TiB2/7050铝基复合材料风扇叶片锻件的研制 被引量:3
1
作者 谭志刚 赵兴东 +2 位作者 唐军 曾卫东 徐建伟 《热加工工艺》 CSCD 北大核心 2018年第11期114-116,119,共4页
应用等温模锻技术研制出Ti B2/7050铝基复合材料发动机风扇叶片,并对原始坯料和叶片进行了组织和力学性能测试。结果表明,原始坯料的纵向为纤维组织,力学性能较好;横向为等轴组织,力学性能稍差,各向异性明显。成形后Ti B2/7050复合材料... 应用等温模锻技术研制出Ti B2/7050铝基复合材料发动机风扇叶片,并对原始坯料和叶片进行了组织和力学性能测试。结果表明,原始坯料的纵向为纤维组织,力学性能较好;横向为等轴组织,力学性能稍差,各向异性明显。成形后Ti B2/7050复合材料叶片的各个部位的各向异性得到不同程度的改善。榫头纵向依然为纤维组织,拉伸性能略有下降,横向的等轴组织被一定程度拉长,力学性能比原始坯料稍有提高。叶身和叶尖的横、纵向组织都呈现细小的纤维状形貌,力学性能趋向一致,各向异性明显改善。 展开更多
关键词 tib2/7050铝基复合材料 风扇叶片 各向异性 等温锻造
下载PDF
Fabrication and analysis of TIG welding-brazing butt joints of in-situ TiB2/7050 composite and TA2
2
作者 Huan-huan Sun Yi-bo Ren +4 位作者 Yang Feng Hao-qiang Ba Dong Chen Chun-juan Xia Hao-wei Wang 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2021年第3期1062-1070,共9页
Lightweight hybrid structures of Al MMCs and titanium alloy dissimilar materials have great prospect in the defence industry application. So, it is necessary to join Al MMCs with Ti metal to achieve this structural de... Lightweight hybrid structures of Al MMCs and titanium alloy dissimilar materials have great prospect in the defence industry application. So, it is necessary to join Al MMCs with Ti metal to achieve this structural design. In this work, in-situ Ti B_(2)/7050 composite and TA2 were firstly attempted to join by TIG welding-brazing technique. The result was that the intact welding-brazing butt joint was successfully fabricated. The joint presents dual characteristics, being a brazing on TA2 side and a welding on Ti B_(2)/7050 side. At brazing joint side, ER4043 filler metal effectively wets on TA2 under TIG heating condition,and a continuous interfacial reaction layer with 1 e3 mm is formed at welded metal/TA2 interface. The whole interfacial reaction layers are composed of Ti(Al Si)3 intermetallic compounds(IMCs), but their morphologies at the different regions present obvious distinguishes. The microhardness of the reaction layers is as much as 141 e190 HV. At welding joints side, the fusion zone appears the equixaed crystal structure, and the grain sizes are much smaller than those of welded metal, which is attributed to the effect of Ti B2 particulates from the melted Ti B_(2)/7050 on acceleration formation and inhibiting growth for the new crystal nucleus. The tensile test results show that average tensile strength of the optimal welding-brazing joint is able to achieve 138 MPa. The failure of the tensile joint occurs by quasi-cleavage pattern, and the cracks initiate from the IMCs layer at the groove surface of TA2 and propagate into the welded metal. 展开更多
关键词 In-situ tib2/7050 composite TA2 TIG welding-brazing FABRICATION Analysis
下载PDF
电解铣削加工TiB_(2)/7050铝基复合材料阴极设计与试验验证 被引量:1
3
作者 崔振 李寒松 +2 位作者 何彬森 卢俞廷 蔡晶 《电加工与模具》 2023年第S01期38-43,共6页
为提高TiB_(2)/7050铝基复合材料电解铣削加工的加工效果,设计了三种具有不同底部出液孔形式的直径工具阴极,通过多组参数下的对比试验,优选出加工效果最好的工具阴极进行后续的试验探究。结果表明:在只改变加工电压的情况下,工具阴极C... 为提高TiB_(2)/7050铝基复合材料电解铣削加工的加工效果,设计了三种具有不同底部出液孔形式的直径工具阴极,通过多组参数下的对比试验,优选出加工效果最好的工具阴极进行后续的试验探究。结果表明:在只改变加工电压的情况下,工具阴极C有最高的材料去除率,工具阴极A可加工得最优的沟槽底面平整度。在加工电压30 V、进给速度70 mm/min下采用工具阴极C进行电解铣削加工,材料去除率和沟槽底面平整度分别达到581.9 mm3/min和0.16 mm,表面粗糙度值达Ra0.648μm。 展开更多
关键词 电解铣削 tib_(2)/7050铝基复合材料 材料去除率
下载PDF