利用X射线衍射(XRD)及差热分析(DSC)等方法研究了添加B对Zr Ti Cu Ni Be块状非晶合金的形成、结晶及热稳定性的影响·结果表明:在Zr Ti Cu Ni Be合金系中添加B可明显改变该合金的玻璃转变温度Tg,一次结晶温度Tx及过冷液相区ΔT等参...利用X射线衍射(XRD)及差热分析(DSC)等方法研究了添加B对Zr Ti Cu Ni Be块状非晶合金的形成、结晶及热稳定性的影响·结果表明:在Zr Ti Cu Ni Be合金系中添加B可明显改变该合金的玻璃转变温度Tg,一次结晶温度Tx及过冷液相区ΔT等参数·当y(B)≤3%时,B的添加可使合金保持块状非晶,提高Tg、Tx并扩大过冷液相区,使非晶热稳定性增加;当y(B)≥6%时,B的添加将诱导大量的粗大Zr2Cu及ZrB2等晶体的析出·由于它们非纳米晶,尺寸较大,形状不规整,不能作为非晶复合材料的增强体·展开更多
The structures of the bulk amorphous Zr41Ti14Cu12.5Nil0.0Be22.5 alloy have been analyzed in solid, supercooled liquid and liquid with X-ray diffraction. The first coordination sphere radii and the first coordination n...The structures of the bulk amorphous Zr41Ti14Cu12.5Nil0.0Be22.5 alloy have been analyzed in solid, supercooled liquid and liquid with X-ray diffraction. The first coordination sphere radii and the first coordination numbers are 0.312 um, 11.2 in solid state.10.932 nm, 10.932 in supercooled liquid region and 0.305 urn, 11.296 in liquid state. The structures are the same in different states. But it shows some tendency to crystallizing that the first coordination sphere radius and the first coordination number drop in supercooled liquid region.展开更多
文摘利用X射线衍射(XRD)及差热分析(DSC)等方法研究了添加B对Zr Ti Cu Ni Be块状非晶合金的形成、结晶及热稳定性的影响·结果表明:在Zr Ti Cu Ni Be合金系中添加B可明显改变该合金的玻璃转变温度Tg,一次结晶温度Tx及过冷液相区ΔT等参数·当y(B)≤3%时,B的添加可使合金保持块状非晶,提高Tg、Tx并扩大过冷液相区,使非晶热稳定性增加;当y(B)≥6%时,B的添加将诱导大量的粗大Zr2Cu及ZrB2等晶体的析出·由于它们非纳米晶,尺寸较大,形状不规整,不能作为非晶复合材料的增强体·
文摘The structures of the bulk amorphous Zr41Ti14Cu12.5Nil0.0Be22.5 alloy have been analyzed in solid, supercooled liquid and liquid with X-ray diffraction. The first coordination sphere radii and the first coordination numbers are 0.312 um, 11.2 in solid state.10.932 nm, 10.932 in supercooled liquid region and 0.305 urn, 11.296 in liquid state. The structures are the same in different states. But it shows some tendency to crystallizing that the first coordination sphere radius and the first coordination number drop in supercooled liquid region.