This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid produ...This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid production carried out simultaneously because the auxiliary agents can be oxidized by bacteria and the oxidation products involve acid. The acid required for dissolving alkaline gangue during bacterial leaching is produced, and acid equilibrium is reached during the ore bio-leaching. The recovery of copper reaches more than 95%.展开更多
A series of alkaline earth sulfides based phosphors Ca_ 0.8 Sr_ 0.2 S∶Eu 2+ ,Tm 3+ were covered with a layer of protective coating with alkaline earth fluorides by heating the mixture of phosphor and NH_4HF_2...A series of alkaline earth sulfides based phosphors Ca_ 0.8 Sr_ 0.2 S∶Eu 2+ ,Tm 3+ were covered with a layer of protective coating with alkaline earth fluorides by heating the mixture of phosphor and NH_4HF_2 at elevated temperatures. The coatings were characterized by means of XRD and SEM. The optical properties of the coated phosphors and the influences of the coating on their properties have been discussed extensively. The stabilities of the coated and uncoated phosphors have been compared.展开更多
文摘This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid production carried out simultaneously because the auxiliary agents can be oxidized by bacteria and the oxidation products involve acid. The acid required for dissolving alkaline gangue during bacterial leaching is produced, and acid equilibrium is reached during the ore bio-leaching. The recovery of copper reaches more than 95%.
文摘A series of alkaline earth sulfides based phosphors Ca_ 0.8 Sr_ 0.2 S∶Eu 2+ ,Tm 3+ were covered with a layer of protective coating with alkaline earth fluorides by heating the mixture of phosphor and NH_4HF_2 at elevated temperatures. The coatings were characterized by means of XRD and SEM. The optical properties of the coated phosphors and the influences of the coating on their properties have been discussed extensively. The stabilities of the coated and uncoated phosphors have been compared.