Sm-Mn离子取代锶铁氧体的制备及其表征
1
作者 余兆伟 吴泽 +3 位作者 单连伟 董丽敏 韩志东 张显友 《哈尔滨理工大学学报》 CAS 北大核心 2018年第1期46-50,共5页
采用高温固相法制备了Sr_(1-x)Sm_xFe_(12-x)Mn_xO_(19)(x=0~0.4)。利用XRD、SEM、VSM等表征手段对锶铁氧体的晶相、形貌和磁性能进行了表征。通过XRD分析发现当掺杂量0≤x<0.2时衍射峰基本没有出现杂峰,衍射峰的强度比较高,粉体为... 采用高温固相法制备了Sr_(1-x)Sm_xFe_(12-x)Mn_xO_(19)(x=0~0.4)。利用XRD、SEM、VSM等表征手段对锶铁氧体的晶相、形貌和磁性能进行了表征。通过XRD分析发现当掺杂量0≤x<0.2时衍射峰基本没有出现杂峰,衍射峰的强度比较高,粉体为结晶度比较高的单一六方相锶铁氧体。通过SEM发现随着掺杂量的增加晶体的晶粒尺寸逐渐增大;通过VSM分析发现:随着掺杂量的增大矫顽力Hc出现先增大后减小的趋势。测试结果表明:当掺杂量在x=0.2时Sm-Mn联合取代锶铁氧体的结晶度最好,矫顽力最大Hc=33.417 emu/g。 展开更多
关键词 sm-mn联合取代 固相法 磁性能
下载PDF
Sm掺量对Sm-MnO_(x)脱硝催化剂结构与性能的影响
2
作者 康天红 谢峻林 +2 位作者 刘小青 方德 公丕军 《武汉理工大学学报》 CAS 北大核心 2019年第2期13-18,共6页
用共沉淀法制备钐锰复合氧化物催化剂,考察不同Sm掺量对Sm-MnO_(x)催化剂结构及其低温脱硝活性的影响规律。结果表明,Sm的不同掺量对催化剂物相组成、微观形貌、孔结构等有不同的影响。Sm/Mn最佳摩尔比为0.10,此时Mn^(2+)和Sm^(3+)可以... 用共沉淀法制备钐锰复合氧化物催化剂,考察不同Sm掺量对Sm-MnO_(x)催化剂结构及其低温脱硝活性的影响规律。结果表明,Sm的不同掺量对催化剂物相组成、微观形貌、孔结构等有不同的影响。Sm/Mn最佳摩尔比为0.10,此时Mn^(2+)和Sm^(3+)可以均匀共沉淀,而得到Sm/Mn原子比接近0.1的钐锰复合氧化物球形结构;Sm掺量过低,不能很好改善锰氧化物的分散性;Sm掺量过高,部分Sm^(3+)会单独沉淀而使最终产物生成较多片状SmO晶体,降低催化剂脱硝性能。Sm/Mn摩尔比为0.10时,催化剂性能最佳,在100~240℃温度范围内,脱硝率保持在80%以上。 展开更多
关键词 钐锰复合氧化物 Sm掺量 脱硝
原文传递
Zn_2SiO_4(ZnB_2O_4):Mn^(2+),Sm^(3+)发光材料的制备与荧光性能 被引量:3
3
作者 张志伟 张卫国 牛少莉 《发光学报》 EI CAS CSCD 北大核心 2011年第2期144-148,共5页
使用高温固相法首次合成了Zn2SiO4(ZnB2O4)∶Mn2+,Sm3+发光材料,探讨了烧结温度、Sm3+含量对样品荧光性能的影响。利用X射线衍射(XRD)、荧光光谱等分析手段对Zn2SiO4(ZnB2O4)∶Mn2+,Sm3+粉末的结构、发光性能进行了表征。确定了该荧光... 使用高温固相法首次合成了Zn2SiO4(ZnB2O4)∶Mn2+,Sm3+发光材料,探讨了烧结温度、Sm3+含量对样品荧光性能的影响。利用X射线衍射(XRD)、荧光光谱等分析手段对Zn2SiO4(ZnB2O4)∶Mn2+,Sm3+粉末的结构、发光性能进行了表征。确定了该荧光材料的最佳合成条件,离子掺杂浓度等。实验结果表明:组成为Zn2SiO4(ZnB2O4)∶1.2%Mn2+,8%Sm3+的样品在950℃还原气氛下烧结,发光强度最高;反应生成的ZnB2O4和掺杂Sm3+可以大幅提高材料发光强度。 展开更多
关键词 Zn2SiO4(ZnB2O4):Mn2+ Sm3+ 发光材料 烧结温度 Sm3+含量
下载PDF
钐掺杂对锰锌铁氧体微波电磁性能的影响 被引量:5
4
作者 宋杰 许乃岑 +1 位作者 王丽熙 张其土 《中国稀土学报》 CAS CSCD 北大核心 2009年第3期414-418,共5页
采用固相法合成了钐掺杂的锰锌铁氧体Mn0.3Zn0.7Fe2-xSmxO4(x=0,0.01,0.02,0.04,0.06),通过XRD对合成粉末进行了晶体结构的分析,结果表明:当x≤0.02时,制得的粉体为相对较纯的尖晶石型铁氧体。稀土掺杂锰锌铁氧体的晶格常数随着掺钐量... 采用固相法合成了钐掺杂的锰锌铁氧体Mn0.3Zn0.7Fe2-xSmxO4(x=0,0.01,0.02,0.04,0.06),通过XRD对合成粉末进行了晶体结构的分析,结果表明:当x≤0.02时,制得的粉体为相对较纯的尖晶石型铁氧体。稀土掺杂锰锌铁氧体的晶格常数随着掺钐量的增加先增大后减少。使用Agilent8722ET网络分析仪在2~18GHz的频率范围内对其微波电磁特性进行测试,结果显示,当掺钐量为0.02时,在9~18GHz的频率范围内电磁参数ε′和ε″稍有增加,ε″最大值出现的位置移向低频。μ″和μ′峰值均大大增加,最大值分别达到6.2和5.5,该掺钐量下微波电磁性能最佳。利用微波电磁理论分析了电磁参数的变化机制。 展开更多
关键词 锰锌铁氧体 微波电磁特性 钐掺杂 稀土
下载PDF
Cr_2O_3改性PbTiO_3压电陶瓷材料的研究
5
作者 姜胜林 张绪礼 +1 位作者 王筱珍 万向红 《压电与声光》 CSCD 北大核心 1996年第1期58-61,共4页
研究了Cr2O3作为改性添加剂对(PbSm)(TiMn)O3系压电陶瓷介电及压电性能的影响.实验表明,添加适量的Cr2O3能得到压电性能好、压电各向异性大、压电稳定性高的优良材料,其kt=45%~50%,kt/kp=... 研究了Cr2O3作为改性添加剂对(PbSm)(TiMn)O3系压电陶瓷介电及压电性能的影响.实验表明,添加适量的Cr2O3能得到压电性能好、压电各向异性大、压电稳定性高的优良材料,其kt=45%~50%,kt/kp=15~18,TCft3=-0.8~-6ppm/℃.因此,在研究、开发高性能压电材料过程中,Cr2O3不失为一种优良的改性材料. 展开更多
关键词 压电陶瓷 压电各向异性 改性 添加剂
下载PDF
Gaseous Penetration of Sm into BaTiO3∶Mn0.006Smx Ceramics and Their NTC Effect
6
作者 郝素娥 黄金祥 孙亮 《Journal of Rare Earths》 SCIE EI CAS CSCD 2007年第S1期497-500,共4页
BaTiO3∶Mn0.006Smx(x=0.001, 0.002, 0.003, 0.004, 0.006 respectively) ceramics were prepared by using sol-gel method and their resistivities at different temperatures were measured. The results showed that Mn element m... BaTiO3∶Mn0.006Smx(x=0.001, 0.002, 0.003, 0.004, 0.006 respectively) ceramics were prepared by using sol-gel method and their resistivities at different temperatures were measured. The results showed that Mn element may enhance the PTC characteristics of BaTiO3 ceramics. But the doped Mn element deteriorated the room temperature resistivities of the modified BaTiO3 ceramics which were greater than 105 Ω·m. Then, rare earth element Sm was penetrated into BaTiO3∶Mn0.06Smx ceramics in gaseous state, which largely decreased the room temperature resistivity to 3.20 Ω·m, and appeared as a NTC effect instead of PTC effect. The forming mechanism of NTC effect was explored through analyses of SEM and electric properties of Sm-penetrated BaTiO3∶Mn0.006Smx ceramics. 展开更多
关键词 BaTiO_3 sm-mn co-doping gaseous penetration NTC effect rare earths
下载PDF
含Sm的Sb-Mn合金自生复合材料与磁性能
7
作者 潘冶 孙国雄 +2 位作者 汤崇熙 孙继科 廖恒成 《金属学报》 SCIE EI CAS CSCD 北大核心 2000年第3期319-324,共6页
采用 Bridgman法制备了 SmMnsb化合物在微米尺度上定向规则排列的含 Sin的 Sb-Mn合金自生复合材料,研究了 Sm对复合材料组织的影响和不同含 Sm量下的共晶平界面生长条件结果表明:加入 Sm使 Sb-Mn合... 采用 Bridgman法制备了 SmMnsb化合物在微米尺度上定向规则排列的含 Sin的 Sb-Mn合金自生复合材料,研究了 Sm对复合材料组织的影响和不同含 Sm量下的共晶平界面生长条件结果表明:加入 Sm使 Sb-Mn合金复合材料的磁化强度大幅度提高,并使其在室温和高温下均呈易轴磁化特征.但当含 Sm量为 5%时,出现富 Sm化合物相,磁化强度有所下降提高生长速度,形成一相枝品加两相共晶混和组织,尽管其磁化强度较完全两相共晶复合材料低,但仍高于不含 Sm的 MuSb/Sb共晶复合材料,并呈现出自旋重取向. 展开更多
关键词 复合材料 Sb-Mn合金 磁性能 定向凝固
下载PDF
铸态和挤压态Mg-4Sm-Al-0.3Mn-xZn合金微观组织和力学性能研究 被引量:3
8
作者 郑嫄 蔡中义 +2 位作者 程丽任 车朝杰 张洪杰 《材料导报》 EI CAS CSCD 北大核心 2019年第8期1354-1360,共7页
本工作通过光学显微镜(OM)、X射线衍射仪(XRD)、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、拉伸试验机对铸态和挤压态Mg-4SmAl-0.3Mn-x Zn(x=0、1、2、3)(质量分数)合金的微观组织及力学性能进行了研究。铸态、固溶态合金中观察到了Mg... 本工作通过光学显微镜(OM)、X射线衍射仪(XRD)、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、拉伸试验机对铸态和挤压态Mg-4SmAl-0.3Mn-x Zn(x=0、1、2、3)(质量分数)合金的微观组织及力学性能进行了研究。铸态、固溶态合金中观察到了Mg-Al-Sm三元析出相,它是一种长条形基面析出相,具有六方结构,其中a=0.556 nm,c=0.521 nm。该相与镁基体的位向关系为:[0001]_(Mg-Al-Sm)‖[0001]_(α-Mg),■_(Mg-Al-Sm)‖■_(α-Mg)。三种元素的原子比为Mg∶Al∶Sm=98.73∶0.71∶0.56。铸态合金中Mg-4Sm-Al-0.3Mn-3Zn合金具有最佳的拉伸性能,其屈服强度、抗拉强度和延伸率分别为96 MPa、138 MPa和7.2%。挤压态合金中Mg-4Sm-Al-0.3Mn-2Zn合金具有最佳的拉伸性能,其屈服强度、抗拉强度和延伸率分别为269 MPa、298 MPa和16%。 展开更多
关键词 Mg-Sm-Al-Mn-Zn 三元相 铸态 挤压态
下载PDF
Sm对挤压Mg-6Al-1.0Ca-0.5Mn镁合金微观组织及力学性能的影响 被引量:7
9
作者 房大庆 梁超 +3 位作者 张克维 武华杰 毕广利 柴跃生 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2017年第4期1110-1114,共5页
制备了Mg-6Al-1.0Ca-0.5Mn-x Sm(x=0.5,1.5,4.5,质量分数,%)合金,研究了合金的显微组织和力学性能。实验结果表明,随着Sm质量分数的增加,Al_2Sm相主要在晶内析出且体积分数增加,相反Mg_(17)Al_(12)相的体积分数降低;挤压后合金发生动态... 制备了Mg-6Al-1.0Ca-0.5Mn-x Sm(x=0.5,1.5,4.5,质量分数,%)合金,研究了合金的显微组织和力学性能。实验结果表明,随着Sm质量分数的增加,Al_2Sm相主要在晶内析出且体积分数增加,相反Mg_(17)Al_(12)相的体积分数降低;挤压后合金发生动态再结晶,晶粒细化。在室温条件下,含1.5%Sm合金显示了最佳的力学性能,其极限抗拉强度、屈服强度和伸长率分别为316 MPa,148 MPa和21.3%。该合金优异的力学性能主要是由于晶粒细化、Al_2Sm颗粒的弥散强化和减少Mg_(17)Al_(12)相的析出。 展开更多
关键词 挤压Mg-Al-Ca-Mn-Sm合金 显微结构 力学性能
原文传递