期刊文献+
共找到730篇文章
< 1 2 37 >
每页显示 20 50 100
Floating-roof steel tanks under harmonic settlement: FE parametric study and design criterion 被引量:1
1
作者 赵阳 曹庆帅 谢新宇 《Journal of Zhejiang University-Science A(Applied Physics & Engineering)》 SCIE EI CAS CSCD 2006年第3期398-406,共9页
Large vertical steel tanks for fluid storage are usually constructed on soft foundations, so it is not surprising that the tank wall will settle unevenly with the settlement of the foundation, thus inducing deformatio... Large vertical steel tanks for fluid storage are usually constructed on soft foundations, so it is not surprising that the tank wall will settle unevenly with the settlement of the foundation, thus inducing deformations and stresses in the tank. This work investigates the linear static behavior of floating-roof tanks under harmonic settlement through finite element (FE) analyses. The influences of the radius-to-thickness ratio, the height-to-radius ratio and the wind girder stiffness on the structural behavior are first analyzed. Comparisons between the circumferential stresses in the wind girder and the vertical stresses in the tank bottom are then made. The displacement and the stress along the tank height are also discussed, and the concept of tank division along its height is presented. Finally, a design approximation for the radial displacement at the tank top is developed based on FE results, and a settlement criterion based on the top radial displacement is proposed which can be used in practical design. 展开更多
关键词 钢结构罐 浮顶 谐波沉降 有限元法
下载PDF
Seismic assessment of unanchored steel storage tanks by endurance time method 被引量:4
2
作者 M. Alembagheri H.E. Estekanchi 《Earthquake Engineering and Engineering Vibration》 SCIE EI CSCD 2011年第4期591-603,共13页
Liquid storage tanks are essential structures that are often located in residential and industrial areas; thus an assessment of their seismic performance is an important engineering issue. In this paper, the seismic r... Liquid storage tanks are essential structures that are often located in residential and industrial areas; thus an assessment of their seismic performance is an important engineering issue. In this paper, the seismic response ofunanchored steel liquid storage tanks is investigated using the endurance time (ET) dynamic analysis procedure and compared to responses obtained for anchored tanks under actual ground motions and intensifying ET records. In most cases, the results from ground motions are properly obtained with negligible differences using ET records. It is observed that uplifting of the tank base, which is closely related to the tank aspect ratio, has the greatest significance in the responses of the tank and can be predicted with reasonable accuracy by using currently available ET records. 展开更多
关键词 steel liquid storage tanks endurance time method seismic assessment intensifying dynamic excitation tank base uplifting
下载PDF
GPR Tomographic Imaging of Concrete Tubes and Steel/Plastic Tanks Buried in IAG/USP Geophysical Test Site, Brazil
3
作者 Jorge Luís Porsani Emerson Rodrigo Almeida +1 位作者 Bruno Poluha Vinícius Rafael Neris dos Santos 《International Journal of Geosciences》 2017年第5期647-658,共12页
In this paper, the Ground Penetrating Radar (GPR) method was used to characterize concrete tubes and steel/plastic tanks buried in IAG/USP test site. The microwave tomography was used to improve the GPR images, aiming... In this paper, the Ground Penetrating Radar (GPR) method was used to characterize concrete tubes and steel/plastic tanks buried in IAG/USP test site. The microwave tomography was used to improve the GPR images, aiming to retrieve the geometry of the targets. The numerical modeling studies also were done in order to predict the GPR results of the buried targets and to give more reliability to the results interpretation. The targets were installed in the first shallow geophysical test site of the Brazil located at Institute of Astronomy, Geophysics, and Atmospheric Science (IAG) of the University of S?o Paulo (USP). GPR profiles of 200 MHz (shielded bistatic antennas) were acquired along three lines containing concrete tubes and steel/plastic tanks buried in subsoil. The concrete tubes show a hyperbolic reflector for the top, and the vertical tube also presented a reflection on its bottom. The horizontal steel tanks were characterized by a strong GPR reflection on their top. The empty plastic tank shows a strong reflector for the top with normal polarity. On the other hand, the plastic tank filled with water shows a weaker reflector for its top characterized by the inverted polarity of GPR signal when compared with empty plastic tank. The plastic tank filled with water also went characterized by the strong reflection to its bottom, being a good indicative to interpret GPR data on target in subsoil with some types of fluid inside of tank. The results of polarity difference for the top of tank can be used as guide pattern to identify buried tank empty or filled with water. The application of microwave tomography to the GPR data permitted to determine the position and get a good identification of the edges of the targets studied. The numeric modeling presented a good accordance with real data reducing the ambiguities in interpretation of results. These results can be used as a reference, and they can be extrapolated for areas where there is no subsurface information. 展开更多
关键词 Ground Penetrating Radar (GPR) Microwave Tomography Numeric Modeling CONCRETE TUBES steel tanks Plastic tanks IAG/USP Test SITE Brazil
下载PDF
Biodiesel Resistance of Thin Resin Cr-Free Steel Sheets for Fuel Tank
4
作者 Dong-Joo Yoon Kyung-Hwan Lee +2 位作者 Jong-Geun Choi Sangkeol Noh Jongsang Kim 《Engineering(科研)》 2011年第5期491-499,共9页
The content of biodiesel mixed with diesel fuel were compared to inspect the fuel resistance of thin resin Cr-free steel sheets, which are widely used as steel sheets of automobile fuel tank. Some additives which can ... The content of biodiesel mixed with diesel fuel were compared to inspect the fuel resistance of thin resin Cr-free steel sheets, which are widely used as steel sheets of automobile fuel tank. Some additives which can be presented during the process of biodiesel preparation were added for CCT (Cyclic Corrosion Test). These additives can accelerate the occurrence of corrosion. The corrosion was appeared on the coating and painting layer and in serious cases even substrate material was corroded. For methanol, mixing with blended fuel showed the reduction in corroded area as the additive concentration was reduced in the mixed fuel. Especially the peroxide hydrogen showed the strongest corrosiveness. It is known that formic acid has a tendency of weaker corrosiveness than peroxide hydrogen, but the corrosion is occurred throughout the specimen. Water is not mixed well with fuel, and does not seem to impact on corrosion significantly. However, water is easily mixed with other additives and is considered to facilitate the corrosion by other additives. 展开更多
关键词 FUEL RESISTANCE Cr-Free steel Sheet FUEL tank Corrosion Formic Acid PEROXIDE Hydrogen
下载PDF
聚脲涂覆大型钢制储罐抗冲击性能数值仿真
5
作者 张博一 蒋月新 +1 位作者 翟德保 王伟 《哈尔滨工业大学学报》 EI CAS CSCD 北大核心 2024年第6期44-51,共8页
为提高大型钢制储罐抗冲击性能,开展聚脲涂覆大型钢制储罐冲击响应的数值模拟和理论分析研究。基于前期工作已验证的数值模型,建立聚脲涂覆钢罐的有限元模型。数值模拟结果表明:将聚脲涂覆于罐体外表面能有效降低冲击载荷作用下局部塑... 为提高大型钢制储罐抗冲击性能,开展聚脲涂覆大型钢制储罐冲击响应的数值模拟和理论分析研究。基于前期工作已验证的数值模型,建立聚脲涂覆钢罐的有限元模型。数值模拟结果表明:将聚脲涂覆于罐体外表面能有效降低冲击载荷作用下局部塑性变形,在冲击体撞击角度为45°时能避免罐体穿孔破坏;聚脲涂层的主要防护机制为降速和垫层作用;提高喷聚脲涂厚度能增加罐体最大吸能值和面密度吸能值;当涂层厚度为15 mm时罐体不产生穿透破坏,满足英国储罐设计规范要求。根据罐体冲击响应特征和聚脲涂层作用机制,建立预测罐体断裂临界冲击速度的理论公式,能较精确预测涂覆罐的最大吸能值,可为聚脲涂覆钢制储罐抗冲击防护设计提供科学参考依据。 展开更多
关键词 钢制储罐 冲击 聚脲 数值模拟 预测公式
下载PDF
Life Cycle Assessment of Household Water Tanks—A Study of LLDPE, Mild Steel and RCC Tanks
6
作者 Kunal N. Shah Nanik S. Varandani Monika Panchani 《Journal of Environmental Protection》 2016年第5期760-769,共10页
A case of household water tanks, 1000 L capacity, made of RCC, LLDPE and mild steel (stainless steel) was evaluated for life cycle analysis. The scope of the research comprised of the raw materials, energy inputs and ... A case of household water tanks, 1000 L capacity, made of RCC, LLDPE and mild steel (stainless steel) was evaluated for life cycle analysis. The scope of the research comprised of the raw materials, energy inputs and corresponding emissions during all phases of product making such as extraction of raw material, it’s processing, followed by manufacturing and transport, as well as use and reuse of the product. Simapro 8 (System for Integrated environMental Assessment of PROducts), a modelling software, from Dutch PRé Consultants was used to conduct the life cycle analysis. Simapro 8 enables systematic and transparent modelling and analysis of complex life cycles based on the recommendations of the ISO 14040 series of standards. In the present study the most common method which is acceptable worldwide “Recipe Endpoint method” (ReCiPe) was employed. ReCiPe computes the impact categories and classifies them into two classes based on relevant arrays of characterization factors. Simapro addresses impact categories viz. ozone depletion, human toxicity, ionizing radiation, photochemical oxidant formation, particulate matter formation, terrestrial acidification, climate change, terrestrial ecotoxicity, agricultural land occupation, urban land occupation, natural land transformation, marine ecotoxicity, marine eutrophication, fresh water eutrophication, fresh water ecotoxicity, fossil fuel depletion, minerals depletion, fresh water depletion at the midpoint level. While at the Endpoint level, the impact categories are multiplied by corresponding damage factors and integrated to be represented as three Endpoint level categories, viz. human health, ecosystems and resource depletion. The three endpoint categories are normalized, weighted, and aggregated into a single score. LCA studies indicate that household water tanks of LLDPE have least environmental implications considering impacts on human health, ecosystems and resource depletion as compared to its counterparts viz. Household water tanks made up of mild steel and RCC. The sequence of the material with decreasing impacts is concrete tanks > mild steel tank > LLDPE tanks. The overall assessment is centred on the elements such as material inputs, energy inputs and environmental emissions. 展开更多
关键词 Life Cycle Assessment Water tanks Linear Low-Density Polyethylene (LLDPE) RCC Mild steel Recipe Endpoint Method
下载PDF
火箭贮箱结构材料应用及发展现状
7
作者 李雨 王建刚 +4 位作者 杨菊鹏 高士康 马领航 许子彦 周利 《宇航材料工艺》 CAS CSCD 北大核心 2024年第2期29-42,共14页
火箭贮箱是运载火箭的重要组成部件,但服役环境相对恶劣,在储存液体推进剂的同时还承担着复杂的结构载荷。结构材料是贮箱制造发展的根本,也是航天运载器变革的关键。本文主要介绍国内外运载火箭贮箱结构材料的应用及其发展现状,对铝合... 火箭贮箱是运载火箭的重要组成部件,但服役环境相对恶劣,在储存液体推进剂的同时还承担着复杂的结构载荷。结构材料是贮箱制造发展的根本,也是航天运载器变革的关键。本文主要介绍国内外运载火箭贮箱结构材料的应用及其发展现状,对铝合金、不锈钢、钛合金等金属材料以及复合材料贮箱进行了综述,系统性地总结了贮箱材料的变革历程和应用情况,并对未来贮箱材料的发展方向提出新的见解与展望。 展开更多
关键词 火箭贮箱 铝合金 复合材料 不锈钢 钛合金
下载PDF
鱼雷罐内加废钢对耐材影响分析
8
作者 蔡昌旺 李天学 《甘肃冶金》 2024年第1期25-28,共4页
对某钢厂25#鱼雷罐的耐材渣样进行分析,结果表明:25#鱼雷罐罐内残留渣成分与高炉渣成分相差较大,尤其MnO含量较高。通过扫描电镜分析可知,MnO、CaO等对铝碳化硅炭砖的骨料和基质熔损较大。25#鱼雷罐锥体出坑与此罐运转过程中,罐内局部... 对某钢厂25#鱼雷罐的耐材渣样进行分析,结果表明:25#鱼雷罐罐内残留渣成分与高炉渣成分相差较大,尤其MnO含量较高。通过扫描电镜分析可知,MnO、CaO等对铝碳化硅炭砖的骨料和基质熔损较大。25#鱼雷罐锥体出坑与此罐运转过程中,罐内局部渣铁成分发生巨大变化,其对铝碳化硅炭砖熔损较快,导致局部出坑。 展开更多
关键词 鱼雷罐 废钢 铝碳化硅炭砖 熔损
下载PDF
不同起爆条件下双钢壁LNG储罐抗爆性能分析
9
作者 于双锴 李晓琳 +4 位作者 芦烨 丁宇奇 尹青锋 李巧珍 谢清 《安全与环境工程》 CAS CSCD 北大核心 2024年第4期45-57,67,共14页
由于双钢壁储罐具有建造周期短、投资小等优点,在LNG储存中应用越来越广泛,但其易在外罐受到外部冲击时引发内罐的破坏。为了分析储罐在不同外爆载荷条件下的破坏行为,以双钢壁LNG储罐为研究对象,考虑内、外罐及保冷材料之间的载荷传递... 由于双钢壁储罐具有建造周期短、投资小等优点,在LNG储存中应用越来越广泛,但其易在外罐受到外部冲击时引发内罐的破坏。为了分析储罐在不同外爆载荷条件下的破坏行为,以双钢壁LNG储罐为研究对象,考虑内、外罐及保冷材料之间的载荷传递与相互作用,建立了外罐-保冷材料-内罐多介质的多相耦合有限元模型,并对多影响因素下储罐在外爆载荷作用下的破坏进行了分析,探究其抗爆性能。结果表明:在外爆载荷作用下,内、外罐从迎爆面中心向内凹陷直至发生破坏,最大应力均在迎爆面中心,且越靠近中心应力值越大;内、外罐材料均先达到屈服强度后发生塑性变形,随后达到失效应变值并发生破坏;与外罐相比,内罐发生破坏的时间晚42.9%,变形范围和破坏范围分别小12.3%、6.7%;储罐的抗爆性能随着储存液位的升高和罐体容积的增大而增强,随着起爆位置从罐壁中心向上、下两侧移动而提高,在罐壁中心起爆时储罐的破坏程度最大。该研究成果可为双钢壁LNG储罐的设计和储存液位的控制等方面提供理论参考依据。 展开更多
关键词 双钢壁LNG储罐 抗爆性能分析 外爆载荷 多相耦合有限元模型 失效准则
下载PDF
3t电弧炉炉膛扩容改造的实践
10
作者 王旭 王双捷 +8 位作者 付超 乔景忠 王雯 谭凤梅 宫伟祥 于博洋 高明 白禹韬 武玉平 《中国铸造装备与技术》 CAS 2024年第1期14-16,共3页
作者针对公司老龄3 t电弧炉冶炼钢水吨位小、单耗高的实际情况,通过对炉壳出钢口进行适度的改造,进而实现了炉膛的扩容和炉料的扩装,并通过加长出钢槽、增大出钢槽倾角措施,解决了由于出钢口提高而带来的钢水包吊车钢丝绳与电弧炉电极... 作者针对公司老龄3 t电弧炉冶炼钢水吨位小、单耗高的实际情况,通过对炉壳出钢口进行适度的改造,进而实现了炉膛的扩容和炉料的扩装,并通过加长出钢槽、增大出钢槽倾角措施,解决了由于出钢口提高而带来的钢水包吊车钢丝绳与电弧炉电极架相互碰撞问题,炉膛扩容改造后从原额定容量3 t扩容到了5 t,显著地提高了钢水冶炼效率,为老龄3 t电弧炉冶炼钢水节能降耗、增产增效提供了技术保障。 展开更多
关键词 电弧炉 炉体 炉壳 出钢槽 扩容 炼钢
下载PDF
9Ni钢焊接接头弯曲试验开裂分析
11
作者 杨伟锋 翁耿贤 +2 位作者 魏笑科 徐勋 沈洪涛 《船海工程》 北大核心 2024年第1期107-111,共5页
针对弯曲试验中9Ni钢焊接经常发生焊接接头试样开裂,焊接接头的质量不满足LNG液货罐产品的建造标准要求的问题,对9Ni钢焊接工艺进行改进,通过系列焊接试验,找出弯曲试样开裂的原因并制定相应的改进对策,将改进后的焊接工艺用于试板焊接... 针对弯曲试验中9Ni钢焊接经常发生焊接接头试样开裂,焊接接头的质量不满足LNG液货罐产品的建造标准要求的问题,对9Ni钢焊接工艺进行改进,通过系列焊接试验,找出弯曲试样开裂的原因并制定相应的改进对策,将改进后的焊接工艺用于试板焊接,试板焊接接头的各项力学性能满足规范要求,且附加的侧向弯曲试样弯曲后也没有出现开裂缺陷。将新焊接工艺应用于9 500 m^(3)LNG运输船C型液货罐的焊接,所有焊接试板均选用10 mm厚的侧弯试样弯曲检测合格,9Ni钢的焊接质量获得了船级社认可,侧弯试样的使用使焊接试板的长度尺寸缩减了一半,既提高了检测效率又节省了试验材料。 展开更多
关键词 LNG液货罐 9NI钢 焊接工艺 弯曲试验 开裂 对策
下载PDF
大型LNG储罐三种高效自动化焊接工艺对比研究
12
作者 房务农 蒋军 +4 位作者 郭广飞 刘孟德 周杨 汪正伟 李雪梅 《压力容器》 北大核心 2024年第1期25-32,共8页
我国建造储存绿色能源LNG用储罐单台已达27万m^(3),针对传统的SMAW焊接效率低、含有锰蒸汽和CO_(2)的烟尘等问题,采用热丝TIG,FCAW及MIG三种自动焊方法,进行了大量的试验研究,从而使LNG储罐的施焊环境大大改善,焊接效率及质量均大幅提... 我国建造储存绿色能源LNG用储罐单台已达27万m^(3),针对传统的SMAW焊接效率低、含有锰蒸汽和CO_(2)的烟尘等问题,采用热丝TIG,FCAW及MIG三种自动焊方法,进行了大量的试验研究,从而使LNG储罐的施焊环境大大改善,焊接效率及质量均大幅提升。结果表明,自动焊焊缝表面成形均远好于SMAW;焊接效率为MIG最高;焊接接头低温冲击韧性为热丝TIG最优。目前三种自动焊对现场组装精度要求均高于SMAW,热丝TIG对组装精度要求最高,因此尚需进一步提升自动化水平,以便在工程中大量推广应用。 展开更多
关键词 9%NI钢 大型LNG储罐 自动化焊接 力学性能
下载PDF
00Cr14Ni14Si4钢在1000 m^(3)储罐中的应用
13
作者 娄秀勇 《能源化工》 CAS 2024年第1期77-80,共4页
介绍了C4钢材料的性能、C4钢储罐的结构、钢储罐的应用现状及应用中的限制因素,00Cr14Ni14Si4钢因其优良的抗非致化态和敏化态晶间腐蚀及抗应力腐蚀的性能在浓硝酸生产储存中具有广泛应用。对00Cr14Ni14Si4钢储罐焊接、制造、检验和验... 介绍了C4钢材料的性能、C4钢储罐的结构、钢储罐的应用现状及应用中的限制因素,00Cr14Ni14Si4钢因其优良的抗非致化态和敏化态晶间腐蚀及抗应力腐蚀的性能在浓硝酸生产储存中具有广泛应用。对00Cr14Ni14Si4钢储罐焊接、制造、检验和验收的要求进行分析和总结,为C4钢在中型储罐上的应用提供了技术支持,从而保证储罐安全、经济合理使用。 展开更多
关键词 00Cr14Ni14Si4钢 浓硝酸 储罐
下载PDF
大型LNG储罐9%Ni钢焊接质量控制探讨
14
作者 赵鹏飞 张宁 +2 位作者 郑金涛 喻祺霖 郭海龙 《云南化工》 CAS 2024年第3期138-141,共4页
以国内在建的22万m~3大型LNG储罐为例,阐述了9%Ni钢焊接的质量控制要点。对9%Ni钢焊接的母材控制、焊材管理、焊接方法、焊评,以及无损检测等要素进行了质量控制分析,简要对比了9%Ni钢手工电弧焊和全自动TT焊接的优缺点、易产生的缺陷... 以国内在建的22万m~3大型LNG储罐为例,阐述了9%Ni钢焊接的质量控制要点。对9%Ni钢焊接的母材控制、焊材管理、焊接方法、焊评,以及无损检测等要素进行了质量控制分析,简要对比了9%Ni钢手工电弧焊和全自动TT焊接的优缺点、易产生的缺陷和预防措施,对焊接过程质量控制进行了总结分析。结果表明:控制手工电弧的焊接热输入是防止裂纹产生的重要措施,手工电弧焊焊接9%Ni钢时,应尽可能采用多层、多道焊接,且层间温度控制在100℃以下;全自动TIPTIG焊接(相比手工电弧焊),焊缝外观优美,焊接一次合格率更高,焊接过程的工艺参数可追溯性强,焊接产生的烟尘少,改善了焊工的职业健康。 展开更多
关键词 LNG储罐 9%NI钢 焊接 质量控制
下载PDF
动力集中动车组真空集便装置污物箱轻量化设计研究
15
作者 孙广合 曹磊 +5 位作者 田阳阳 刘志杰 周丽铭 李成 赵儒家 阎旭 《铁路节能环保与安全卫生》 2024年第1期26-35,共10页
动车组真空集便装置污物箱轻量化对于提高轨道车辆动力学特性、降低紧急刹车下的制动安全风险及降低制造工艺成本有积极意义。以时速160 km动力集中动车组真空集便装置污物箱为研究对象,利用有限元受力分析软件,依据相关标准试验条件和... 动车组真空集便装置污物箱轻量化对于提高轨道车辆动力学特性、降低紧急刹车下的制动安全风险及降低制造工艺成本有积极意义。以时速160 km动力集中动车组真空集便装置污物箱为研究对象,利用有限元受力分析软件,依据相关标准试验条件和参数设定要求,对污物箱进行静强度试验、稳态试验、模态试验和振动试验。参考模拟试验结果,在满足使用要求的基础上,对污物箱的系统结构进行轻量化方案研究。 展开更多
关键词 真空集便装置 污物箱 钢结构组成 有限元分析 轻量化设计
下载PDF
LNG储罐9Ni钢焊接接头射线检测试验研究与工程应用
16
作者 钱盛杰 王三军 +3 位作者 周鑫 张亮 王磊 张亮 《石油化工设备技术》 2024年第1期22-25,I0002,共5页
9Ni钢具有良好的机械性能、可焊性以及低温韧性,已广泛应用于LNG低温储罐。但由于LNG储罐焊缝余高的存在,9Ni钢材料的焊缝和母材对射线的吸收性不同,常规胶片技术的底片质量往往难以满足标准要求,给射线检测带来很大的困难。文章通过对... 9Ni钢具有良好的机械性能、可焊性以及低温韧性,已广泛应用于LNG低温储罐。但由于LNG储罐焊缝余高的存在,9Ni钢材料的焊缝和母材对射线的吸收性不同,常规胶片技术的底片质量往往难以满足标准要求,给射线检测带来很大的困难。文章通过对数字射线技术和常规胶片技术进行成像效果比对与分析,得出了数字射线技术的成像质量优于胶片技术的结论,再通过合理的工艺设置,成功解决了9Ni钢焊接接头检测难题。此外,文章还以某容积为20万m 3的LNG低温储罐为例,对数字射线技术在LNG安装工程项目中的应用情况进行了介绍,应用结果显示,数字射线技术在成像质量和检测工时两个方面具有显著优势,有望得到进一步的推广应用。 展开更多
关键词 LNG储罐 9NI钢 数字射线 对接焊缝
下载PDF
储罐9%Ni钢纵缝自动焊接技术应用分析
17
作者 方玉晨 《科技创新与应用》 2024年第10期59-62,共4页
对比分析目前国内外大型LNG储罐内罐常见的焊接方式及储罐现状,介绍SMAW(Shielded Metal Arc Welding)、FCAW(Flux Cored Arc Welding)及TT焊(TIP-TIG)的优缺点。根据试验发现,TT焊工艺对9%Ni钢焊缝成型好,过渡圆滑、鱼鳞纹规则且余高较... 对比分析目前国内外大型LNG储罐内罐常见的焊接方式及储罐现状,介绍SMAW(Shielded Metal Arc Welding)、FCAW(Flux Cored Arc Welding)及TT焊(TIP-TIG)的优缺点。根据试验发现,TT焊工艺对9%Ni钢焊缝成型好,过渡圆滑、鱼鳞纹规则且余高较小,热影响区宽度小,枝晶分布均匀,焊丝(条)熔敷率高、坡口较多为U型,且通过已在东部沿海某试运行的LNG储罐可知,其试运行稳定,并已投入使用。 展开更多
关键词 LNG储罐 9%NI钢 纵缝自动焊 TIP-TIG 焊接技术
下载PDF
邯钢新区铁钢界面汽车“一罐到底”运行实践
18
作者 刘志朝 程子波 王宗德 《炼钢》 CAS 北大核心 2024年第4期85-90,共6页
河钢集团邯钢新区系邯钢东区退城整合搬迁项目,受山区地形及土地面积限制,该项目采用紧凑式布局,高炉到转炉最近距离450 m,吨钢占地面积仅0.3 m 2,铁钢界面采用汽车“一罐到底”模式进行铁水驳运,铁水罐受铁完毕后10 min即可拉到炼钢生... 河钢集团邯钢新区系邯钢东区退城整合搬迁项目,受山区地形及土地面积限制,该项目采用紧凑式布局,高炉到转炉最近距离450 m,吨钢占地面积仅0.3 m 2,铁钢界面采用汽车“一罐到底”模式进行铁水驳运,铁水罐受铁完毕后10 min即可拉到炼钢生产,并运用了数字、物联网等新技术加以辅助,经过投产以来的改进优化,新区铁水罐周转率达到7.0次/日、进炼钢铁水温度1440℃、“一罐到底”比例99%,较搬迁前分别提高4.0次/日、98℃、39百分点;铁水温降降低到82℃,较搬迁前减少81℃,界面热量损耗大幅降低,为炼钢工序增钢降耗创造了有利条件,符合国家节能减排的理念,对行业“双碳”战略具有一定借鉴意义。 展开更多
关键词 铁钢界面 紧凑式 一罐到底 铁水罐周转率 铁水温降
下载PDF
关于液氢储罐内罐用奥氏体不锈钢的研发探讨
19
作者 杨作宏 《酒钢科技》 2024年第2期7-12,共6页
本文介绍了液氢储运储罐的结构特点、用材情况及产业应用发展状况;分析论述了液氢储罐内罐用奥氏体不锈钢的主要技术要求;简要介绍了内罐用钢的相关国家标准与团体标准;结合酒钢公司在氢能储运用钢方面的研发进展,提出了研发液氢储罐内... 本文介绍了液氢储运储罐的结构特点、用材情况及产业应用发展状况;分析论述了液氢储罐内罐用奥氏体不锈钢的主要技术要求;简要介绍了内罐用钢的相关国家标准与团体标准;结合酒钢公司在氢能储运用钢方面的研发进展,提出了研发液氢储罐内罐用系列奥氏体不锈钢的建议。 展开更多
关键词 液氢储罐 结构 奥氏体不锈钢
下载PDF
大型LNG储罐穹顶钢结构施工阶段受力分析
20
作者 付裕 苏娟 《低温建筑技术》 2024年第2期91-95,共5页
为揭示大型LNG储罐穹顶钢结构在施工过程中的受力特征,文中通过有限元模型建立了混凝土弹性模量与龄期关系,并利用生死单元模拟分环浇筑过程,得到浇筑工况下穹顶钢结构力学响应特征,给出了穹顶钢结构不同位置应力随混凝土龄期变化规律... 为揭示大型LNG储罐穹顶钢结构在施工过程中的受力特征,文中通过有限元模型建立了混凝土弹性模量与龄期关系,并利用生死单元模拟分环浇筑过程,得到浇筑工况下穹顶钢结构力学响应特征,给出了穹顶钢结构不同位置应力随混凝土龄期变化规律和穹顶最大位移分布特征,确定了最大位移随龄期变化关系表达式。结果表明浇筑过程中穹顶钢结构的应力和位移分布与混凝土龄期密切相关,浇筑初期穹顶钢结构位移最大,最大应力出现在浇筑区域附近。 展开更多
关键词 LNG储罐 混凝土弹塑性模型 穹顶钢结构
下载PDF
上一页 1 2 37 下一页 到第
使用帮助 返回顶部