In-situ TiB2 particles reinforced ZA27 composite was prepared by the stir-casting technique and a two-step method. TiB2/Al composite was produced by incorporating K2TiF6, KBF4 salts and other agents into Al melt. As a...In-situ TiB2 particles reinforced ZA27 composite was prepared by the stir-casting technique and a two-step method. TiB2/Al composite was produced by incorporating K2TiF6, KBF4 salts and other agents into Al melt. As a master alloy, TiB2/Al composite was used to manufacture TiB2/ZA27 composite, which results in the generation of well-distributed reinforcing TiB2 phase. The hardness, friction and wear behavior of TiB2/ZA27 composite were investigated. The results show that the hardness of the composite is enhanced with increasing the content of TiB2 particles, the incorporation of TiB2 reduces the wear rate of TiB2/ZA27 composite and improves the friction property under lubricated and dry sliding friction conditions. The worn track width of ZA27 alloy is 1.6 and 2.5 times as long as that of (2.1%)TiB2/ZA27 composite at 150N and 700N load under lubricated conditions, which indicates that TiB2/ZA27 composite possesses higher bearing ability.展开更多
文摘In-situ TiB2 particles reinforced ZA27 composite was prepared by the stir-casting technique and a two-step method. TiB2/Al composite was produced by incorporating K2TiF6, KBF4 salts and other agents into Al melt. As a master alloy, TiB2/Al composite was used to manufacture TiB2/ZA27 composite, which results in the generation of well-distributed reinforcing TiB2 phase. The hardness, friction and wear behavior of TiB2/ZA27 composite were investigated. The results show that the hardness of the composite is enhanced with increasing the content of TiB2 particles, the incorporation of TiB2 reduces the wear rate of TiB2/ZA27 composite and improves the friction property under lubricated and dry sliding friction conditions. The worn track width of ZA27 alloy is 1.6 and 2.5 times as long as that of (2.1%)TiB2/ZA27 composite at 150N and 700N load under lubricated conditions, which indicates that TiB2/ZA27 composite possesses higher bearing ability.