A new improved two-step method in fabricating Tl_(2)Ba_(2)CaCu_(2)O_(8)(Tl-2212)thin films is presented in this paper.In the first process of dc magnetron sputtering,the thallium content in the precursor film is large...A new improved two-step method in fabricating Tl_(2)Ba_(2)CaCu_(2)O_(8)(Tl-2212)thin films is presented in this paper.In the first process of dc magnetron sputtering,the thallium content in the precursor film is largely increased by adjusting the ratio of thallium in the sputtering targets.After the second annealing process in the absence of additional thallium pellets or powder source,high-quality Tl-2212 thin films can be obtained.The proper content of thallium in the precursor film provides a relatively stable atmosphere to guarantee the growth of Tl-2212 film.This method avoids the repeated production of the thallium pellets in the post-annealing process,the repeatability and controllability of the experiment are greatly improved.X-ray diffraction(XRD)scans show that all of the sharp peaks of the sample films can be assigned to the(00 l)peaks of Tl-2212 phase.The highest superconducting critical temperature(T_(c))of the films is 105 K and the critical current density(J_(c))can achieve 1.93 MA/cm^(2) in zero magnetic field at 77 K for a 600 nm film.展开更多
The rocking curve of Tl-2212 thin films in Fig.2 of our original paper[1]should be replaced with the following new one.Accordingly,in the fifth paragraph of Section 3 of the original paper,the statement“The full widt...The rocking curve of Tl-2212 thin films in Fig.2 of our original paper[1]should be replaced with the following new one.Accordingly,in the fifth paragraph of Section 3 of the original paper,the statement“The full width at half maximum(FWHM)of the(0012)peak of the Tl-2212 phase is about 0.24°”should be“The full width at half maximum(FWHM)of the(0012)peak of the Tl-2212 phase is about 0.42°”.展开更多
YBa2Cu3O7-δ and Tl2Ba2CaCu2O8 thin films for microwave filters were synthesized by pulsed laser deposition and the two-step thalliation process. Substrate quality requirements and the relation of thin film morphology...YBa2Cu3O7-δ and Tl2Ba2CaCu2O8 thin films for microwave filters were synthesized by pulsed laser deposition and the two-step thalliation process. Substrate quality requirements and the relation of thin film morphology, microstructure with microwave surface resistance were discussed.展开更多
基金Project supported by the National Natural Science Foundation of China(Grant No.51002081)the Fundamental Research Funds for the Central Universities,Chinathe Research Program of Application Foundation and Advanced Technology of Tianjin,China(Grant No.15JCQNJC01300)
文摘A new improved two-step method in fabricating Tl_(2)Ba_(2)CaCu_(2)O_(8)(Tl-2212)thin films is presented in this paper.In the first process of dc magnetron sputtering,the thallium content in the precursor film is largely increased by adjusting the ratio of thallium in the sputtering targets.After the second annealing process in the absence of additional thallium pellets or powder source,high-quality Tl-2212 thin films can be obtained.The proper content of thallium in the precursor film provides a relatively stable atmosphere to guarantee the growth of Tl-2212 film.This method avoids the repeated production of the thallium pellets in the post-annealing process,the repeatability and controllability of the experiment are greatly improved.X-ray diffraction(XRD)scans show that all of the sharp peaks of the sample films can be assigned to the(00 l)peaks of Tl-2212 phase.The highest superconducting critical temperature(T_(c))of the films is 105 K and the critical current density(J_(c))can achieve 1.93 MA/cm^(2) in zero magnetic field at 77 K for a 600 nm film.
文摘The rocking curve of Tl-2212 thin films in Fig.2 of our original paper[1]should be replaced with the following new one.Accordingly,in the fifth paragraph of Section 3 of the original paper,the statement“The full width at half maximum(FWHM)of the(0012)peak of the Tl-2212 phase is about 0.24°”should be“The full width at half maximum(FWHM)of the(0012)peak of the Tl-2212 phase is about 0.42°”.
基金The authors are grateful for the measurement of Rs by the University of Electronic Science andTechnology, Chengdu, and the fabrication of filters by the Institute 55, Nanjing. We are also thankful for Prof. Y. F. Chen for her useful discussion and read
文摘YBa2Cu3O7-δ and Tl2Ba2CaCu2O8 thin films for microwave filters were synthesized by pulsed laser deposition and the two-step thalliation process. Substrate quality requirements and the relation of thin film morphology, microstructure with microwave surface resistance were discussed.