The supra fine particles of poly-o-toluidine were prepared in (OT + O/W mi-croemulsion) two phase system in which OT phase was used as monomer soure and the poly-o-toluidine was carried out in O/W micr0emulsion phase....The supra fine particles of poly-o-toluidine were prepared in (OT + O/W mi-croemulsion) two phase system in which OT phase was used as monomer soure and the poly-o-toluidine was carried out in O/W micr0emulsion phase. The particle size of poly-o-tolui-dine was about 5 nm.展开更多
文摘The supra fine particles of poly-o-toluidine were prepared in (OT + O/W mi-croemulsion) two phase system in which OT phase was used as monomer soure and the poly-o-toluidine was carried out in O/W micr0emulsion phase. The particle size of poly-o-tolui-dine was about 5 nm.