An antireflection (AR) coating is fabricated by applying an optimal spin-coating method and a pH-modified SiO2 nanoparticle solution on a cover glass. Because the pH value of the solution will affect the aggregation...An antireflection (AR) coating is fabricated by applying an optimal spin-coating method and a pH-modified SiO2 nanoparticle solution on a cover glass. Because the pH value of the solution will affect the aggregation and dispersion of the SiO2 particles, the transmittance of the AR-treated cover glass will be enhanced under optimal fabricated conditions. The experimental results show that an AR coating fabricated by an SiO2 nano- particle solution of pH 11 enhances the transmittance approximately by 3% and 5% under normal and oblique incident conditions, respectively. Furthermore, the AR-treated cover glass exhibits hydrophobicity and shows a 65% enhancement at a contact angle to bare glass.展开更多
基金financially supporting this research under Contract No. NSC 102-2221-E-155-076-MY3
文摘An antireflection (AR) coating is fabricated by applying an optimal spin-coating method and a pH-modified SiO2 nanoparticle solution on a cover glass. Because the pH value of the solution will affect the aggregation and dispersion of the SiO2 particles, the transmittance of the AR-treated cover glass will be enhanced under optimal fabricated conditions. The experimental results show that an AR coating fabricated by an SiO2 nano- particle solution of pH 11 enhances the transmittance approximately by 3% and 5% under normal and oblique incident conditions, respectively. Furthermore, the AR-treated cover glass exhibits hydrophobicity and shows a 65% enhancement at a contact angle to bare glass.