEPOSITION Zn-Ni-SiO_(2)composite coating silane coupling reatment CHROME-FREE environmental friendlines
下载PDF
Abrasive wear characteristics and mechanisms of Al_2O_3/PA1010 composite coatings 被引量:3
16
作者 JIAXian LINGXiaomei 《Rare Metals》 SCIE EI CAS CSCD 2004年第1期59-63,共5页
The abrasive wear characteristics of Al_2O_3/PA1010 composite coatings on thesurface of quenched and low-temperature temper steel 45 were tested on the template abrasive weartesting machine and the same uncoated steel... The abrasive wear characteristics of Al_2O_3/PA1010 composite coatings on thesurface of quenched and low-temperature temper steel 45 were tested on the template abrasive weartesting machine and the same uncoated steel 45 was used as a reference material. Experimentalresults showed that the abrasive wear resistance of Al_2O_3/PA1010 composite coatings has a goodlinear relationship with the volume fraction of Al_2O_3 particles in Al_2O_3/PA1010 compositecoatings, and the linear correlative coefficient is 0.979. Under the experimental conditions, thesize of Al_2O_3 particles (40.5-161.0 μm) has little influence on the abrasive wear resistance ofAl_2O_3/PA1010 composite coatings. By treating the surface of Al_2O_3 particles with a suitablebonding agent, the distribution of Al_2O_3 particles in matrix PA1010 is more homogeneous and thebonding state between Al_2O_3 particles and matrix PA1010 is better. Therefore, the Al_2O_3particles in Al_2O_3/PA1010 composite coatings make the Al_2O_3/PA1010 composite coatings havebetter abrasive wear resistance than PA1010 coatings. The wear resistance of Al_2O_3/PA1010composite coatings is about 45% compared with that of steel 45. 展开更多
关键词 composite material coating abrasive wear Al_2O_3 NYLON
下载PDF
Preparation and tribological performance of electrodeposited Ni-TiB_2-Dy_2O_3 composite coatings 被引量:3
17
作者 刘小珍 李昕 +1 位作者 余艾冰 黄玮珏 《Journal of Rare Earths》 SCIE EI CAS CSCD 2009年第3期480-485,共6页
TiB2 and Dy2O3 were used as codeposited particles in the preparation of Ni-TiB2-Dy2O3 composite coatings to improve its performance. Ni-TiB2-Dy2O3 composite coatings were prepared by electrodeposition method with a ni... TiB2 and Dy2O3 were used as codeposited particles in the preparation of Ni-TiB2-Dy2O3 composite coatings to improve its performance. Ni-TiB2-Dy2O3 composite coatings were prepared by electrodeposition method with a nickel cetyltrimethylammonium bromide and hexadecylpyridinium bromide solution containing TiB2 and Dy2O3 particles. The content of codeposited TiB2 and Dy2O3 in the composite coatings was controlled by adding TiB2 and Dy2O3 particles of different concentrations into the solution, respectively. The effects of TiB2 and Dy2O3 content on microhardness, wear mass loss and friction coefficients of composite coatings were investigated. The composite coatings were characterized by X-ray diffraction (XRD), inductively coupled plasma-atomic emission spectrometer (ICP-AES) and scanning electron microscopy (SEM) techniques. Ni-TiBE-Dy2O3 composite coatings showed higher microhardness, lower wear mass loss and friction coefficient compared with those of the pure Ni coating and Ni-TiB2 composite coatings. The wear mass loss of Ni-TiB2-Dy2O3 composite coatings was 9 and 1.57 times lower than that of the pure Ni coating and Ni-TiB2 composite coatings, respectively. The friction coefficient of pure Ni coating, Ni-TiB2 and Ni-TiB2-Dy2O3 composite coatings were 0.723, 0.815 and 0.619, respectively. Ni-TiBE-Dy2O3 composite coatings displayed the least friction coefficient among the three coatings. Dy2O3 particles in composite coatings might serve as a solid lubricant between contact surfaces to decrease the friction coefficient and abate the wear of the composite coatings. The loading-bearing capacity and the wear-reducing effect of the Dy2O3 particles were closely related to the content of Dy2O3 particles in the composite coatings. 展开更多
关键词 ELECTRODEPOSITION composite coatings nickel TIB2 Dy2O3 friction and wear rare earths
下载PDF
Effect of Al_2O_3on Structure and Wearability of Composite Coating 被引量:1
18
作者 DING Hong-yan ZHANG Yue 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2004年第3期59-62,共4页
The composite coating was prepared by thermal spray welding after making composite powder,which is composed of Ni-based self-melted alloy and AlOceramic powder including nano,sub-micron and micron powders.The influenc... The composite coating was prepared by thermal spray welding after making composite powder,which is composed of Ni-based self-melted alloy and AlOceramic powder including nano,sub-micron and micron powders.The influences of contents and sizes of AlOon the structure and wearability were investigated.The results show that the wear resistance of the coating would be increased greatly by adding AlO,but the spray weldability decreases with increasing AlOcontent.So there is an optimal content of AlOpowder.The composite coating with AlOnano or sub-micron powder of 0.5% has the best abrasive resistance,while the optimal content of AlOmicron powder is 1 %. 展开更多
关键词 ceramic powder thermal spray welding composite coating AL2O3 NANO-POWDER
下载PDF
Influence of current density on nano-Al_2O_3/Ni+Co bionic gradient composite coatings by electrodeposition 被引量:1
19
作者 Yan Liu Luquan Ren +1 位作者 Sirong Yu Zhuwu Han 《Journal of University of Science and Technology Beijing》 CSCD 2008年第5期633-637,共5页
Metal and nano-ceramic nanocomposite coatings were prepared on the gray cast iron surface by the electrodeposition method. The Ni-Co was used as the metal matrix,and nano-Al2O3 was chosen as the second-phase particula... Metal and nano-ceramic nanocomposite coatings were prepared on the gray cast iron surface by the electrodeposition method. The Ni-Co was used as the metal matrix,and nano-Al2O3 was chosen as the second-phase particulates. To avoid poor inter-face bonding and stress distribution,the gradient structure of biology materials was found as the model and therefore the gradient composite coating was prepared. The morphology of the composite coatings was flatter and the microstructure was denser than that of pure Ni-Co coatings. The composite coatings were prepared by different current densities,and the 2-D and 3-D morphologies of the surface coatings were observed. The result indicated that the 2-D structure became rougher and the 3-D surface density of apices became less when the current density was increased. The content of nanoparticulates reached a maximum value at the current density of 40mA·cm^-2,at the same time the properties including microhardness and wear-resistance were analyzed. The microhardness reached a maximum value and the wear volume was also less at the current density of 40mA·cm^-2. The reason was that nano-Al2O3 particles caused dispersive strengthening and grain refining. 展开更多
关键词 ELECTRODEPOSITION composite coating current density NANO-AL2O3 microstructure mechanical properties
下载PDF
Laser Cladding Al-Si/Al_2O_3-TiO_2 Composite Coatings on AZ31B Magnesium Alloy 被引量:1
20
作者 崔泽琴 YANG Hongwei +2 位作者 王文先 WU Hongliang XU Bingshe 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2012年第6期1042-1047,共6页
To improve the wear resistance and corrosion resistance of magnesium alloys, a 5 kW continuous wave CO2 laser was used to investigate the laser surface cladding on AZ31 B magnesium alloys with Al-Si/Al2O3-TiO2 composi... To improve the wear resistance and corrosion resistance of magnesium alloys, a 5 kW continuous wave CO2 laser was used to investigate the laser surface cladding on AZ31 B magnesium alloys with Al-Si/Al2O3-TiO2 composite powders. A detailed microstructure, chemical composition, and phase analysis of the composite coatings were studied by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and X-ray diffraction (XRD). The laser cladding shows good metallurgical bonding with the substrate. The composite coatings are composed of Mgl7Al12, Al3Mg2, Mg2Si, Al2O3, and TiO2 phases. Compared to the average microhardness (50HV0.05) of the AZ3 1 B substrate, that of the composite coatings (230HV0.05) is improved significantly. The wear resistances of the surface layers were evaluated in detail. The results demonstrate that the wear resistances of the laser surface-modified samples are considerably improved compared to the substrate. It also show that the composite coatings exhibit better corrosion resistance than that of the substrate in 3.5wt% NaCI solution. 展开更多
关键词 AZ31B magnesium alloy laser cladding Al-Si/Al2O3-TiO2 composite coating wear resistance corrosion resistance