Preparation and wear properties of TiB_2/Al-30Si composites via in-situ melt reactions under high-energy ultrasonic field 被引量:3
1
作者 张松利 董宪伟 +5 位作者 赵玉涛 刘满平 陈刚 张振坤 张宇荧 高雪华 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第12期3894-3900,共7页
TiB2/Al-30Si composites were fabricated via in-situ melt reaction under high-energy ultrasonic field. The microstructure and wear properties of the composite were investigated by XRD, SEM and dry sliding testing. The ... TiB2/Al-30Si composites were fabricated via in-situ melt reaction under high-energy ultrasonic field. The microstructure and wear properties of the composite were investigated by XRD, SEM and dry sliding testing. The results indicate that TiB2 reinforcement particles are uniformly distributed in the aluminum matrix under high-energy ultrasonic field. The morphology of the TiB2 particles is in circle-shape or quadrangle-shape, and the size of the particles is 0.1-1.5μm. The primary silicon particles are in quadrangle-shape and the average size of them is about 10μm. Hardness values of the Al-30Si matrix alloy and the TiB2/Al-30Si composites considerably increase as the high energy ultrasonic power increases. In particular, the maximum hardness value of the in-situ composites is about 1.3 times as high as that of the matrix alloy when the ultrasonic power is 1.2 kW, reaching 412 MPa. Meanwhile, the wear resistance of the in-situ TiB2/Al-30Si composites prepared under high-energy ultrasonic field is obviously improved and is insensitive to the applied loads of the dry sliding testing. 展开更多
关键词 tib2/al-30si composite in-situ melt reaction high-energy ultrasonic field wear properties
下载PDF
Mg对原位合成TiB_2/Al-7Si复合材料的微观组织及力学性能的影响 被引量:7
2
作者 赵瑞锋 刘忠侠 +4 位作者 杨明生 张天清 余焕伟 任波 刘栓江 《中国有色金属学报》 EI CAS CSCD 北大核心 2009年第9期1548-1554,共7页
采用K2TiF6和KBF4混合盐原位反应法制备TiB2/Al-7Si复合材料,利用XRD、SEM、金相显微镜、HV硬度测试和磨损实验等方法研究了Mg对复合材料的微观组织和力学性能的影响。结果表明:反应生成的TiB2颗粒平均尺寸约为0.5μm,材料的硬度和耐磨... 采用K2TiF6和KBF4混合盐原位反应法制备TiB2/Al-7Si复合材料,利用XRD、SEM、金相显微镜、HV硬度测试和磨损实验等方法研究了Mg对复合材料的微观组织和力学性能的影响。结果表明:反应生成的TiB2颗粒平均尺寸约为0.5μm,材料的硬度和耐磨性随着TiB2含量的增加而提高;添加1.5%Mg(质量分数)元素可明显细化TiB2颗粒,且使其分布更加均匀,增强TiB2颗粒的弥散强化和细晶强化效果,复合材料的硬度和耐磨性显著改善;过量的Mg元素(3%)会造成TiB2颗粒细化效果的下降,但其硬度和耐磨性能继续得到改善。 展开更多
关键词 tib2/al-7si复合材料 Mg 微观组织 硬度 力学性能
下载PDF
RE对原位TiB_2/Al-7Si复合材料组织及性能的影响 被引量:3
3
作者 李俊青 刘扭参 赵瑞锋 《铸造技术》 CAS 北大核心 2010年第9期1182-1186,共5页
采用混合盐反应法原位合成TiB2/Al-7Si复合材料,在添加适量Mg元素的基础上,研究了RE元素对复合材料微观组织和力学性能的影响。结果表明,加入适量RE元素,不仅能够细化α-Al和共晶Si相,而且能够增大TiB2颗粒与铝基体的润湿性,有效地阻止T... 采用混合盐反应法原位合成TiB2/Al-7Si复合材料,在添加适量Mg元素的基础上,研究了RE元素对复合材料微观组织和力学性能的影响。结果表明,加入适量RE元素,不仅能够细化α-Al和共晶Si相,而且能够增大TiB2颗粒与铝基体的润湿性,有效地阻止TiB2颗粒的团聚,使TiB2颗粒更加细小且分布均匀;加入0.6%RE后,硬度提高幅度约为12.9%,磨损失重量减少11%~19%,摩擦因数减小6%~12%,复合材料的硬度和耐磨性明显改善。 展开更多
关键词 tib2/al-7si复合材料 RE 微观组织 力学性能
下载PDF
Mg对原位合成TiB_2/Al-7Si复合材料的微观组织及力学性能的影响 被引量:1
4
作者 赵瑞锋 刘忠侠 +4 位作者 杨明生 张天清 余焕伟 任波 刘栓江 《特种铸造及有色合金》 CAS CSCD 北大核心 2008年第S1期309-313,共5页
通过向铝液中加入一定比例的KBF4和K2TiF6制备出了TiB2/Al-7Si复合材料,利用XRD,SEM,金相显微镜,硬度(HV)测试和磨损试验等材料分析方法研究了Mg对复合材料的微观组织和力学性能的影响。研究表明,K2TiF6和KBF4混合盐原位反应的生成物为... 通过向铝液中加入一定比例的KBF4和K2TiF6制备出了TiB2/Al-7Si复合材料,利用XRD,SEM,金相显微镜,硬度(HV)测试和磨损试验等材料分析方法研究了Mg对复合材料的微观组织和力学性能的影响。研究表明,K2TiF6和KBF4混合盐原位反应的生成物为平均尺寸为0.5μm左右的TiB2颗粒。复合材料的硬度和耐磨性随着TiB2含量的增加提高。添加1.5%的Mg改善了TiB2颗粒与铝液界面的润湿性,增加了合金熔体的粘度,阻碍了TiB2颗粒的团聚,明显细化了TiB2颗粒且分布更加均匀,增强了TiB2颗粒的弥散强化和细晶强化效果,复合材料的硬度和耐磨性显著改善。过量的Mg元素(3.0%)会造成TiB2颗粒细化效果的下降,但硬度和耐磨性能继续得到改善,这可能与合金凝固中析出的初晶Mg2Si颗粒和时效过程中析出β′或β″相有关。 展开更多
关键词 tib2/al-7si复合材料 Mg元素 微观组织 硬度 耐磨性能
下载PDF
工艺参数对原位合成TiB_2/Al-7Si复合材料微观组织的影响 被引量:1
5
作者 任波 赵瑞锋 +2 位作者 刘忠侠 刘扭参 张红松 《铸造》 CAS CSCD 北大核心 2017年第7期711-714,共4页
采用混合盐反应法在不同工艺参数下制备出TiB_2/Al-7Si复合材料,采用XRD、SEM和金相显微镜对复合材料的微观组织进行了分析。结果表明:TiB_2/Al-7Si复合材料主要由α-Al相、共晶Si相和TiB_2相组成;加盐温度过高或过低时,TiB_2颗粒由于... 采用混合盐反应法在不同工艺参数下制备出TiB_2/Al-7Si复合材料,采用XRD、SEM和金相显微镜对复合材料的微观组织进行了分析。结果表明:TiB_2/Al-7Si复合材料主要由α-Al相、共晶Si相和TiB_2相组成;加盐温度过高或过低时,TiB_2颗粒由于沉降或不易扩散而严重聚集,而反应时间过长或过短,TiB_2颗粒会出现沉降或反应不充分而聚集长大;当加盐温度为875℃,反应时间为20 min时,可获得尺寸细小、分布相对均匀的TiB_2/Al-7Si复合材料。 展开更多
关键词 tib3/al-7si复合材料 工艺参数 团聚 微观组织
下载PDF
Mechanical properties of Al-15Mg_(2)Si composites prepared under different solidification cooling rates 被引量:3
6
作者 E.Safary R.Taghiabadi M.H.Ghoncheh 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2022年第6期1249-1260,共12页
The effect of different cooling rates(2.7,5.5,17.1,and 57.5℃/s)on the solidification parameters,microstructure,and mechanical properties of Al-15Mg_(2)Si composites was studied.The results showed that a high cooling ... The effect of different cooling rates(2.7,5.5,17.1,and 57.5℃/s)on the solidification parameters,microstructure,and mechanical properties of Al-15Mg_(2)Si composites was studied.The results showed that a high cooling rate refined the Mg_(2)Si particles and changed their morphology to more compacted forms with less microcracking tendency.The average radius and fraction of primary Mg_(2)Si particles decreased from 20μm and 13.5%to about 10μm and 7.3%,respectively,as the cooling rate increased from 2.7 to 57.5℃/s.Increasing the cooling rate also improved the distribution of microconstituents and decreased the grain size and volume fraction of micropores.The mechanical properties results revealed that augmenting the cooling rate from 2.7 to about 57.5℃/s increased the hardness and quality index by 25%and245%,respectively.The high cooling rate also changed the fracture mechanism from a brittle-dominated mode to a high-energy ductile mode comprising extensive dimpled zones. 展开更多
关键词 al-15Mg_(2)si composite solidification cooling rate thermal analysis mechanical properties
下载PDF
原位生成TiB_2/Al-Si-Mg复合材料的组织与性能 被引量:10
7
作者 韩延峰 刘相法 边秀房 《中国有色金属学报》 EI CAS CSCD 北大核心 2001年第5期840-845,共6页
结合LSM法和MCR法原位反应生成TiB2 粒子增强Al Si Mg复合材料。研究发现 :原位生成TiB2 粒子呈等轴状且尺寸 <1μm ,大都均匀分布在共晶组织中 ,与共晶Si交织在一起 ,在α(Al)中只有少量的TiB2 粒子 ;原位TiB2 粒子可明显强化Al Si... 结合LSM法和MCR法原位反应生成TiB2 粒子增强Al Si Mg复合材料。研究发现 :原位生成TiB2 粒子呈等轴状且尺寸 <1μm ,大都均匀分布在共晶组织中 ,与共晶Si交织在一起 ,在α(Al)中只有少量的TiB2 粒子 ;原位TiB2 粒子可明显强化Al Si Mg复合材料 ,且随着TiB2 粒子数量的增加 ,强化效果也随之提高 ,而且延伸率也略有升高 ,如 6 %TiB2 /ZL10 4复合材料室温拉伸强度可达 2 96MPa ,延伸率为 5 .5 %;热处理 (T6)可将共晶Si由原先的连续棒状变为孤立的颗粒状 ,大幅度提高材料抗拉强度 ,使 6 %TiB2 /ZL10 4复合材料室温拉伸强度达386MPa 。 展开更多
关键词 tib2/al-si-Mg复合材料 原位反应 显微组织 力学性能
下载PDF
SiC_(f)/SiC复合材料表面Si/Yb_(2)Si_(2)O_(7)涂层1350℃抗热冲击和抗热冲刷性能研究
8
作者 陈易诚 邓杨芳 +3 位作者 张乐 韦林 李其连 周国栋 《材料保护》 CAS CSCD 2024年第8期58-64,104,共8页
为了研究Si/Yb_(2)Si_(2)O_(7)涂层在1350℃条件下的抗热冲击和抗热冲刷性能,首先在SiC_(f)/SiC复合材料上采用真空等离子喷涂技术制备了Si/Yb_(2)Si_(2)O_(7)涂层,并采用金相、物相、SEM、EDS、燃气热冲击设备和燃气热冲刷设备对试样... 为了研究Si/Yb_(2)Si_(2)O_(7)涂层在1350℃条件下的抗热冲击和抗热冲刷性能,首先在SiC_(f)/SiC复合材料上采用真空等离子喷涂技术制备了Si/Yb_(2)Si_(2)O_(7)涂层,并采用金相、物相、SEM、EDS、燃气热冲击设备和燃气热冲刷设备对试样进行了结构及性能表征。结果表明:涂层与SiC_(f)/SiC复合材料的结合强度为25.01 MPa。经过1350℃燃气热冲击1000次,1350℃、550 m/s燃气热冲刷1 h后,Yb_(2)Si_(2)O_(7)涂层的表面物相均主要为Yb_(2)Si_(2)O_(7)、Yb_(2)SiO_(5)、Yb_(2)O_(3)和SiO_(2),抗热冲击和抗热冲刷2项性能测试结果均达设计要求。涂层结合强度很高,复合材料、Si层和Yb_(2)Si_(2)O_(7)层耐高温且热匹配性能较好,且面层的抗燃气腐蚀能力很强,是涂层热冲击、热冲刷性能良好的主要原因。燃气热冲刷的燃气燃烧时间比燃气热冲击的总时间短,且热冲刷为恒温连续冲刷,无冷热的剧烈交替变化,故燃气冲刷后涂层边缘处靠近工装装卡的地方未见明显开裂,且连续冲刷后的黑色烧蚀区域较燃气热冲击的面积小。 展开更多
关键词 siCf/siC复合材料 si/Yb_(2)si_(2)O_(7)涂层 真空等离子喷涂 抗热冲击 抗热冲刷
下载PDF
Mg对原位合成5TiB_2/Al-7Si复合材料冲击性能的影响
9
作者 任波 赵瑞锋 +2 位作者 刘忠侠 刘扭参 张红松 《特种铸造及有色合金》 CAS CSCD 北大核心 2018年第9期1003-1007,共5页
采用混合盐原位反应方法制备了不同TiB_2含量的TiB_2/Al-7Si复合材料,研究了TiB_2含量和Mg含量对复合材料冲击性能的影响。随TiB_2或Mg含量的增加,复合材料中的α-Al相和共晶Si细化,但冲击性能均呈下降趋势。未添加TiB_2和Mg时,Al-7Si... 采用混合盐原位反应方法制备了不同TiB_2含量的TiB_2/Al-7Si复合材料,研究了TiB_2含量和Mg含量对复合材料冲击性能的影响。随TiB_2或Mg含量的增加,复合材料中的α-Al相和共晶Si细化,但冲击性能均呈下降趋势。未添加TiB_2和Mg时,Al-7Si合金的冲击韧度最高,约为14.2J/cm^2,加入5%的TiB_2后,冲击韧度降低至12.6J/cm^2,再加入1.5%和3%的Mg后,冲击韧度进一步降低至10.9和10.4J/cm^2。5TiB_2/Al-7Si复合材料断口形貌主要呈韧窝和准解理断裂,具有混合型断口特征。 展开更多
关键词 tib2/al-7si复合材料 Mg含量 冲击性能
原文传递