MECHANICAL STABILIZATION OF DEFORMED AUSTENITEDURING CONTINUOUS COOLING TRANSFORMATION IN AC-Mn-Cr-Ni-Mo PLASTIC DIE STEEL 被引量:7
1
作者 D.S.Liu G.D.Wang +1 位作者 X.H.Liu G.Z.Cui 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1998年第2期93-99,共7页
The influence of prior austenite deformed at different temperature on the subsequent continuous cooling bainitic transformation has been investigated in an C-Ma-Cr-Ni-Mo plastic die steel. The results show that the pr... The influence of prior austenite deformed at different temperature on the subsequent continuous cooling bainitic transformation has been investigated in an C-Ma-Cr-Ni-Mo plastic die steel. The results show that the prior deformation in low temperature region of austenite retards significantly the bainitic transformation. For the same continuous cooling schedule, as austenite deformed at lower temperature, the quantity of the classical sheaf-like bainite becomes less. The present results show that severe deformation leads to mechanical stabilization of austenite and causes the difficulty of bainitic ferrite propagation into the austenite. 展开更多
关键词 plastic die steel deformed austenite continuous cooling bainitic transformation mechanical stabilization of austenite
下载PDF
经济型P20塑料模具钢的组织与硬度研究 被引量:1
2
作者 斯松华 王锐 +1 位作者 张逖 王娜 《热处理》 CAS 2010年第5期31-34,共4页
设计了一种经济型JP 20塑料模具钢。试验结果表明,在热轧生产线上,通过控制冷却速度实现了20~50 mm厚度钢板的在线预硬化;热轧板组织为珠光体加少量晶界铁素体,硬度为280~330HB,达到了P 20塑料模具钢的预硬化硬度水平。JP 20钢热轧板在... 设计了一种经济型JP 20塑料模具钢。试验结果表明,在热轧生产线上,通过控制冷却速度实现了20~50 mm厚度钢板的在线预硬化;热轧板组织为珠光体加少量晶界铁素体,硬度为280~330HB,达到了P 20塑料模具钢的预硬化硬度水平。JP 20钢热轧板在一定的厚度范围内可替代P 20钢用于制作塑料模具。 展开更多
关键词 塑料模具钢 预硬化 控制冷却
下载PDF
非调质预硬型塑料模具钢P20的开发 被引量:3
3
作者 李行 秦坤 +3 位作者 任树洋 刘志勇 孟庆勇 尹绍江 《宽厚板》 2017年第6期41-43,共3页
唐钢在非调质预硬型塑料模具钢P20的研发过程中,合理地控制生产工艺,实施轧后堆垛缓冷,并根据模具钢堆垛缓冷却后获得硬度设定合理的回火热处理温度,得到了理想贝氏体组织,硬度值达到HRC28~32,满足了相关技术条件的要求。