Broadening and height reduction of X-ray diffraction peaks were observed after cold-pressing of unmilled Co-W powder mixture. It seems the effect of cold pressing has slightly reduced the lattice parameter of W from 3...Broadening and height reduction of X-ray diffraction peaks were observed after cold-pressing of unmilled Co-W powder mixture. It seems the effect of cold pressing has slightly reduced the lattice parameter of W from 3.165 to 3.143?. Consequent annealing of unmilled compacts yielded metastable phases. Upon 10 and 20 h ball milling of Co-W powder, no alloying was obtained. Although milling did not yield significant crystal changes in W and Co ground state structures, its effect is evident during subsequent annealing. An eta phase is obtained for the first time from unmilled-annealed Co-W powder mixture in the absence of interstitial elements like carbon, while the milled counterpart yielded the rhombohedral Co7W6-type phase with composition deviated from stoichiometric value.展开更多
Mechanically activated W-Cu powders were sintered by a spark plasma sinteringsystem (SPS) in order to develop a new process and improve the properties of the alloy. Propertiessuch as density and hardness were measured...Mechanically activated W-Cu powders were sintered by a spark plasma sinteringsystem (SPS) in order to develop a new process and improve the properties of the alloy. Propertiessuch as density and hardness were measured. The microstructures of the sintered W-Cu alloy sampleswere observed by SEM (scanning electron microscope). The results show that spark plasma sinteringcan obviously lower the sintering temperature and increase the density of the alloy. This processcan also improve the hardness of the alloy. SPS is an effective method to obtain W-Cu powders withhigh density and superior physical properties.展开更多
The effects of microwave sintering on the properties, phases and microstructure of W-2OCu alloy, using composite powder fabricated by spray pyrolysis-continuous reduction technology, were investigated. Compared with t...The effects of microwave sintering on the properties, phases and microstructure of W-2OCu alloy, using composite powder fabricated by spray pyrolysis-continuous reduction technology, were investigated. Compared with the conventional hot-press sintering, microwave sintering to W-2OCu composites could be achieved with lower sintering temperature and shorter sintering time. Furthermore, microwave sintered W-Cu composites with high densification, homogenous microstructure and excellent properties were obtained. Microwave sintering could also result in finer microstructures. :~展开更多
The effects of preheating temperature and W powder size on the Self propagating High temperature Synthesis(SHS) of Ti W C system were studied. Preheated mixtures and the decrease of W powder size can accelerate the fo...The effects of preheating temperature and W powder size on the Self propagating High temperature Synthesis(SHS) of Ti W C system were studied. Preheated mixtures and the decrease of W powder size can accelerate the formation of (W,Ti)C powders. The uniphase (W,Ti)C (WC∶TiC=5∶5) powders with 0.32% free carbon were synthesized from Ti, W, C powders by SHS. The powder size of the product was 3~5 μm.展开更多
W-15% Cu (mass fraction) alloys were sintered with mechanically activated powder in order to develop new preparing processes and improve properties of alloys. The microstructures of the activated powder and the sinter...W-15% Cu (mass fraction) alloys were sintered with mechanically activated powder in order to develop new preparing processes and improve properties of alloys. The microstructures of the activated powder and the sintered alloy were observed. Properties such as density were measured. The results show that through mechanical activation, the particle size of the powder becomes finer to sub-micron or nanometer level, some copper was soluble in tungsten, and high density W-Cu alloys can be obtained by mechanically activated powder for its action to the activation sintering.展开更多
Cu(NO3)(2) and (NH4)(6)H(2)W(12)O(40)center dot 4H(2)O were used to prepare W/Cu nanosized composite powder by sol-gel technique. The influences of heat treatment process, pH value of the solution and the amount of an...Cu(NO3)(2) and (NH4)(6)H(2)W(12)O(40)center dot 4H(2)O were used to prepare W/Cu nanosized composite powder by sol-gel technique. The influences of heat treatment process, pH value of the solution and the amount of an addition agent on particle size were investigated by DSC, XRD and TEM. The results show that, at a certain heat treatment temperature, the W/Cu nanoparticle size increases with the pH value or the amount of the addition agent increasing.展开更多
A direct electroless copper (Cu) coating on tungsten powders method requiring no surface treatment or stabilizing agent and using glyoxylic acid (C2H203) as a reducing agent was reported. The effects of copper sul...A direct electroless copper (Cu) coating on tungsten powders method requiring no surface treatment or stabilizing agent and using glyoxylic acid (C2H203) as a reducing agent was reported. The effects of copper sulfate concentration and the pH of the plating solution on the properties of the prepared W@Cu composite powders were assessed. The content of Cu in the composite powders was controlled by adjusting the concentration of copper sulfate in the electroless plating solution. A uniform, dense, and consistent Cu coating was obtained under the established optimum conditions (flow rate of C2H203 = 5.01 mL/min, solution pH = 12.25 and reaction temperature 45.35℃) by using central composite design method. In addition, the crystalline Cu coating was evenly dispersed within the W@Cu composite powders and Cu element in the coating existed as Cu~. The formation mechanism for the W@Cu composite powders by electroless plating in the absence of surface treatment and stabilizing agent was also proposed.展开更多
The effects of microwave sintering and conventional H2 sintering on the microstructure and properties of W-15Cu alloy using ultrafine W-15Cu composite powder fabricated by spray drying & calcining-continuous reductio...The effects of microwave sintering and conventional H2 sintering on the microstructure and properties of W-15Cu alloy using ultrafine W-15Cu composite powder fabricated by spray drying & calcining-continuous reduction technology were investigated. In comparison to the conventional HE sintering processing, microwave sintering to W-15Cu can be achieved at lower sintering temperature and shorter sintering time. Furthermore, higher performances in microwave sintered compacts were obtained, but high microwave sintering temperature or long microwave sintering time could result in coarser microstructures.展开更多
文摘Broadening and height reduction of X-ray diffraction peaks were observed after cold-pressing of unmilled Co-W powder mixture. It seems the effect of cold pressing has slightly reduced the lattice parameter of W from 3.165 to 3.143?. Consequent annealing of unmilled compacts yielded metastable phases. Upon 10 and 20 h ball milling of Co-W powder, no alloying was obtained. Although milling did not yield significant crystal changes in W and Co ground state structures, its effect is evident during subsequent annealing. An eta phase is obtained for the first time from unmilled-annealed Co-W powder mixture in the absence of interstitial elements like carbon, while the milled counterpart yielded the rhombohedral Co7W6-type phase with composition deviated from stoichiometric value.
基金This work was financially supported by the National Natural Science Foundation of China (No. 50174007)
文摘Mechanically activated W-Cu powders were sintered by a spark plasma sinteringsystem (SPS) in order to develop a new process and improve the properties of the alloy. Propertiessuch as density and hardness were measured. The microstructures of the sintered W-Cu alloy sampleswere observed by SEM (scanning electron microscope). The results show that spark plasma sinteringcan obviously lower the sintering temperature and increase the density of the alloy. This processcan also improve the hardness of the alloy. SPS is an effective method to obtain W-Cu powders withhigh density and superior physical properties.
基金the Project for Science and Technology Plan of Wuhan City (No. 200910321092)the Youth Science Plan for Light of the Morning Sun of Wuhan City (No. 200750731270)the Fundamental Research Funds for the Central Universities (No. 2010-Ⅱ-020)
文摘The effects of microwave sintering on the properties, phases and microstructure of W-2OCu alloy, using composite powder fabricated by spray pyrolysis-continuous reduction technology, were investigated. Compared with the conventional hot-press sintering, microwave sintering to W-2OCu composites could be achieved with lower sintering temperature and shorter sintering time. Furthermore, microwave sintered W-Cu composites with high densification, homogenous microstructure and excellent properties were obtained. Microwave sintering could also result in finer microstructures. :~
文摘The effects of preheating temperature and W powder size on the Self propagating High temperature Synthesis(SHS) of Ti W C system were studied. Preheated mixtures and the decrease of W powder size can accelerate the formation of (W,Ti)C powders. The uniphase (W,Ti)C (WC∶TiC=5∶5) powders with 0.32% free carbon were synthesized from Ti, W, C powders by SHS. The powder size of the product was 3~5 μm.
文摘W-15% Cu (mass fraction) alloys were sintered with mechanically activated powder in order to develop new preparing processes and improve properties of alloys. The microstructures of the activated powder and the sintered alloy were observed. Properties such as density were measured. The results show that through mechanical activation, the particle size of the powder becomes finer to sub-micron or nanometer level, some copper was soluble in tungsten, and high density W-Cu alloys can be obtained by mechanically activated powder for its action to the activation sintering.
基金This Project was financially supported by the National Natural Science Foundation of China (No. 50471033).
文摘Cu(NO3)(2) and (NH4)(6)H(2)W(12)O(40)center dot 4H(2)O were used to prepare W/Cu nanosized composite powder by sol-gel technique. The influences of heat treatment process, pH value of the solution and the amount of an addition agent on particle size were investigated by DSC, XRD and TEM. The results show that, at a certain heat treatment temperature, the W/Cu nanoparticle size increases with the pH value or the amount of the addition agent increasing.
基金Funded by the National Natural Science Foundation of China(Nos.51202175 and 11072228)the National 111 Project(No.B13035)
文摘A direct electroless copper (Cu) coating on tungsten powders method requiring no surface treatment or stabilizing agent and using glyoxylic acid (C2H203) as a reducing agent was reported. The effects of copper sulfate concentration and the pH of the plating solution on the properties of the prepared W@Cu composite powders were assessed. The content of Cu in the composite powders was controlled by adjusting the concentration of copper sulfate in the electroless plating solution. A uniform, dense, and consistent Cu coating was obtained under the established optimum conditions (flow rate of C2H203 = 5.01 mL/min, solution pH = 12.25 and reaction temperature 45.35℃) by using central composite design method. In addition, the crystalline Cu coating was evenly dispersed within the W@Cu composite powders and Cu element in the coating existed as Cu~. The formation mechanism for the W@Cu composite powders by electroless plating in the absence of surface treatment and stabilizing agent was also proposed.
基金Funded by the Project for Science and Technology Plan of Wuhan City(200910321092)the Youth Science Plan for Light of the Morning Sun of Wuhan City (200750731270)
文摘The effects of microwave sintering and conventional H2 sintering on the microstructure and properties of W-15Cu alloy using ultrafine W-15Cu composite powder fabricated by spray drying & calcining-continuous reduction technology were investigated. In comparison to the conventional HE sintering processing, microwave sintering to W-15Cu can be achieved at lower sintering temperature and shorter sintering time. Furthermore, higher performances in microwave sintered compacts were obtained, but high microwave sintering temperature or long microwave sintering time could result in coarser microstructures.