Preparation,characterization and catalytic properties of S_2O_8^(2-)/ZrO_2-CeO_2 solid superacid catalyst 被引量:25
1
作者 樊国栋 沈茂 +1 位作者 张昭 贾发瑞 《Journal of Rare Earths》 SCIE EI CAS CSCD 2009年第3期437-442,共6页
A novel solid superacid catalyst S2O8^2-/ZrO2-CeO2 was prepared by a coprecipitation method and characterized by means of XRD FTIR, BET, TEM and DSC/TG analysis methods. The results indicated that incorporation of app... A novel solid superacid catalyst S2O8^2-/ZrO2-CeO2 was prepared by a coprecipitation method and characterized by means of XRD FTIR, BET, TEM and DSC/TG analysis methods. The results indicated that incorporation of appropriate amounts of Ce into the catalyst was beneficial to the formation of sole tetragonal ZrO2 and effectively prevented from the formation of monoclinic ZrO〉 and restrained the loss of sulfated species. XRD revealed the presence of tetragonal Ce0.16Zr0.84O2phase in the case of S2O8^2-/ZrO2-CeO2 calcined above 500 ℃. Catalytic activities of S2O8^2-/ZrO2-CeO2 for the esterification of lactic acid with n-butanol was studied. The results showed that the optimum conditions were as follows: calcination temperature of the catalyst 600 ℃, n(lactic acid):n(n-butyl alcohol)=1.0:3.0, w(S2O8^2-/ZrO2- CeO2)=12.0%, reaction temperature 145 ℃, and reaction time 2 h. The esterification efficiency of lactic acid was about 96.6%. 展开更多
关键词 solid superacid catalyst s2o8^2-/zro2-Ceo2 n-butyl lactate esterification rare earths
下载PDF
S_2O_8^(2-)/ZrO_2-Al_2O_3固体超强酸催化剂的研制与应用 被引量:46
2
作者 但悠梦 米远祝 田大听 《应用化学》 CAS CSCD 北大核心 2001年第10期840-842,共3页
A S 2O 2- 8/ZrO 2 Al 2O 3 type solid superacid catalyst was prepared from ZrOCl 2·8H 2O, AlCl 3· 6H 2O and (NH 4) 2S 2O 8 by coprecipitation, maceration and calcination processes. Their crystal structures an... A S 2O 2- 8/ZrO 2 Al 2O 3 type solid superacid catalyst was prepared from ZrOCl 2·8H 2O, AlCl 3· 6H 2O and (NH 4) 2S 2O 8 by coprecipitation, maceration and calcination processes. Their crystal structures and acidities were determined by XRD and Hammett method, respectively. The activity of the catalyst was studied as function of Al 2O 3 content, calcination temperature and time in the esterification of acetic acid with butanol, and a conversion of 96 5% was obtained. The catalyst gave also higher yields in syntheses of ketals and acetals: cyclohexanone ethylene ketal(86 2%), acetophenone ethylene ketal(78 5%), acetylacetic ester ketal(88 5%), benzaldehyde glycol acetal(76 3%). The chemical structures of the products were confirmed by IR spectra. 展开更多
关键词 s2o8^2-/zro2-al2o3 固体超强酸催化剂 酯化 缩酮化 缩醛化 制备 应用 氧化锆 氧化铝 硫酸 催化活性
下载PDF
固体超强酸S_2O^(2-)_8ZrO_2-Al_2O_3催化合成丙酸苄酯的研究 被引量:7
3
作者 但悠梦 《湖北民族学院学报(自然科学版)》 CAS 2002年第3期46-48,共3页
用固体超强酸S2 O2 -8 ZrO2 -Al2 O3催化苯甲醇与丙酸的酯化反应合成了丙酸苄酯 .实验结果表明 :S2 O2 -8 ZrO2 -Al2 O3具有较高的催化活性 .考察了苯甲醇与丙酸摩尔比、催化剂用量、反应温度、反应时间、带水剂环己烷用量对酯收率的影... 用固体超强酸S2 O2 -8 ZrO2 -Al2 O3催化苯甲醇与丙酸的酯化反应合成了丙酸苄酯 .实验结果表明 :S2 O2 -8 ZrO2 -Al2 O3具有较高的催化活性 .考察了苯甲醇与丙酸摩尔比、催化剂用量、反应温度、反应时间、带水剂环己烷用量对酯收率的影响 .在典型反应条件下 (苯甲醇与丙酸摩尔比 =1.2∶1,1.0g催化剂 0 .33mol丙酸 ,反应温度 16 0℃ ,反应时间 3.0h和 10ml环己烷 ) ,丙酸苄酯的收率可以达到 86 .6 % .该催化剂易于回收且可重复使用 。 展开更多